JPS62190114A - Method for filling and solidification of cosmetic and apparatus therefor - Google Patents

Method for filling and solidification of cosmetic and apparatus therefor

Info

Publication number
JPS62190114A
JPS62190114A JP3068986A JP3068986A JPS62190114A JP S62190114 A JPS62190114 A JP S62190114A JP 3068986 A JP3068986 A JP 3068986A JP 3068986 A JP3068986 A JP 3068986A JP S62190114 A JPS62190114 A JP S62190114A
Authority
JP
Japan
Prior art keywords
container
cosmetic
solvent
bottom plate
porous absorbent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP3068986A
Other languages
Japanese (ja)
Inventor
Yoshiharu Hatakeyama
畠山 喜治
Mitsuo Ishiguro
石黒 光雄
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
YKK Corp
Original Assignee
YKK Corp
Yoshida Kogyo KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by YKK Corp, Yoshida Kogyo KK filed Critical YKK Corp
Priority to JP3068986A priority Critical patent/JPS62190114A/en
Priority to US07/013,423 priority patent/US4817686A/en
Priority to FR878701941A priority patent/FR2594409B1/en
Publication of JPS62190114A publication Critical patent/JPS62190114A/en
Priority to US07/239,745 priority patent/US4884601A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To carry out filling and solidification of a viscous cosmetic, by placing a water-absorbing membrane on a bottom plate of an inner cavity of a compact, etc., and using a porous absorbent as a lower mold. CONSTITUTION:A proper amount of a viscous cosmetic 1 dissolved with a solvent is filled in a dish-shaped vessel 12 from above. The vessel 12 has opened top and is furnished with an air-permeable bottom plate 14 having water- absorbing membrane 19 and vertically movable in an outer frame 13 constituting circumferential wall. An upper mold is pressed against the top edge of the circumferential wall of the vessel 12. The cosmetic 1 in the vessel 12 is pressed by pushing up the bottom plate 14 of the vessel 12 with a porous absorbent 29 attached to a lower mold 27. The solvent in the cosmetic 1 is absorbed through the absorptive membrane 19 and the porous absorbent 29 by the pressing step. The cosmetic can be filled and solidified by this process. EFFECT:There is little cosmetic loss such as leakage. The solvent in the viscous cosmetic can be easily squeezed out and the solvent is easily absorbed. Accordingly, the solidification of the cosmetic completes in a short time.

Description

【発明の詳細な説明】 (産業上の利用分野) この発明はコンパクトの中皿などの容器に粘性化粧料を
充填して固化づる方法及びiaに関するものである。
DETAILED DESCRIPTION OF THE INVENTION (Field of Industrial Application) The present invention relates to a method and ia for filling a container such as a compact inner plate with a viscous cosmetic and solidifying the same.

(従来の技術) 従来コンバク1〜の容器に化粧料を充填固化する方法及
び装置の1つとして、圧力注入充填方式を採用した特公
昭57−60004号公報に開示された技術がある。こ
れは溶剤で溶かして粘性化した化粧料をノズルを通して
コンパクトの中1111などに圧力注入充填すると同時
に、吸収体を通して溶剤を吸収して化II料を固化させ
るものである。
(Prior Art) As one of the conventional methods and devices for filling and solidifying cosmetics into containers, there is a technique disclosed in Japanese Patent Publication No. 57-60004 that employs a pressure injection filling method. In this method, a cosmetic material that has been dissolved and made viscous with a solvent is pressure-injected into a compact such as 1111 through a nozzle, and at the same time, the solvent is absorbed through an absorber to solidify the compound II material.

この方式では溶剤を用いずに粘着材を添加した粉末状化
粧料を金属器に収容しプレス圧縮することによって固化
する方法や、溶剤で溶がした化粧料を金属器などに流し
込んだ後乾燥により溶剤を蒸発させて固化する方法に比
べ、作業性及び充填後の外観が向上するなどの利点を有
Jる。
In this method, powdered cosmetics with an adhesive added are placed in a metal container and solidified by press compression without using a solvent, or the cosmetics dissolved in a solvent are poured into a metal container and then dried. Compared to the method of solidifying by evaporating the solvent, it has advantages such as improved workability and improved appearance after filling.

具体的には特公昭57−6000’l@の方法及び装δ
は次のようになっている。底部に充填孔を有する受皿を
受は冶具上の凹所にセットする。次いで、受は冶具側の
射出ノズルが受■1の充填孔に圧着されるとともに受皿
の上面開口部を網布を介して多孔質吸収体で圧接する。
Specifically, the method and equipment δ of Special Publick Publication No. 57-6000
is as follows. A saucer with a filling hole at the bottom is set in a recess on the jig. Next, the injection nozzle on the jig side of the receiver is pressed into the filling hole of receiver 1, and the upper opening of the receiver is pressed with the porous absorbent material through the mesh cloth.

この状態で射出ノズルから受皿内に粘性化Itl′!l
を圧力注入充wAする。
In this state, it becomes viscous from the injection nozzle into the saucer! l
Pressure injection is performed.

圧ノコ注入充填後、化粧料中の溶剤は上記網布から上記
多孔質吸収体に吸収される。更に吸収された溶剤の減少
分は射出ノズルからオーバーパックされる。
After pressure saw injection and filling, the solvent in the cosmetic is absorbed into the porous absorbent body through the mesh cloth. Further absorbed solvent loss is overpacked from the injection nozzle.

