JPS6343242A - Color picture tube - Google Patents

Color picture tube

Info

Publication number
JPS6343242A
JPS6343242A JP18554286A JP18554286A JPS6343242A JP S6343242 A JPS6343242 A JP S6343242A JP 18554286 A JP18554286 A JP 18554286A JP 18554286 A JP18554286 A JP 18554286A JP S6343242 A JPS6343242 A JP S6343242A
Authority
JP
Japan
Prior art keywords
shadow mask
frame
spring
thermal expansion
metal piece
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP18554286A
Other languages
Japanese (ja)
Inventor
Nobumitsu Aihara
伸光 相原
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NEC Corp
Original Assignee
NEC Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NEC Corp filed Critical NEC Corp
Priority to JP18554286A priority Critical patent/JPS6343242A/en
Publication of JPS6343242A publication Critical patent/JPS6343242A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To increase the strength of a shadow mask structure, by fixing a shadow mask comprising a low temperature expansion material with a frame comprising a high temperature expansion member through a spring-shaped metal piece to increase a number of welding points. CONSTITUTION:A shadow mask 11 comprising a low temperature expansion member is welded to a spring-shaped metal piece 13 at a welding point 14-a. Then, the shadow mask 11 is fixed at a prescribed position and the spring- shaped metal piece 13 is welded to a frame 12 at a welding point 14-b. With the arrangement, the deformation of the mask 11 caused by the thermal expansion of the frame 12 is adsorbed byre spring-shaped metal piece 13.

Description

【発明の詳細な説明】 〔産業上の利用分野〕 本発明は、シャドウマスク型カラー受像管、特にそのシ
ャドウマスク構体に関するものである。
DETAILED DESCRIPTION OF THE INVENTION [Field of Industrial Application] The present invention relates to a shadow mask type color picture tube, and particularly to a shadow mask structure thereof.

〔従来の技術〕[Conventional technology]

−iにシャドウマスク構体は、スリット状もしくはドツ
ト状に電子ビーム通過孔が設けられているシャドウマス
クと、このシャドウマスクのスカート部において固定し
たフレームと、このフレームをパネルに係合させるスプ
リングとからなっている。電子銃より発射された電子ビ
ームは、シャドウマスクを通過後けい光面に射突するこ
とにより所定のカラー画像を表示している。
-i The shadow mask structure consists of a shadow mask in which electron beam passage holes are provided in the form of slits or dots, a frame fixed at the skirt portion of this shadow mask, and a spring that engages this frame with the panel. It has become. An electron beam emitted from an electron gun passes through a shadow mask and hits a fluorescent surface to display a predetermined color image.

シャドウマスクの電子ビーム透過率は低く、その大部分
(約80〜85%)はシャドウマスクに射突して熱とな
るため、シャドウマスクは熱膨張を生じ、その結果とし
て電子ビームのミスランディングとなり色純度が劣化す
る。これを一般にドーミングと称している。一方、フレ
ームにもシャドウマスク同様に電子ビームが射突するこ
とにより熱膨張が生じるが、シャドウマスクに比べてフ
レームはその熱容量が大きいため、先のドーミングに比
べ緩やかな変化である。これもやはりカラー受像管の色
純度を劣化させる一因となっている。
The electron beam transmittance of the shadow mask is low, and most of it (approximately 80 to 85%) hits the shadow mask and becomes heat, causing thermal expansion of the shadow mask, resulting in mislanding of the electron beam. Color purity deteriorates. This is generally called doming. On the other hand, similar to the shadow mask, thermal expansion occurs in the frame due to the impact of the electron beam, but since the frame has a larger heat capacity than the shadow mask, the change is more gradual than in the previous doming. This is also a factor in degrading the color purity of the color picture tube.

この色純度の劣化を抑えるために、F、−N。In order to suppress this deterioration of color purity, F, -N.

合金、co−Fe合金といった低熱膨張材をシャドウマ
スク構体に使用したものが実用化されている。シャドウ
マスクに低熱膨張材を用いれば、ドーミングによるミス
ランディングを軽減でき、その効果は、パネルの曲率半
径が1000mmを越えるようなフラットフェース管に
おいては顕著である。−例として12型90°フラツト
フエース管において、低熱膨張材によるシャドウマスク
は、従来の鉄を主成分とした例えばアルミキルト低炭素
鋼に比べて電子ビームの最大ランディング移動量を11
5以下に抑えちれている。但しこの値は、水平軸上中間
部(中央から70 m+a )での移動量である。
Shadow mask structures using low thermal expansion materials such as alloys and co-Fe alloys have been put into practical use. If a low thermal expansion material is used for the shadow mask, mislanding due to doming can be reduced, and this effect is remarkable in flat-face tubes in which the radius of curvature of the panel exceeds 1000 mm. - For example, in a 12-inch 90° flat-face tube, the shadow mask made of a low thermal expansion material reduces the maximum landing movement of the electron beam by 11% compared to conventional iron-based materials such as aluminum quilted low carbon steel.
It has been kept below 5. However, this value is the amount of movement at the middle part on the horizontal axis (70 m+a from the center).

