JPS6059532A - Polishing head of magnetic disc - Google Patents
Polishing head of magnetic discInfo
- Publication number
- JPS6059532A JPS6059532A JP16675183A JP16675183A JPS6059532A JP S6059532 A JPS6059532 A JP S6059532A JP 16675183 A JP16675183 A JP 16675183A JP 16675183 A JP16675183 A JP 16675183A JP S6059532 A JPS6059532 A JP S6059532A
- Authority
- JP
- Japan
- Prior art keywords
- polishing
- tape
- disc
- magnetic disc
- head
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
【発明の詳細な説明】
技術分野
本発明は磁気ディスクを研摩して、表面の突起を除去す
るへ、ドに関する。TECHNICAL FIELD The present invention relates to polishing a magnetic disk to remove surface protrusions.
背景技術
磁気ディスクは記録密度を高めるために、磁気ヘッドの
浮上量を最小にすることが望ましい。磁気ディスクの塗
膜に突起が著しい場合は、浮上量を大きくする必要がお
きる。BACKGROUND ART In order to increase the recording density of magnetic disks, it is desirable to minimize the flying height of the magnetic head. If the coating film of the magnetic disk has significant protrusions, it may be necessary to increase the flying height.
従来技術と問題点
磁気ディスクの塗膜表面の突起を除去するためには、研
摩テープをベース部分に取付けた研摩用へ、ドを、磁気
ディスクを回転させながら、ディスクの半径方向に往復
させて、研摩テープで塗膜表面を研摩する。しかし、従
来のヘッドはベース部分が剛性を有する平板であるので
、僅小な凹凸を有する塗膜表面に対して、均一な間隔を
保って接触することが困難である。従って均一な突起除
去を達成できないので、研摩へ、ドの往復回数は10〜
15回を必要とし、しかも残留する突起は高さ0.15
μm程度とかなり大きい欠点がある。Prior Art and Problems In order to remove protrusions on the coating surface of a magnetic disk, an abrasive tape attached to the base is moved back and forth in the radial direction of the disk while rotating the disk. , polish the coating surface with abrasive tape. However, since the base portion of the conventional head is a flat plate having rigidity, it is difficult to maintain uniform spacing and contact with the surface of the coating film having minute irregularities. Therefore, uniform removal of protrusions cannot be achieved, so the number of reciprocations between polishing and de is 10 to 10 times.
15 times are required, and the height of the remaining protrusion is 0.15
It has a rather large drawback of about μm.
発明の目的
本発明の目的は上記欠点を解消した研摩へ、ドを提供す
ることである◎
発明の構成
本発明の上記目的は、磁気ディスク製造工程の一つであ
る塗膜表面の研摩に使用するへ、ドであって、研摩テー
プと、このテープを取付けるベースとの間に緩衝材を設
けたことを特徴とする磁気ディスク研摩へ、ドによって
達成することができる。Purpose of the Invention The purpose of the present invention is to provide a method for polishing that eliminates the above-mentioned drawbacks. ◎ Structure of the Invention The purpose of the present invention is to provide a method for polishing the surface of a coating film, which is one of the magnetic disk manufacturing processes. This can be achieved by polishing a magnetic disk, which is characterized by providing a cushioning material between the polishing tape and the base on which the tape is attached.
実施例
第1図を参照して、本発明の実施態様を説明する。アー
ム1は先端のベース部分2に研摩テープ6を有する。ベ
ース部分2と、研摩テープ3との間に緩衝材4として、
シリコーンゴム膜(硬度40±10度)膜厚2〜311
i1を設けた。磁気ディスク5を500rpm程度で回
転させながら、ディスクの半径方向に約1.8馴/Sの
速さで、6〜5回往復させて得られた磁気ディスクは突
起の高さが0.1μm程度であった。Embodiment An embodiment of the present invention will be described with reference to FIG. The arm 1 has an abrasive tape 6 on the base portion 2 at its tip. As a cushioning material 4 between the base portion 2 and the abrasive tape 3,
Silicone rubber film (hardness 40±10 degrees) film thickness 2-311
i1 was established. The magnetic disk obtained by rotating the magnetic disk 5 at about 500 rpm and reciprocating it 6 to 5 times in the radial direction of the disk at a speed of about 1.8/S has a protrusion height of about 0.1 μm. Met.
発明の効果
本発明の研摩へ、ドは塗膜表面をむらなく研摩すること
ができるので、従来の研摩へ、ドより短時間で、同等以
上の突起除去効果を得られる。Effects of the Invention Since the polishing method of the present invention can evenly polish the surface of a coating film, it is possible to obtain the same or better protrusion removal effect than conventional polishing methods in a shorter time.
第1図は本発明の磁気デ°イスク研摩ヘッドの部分断面
図である。
1・・・アーム、2・・・ベース部分、3・・・研摩テ
ープ、4・・・緩衝材、5・・・磁気ディスク。
第1図FIG. 1 is a partial cross-sectional view of the magnetic disk polishing head of the present invention. DESCRIPTION OF SYMBOLS 1... Arm, 2... Base part, 3... Abrasive tape, 4... Cushioning material, 5... Magnetic disk. Figure 1
Claims (1)
に使用するヘッドであって、研摩テープと、このテープ
を取付けるベースとの間に緩衝材を設けたことを特徴と
する磁気ディスク研摩ヘッド。1. A magnetic disk polishing head used for polishing the surface of a coating film, which is one of the magnetic disk manufacturing processes, characterized in that a cushioning material is provided between the polishing tape and the base on which this tape is attached. head.