(発明が解決しようとする問題点) しかし、上述の従来技術においては射出ノズルを通して
圧力注入充填するため、受皿内の粘性化粧料が射出ノズ
ル内の粘性化粧料と常に連通していな【ブればならない
。従って、この状態で受刑内の粘性化粧料の溶剤を吸収
しても常に射出ノズル内の粘性化粧料から溶剤が補給さ
れることとなり、吸収効果が悪く(射出圧力4〜6kg
7cd及び充填時間5〜10秒で溶剤の60〜70%を
吸水し固化完了する)、残存する溶剤は自然蒸発を期待
しな1ブればならなかった。この自然蒸発の際には化粧
料にひび割れなどが発生し、外観が悪くなるという欠点
があった。また、溶剤を吸収して化粧料を固化さゼる時
に受皿内の化粧料のみならず割出ノズル内の化粧料も固
化させることになり、ノズルが詰まったり、受皿内に注
入された化粧IIは粘性化粧II 、と固化化粧料とが
混在づるためその分布が不均一となったりするので、作
業性が恕いとともに固化後の化粧料表面の色調ムラや光
沢ムラが発生しゃ1かった。
(Problems to be Solved by the Invention) However, in the above-mentioned conventional technology, the viscous cosmetic in the tray is not always in communication with the viscous cosmetic in the injection nozzle because it is filled by pressure injection through the injection nozzle. Must be. Therefore, even if the solvent of the viscous cosmetic in the prison is absorbed in this state, the solvent will always be replenished from the viscous cosmetic in the injection nozzle, and the absorption effect will be poor (injection pressure of 4 to 6 kg).
7 cd and filling time of 5 to 10 seconds, 60 to 70% of the solvent was absorbed and solidification was completed), and the remaining solvent had to be evaporated without expecting natural evaporation. This natural evaporation has the disadvantage that cracks occur in the cosmetic, resulting in a poor appearance. In addition, when the cosmetic is absorbed by the solvent and solidified, not only the cosmetic in the saucer but also the cosmetic in the indexing nozzle will solidify, which may cause the nozzle to become clogged or cause the makeup poured into the saucer to solidify. Because the viscous cosmetic II and the solidified cosmetic are mixed together, the distribution becomes uneven, which impairs workability and prevents uneven color tone and gloss on the surface of the cosmetic after solidifying.

更に、溶剤を較り出ずために、この方式では高圧で割出
ノズルから受皿内に注入しなければならない。この注入
時、受皿の充填孔に位置または寸法誤差や変形があった
り、受皿の充填孔と創出ノズルとの位置合わせが不完全
であると、射出ノズルから高圧で注入される粘性化at
利が充填孔の外側に漏れ、化11料ロスとなるため化粧
料の歩留りが悪かった。
Furthermore, in order to prevent the solvent from leaking out, this system requires that it be injected into the pan through an indexing nozzle at high pressure. During this injection, if there is a positional or dimensional error or deformation in the filling hole of the saucer, or if the alignment between the filling hole of the saucer and the creation nozzle is incomplete, the viscosity of the injected at high pressure from the injection nozzle may increase.
The yield of cosmetics was poor because the oil leaked to the outside of the filling hole, resulting in a loss of chemical compound 11.

この発明は前述した従来の問題点に鑑みてなされたもの
で・あり、その目的は、容器内の粘性化粧料の溶剤の吸
収効果を高めることによって化It P+のひび割れや
色調ムラ、光沢ムラをなく覆とともに化粧料の歩留りが
良く、更に新規なコンパクト容器が提供でさる化粧料の
充填固化方法及び装置を提供することにある。
This invention was made in view of the above-mentioned conventional problems, and its purpose is to improve the absorption effect of the solvent of the viscous cosmetic in the container, thereby reducing cracks, uneven color tone, and uneven gloss of the viscous cosmetic. It is an object of the present invention to provide a method and apparatus for filling and solidifying cosmetics, which has a good yield of cosmetics and provides a novel compact container.

(問題点を解決するための手段) 上記の目的を達成づるため、この発明においては上面が
開[I L底面を構成する底板が通気性を付与されると
ともに吸水性膜材を有しかつ外周壁を構成する外枠内で
上下に移動可能とされたll1l状の容器を使用する。
(Means for Solving the Problems) In order to achieve the above object, in the present invention, the top surface is open [I A ll1l-shaped container is used that is movable up and down within the outer frame that constitutes the wall.

この容器内に溶剤で溶かして粘性化した化粧料を上面側
から適宜吊充f11る工程と、前記容器の外周壁上面に
上型を圧接する工程と、前記容器を収容づる下型に設け
た多孔質吸収体によって前記容器の底板を上方に押し上
げて内部の前記化粧料を圧縮Jる工程と、前記圧縮■稈
口)に前記吸水性膜材及び前記多孔質吸収体を通して前
記化粧料中の溶剤を吸収づる工程とからなるようにして
いる。
A step of appropriately suspending a cosmetic material dissolved in a solvent to make it viscous in this container from the upper surface side, a step of pressing an upper mold onto the upper surface of the outer circumferential wall of the container, and a step provided in a lower mold for accommodating the container. A step of compressing the cosmetic inside by pushing up the bottom plate of the container using a porous absorbent; The method consists of a step of absorbing a solvent.

また、第2発明の方法では、上記のように構成された容
器内に粘性化粧料を適宜伍充填づる工程と、前記容器の
上面側に吸水性Illを介在させてイの上から少なくと
も前記容器の上面開口部を覆う多孔質吸収体を右する上
型を前記容器の外周壁上面に圧接する工程と、前記容器
を収容する下型に設けた多孔質吸収体によって前記容器
の底板を上方に押し上げC内部の前記化粧料を圧縮する
工程と、該圧縮工程時に前記容器の吸水性膜材と前記下
型に設【ノだ多孔質吸収体を通してまたは前記容器の上
面側に介在させた吸水性膜材と前記上型に設Gプだ多孔
質吸収体を通して、前記化粧料中の溶剤を吸収する■稈
とからなるようにしている。
The method of the second invention also includes a step of appropriately filling a viscous cosmetic into the container configured as described above, and interposing a water-absorbent Ill on the upper surface side of the container so as to cover at least the container. a step of press-contacting an upper mold that holds a porous absorbent body covering the upper surface opening to the upper surface of the outer peripheral wall of the container; and a step of pushing the bottom plate of the container upwardly by the porous absorbent body provided on the lower mold that accommodates the container. A step of compressing the cosmetic inside the push-up C, and a step of compressing the cosmetic material inside the push-up C, and at the time of the compression step, compressing the water-absorbing material through the water-absorbing membrane material of the container and the porous absorbent material provided in the lower mold or interposed on the upper surface side of the container. It consists of a membrane material and a culm that absorbs the solvent in the cosmetic through a porous absorbent material provided in the upper mold.