低熱膨張材は高価であるため、シャドウマスク、フレー
ム共に低=m張材を用いることはカラー受像管のコスト
アップとなり、また溶接性などの問題により量産化が容
易でない。そのため、フレームは通常の純鉄とし、シャ
ドウマスクのみを低膨張材としたシャドウマスク構体が
使用されている。このシャドウマスク構体は、シャドウ
マスクとフレームの7145’5張係数が0〜100℃
において約1桁異なっている。そのため、従来の鉄を主
成分としたシャドウマスク同様にフレームとの溶接点を
多数取ると、カラー受像管の製造工程における封着や排
気の炉を通した際やカラー受像管をオーバースキャンで
動作した際その熱膨張量の差によりシャドウマスクはス
カート部の溶接点においてフレームに引張られることに
なり部分的変形が生じる。この現象はシャドウマスクの
周縁部において顕著であり、電子ビームのミスランディ
ングとなって色純度を劣化させる。そのなめこれまでは
、シャドウマスクとフレームの溶接点を例えば水平、垂
直、対角の各軸上のみとする様にその数を減らして対処
していた。
Since low thermal expansion materials are expensive, using low-m tensile materials for both the shadow mask and the frame increases the cost of the color picture tube, and mass production is not easy due to problems such as weldability. Therefore, a shadow mask structure is used in which the frame is made of ordinary pure iron and only the shadow mask is made of a low-expansion material. This shadow mask structure has a 7145'5 tensile coefficient of 0 to 100℃ between the shadow mask and the frame.
There is a difference of about one order of magnitude. Therefore, if there are many welding points with the frame, as with conventional iron-based shadow masks, it will not work when the color picture tube is sealed or passed through an exhaust furnace in the manufacturing process, or when the color picture tube is overscanned. When this occurs, the shadow mask is pulled by the frame at the welding point of the skirt portion due to the difference in the amount of thermal expansion, resulting in partial deformation. This phenomenon is noticeable at the periphery of the shadow mask, resulting in mislanding of the electron beam and degrading color purity. Up until now, this has been dealt with by reducing the number of welding points between the shadow mask and the frame, such as only on the horizontal, vertical, and diagonal axes.

〔発明が解決しようとする問題点〕[Problem that the invention seeks to solve]

上述したようにシャドウマスクとフレームの溶接点を減
らすことで熱膨張量の差によるシャドウマスクの部分的
変形は抑えることができる。しかしながら溶接点を減ら
すことは耐振強度が弱くなり、シャドウマスク構体とし
ての機械的強度も弱くなる。そのためカラー受像管の製
造において熱以外の外力によるシャドウマスクの部分的
変形が生じ易く、またカラー受像管となった後も外部か
らの衝撃や振動による画面のゆれが著しいという問題点
があった。
As described above, by reducing the number of welding points between the shadow mask and the frame, partial deformation of the shadow mask due to differences in thermal expansion can be suppressed. However, reducing the number of welding points weakens the vibration resistance and also weakens the mechanical strength of the shadow mask structure. Therefore, in the manufacture of color picture tubes, partial deformation of the shadow mask is likely to occur due to external forces other than heat, and even after the color picture tube is manufactured, there is a problem in that the screen shakes significantly due to external shocks and vibrations.

〔問題点を解決するための手段〕[Means for solving problems]

本発明のカラー受像管は、シャドウマスクとフレームの
固定点において、シャドウマスクとフレームの熱膨張量
の差を吸収するためにバネ状の金属片を介したシャドウ
マスク構体を有している。
The color picture tube of the present invention has a shadow mask structure with a spring-like metal piece interposed at a fixed point between the shadow mask and the frame to absorb the difference in thermal expansion between the shadow mask and the frame.

