JPS57205702A - Rotary polyhedral mirror and its production - Google Patents
Rotary polyhedral mirror and its productionInfo
- Publication number
- JPS57205702A JPS57205702A JP16102081A JP16102081A JPS57205702A JP S57205702 A JPS57205702 A JP S57205702A JP 16102081 A JP16102081 A JP 16102081A JP 16102081 A JP16102081 A JP 16102081A JP S57205702 A JPS57205702 A JP S57205702A
- Authority
- JP
- Japan
- Prior art keywords
- layer
- vapor
- die
- master
- adhesive
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To produce reproduced products bearing good resemblance to a master efficiently by vapor-depositing a release agent layer on the specular surfaces of a master female mold, then vapor-depositing a high reflection film thereon, adhering a backing structural body thereon, and pulling these with the mold release agent layer thereby forming the specular surfaces of a polyhedral mirror. CONSTITUTION:Silicone oil is vapor-deposited as a mold release agent 22A on the respective specular surface 77 of a master polyhedral mirror 40, and a highly reflective film 33A of Al or the like is vapor-deposited thereon. This is inserted into the hollow part of a die 51. After these are so set that the center of a revolving shaft 78 and the center of the die 51 align, adhesive of low viscosity is forced into the space between the die 51 and the layer 33A, whereby an adhesive layer 44A is formed. When the polyhedral mirror 44A is pulled out after the curing of the adhesive, the female mold made of metal having the layer 44A and the layer 33A is completed. A mold release agent 33B is vapor-deposited successively on the layer 33A in a similar manner, and a core 40B made of metal is set. After the forcing and curing of the adhesive 44V, the mirror is pulled from the die, whereby the reproduced product bearing good resemblance to the master is produced with good efficiency.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16102081A JPS57205702A (en) | 1981-10-12 | 1981-10-12 | Rotary polyhedral mirror and its production |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16102081A JPS57205702A (en) | 1981-10-12 | 1981-10-12 | Rotary polyhedral mirror and its production |
Related Parent Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP10979176A Division JPS5336249A (en) | 1976-09-16 | 1976-09-16 | Metod of making mirror replica |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS57205702A true JPS57205702A (en) | 1982-12-16 |
Family
ID=15727054
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP16102081A Pending JPS57205702A (en) | 1981-10-12 | 1981-10-12 | Rotary polyhedral mirror and its production |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS57205702A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58216201A (en) * | 1982-06-10 | 1983-12-15 | Copal Erekutora:Kk | Polygonal mirror and its production |
JPS624718U (en) * | 1985-06-24 | 1987-01-12 |
Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS50155243A (en) * | 1974-06-05 | 1975-12-15 | ||
JPS52141239A (en) * | 1976-05-19 | 1977-11-25 | Xerox Corp | Method of manufacturing highhspeed multii surface scanner |
JPS5336249A (en) * | 1976-09-16 | 1978-04-04 | Fuji Xerox Co Ltd | Metod of making mirror replica |
-
1981
- 1981-10-12 JP JP16102081A patent/JPS57205702A/en active Pending
Patent Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS50155243A (en) * | 1974-06-05 | 1975-12-15 | ||
JPS52141239A (en) * | 1976-05-19 | 1977-11-25 | Xerox Corp | Method of manufacturing highhspeed multii surface scanner |
JPS5336249A (en) * | 1976-09-16 | 1978-04-04 | Fuji Xerox Co Ltd | Metod of making mirror replica |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58216201A (en) * | 1982-06-10 | 1983-12-15 | Copal Erekutora:Kk | Polygonal mirror and its production |
JPH0334044B2 (en) * | 1982-06-10 | 1991-05-21 | Copal Electronics | |
JPS624718U (en) * | 1985-06-24 | 1987-01-12 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CA1001845A (en) | Process for manufacturing of a pattern composite coating and of the products resulted therefrom | |
JPS57205702A (en) | Rotary polyhedral mirror and its production | |
CA979889A (en) | Soap stock reclamation process for producing fatty acids, glycerine and salts | |
GB777025A (en) | Improvements in or relating to commutator manufacture | |
US1578982A (en) | Decorative material for ornamental panels, plaques, or the like | |
CA962860A (en) | Method of making a master die for use in an abrasion process | |
JPS532899A (en) | Process for producing composite material wing | |
GB1433214A (en) | Process of forming a decorated or inscribed sheet of acrylic resin | |
GB1479194A (en) | Method for the coating of a shaped article of hardenable plastics material | |
JPS5838133A (en) | Manufacture of three-dimensional resin molding with picture | |
CA1006671A (en) | Molded article having three-dimensional, decorated surface and method of producing same | |
JPS6490067A (en) | Production of patterned decorative material | |
IL43741A (en) | Method of metal coating the interior surfaces of a die casting | |
JPS648004A (en) | Shaping method for ornament | |
GB1375396A (en) | ||
CN1084448A (en) | Copying hologram and grating technology on crust | |
JPS6484078A (en) | Handle decorative cover for refrigerator and manufacture thereof | |
FR2097510A5 (en) | Polyester laminates - with a finishing coat applied to the mould | |
CA997989A (en) | Composition and method for producing brown coatings on brass | |
JPS58201609A (en) | Preparation of container for hydrostatic forming | |
AU462224B2 (en) | A process FOR PRODUCING SURFACES OF SPECIFIED TEXTURE | |
CA962138A (en) | Method of making a decorative article | |
JPS5241078A (en) | Method for producing an ornament having a metallic appearance | |
JPS53139651A (en) | Method of coating hollow article | |
KR910007663A (en) | How to Make Metaric Hotfixes |