更に、上記の方法を実施するだめの第3光明の装置では
、上記のように構成された容器を位置決め載置丈るため
の四部と、該凹部の底に連続して形成された真空吸引用
流通路と、前記容器を多孔質吸収体で上方に押し上げる
加圧手段とを右りる下型と、前記加圧手段に連結されて
該加圧手段を上下動させるだめの駆動機構と、前記下型
上の前記容器の外周壁上面に圧接可能に上下動させるだ
の駆動機構を有する上型とから構成されている。
Furthermore, the third light device for carrying out the above method has four parts for positioning and mounting the container configured as described above, and a vacuum suction part formed continuously at the bottom of the recess. a lower mold that holds a flow path, a pressurizing means for pushing the container upward with a porous absorbent body, a drive mechanism connected to the pressurizing means to move the pressurizing means up and down; The upper mold has a drive mechanism for vertically moving the mold so as to be able to press against the upper surface of the outer peripheral wall of the container on the lower mold.

(実 施 例) 以下に本発明の好適な実施例について添Fl!!図面を
参照して説明する。
(Examples) Below are attached Fl! preferred examples of the present invention. ! This will be explained with reference to the drawings.

第1図は容器に適宜毎の粘性化粧料を充填する工程を示
している。溶剤で溶かして粘性化した化粧料1(以下粘
性化粧料1という)は、撹拌槽2に蓄えられバルブ3が
閉じた状態で撹拌棒4によって粘性を均一にするため撹
拌される。撹拌された粘性化粧料1はバルブ3が開かれ
吐出口5の閉じられたバルブ6まで連通ずる。次いで、
エアシリンダ7のピストンロッド7aを進出させること
によって撹拌1ft2からの粘性化粧F11の流出を止
める。この状態で吐出口5のバルブ6を開ぎ、エアシリ
ンダ8のピストンロッド8aを進出させると配管9内の
一定聞の粘性化粧料1が吐出口5から容器12に吐出滴
下される。尚、吐出口5のバルブ6を閉じ、バルブ10
を開くことによって撹拌槽2の粘性化粧料1は配管11
を通って循環させ得るので粘性化粧料の粘性を更に均一
にすることができる。
FIG. 1 shows the process of filling containers with appropriate viscous cosmetics. Cosmetic composition 1 (hereinafter referred to as viscous cosmetic composition 1) dissolved in a solvent and made viscous is stored in a stirring tank 2 and stirred with a stirring rod 4 with a valve 3 closed to make the viscosity uniform. The stirred viscous cosmetic 1 communicates with the valve 3 which is opened and the valve 6 of the discharge port 5 which is closed. Then,
By advancing the piston rod 7a of the air cylinder 7, the outflow of the viscous makeup F11 from the stirring 1ft2 is stopped. In this state, when the valve 6 of the discharge port 5 is opened and the piston rod 8a of the air cylinder 8 is advanced, a certain amount of the viscous cosmetic 1 in the pipe 9 is discharged and dripped from the discharge port 5 into the container 12. Note that the valve 6 of the discharge port 5 is closed, and the valve 10 is closed.
By opening the viscous cosmetic 1 in the stirring tank 2, the piping 11
The viscosity of the viscous cosmetic can be made more uniform because the viscosity can be circulated through the viscous cosmetic material.

第2図は本発明で使用される、例えばコンパクトの中間
である容器の実施例を示すもので、第2図(a )は外
周壁を構成する外枠13と、底面を構成する底板14と
の2つの部材からなる容器12を示している。この底板
14は円形リング状部材15,16.17が同心状に配
置され、かつこれらは支持梁18によって一体的に連結
されるとともにその底面に絹布、s!布、不織布、吸取
Mなどの吸水性膜材19が接着されている。従って、底
板14は円形リング状部U15.16.17が同心状に
配置されることによって通気孔20を形成りるため通気
性が付与されている。
FIG. 2 shows an embodiment of a container used in the present invention, for example, an intermediate type of compact. FIG. 1 shows a container 12 consisting of two members. This bottom plate 14 has circular ring-shaped members 15, 16, and 17 arranged concentrically, and these are integrally connected by a support beam 18, and a silk cloth is attached to the bottom surface of the bottom plate. A water-absorbing membrane material 19 such as cloth, non-woven fabric, or absorbent material 19 is adhered. Therefore, the bottom plate 14 is provided with air permeability because the circular ring portions U15, 16, and 17 are arranged concentrically to form ventilation holes 20.

第2図(b)は142図(a )の底板14の底面に接
むされた吸水性膜材19を底板14′の上面に接おした
容器12を示している。
FIG. 2(b) shows the container 12 in which the water-absorbing membrane material 19, which is in contact with the bottom surface of the bottom plate 14 of FIG. 142(a), is in contact with the top surface of the bottom plate 14'.

第3図(C)は第2図(a )の底板14の円形リング
状部材17に一体的に傾斜を有するフランジ21を設け
た底板22を有(る容器12を示1もので、外枠13と
の嵌合係止状態では、底板22の下面は外枠13の下面
よりも−1・に位v!iする。
FIG. 3(C) shows a container 12 having a bottom plate 22 which is integrally provided with an inclined flange 21 on the circular ring-shaped member 17 of the bottom plate 14 in FIG. 2(a). 13, the lower surface of the bottom plate 22 is at a position v!i of −1· with respect to the lower surface of the outer frame 13.