〔実施例〕〔Example〕

本発明について図面を参照して説明する。第1図は、本
発明の1実施例を示しており、低熱膨張材からなるシャ
ドウマスク11と高熱膨張材からなるフレーム12の固
定を断面N字状の金属片13を介して行なったシャドウ
マスク構体の断面図である。
The present invention will be explained with reference to the drawings. FIG. 1 shows one embodiment of the present invention, in which a shadow mask 11 made of a low thermal expansion material and a frame 12 made of a high thermal expansion material are fixed via a metal piece 13 having an N-shaped cross section. FIG. 3 is a cross-sectional view of the structure.

シャドウマスク11とバネ状金属片13を溶接点14−
aにおいて溶接した後パネルとシャドウマスク構体が所
定の間隔となるような治具を用いてフレーム12にシャ
ドウマスク11とバネ状金属片13からなるものを溶接
点14−bにおいて溶接する。バネ状金属片の材料とし
ては、たとえばステンレスなどを用いることができる。
Weld the shadow mask 11 and the spring-like metal piece 13 at a welding point 14-
After welding in step a, the shadow mask 11 and the spring-like metal piece 13 are welded to the frame 12 at a welding point 14-b using a jig that allows the panel and shadow mask structure to be spaced at a predetermined distance. As the material of the spring-like metal piece, for example, stainless steel or the like can be used.

第2図(a)、(b)、(c)は本発明の他の実施例を
示すものであり、バネ状の金属片として断面V字型のも
の(a>、(c)およびL字型のもの(c)を使用した
場合を示している。これらバネ状金属片の形状は、フレ
ーム12の熱膨張によりシャドウマスク11が引張られ
るのを吸収するように働くものであれば、任意である。
Figures 2 (a), (b), and (c) show other embodiments of the present invention, in which the spring-like metal pieces are V-shaped in cross section (a>, (c) and L-shaped). The shape of these spring-like metal pieces can be arbitrary as long as it works to absorb the stretching of the shadow mask 11 due to thermal expansion of the frame 12. be.

〔発明の効果〕〔Effect of the invention〕

以上説明したように、本発明はシャドウマスクとして低
熱膨張材、フレームとしてシャドウマスクより熱膨張係
数の大きい材料からなるシャドウマスク構体において、
シャドウマスクとフレームの固定をその熱膨張量の差を
吸収するようなバネ状の金属片を介して行なっている。
As explained above, the present invention provides a shadow mask structure in which the shadow mask is made of a low thermal expansion material and the frame is made of a material with a larger coefficient of thermal expansion than the shadow mask.
The shadow mask and frame are fixed via a spring-like metal piece that absorbs the difference in thermal expansion.

従って、熱膨張によりシャドウマスクがフレームに引張
られることがないため、溶接点を増やすことができ、シ
ャドウマスク構体の強度を強くできる。また、シャドウ
マスクのスカート部が比較的自由であるため、管軸方向
の衝撃によるシャドウマスクの変形が生じ難く、外部か
らの振動もシャドウマスクに伝わり難いという効果があ
る。
Therefore, since the shadow mask is not pulled by the frame due to thermal expansion, the number of welding points can be increased and the strength of the shadow mask structure can be increased. Furthermore, since the skirt portion of the shadow mask is relatively free, deformation of the shadow mask due to impact in the tube axis direction is less likely to occur, and external vibrations are also less likely to be transmitted to the shadow mask.

【図面の簡単な説明】[Brief explanation of the drawing]

第1図及び第2図(a>、(b)、(c)は本発明の実
施例であり、共にシャドウマスク構体の要部断面図であ
る。 11・・・シャドウマスク、12・・・フレーム、13
゜2]、22.23・・・バネ状金属片。 茶 / 図 (a+              (J−ン    
        (c)井 2I¥]
1 and 2 (a>, (b), and (c) are embodiments of the present invention, and both are sectional views of essential parts of the shadow mask structure. 11...Shadow mask, 12... frame, 13
゜2], 22.23... Spring-shaped metal piece. Brown / Figure (a+ (J-n)
(c) I 2I ¥]

Claims (1)

【特許請求の範囲】[Claims] 低熱膨張材からなるシャドウマスクと、該シヤドウマス
クより熱膨張係数の大きい材料からなるフレームによっ
て構成されるシャドウマスク構体を有するカラー受像管
において、前記シャドウマスクと前記フレームの固定が
バネ状の金属片を介して行なわれていることを特徴とす
るカラー受像管。
In a color picture tube having a shadow mask structure constituted by a shadow mask made of a low thermal expansion material and a frame made of a material having a larger coefficient of thermal expansion than the shadow mask, the shadow mask and the frame are fixed using a spring-like metal piece. A color picture tube characterized by the fact that
JP18554286A 1986-08-06 1986-08-06 Color picture tube Pending JPS6343242A (en)