Prior art keywords
exfoliation
solder
electrolyte
phosphoric acid
concentration
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP7982979A
Other languages
Japanese (ja)
Inventor
Yasuo Nakajima
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NEC Corp
Original Assignee
NEC Corp
Nippon Electric Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NEC Corp, Nippon Electric Co Ltd filed Critical NEC Corp
Priority to JP7982979A priority Critical patent/JPS563700A/en
Publication of JPS563700A publication Critical patent/JPS563700A/en
Pending legal-status Critical Current

Links

Landscapes

  • Electrolytic Production Of Metals (AREA)

Abstract

PURPOSE: Solder exfoliation electrolyte, obtained by using phosphoric acid solution added anion fluorinated hydrocarbon compound and made the solder exfoliation condition uniform and also, able to easily confirm the end of exfoliation.
CONSTITUTION: Phosphoric acid for industrial use is used for the phosphoric acid and concentration in exfoliation electrolyte is 0.001% or more. FC-95 or FC-98 etc. is used for anion fluorinated hydrocarbon compound and the concentration in the electrolyte is 0.005% or more. Electrolysis for solder exfoliation is carried out at a normal temperature of 15W25°C and current density of 5W10A/cm2.
COPYRIGHT: (C)1981,JPO&Japio
JP7982979A 1979-06-25 1979-06-25 Solder exfoliation electrolyte Pending JPS563700A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP7982979A JPS563700A (en) 1979-06-25 1979-06-25 Solder exfoliation electrolyte

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP7982979A JPS563700A (en) 1979-06-25 1979-06-25 Solder exfoliation electrolyte

Publications (1)

Publication Number Publication Date
JPS563700A true JPS563700A (en) 1981-01-14

Family

ID=13701090

Family Applications (1)

Application Number Title Priority Date Filing Date
JP7982979A Pending JPS563700A (en) 1979-06-25 1979-06-25 Solder exfoliation electrolyte

Country Status (1)

Country Link
JP (1) JPS563700A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2023157540A1 (en) 2022-02-16 2023-08-24 株式会社エアレックス Continuous decontamination and sterilization apparatus

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2023157540A1 (en) 2022-02-16 2023-08-24 株式会社エアレックス Continuous decontamination and sterilization apparatus

Similar Documents

Publication Publication Date Title
JPS5271000A (en) Production of hydrogen peroxide
JPS5323939A (en) Preparation of divalent phenols
JPS5297394A (en) Removal of organic matter in phosphoric acid
JPS563700A (en) Solder exfoliation electrolyte
IT7925016A0 (en) PROCEDURE FOR PRODUCING HYDROGEN AND SULFURIC ACID BY ELECTROCHEMICAL DECOMPOSITION OF AN ELECTROLYTE, AS WELL AS AN ELECTRODE TO IMPLEMENT THE ELECTROCHEMICAL DECOMPOSITION.
JPS536213A (en) Carbon electrode coated with antioxidant for al electrolysis
JPS57171979A (en) Preparation of 5-fluorocytosine salt
JPS527819A (en) Process for smooth electrodeposition of copper
JPS52103396A (en) Production of wet process phosphoric acid
JPS52127496A (en) Removal of trace amounts of halogen in sulfuric acid
JPS574951A (en) Synthesizing method of acrylamide
ES8301831A1 (en) "Process for preparing hydrofluoric acid from fluorine-containing organic compounds"
SU1045049A2 (en) Method of part running-in
JPS54137478A (en) Ozone removal
JPS5295100A (en) Improvement of cellulose insulator
JPS5740434A (en) Preparative method of difluorobromoacetyl fluoride
JPS5227739A (en) Process for preparation of 3-substituted or non-substituted-4-hydroxyb enzaldehyde by electrolytic oxidation
JPS5578021A (en) Anion exchange membrane
JPS52119487A (en) Removal of nitrogen oxide in exhaust gas
JPS55145184A (en) Manufacture of ketazines
JPS545889A (en) Cation exchange membrane and method of fabricating the same and electrolysis method of using the same
JPS52143971A (en) Treatment of exhaust gas containing hydrogen fluorid e etc.
JPS55119491A (en) Removing method for hydrazine in dilute water solution
JPS53119779A (en) Removing method for hydrogen sulfide and ammonia in gas of high temperature
JPS5297390A (en) Removal of sulfate ion in phosphoric acid