即ち、底板22はフランジ21が形成されているため化
粧料を収容する収容部23を有している。
That is, since the bottom plate 22 is formed with the flange 21, it has a storage section 23 for storing cosmetics.

この収容8I+ 23は本発明の化粧料の充填固化時に
溶剤が吸収されて化粧料の容積収縮分を補うだけの空間
を有している。
This housing 8I+ 23 has a space sufficient to compensate for the volumetric shrinkage of the cosmetic by absorbing the solvent during filling and solidification of the cosmetic of the present invention.

第2図(d )に示づ容器12は、外枠13′が内周下
端に底板25を係止する鍔24を有し、底面を構成する
底板25が例えば多孔質プラスヂックヤ焼結金属、セラ
ミックなどの粉粒体で焼結して製造される通気性を有す
る多孔質吸収体26と、その上面に接着された吸水性膜
材19とから構成されている。尚、上記容器12がコン
バクl−の中皿として使用される場合、外枠13−の鍔
24を設けなくとも実施できるが、好ましくは外枠13
には優かの鍔24を設(プたほうが良い。
In the container 12 shown in FIG. 2(d), an outer frame 13' has a collar 24 for locking a bottom plate 25 at the lower end of the inner periphery, and the bottom plate 25 constituting the bottom surface is made of porous plastic, sintered metal, ceramic, etc. It is composed of a porous absorbent body 26 having air permeability manufactured by sintering powder or granules such as the like, and a water-absorbing membrane material 19 adhered to the upper surface of the porous absorbent body 26. Incidentally, when the container 12 is used as an inner plate of the container 1-, it can be implemented without providing the flange 24 of the outer frame 13-, but it is preferable that the outer frame 13- is not provided with the collar 24.
It is better to set up a tsuba of 24.

以上に示した容器の実施例は、いずれも上面が開口し底
面を構成する底板が通気性を付与されるとともに吸水性
膜11で上面または下面が覆われかつ外周壁を構成する
外枠内で上下に移動可能とされている。
In all of the above-mentioned container embodiments, the top surface is open, the bottom plate constituting the bottom surface is provided with breathability, the top surface or the bottom surface is covered with a water-absorbing film 11, and the container is located within the outer frame constituting the outer peripheral wall. It is said to be able to move up and down.

第3図は化粧料の固化方法及び本発明を実施1゛る装置
の第1実施例を示している。この実施例では第2図(C
)で示す容器12が使用されている。
FIG. 3 shows a first embodiment of a method for solidifying cosmetics and an apparatus for carrying out the present invention. In this example, Fig. 2 (C
) is used.

下型27は容器12の外形に対応した四部28を有し、
この凹部28に容器12が1■合装着される。四部28
の底の中心部から下面には更に焼結金属やセラミックな
どの粉粒体から製造された多孔質吸収体29を収容する
凹部30が形成されるとともに、この凹部30の中央部
下面は穿設されて凹部ご31が形成されている。この四
部31の中央部下面には上記多孔質吸収体19に上端が
ネジ留めされIご加圧ロッド32が挿入される挿入孔3
3が穿設されている。加圧ロツl532はOリング34
を有して外部の空気を吸込まないように気密性を保持し
ており、下端は例えばエアーシリンダ38に連結される
。また、上記凹81131と連通づる真空吸引流通路3
5が下型27に設けられており、接続金具36がこの真
空吸引流通路35にネジ込まれることによって図示しな
いが真空ポンプ37と連結され、下型27の凹部30を
真空に引けるように構成されている。
The lower mold 27 has four parts 28 corresponding to the outer shape of the container 12,
One container 12 is fitted into this recess 28. Part 4 28
A recess 30 is further formed on the lower surface from the center of the bottom to accommodate a porous absorbent 29 made of powder or granular material such as sintered metal or ceramic, and the central lower surface of this recess 30 is provided with a perforation. A recess 31 is formed. An insertion hole 3 in the central lower surface of the four parts 31 has an upper end screwed to the porous absorbent body 19 and into which a pressure rod 32 is inserted.
3 is drilled. Pressure rod l532 is O-ring 34
The lower end is connected to an air cylinder 38, for example. Also, the vacuum suction flow path 3 communicating with the recess 81131
5 is provided on the lower mold 27, and a connecting fitting 36 is screwed into this vacuum suction flow path 35 to be connected to a vacuum pump 37 (not shown), so that the recess 30 of the lower mold 27 can be evacuated. has been done.

上型39は少なくとも容器12の外枠13の」。The upper mold 39 covers at least the outer frame 13 of the container 12.

面を覆うブロックであって、上面にピストン0ツド40
を介してエアーシリンダ41と連結され上下に移動可能
となっている。
A block that covers the surface and has a piston 40 on the top surface.
It is connected to the air cylinder 41 via the air cylinder 41 and is movable up and down.

また、上型と下型との間にはローラ46及び巻取装置4
7によって間歇的に移送される吸取紙等の吸水性膜材4
8が介在されるように構成されている。
Further, a roller 46 and a winding device 4 are provided between the upper mold and the lower mold.
Water-absorbing membrane material 4 such as absorbent paper is intermittently transferred by 7.
8 is interposed.

下型27は例えばこれを把持する回転アームによって移
動されるようになっており、まず容612を凹部28に
セットし、次いで第1図に示づ粘性化粧料充填装置の吐
出口5の直下に位置させて一定量の粘性化粧料1を容器
12に滴下し充填でる。次に、下型27は容器12をセ
ットしたまま固化工程へ移動させ、上型39と組合され
る。
The lower mold 27 is moved by, for example, a rotary arm that grips it. First, the container 612 is set in the recess 28, and then the container 612 is placed directly below the discharge port 5 of the viscous cosmetic filling device shown in FIG. A predetermined amount of the viscous cosmetic 1 is dropped into the container 12 and filled. Next, the lower mold 27 is moved to a solidification process with the container 12 set therein, and is combined with the upper mold 39.

