JPS575819A - Preparation of seamless line pipe having excellent sulfide hydrogen cracking resistance - Google Patents
Preparation of seamless line pipe having excellent sulfide hydrogen cracking resistanceInfo
- Publication number
- JPS575819A JPS575819A JP7908680A JP7908680A JPS575819A JP S575819 A JPS575819 A JP S575819A JP 7908680 A JP7908680 A JP 7908680A JP 7908680 A JP7908680 A JP 7908680A JP S575819 A JPS575819 A JP S575819A
- Authority
- JP
- Japan
- Prior art keywords
- preparation
- cracking resistance
- line pipe
- hydrogen cracking
- sulfide hydrogen
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To prepare the titled pipe by quenching before tempering the seamless pipe made of the special composition steel containing C, Si, Mn, P, S, O, sol.Al, Nb and V. CONSTITUTION:The seamless pipe is formed with the steel containing 0.05- 0.20% C, 0.1-1.0% Si, 0.5-2.0% Mn, 0.03% or less P, 0.006% or less S, 0.005% or less O, 0.01-0.07% sol.Al, 0.05-0.1% one or more elements of Nb and V and, if necessary, further one or more elements of 0.10-0.40% Cu, 0.05-0.20% Ni, 0.05-0.8% one or more elements of Cr and Mo and 0.0005-0.005% B. The pipe is quenched through its both inner and outer surfaces from a temperature of 900 deg.C or higher with the cooling water having a temperature of 100 deg.--50 deg.C. Subsequently, it is tempered at a temperature within the range of 550 deg.C-AC1.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7908680A JPS575819A (en) | 1980-06-13 | 1980-06-13 | Preparation of seamless line pipe having excellent sulfide hydrogen cracking resistance |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7908680A JPS575819A (en) | 1980-06-13 | 1980-06-13 | Preparation of seamless line pipe having excellent sulfide hydrogen cracking resistance |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS575819A true JPS575819A (en) | 1982-01-12 |
Family
ID=13680066
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP7908680A Pending JPS575819A (en) | 1980-06-13 | 1980-06-13 | Preparation of seamless line pipe having excellent sulfide hydrogen cracking resistance |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS575819A (en) |
Cited By (11)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6155126A (en) * | 1984-08-24 | 1986-03-19 | Japan Synthetic Rubber Co Ltd | Crosslinked foam |
JPS62146223A (en) * | 1985-12-21 | 1987-06-30 | Kawasaki Steel Corp | Manufacture of seamless steel pipe superior in hydrogen induced cracking resistance |
EP1375683A1 (en) * | 2001-03-29 | 2004-01-02 | Sumitomo Metal Industries, Ltd. | High strength steel tube for air bag and method for production thereof |
WO2004031420A1 (en) * | 2002-10-01 | 2004-04-15 | Sumitomo Metal Industries, Ltd. | High strength seamless steel pipe excellent in hydrogen-induced cracking resistance and its production method |
EP1568792A1 (en) * | 2004-02-24 | 2005-08-31 | JFE Steel Corporation | Hot-rolled steel sheet for high-strength electric-resistance welded pipe and method for manufacturing the same |
US7416617B2 (en) | 2002-10-01 | 2008-08-26 | Sumitomo Metal Industries, Ltd. | High strength seamless steel pipe excellent in hydrogen-induced cracking resistance |
CN100415922C (en) * | 2003-05-21 | 2008-09-03 | 住友金属工业株式会社 | Steel pipe for an airbag system and a method for its manufacture |
CN100420758C (en) * | 2002-10-01 | 2008-09-24 | 住友金属工业株式会社 | High strength seamless steel pipe excellent in hydrogen-induced cracking resistance and its production method |
CN105358725A (en) * | 2013-07-04 | 2016-02-24 | 新日铁住金株式会社 | Seamless steel tube for line pipe used in acidic environment |
WO2018020972A1 (en) * | 2016-07-28 | 2018-02-01 | 新日鐵住金株式会社 | High strength seamless steel pipe and riser |
DE10143073B4 (en) | 2000-09-01 | 2022-06-09 | Nippon Steel & Sumitomo Metal Corporation | Low carbon steel and method of making structural steel tube with high cold temperature toughness |
-
1980
- 1980-06-13 JP JP7908680A patent/JPS575819A/en active Pending
Cited By (18)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0449860B2 (en) * | 1984-08-24 | 1992-08-12 | Japan Synthetic Rubber Co Ltd | |
JPS6155126A (en) * | 1984-08-24 | 1986-03-19 | Japan Synthetic Rubber Co Ltd | Crosslinked foam |
JPS62146223A (en) * | 1985-12-21 | 1987-06-30 | Kawasaki Steel Corp | Manufacture of seamless steel pipe superior in hydrogen induced cracking resistance |
DE10143073B4 (en) | 2000-09-01 | 2022-06-09 | Nippon Steel & Sumitomo Metal Corporation | Low carbon steel and method of making structural steel tube with high cold temperature toughness |
