Prior art keywords
stub
welding
tube
welded
tube plate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP13065780A
Other languages
Japanese (ja)
Inventor
Koji Tamura
Nobuo Hosoya
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mitsubishi Power Ltd
Original Assignee
Babcock Hitachi KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Babcock Hitachi KK filed Critical Babcock Hitachi KK
Priority to JP13065780A priority Critical patent/JPS5756193A/en
Publication of JPS5756193A publication Critical patent/JPS5756193A/en
Pending legal-status Critical Current

Links

Landscapes

  • Butt Welding And Welding Of Specific Article (AREA)

Abstract

PURPOSE: To improve the reliability of welding joint through forming stub with welding metal by cutting out the stub from a welding part where beveling groove formed at a tubular hole position in a tube plate is narrow-gap-welded.
CONSTITUTION: At a position where a tubular hole 6 of a tube plate 1 to be worked, a beveling groove 6 having an inner diameter smaller than that of stub, an outer diameter larger than that of the stub and a depth deeper than that of the stub is formed. Next, after the groove 6 is multilayer welded with low heat input through the way of narrow gap welding the stub 8 of welding having the same cross section as a tube is cut out from a welding part 7 through machine work. Then, a tube 4 and the stub 8 are butt-welded through the ordinary welding way.
COPYRIGHT: (C)1982,JPO&Japio
JP13065780A 1980-09-22 1980-09-22 Welding method for tube and tube plate Pending JPS5756193A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP13065780A JPS5756193A (en) 1980-09-22 1980-09-22 Welding method for tube and tube plate

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP13065780A JPS5756193A (en) 1980-09-22 1980-09-22 Welding method for tube and tube plate

Publications (1)

Publication Number Publication Date
JPS5756193A true JPS5756193A (en) 1982-04-03

Family

ID=15039485

Family Applications (1)

Application Number Title Priority Date Filing Date
JP13065780A Pending JPS5756193A (en) 1980-09-22 1980-09-22 Welding method for tube and tube plate

Country Status (1)

Country Link
JP (1) JPS5756193A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US7017792B2 (en) * 2001-02-02 2006-03-28 Mitsubishi Heavy Industries, Ltd. Integrated piping plate, machining method for same, machining apparatus for same, and machining equipment for same

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US7017792B2 (en) * 2001-02-02 2006-03-28 Mitsubishi Heavy Industries, Ltd. Integrated piping plate, machining method for same, machining apparatus for same, and machining equipment for same
US7367360B2 (en) 2001-02-02 2008-05-06 Mitsubishi Heavy Industries, Ltd. Integrated piping plate, machining method for same, machining apparatus for same, and machining equipment for same
US7434598B2 (en) 2001-02-02 2008-10-14 Mitsubishi Heavy Industries, Ltd. Integrated piping plate, machining method for same, machining apparatus for same, and machining equipment for same
US7640948B2 (en) 2001-02-02 2010-01-05 Mitsubishi Heavy Industries, Ltd. Integrated piping plate, machining method for same, machining apparatus for same, and machining equipment for same

Similar Documents

Publication Publication Date Title
JPS55112181A (en) Welding method for production of large-diameter thick-walled steel pipe
JPS5756193A (en) Welding method for tube and tube plate
JPS5510395A (en) Electron beam welding method for dissimilar metal
JPS5671595A (en) Welding method for tube and tube plate in heat exchanger
JPS53113734A (en) One-side arc welding method for 9% ni steel
JPS53130242A (en) Welding method for manufacture of thick-walled large diameter welded steel pipe
JPS53130241A (en) Welding method for manufacture of thick walled steel pipe
JPS56131083A (en) Welded joint method for stainless steel tube
JPS53142348A (en) Welding method for metallic pipe
JPS5493652A (en) Method and apparatus for manufacture of crossed pipe parts
JPS53106361A (en) Submerged arc welding method for steel plate
JPS5542128A (en) Repair welding method of stainless steel pipe welded joint
JPS56105831A (en) Manufacture of punch for use of press work
JPS56131094A (en) Branch pipe welding method
JPS564392A (en) Connecting method of piping
JPS56158288A (en) Electron beam welding
JPS56168994A (en) Welding method for piping
JPS5647290A (en) Welding method of pipe and pipe plate
JPS5797889A (en) Welding method for plate material
JPS54158366A (en) Manufacture of composite rod
JPS5396944A (en) Welding method for tubes to tube plate of heat exchanger
JPS5614094A (en) Welding method
JPS54119345A (en) Fixing method for dynamo-bracket of bicycle by welding
GB2012645A (en) Improving spot weld penetration in metal sheets
JPS54101737A (en) Welding method by high output high density electron beam