化粧料の固化方法について述べると、下型27にセット
され一定量の粘性化粧料を充填された容器12の上面に
吸水性膜材48を介在させ、外周壁上面に上型39をエ
アーシリンダ7111によって不時ざぜて圧接する。次
いで、下型側のエアーシリンダ38を介して加圧ロッド
32を上方に押し上げると加圧ロンドにネジ込まれた多
孔質吸収体29が容器12の底板22を上方に押し上げ
、粘性化粧料1は上型との間で加圧圧縮される。この圧
縮時に下型の真空吸引流通路を介して真空ポンプ37に
より下型内を真空に引く。
Regarding the method of solidifying the cosmetic, a water-absorbing membrane material 48 is interposed on the upper surface of the container 12 set in the lower mold 27 and filled with a certain amount of viscous cosmetic, and the upper mold 39 is placed on the upper surface of the outer peripheral wall of the container 12 using an air cylinder 7111. Pressure is applied inadvertently. Next, when the pressure rod 32 is pushed upward via the air cylinder 38 on the lower mold side, the porous absorber 29 screwed into the pressure rod pushes the bottom plate 22 of the container 12 upward, and the viscous cosmetic 1 is It is compressed under pressure between it and the upper mold. During this compression, the inside of the lower mold is evacuated by the vacuum pump 37 via the vacuum suction flow path of the lower mold.

この方法によれば、粘性化粧料1は通気孔20を有しか
つ吸水性膜材19が接着された容器12の底板22及び
多孔質吸収体29によって圧縮されるので、溶剤が絞り
出されや1く較り出された溶剤は直ぐに吸水性膜材19
による毛細管現象によって吸収され、更に多孔質吸収体
29を介して真空吸引されるので溶剤の吸収効果が増幅
されて速やかに吸収され固化が完了する。
According to this method, the viscous cosmetic 1 is compressed by the porous absorbent body 29 and the bottom plate 22 of the container 12 which has ventilation holes 20 and has the water-absorbent membrane material 19 adhered thereto, so that the solvent is not squeezed out. The solvent drawn out in step 1 is immediately added to the water-absorbing membrane material 19.
The solvent is absorbed by the capillary phenomenon, and is further vacuumed through the porous absorbent body 29, so the absorption effect of the solvent is amplified, and the solvent is quickly absorbed and solidification is completed.

従って、圧縮時の加圧圧力は射出ノズルによる圧力注入
充填方法よりも低くてよく、かつ残存する溶剤も固化化
粧斜向には殆ど存在しない。
Therefore, the pressurizing pressure during compression may be lower than that in the pressure injection filling method using an injection nozzle, and almost no residual solvent is present in the solidified makeup layer.

これで本発明の化粧料の固化工程の終了であり、加圧ロ
ッド32を下°陪させるとともに上型39を上昇さUて
容器12を下型27から取り出す。
This is the end of the solidifying process for the cosmetic of the present invention, and the pressure rod 32 is lowered and the upper mold 39 is raised to remove the container 12 from the lower mold 27.

筒、容器12の上面に介在した吸水性膜材48の目的は
、容器12内の粘性化粧料を加圧圧縮する際に外周壁上
面より遺漏しないためのバッキング効果と、圧縮成形さ
れた固形化粧料が上型下面に付着しないための離型組と
なるとともに化粧料の表面との1lllをを吸水状態で
良好にする効果がある。
The purpose of the water-absorbing membrane material 48 interposed on the upper surface of the tube or container 12 is to provide a backing effect to prevent leakage from the upper surface of the outer peripheral wall when the viscous cosmetic in the container 12 is compressed under pressure, and to provide a backing effect to prevent the viscous cosmetic material in the container 12 from leaking from the upper surface of the outer peripheral wall, and to prevent the solid cosmetic material that has been compression-molded from leaking. It serves as a mold release agent to prevent the cosmetic from adhering to the lower surface of the upper mold, and also has the effect of improving the water absorption state between the surface of the cosmetic and the surface of the cosmetic.

第4図は本発明の第2実施例を示ず化粧料の固化方法及
び装置であって、下型27及び容器12の構成は第3図
に示づ第1実施例と同じであるので説明は省略する。
FIG. 4 does not show the second embodiment of the present invention, but shows a method and apparatus for solidifying cosmetics, and the structure of the lower mold 27 and container 12 is the same as the first embodiment shown in FIG. 3, so it will be explained. is omitted.

第2実施例における上型39′は、例えば焼結金属やゼ
ラミックなどの粉粒体を焼結して得られる多孔質吸収体
42を嵌合して止めボルト43によって固定することに
よって形成される凹部44を有し、多孔質吸収体42は
上記凹部の前面より僅かに突出し容器12の開口部内を
覆うようにされている。更に、上型39−は凹部44の
中心部から連通された真空流通路45を右し、接続金具
36を介して吸引装置である真空ポンプ37に連結され
るとともにピストンロンド40を介してエアーシリンダ
41ど連結され上下に移動可能とされている。
The upper mold 39' in the second embodiment is formed by fitting a porous absorbent body 42 obtained by sintering a powder material such as sintered metal or ceramic material and fixing it with a fixing bolt 43. It has a recess 44, and the porous absorbent body 42 slightly protrudes from the front surface of the recess to cover the inside of the opening of the container 12. Further, the upper die 39- is connected to a vacuum flow path 45 communicating from the center of the recess 44, and is connected to a vacuum pump 37, which is a suction device, via a connecting fitting 36, and is also connected to an air cylinder via a piston rod 40. 41 are connected and can be moved up and down.