US7846274B2 (en) | 2001-03-29 | 2010-12-07 | Sumitomo Metal Industries, Ltd. | High strength steel pipe for an air bag |
EP1375683A1 (en) * | 2001-03-29 | 2004-01-02 | Sumitomo Metal Industries, Ltd. | High strength steel tube for air bag and method for production thereof |
EP1375683A4 (en) * | 2001-03-29 | 2006-01-11 | Sumitomo Metal Ind | High strength steel tube for air bag and method for production thereof |
WO2004031420A1 (en) * | 2002-10-01 | 2004-04-15 | Sumitomo Metal Industries, Ltd. | High strength seamless steel pipe excellent in hydrogen-induced cracking resistance and its production method |
US7416617B2 (en) | 2002-10-01 | 2008-08-26 | Sumitomo Metal Industries, Ltd. | High strength seamless steel pipe excellent in hydrogen-induced cracking resistance |
CN100420758C (en) * | 2002-10-01 | 2008-09-24 | 住友金属工业株式会社 | High strength seamless steel pipe excellent in hydrogen-induced cracking resistance and its production method |
AU2003264947B2 (en) * | 2002-10-01 | 2006-08-31 | Nippon Steel Corporation | High strength seamless steel pipe excellent in hydrogen-induced cracking resistance and its production method |
NO339589B1 (en) * | 2002-10-01 | 2017-01-09 | Sumitomo Metal Ind | High-strength seamless steel pipe with excellent resistance to hydrogen-induced cracks, as well as manufacturing process |
CN100415922C (en) * | 2003-05-21 | 2008-09-03 | 住友金属工业株式会社 | Steel pipe for an airbag system and a method for its manufacture |
CN100354436C (en) * | 2004-02-24 | 2007-12-12 | 杰富意钢铁株式会社 | Hot-rolled steel sheet for high-strength electric-resistancewelded pipe having sour-gas resistance and excellent weld toughness, and method for manufacturing the same |
US7879287B2 (en) | 2004-02-24 | 2011-02-01 | Jfe Steel Corporation | Hot-rolled steel sheet for high-strength electric-resistance welded pipe having sour-gas resistance and excellent weld toughness, and method for manufacturing the same |
EP1568792A1 (en) * | 2004-02-24 | 2005-08-31 | JFE Steel Corporation | Hot-rolled steel sheet for high-strength electric-resistance welded pipe and method for manufacturing the same |
CN105358725A (en) * | 2013-07-04 | 2016-02-24 | 新日铁住金株式会社 | Seamless steel tube for line pipe used in acidic environment |
WO2018020972A1 (en) * | 2016-07-28 | 2018-02-01 | 新日鐵住金株式会社 | High strength seamless steel pipe and riser |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB8505647D0 (en) | Bearing steel | |
JPS575819A (en) | Preparation of seamless line pipe having excellent sulfide hydrogen cracking resistance | |
SE8003567L (en) | PROCEDURAL KIT FOR MANUFACTURING STAINLESS, FERRITAUSTENITIC STEEL | |
DE60124646D1 (en) | Stainless cast steel with good heat resistance and good tensionability | |
KR960706569A (en) | High corrosion resistance martensitic stainless steel with excellent weldability and manufacturing method | |
JPS56116858A (en) | Steam turbine rotor | |
JPS5496418A (en) | Heat resistant cast steel | |
JPS5524932A (en) | Manufacture of bainite tough hardening steel | |
JPS5713152A (en) | Steel for seamless steel pipe with superior corrosion resistance | |
JPS575849A (en) | Steel excellent in corrosion resistance for use as seamless steel pipe | |
JPS5789426A (en) | Manufacture of high-hardness and wear resistant steel having excellent weldability | |
JPS5541929A (en) | Steel for high efficiency welding and low temperature use | |
JPS5573848A (en) | High strength steel for welded structure with superior sulfide stress corrosion cracking resistance | |
JPS5754252A (en) | Soft magnetic material containing chromium | |
JPS5524966A (en) | High tension steel with excellent resistance to sr cracking | |
JPS5735622A (en) | Manufacture of high strength steel for oil well with superior delayed fracture resistance | |
JPS565949A (en) | High tensile steel with superior sulfide corrosion crack resistance and superior corrosion resistance | |
JPS5629667A (en) | Preparation of metal mold | |
FR2630132B1 (en) | AUSTENO-FERRITIC STAINLESS STEEL | |
JPS5794559A (en) | Stainless steel with resistance to hydrogen sulfide | |
JPS5589426A (en) | Preparation of high tensile steel with excellent delayed destruction resistance | |
JPS5413414A (en) | Medium cr low ni stainless cast steel of high corrosion resistance and high strength | |
JPS5573849A (en) | Refined high strength steel of low surface hardness | |
JPS54127821A (en) | Line pipe steel resistant to hydrogen induced cracking and production thereof | |
JPS56158847A (en) | Heat resistant chromium steel |