JPS5711719A - Hydrostatic extruding method - Google Patents
Hydrostatic extruding methodInfo
- Publication number
- JPS5711719A JPS5711719A JP8545980A JP8545980A JPS5711719A JP S5711719 A JPS5711719 A JP S5711719A JP 8545980 A JP8545980 A JP 8545980A JP 8545980 A JP8545980 A JP 8545980A JP S5711719 A JPS5711719 A JP S5711719A
- Authority
- JP
- Japan
- Prior art keywords
- hardness
- nose
- extrusion
- sectional area
- heat treatment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To safely practice an extrusion work without generating a peak pressure, by changing a condition of an aging heat treatment of a nose material in order to adjust its hardness, in a hyraostatic extruding method for shrinking diameter of a composite billet.
CONSTITUTION: In a composite billet, a coating material 3 is put on outside of a core material 2, and the tip of this coating material 3 is welded to a nose material 4 shaped so as to be fittable to an extrusion die 8. The nose material 4 is made of a Cr-Cu alloy wherein Cr content is limited to about 0.5W1.2%; a heating and hardening treament is applied previously to the nose material 4 by a nonoxidizing furnace at temperatures 950W1,050°C, and then an aging heat treatment for the purpose of a precipitation hardening is applied. The temperature and duration of this treatment are selected correspondingly to a required hardness. The aimed hardness is determine correspondingly to hardness of the coating metal 3 and core material 2, and to a ratio of each sectional area to whole sectional area. By the present method, an ideal extrusion condition C free from generation of a peak pressure is obtained.
COPYRIGHT: (C)1982,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8545980A JPS591487B2 (en) | 1980-06-24 | 1980-06-24 | Hydrostatic extrusion method |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8545980A JPS591487B2 (en) | 1980-06-24 | 1980-06-24 | Hydrostatic extrusion method |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5711719A true JPS5711719A (en) | 1982-01-21 |
JPS591487B2 JPS591487B2 (en) | 1984-01-12 |
Family
ID=13859458
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP8545980A Expired JPS591487B2 (en) | 1980-06-24 | 1980-06-24 | Hydrostatic extrusion method |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS591487B2 (en) |
-
1980
- 1980-06-24 JP JP8545980A patent/JPS591487B2/en not_active Expired
Also Published As
Publication number | Publication date |
---|---|
JPS591487B2 (en) | 1984-01-12 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
KR970014875A (en) | METHOD FOR MANUFACTURING MOISTURE MATERIAL FOR COPY ALLOY FOR STEEL STEEL CASTING AND METHOD THEREOF | |
ES486912A1 (en) | Process of treatment of a precipitation hardenable Al-Mg-Si-alloy | |
JPS5711719A (en) | Hydrostatic extruding method | |
JPS5420943A (en) | Manufacture of composite metallic wire and rod | |
JPS53122612A (en) | Method of fabricating high tensile cold rolled steel plate | |
JPS5392313A (en) | Directly heat treating method for wire rod | |
JPS5435812A (en) | Manufacture of high tensile aluminum alloy | |
JPS5739128A (en) | Preparation of heat resistant cutter bit for dental die | |
JPS5594730A (en) | Manufacture of composite metallic wire | |
JPS5360310A (en) | Continuous annealing method for titanium and titanium alloy | |
JPS5220912A (en) | Method of operating metal heating furnaces | |
JPS53135817A (en) | Continuously casting and rolling method for al and al alloy | |
JPS53135809A (en) | Continuous heat treatment method for steel wire covered with copper | |
JPS5562103A (en) | Production of deformed composite heat resistant alloy member | |
JPS6430114A (en) | Manufacture of oxide superconductor | |
JPS5511137A (en) | Corrosion resistant structural aluminum alloy material | |
JPS5636384A (en) | Welding method of spheroidal graphite cast iron | |
JPS54133458A (en) | Rolling method for thin clad sheet | |
JPS53108844A (en) | Method and apparatus for treating metal bar with solder | |
JPS53147653A (en) | Method of producing rotor material | |
JPS56128668A (en) | Soldering method | |
JPS53147298A (en) | Method of manufacturing the magnetic core for magnetic head | |
JPS5480264A (en) | Manufacture of pipe of zirconium or zirconium base alloy | |
JPS5672158A (en) | Manufacture of aluminum alloy brazing material hard to buckling deform at high temperature | |
JPS5395850A (en) | Multiple wire submerged arc welding method |