また、上型と下y(どの聞にはローラ46及び巻取装置
47によって間歇的に移送される吸取紙などの吸水性I
Q材48が介入されるように構成されている。
In addition, between the upper die and the lower die (where between the upper die and the lower die, a water-absorbing material such as absorbent paper, etc., which is intermittently transferred by the roller 46 and the winding device 47)
Q material 48 is configured to intervene.

化粧料の固化方法について述べると、下型27上にセッ
トされた容器12の上面に吸水性膜4i1/18を介入
させ、次いでエアーシリンダ41によって上型39′を
下降ざして容器12の外周壁上面に上型39′を圧接ダ
る。このとき上型の多孔質吸収体42は容器の間口部内
に嵌入されて僅かながら粘性化粧料1を圧縮し、吸水性
膜材48を介して溶剤が吸収される。更に下型側から多
孔質吸収体29を上昇させて容器の底板22を押し」−
げ粘性化粧料を加圧圧縮する。同時に、下型及び十yν
の真空吸引流通路35.45を介して真空ポンプ37に
より下型内及び上型内を真空に引く。
Regarding the method of solidifying cosmetics, the water-absorbing film 4i1/18 is interposed on the upper surface of the container 12 set on the lower mold 27, and then the upper mold 39' is lowered by the air cylinder 41 to cover the outer peripheral wall of the container 12. An upper die 39' is pressed onto the upper surface. At this time, the upper mold porous absorbent body 42 is fitted into the opening of the container and slightly compresses the viscous cosmetic 1, and the solvent is absorbed through the water-absorbing membrane material 48. Furthermore, raise the porous absorber 29 from the lower mold side and press the bottom plate 22 of the container.
Compress viscous cosmetics under pressure. At the same time, the lower mold and
The inside of the lower mold and the upper mold are evacuated by the vacuum pump 37 through the vacuum suction flow passages 35 and 45.

この方法によれば、粘性化粧料1は底板22及び下型側
の多孔質吸収体29によって圧縮されるので溶剤が絞り
出され易く、かつ絞り出された溶剤は底板22の吸水性
膜材19及び下型側の多孔質吸収体29を介して直ぐに
真空吸引されるとともに、容器の上面側からも吸水性膜
材48及び上型の多孔質吸収体42を介して絞り出され
た溶剤が真空吸引されるので、溶剤の吸収効果が高く速
やかに固化が完了する。
According to this method, the viscous cosmetic 1 is compressed by the bottom plate 22 and the porous absorbent body 29 on the lower mold side, so that the solvent is easily squeezed out, and the squeezed out solvent is transferred to the water-absorbing membrane material 19 of the bottom plate 22. The solvent is immediately vacuum-suctioned through the porous absorber 29 on the lower mold side, and the solvent is also squeezed out from the upper surface of the container through the water-absorbing membrane material 48 and the porous absorber 42 on the upper mold. Since it is suctioned, the solvent is highly effective in absorbing the solvent and solidification is completed quickly.

尚、この実施例において上型側及び下型側で同時に真空
吸引させて溶剤の吸収効果を速めているが、上型側また
は下型側のいずれか一方を真空吸引させて溶剤を吸収さ
せても良いことは勿論である。要は、通気性が付与され
かつ吸水性膜材を有する容器の底板と多孔質吸収体29
によって粘性化粧料1を圧縮゛することで、溶剤が絞り
出され易くしたことが本発明のポイントであり、この絞
り出された溶剤を吸水性Igluと多孔質吸収体を介し
て真空吸引ずれば速やかに固化が完了するのである。
In this example, the upper mold side and the lower mold side are simultaneously vacuum-suctioned to accelerate the absorption effect of the solvent, but either the upper mold side or the lower mold side is vacuum-suctioned to absorb the solvent. Of course, this is also a good thing. In short, the bottom plate of the container is provided with breathability and has a water-absorbing membrane material, and the porous absorbent body 29
The key point of the present invention is to make it easier to squeeze out the solvent by compressing the viscous cosmetic 1 with Solidification is completed quickly.

化粧料の固化が完了づると多孔質吸収体42によって圧
縮された分だけ化粧料の上面が収縮により下がるが、こ
の実施例による容器12は、第2図(C)に示ゴように
底板22の下面が外枠13の下端より下方に突出してい
て、この収縮分を補償する化粧料収容部23を有してい
るため、第5図(a )に示づようにコンパクト49に
容器12を収容したとぎ、コンパクトの底面により底板
22が押し上げられて化粧料の上面が外枠13の上面と
一致1Jる。また、底板4降式容器のメリットとして、
例えばコンパクト49の底面に小孔50を穿設すれば化
Il料が使用により減った場合でも、この小孔50を介
して底板22を押し上げることによってコンパクトの上
面で化粧r1を使用できるので使い勝手が良い。
When the solidification of the cosmetic is completed, the top surface of the cosmetic drops by the amount compressed by the porous absorbent body 42 due to contraction. The lower surface protrudes downward from the lower end of the outer frame 13, and has a cosmetic storage portion 23 that compensates for this shrinkage, so that the container 12 can be placed in the compact 49 as shown in FIG. 5(a). Once stored, the bottom plate 22 is pushed up by the bottom of the compact so that the top surface of the cosmetic is aligned with the top surface of the outer frame 13. In addition, as an advantage of the four-bottom type container,
For example, if a small hole 50 is formed in the bottom of the compact 49, even if the chloride content decreases due to use, the cosmetic r1 can be used on the top of the compact by pushing up the bottom plate 22 through the small hole 50, making it easier to use. good.

第5図(b >は底板51がフランジ52をイーi’7
する多孔質吸収体29と吸水性膜材19とで構成され、
外枠13が鍔24を有づる容器に本発明を適用した実施
例を示している。
Fig. 5 (b) indicates that the bottom plate 51 is attached to the flange 52
It is composed of a porous absorbent body 29 and a water-absorbing membrane material 19,
An embodiment in which the present invention is applied to a container in which the outer frame 13 has a flange 24 is shown.

(発明の効果) 上記のように構成した本発明によれば、溶剤で溶かした
粘性化粧料の適宜量を容器に滴下して充填するので、化
粧料の漏れやはみ出しなどがなく化粧料のロスがない。
(Effects of the Invention) According to the present invention configured as described above, an appropriate amount of viscous cosmetics dissolved in a solvent is dropped into a container and filled, so there is no leakage or overflow of the cosmetics, and there is no loss of cosmetics. There is no.

また、容器として上面が開口し底面を構成する底板が通
気性を付与されているとともに吸水性膜材を有しかつ外
周壁を構成する外枠内で上下に移動可能とされた皿状の
容器を使用しているので、この容器の底板を下型に設け
た多孔質吸収体で上すに押し上げて上型との間で容器に
収容された粘性化粧料を加圧圧縮することができるため
、粘性化粧料の溶剤が絞り出され易く、かつ絞り出され
た溶剤は吸水性膜材及び多孔質吸収体を介して直ぐに真
空吸引されるので溶剤の吸収効果が高く速やかに固化か
完了する。従って、粘性化粧料の圧縮部の加圧圧力は割
出ノズルによる圧力注入充填方式に比べて低くてよく、
かつ残存する溶剤も固化化粧料内には殆ど存在しないた
め化粧料のひび割れや色調ムラ、光沢ムラがないととも
に化粧料の歩留りが良い。
In addition, the container is a dish-shaped container that has an open top, a bottom plate that is breathable, has a water-absorbing membrane material, and is movable up and down within the outer frame that forms the outer peripheral wall. Since the bottom plate of this container is pushed up to the top by the porous absorbent material provided in the lower mold, the viscous cosmetic stored in the container can be compressed under pressure between it and the upper mold. The solvent of the viscous cosmetic is easily squeezed out, and the squeezed out solvent is immediately vacuum-sucked through the water-absorbing membrane material and the porous absorber, so the solvent absorption effect is high and solidification is completed quickly. Therefore, the pressurizing pressure of the viscous cosmetic compression section may be lower than that of the pressure injection filling method using an index nozzle.
Moreover, since almost no residual solvent is present in the solidified cosmetic, there is no cracking, uneven color tone, or uneven gloss of the cosmetic, and the yield of the cosmetic is good.

更に、容器の底板が昇降式であるのでコンバク(−の底
面に小孔を穿設しておくと化粧料がなくなくなった場合
、この小孔を介して底板を押し上げコンパクトの上面で
化粧1’i+を使用することもできるので使い勝手が良
い。
Furthermore, since the bottom plate of the container can be raised and lowered, a small hole is drilled in the bottom of the compact (-) so that when the cosmetics run out, the bottom plate is pushed up through the small hole and the makeup 1' is removed from the top of the compact. It is easy to use because you can also use i+.

【図面の簡単な説明】[Brief explanation of drawings]

第1図は本発明の化粧料充填工程を示す断面図、第2図
は本発明に使用される容器を示す一部切欠き斜視図、第
3図は本発明の固化工程及びiAnの第1実施例を示す
断面図、第4図は同上第2実施例を示す断面図、第5図
は本発明を適用した容器をコンパクトに収容した断面図
である。 1・・・・・・・・・粘性化粧料  2・・・・・・・
・・撹拌槽5・・・・・・・・・吐出口    12・
・・・・・容 器13・・・・・・外 枠    14
・・・・・・底 板19・・・・・・吸水性膜材  2
0・・・・・・通気孔21・・・・・・フランジ   
24・・・・・・鍔27・・・・・・下 型    2
9・・・・・・多孔質吸収体32・・・・・・加圧ロッ
ド  35・・・・・・真空吸引流通路37・・・・・
・真空ポンプ  39.39−・・・上 型41・・・
・・・エアーシリンダ 42・・・・・・多孔質吸収体 45・・・・・・真空
吸引流通路48・・・・・・吸水性膜材 49・・・・
・・コンパクト50・・・・・・小 孔 特許出願人         吉田工業株式会社代 理
 人         弁理士 −色健輔第1図 第2図 第3図
Fig. 1 is a cross-sectional view showing the cosmetic filling process of the present invention, Fig. 2 is a partially cutaway perspective view showing a container used in the present invention, and Fig. 3 is a solidification process of the present invention and the FIG. 4 is a sectional view showing the second embodiment of the present invention, and FIG. 5 is a sectional view showing a compact container to which the present invention is applied. 1... Viscous cosmetics 2...
・・Stirring tank 5・・・・・・・Discharge port 12・
...Container 13 ... Outer frame 14
...Bottom plate 19...Water absorbent membrane material 2
0...Vent hole 21...Flange
24...Brim 27...Lower mold 2
9... Porous absorber 32... Pressure rod 35... Vacuum suction flow path 37...
・Vacuum pump 39.39-... Upper mold 41...
... Air cylinder 42 ... Porous absorber 45 ... Vacuum suction flow path 48 ... Water-absorbing membrane material 49 ...
... Compact 50 ... Koko Patent applicant Yoshida Kogyo Co., Ltd. Agent Patent attorney - Kensuke Shiro Figure 1 Figure 2 Figure 3

Claims (4)

【特許請求の範囲】[Claims] (1)上面が開口し底面を構成する底板が通気性を付与
されるとともに吸水性膜材を有しかつ外周壁を構成する
外枠内で上下に移動可能とされた皿状の容器内に、溶剤
で溶かして粘性化した化粧料を上面側から適宜量充填す
る工程と、前記容器の外周壁上面に上型を圧接する工程
と、前記容器を収容する下型に設けた多孔質吸収体によ
って前記容器の底板を上方に押し上げて内部の前記化粧
料を圧縮する工程と、該圧縮工程時に前記吸水性膜材及
び前記多孔質吸収体を通して前記化粧料中の溶剤を吸収
する工程とを包含してなる化粧料の充填固化方法。
(1) Inside a dish-shaped container with an open top and a bottom plate that is breathable, has a water-absorbing membrane material, and is movable up and down within the outer frame that forms the outer peripheral wall. , a step of filling an appropriate amount of cosmetics dissolved in a solvent and made viscous from the upper surface side, a step of pressing an upper mold onto the upper surface of the outer peripheral wall of the container, and a porous absorbent body provided in a lower mold that accommodates the container. compressing the cosmetic inside by pushing up the bottom plate of the container, and absorbing the solvent in the cosmetic through the water-absorbing membrane material and the porous absorbent body during the compression step. A method for filling and solidifying cosmetics.
(2)上面が開口し底面を構成する底板が通気性を付与
されるとともに吸水性膜材を有しかつ外周壁を構成する
外枠内で上下に移動可能とされた皿状の容器内に、溶剤
で溶かして粘性化した化粧料を上面側から適宜量充填す
る工程と、前記容器の上面側に吸水性膜材を介在させそ
の上から少なくとも前記容器の上面開口部を覆う多孔質
吸収体を有する上型を前記容器の外周壁上面に圧接する
工程と、前記容器を収容する下型に設けた多孔質吸収体
によって前記容器の底板を上方に押し上げて内部の前記
化粧料を圧縮する工程と、該圧縮工程時に前記容器の吸
水性膜材と前記下型に設けた多孔質吸収体を通して、ま
たは前記容器の上面側に介在させた吸水性膜材と前記上
型に設けた多孔質吸収体を通して前記化粧料中の溶剤を
吸収する工程とを包含してなる化粧料の充填固化方法。
(2) Inside a dish-shaped container with an open top and a bottom plate that is breathable, has a water-absorbing membrane material, and is movable up and down within the outer frame that forms the outer peripheral wall. , a step of filling an appropriate amount of cosmetics dissolved in a solvent and made viscous from the top surface side, and a porous absorbent material that interposes a water-absorbing membrane material on the top surface side of the container and covers at least the top opening of the container from above. a step of pressing an upper mold having an upper mold onto the upper surface of the outer circumferential wall of the container, and a step of pushing up the bottom plate of the container by a porous absorbent provided in a lower mold that accommodates the container to compress the cosmetic material inside. During the compression step, the water-absorbing membrane material of the container and the porous absorbent body provided on the lower mold are passed through, or the water-absorbing membrane material interposed on the upper surface side of the container and the porous absorbent body provided on the upper mold. A method for filling and solidifying a cosmetic, which includes the step of absorbing a solvent in the cosmetic through the body.
(3)上面が開口し底面を構成する底板が通気性を付与
されるとともに吸水性膜材を有しかつ外周壁を構成する
外枠内で上下に移動可能な皿状の容器を位置決め載置す
るための凹部と、該凹部の底に連続して形成された真空
吸引用流通路と、前記容器を多孔質吸収体で上方に押し
上げる加圧手段とを有する下型と、前記加圧手段に連結
されて該加圧手段を上下動させるための駆動機構と、前
記下型上の前記容器の外周壁上面に圧接可能に上下動さ
せるための駆動機構を有する上型との組合せよりなる化
粧料の充填固化装置。
(3) Position and place a dish-shaped container whose top surface is open and whose bottom plate is breathable and has a water-absorbing membrane material and which is movable up and down within the outer frame that forms the outer peripheral wall. a lower mold having a recessed portion for the purpose of cleaning the container, a flow path for vacuum suction formed continuously at the bottom of the recessed portion, and a pressurizing means for pushing the container upward with a porous absorbent; A cosmetic comprising a combination of a drive mechanism that is connected to move the pressure means up and down, and an upper mold that has a drive mechanism that moves the pressure means up and down so as to be able to press against the upper surface of the outer peripheral wall of the container on the lower mold. filling solidification equipment.
(4)上面が開口し底面を構成する底板が通気性を付与
されるとともに吸水性膜材を有しかつ外周壁を構成する
外枠内で上下に移動可能な皿状の容器を位置決め載置す
るための凹部と、該凹部の底に通続して形成された真空
吸引用流通路と前記容器を多孔質吸収体で上方に押し上
げる加圧手段とを有する下型と、前記加圧手段に連結さ
れて該加圧手段を上下動させるための駆動機構と、下面
に少なくとも前記容器の上面開口部を覆う多孔質吸収体
が嵌合された凹部と該凹部の底に連続して形成された真
空吸引用流通路と前記下型上の前記容器の上面に圧接可
能に上下動させるための駆動機構とを有する上型との組
合せよりなる化粧料の固化装置。
(4) Position and place a dish-shaped container whose top surface is open and whose bottom plate is breathable and has a water-absorbing membrane material and is movable up and down within the outer frame that forms the outer peripheral wall. a lower mold having a recess for the purpose of cleaning the container, a vacuum suction passage formed in communication with the bottom of the recess, and a pressurizing means for pushing the container upward with a porous absorbent; A drive mechanism is connected to the drive mechanism for vertically moving the pressurizing means, and a recess in which a porous absorbent material covering at least the upper opening of the container is fitted on the lower surface is formed continuously at the bottom of the recess. A cosmetic solidifying device comprising a combination of an upper mold having a vacuum suction flow passage and a drive mechanism for moving up and down so as to be able to press against the upper surface of the container on the lower mold.
JP3068986A 1986-02-17 1986-02-17 Method for filling and solidification of cosmetic and apparatus therefor Pending JPS62190114A (en)