JPS5633193A - Preventing method for strain ageing embrittlement of weld zone of low alloy steel - Google Patents
Preventing method for strain ageing embrittlement of weld zone of low alloy steelInfo
- Publication number
- JPS5633193A JPS5633193A JP10721079A JP10721079A JPS5633193A JP S5633193 A JPS5633193 A JP S5633193A JP 10721079 A JP10721079 A JP 10721079A JP 10721079 A JP10721079 A JP 10721079A JP S5633193 A JPS5633193 A JP S5633193A
- Authority
- JP
- Japan
- Prior art keywords
- weld
- alloy steel
- low alloy
- last
- welding
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To prevent the strain ageing embrittlement of weld bond part at the butt welding method of low alloy steel by carrying out the build up welding on the weld zone of the last layer and making the coarse crystalline grain minute.
CONSTITUTION: The coarse crystal grain 4 is left on the base material neighboring the weld boundary by the thermal influence of the last weld layer 3, on occasion of carrying out the butt welding 2 of the low alloy steel 1, such as Mn-Mo alloy. The build up welding 5 of maximum 80% for the width of the last weld bead, is carried out on the last welding layer 3 moreover, in order to make the coarse structure 4 minute. thus, embrittlement by the strain aging is prevented by improving the toughness.
COPYRIGHT: (C)1981,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10721079A JPS5633193A (en) | 1979-08-24 | 1979-08-24 | Preventing method for strain ageing embrittlement of weld zone of low alloy steel |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10721079A JPS5633193A (en) | 1979-08-24 | 1979-08-24 | Preventing method for strain ageing embrittlement of weld zone of low alloy steel |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5633193A true JPS5633193A (en) | 1981-04-03 |
Family
ID=14453266
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP10721079A Pending JPS5633193A (en) | 1979-08-24 | 1979-08-24 | Preventing method for strain ageing embrittlement of weld zone of low alloy steel |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5633193A (en) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS603997A (en) * | 1983-06-22 | 1985-01-10 | Tomoegumi Giken:Kk | Positioning device for work |
US4585917A (en) * | 1983-02-28 | 1986-04-29 | Ishikawajima-Harima Jukogyo Kabushiki Kaisha | Method for relieving residual stresses by build-up welding over outer surface of pipe |
US4588869A (en) * | 1983-02-28 | 1986-05-13 | Ishikawajima-Harima Jukogyo Kabushiki Kaisha | Method for relieving residual stresses by controlling weld heat input |
-
1979
- 1979-08-24 JP JP10721079A patent/JPS5633193A/en active Pending
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4585917A (en) * | 1983-02-28 | 1986-04-29 | Ishikawajima-Harima Jukogyo Kabushiki Kaisha | Method for relieving residual stresses by build-up welding over outer surface of pipe |
US4588869A (en) * | 1983-02-28 | 1986-05-13 | Ishikawajima-Harima Jukogyo Kabushiki Kaisha | Method for relieving residual stresses by controlling weld heat input |
JPS603997A (en) * | 1983-06-22 | 1985-01-10 | Tomoegumi Giken:Kk | Positioning device for work |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5431062A (en) | Manufacture of structure superior in stress corrosion cracking resistivity | |
JPS5751243A (en) | Steel products for welding | |
JPS5633193A (en) | Preventing method for strain ageing embrittlement of weld zone of low alloy steel | |
JPS542952A (en) | Method and apparatus for electron beam welding | |
JPS5241111A (en) | Refining type low alloy high tension steel having excellent toughness of welded part with large heat input | |
JPS5411846A (en) | Welding means with low weld crack susceptibility and method of making same | |
JPS577374A (en) | One side welding method for low temperature steel material | |
JPS5428243A (en) | Welder for fine grain and high toughness | |
JPS5317903A (en) | Manufacturing method of stator iron core | |
JPS55165285A (en) | Welding defect occurrence preventing method of high-frequency electric welding | |
JPS5362725A (en) | Welding structural steel with weld heat-affected zone of high toughness | |
JPS5447814A (en) | Hot rolled steel material for welding with superior resistance to inclusion opening crack in weld held heat-affected | |
JPS53119236A (en) | Highly effecient welding method to obtain bond zone of high toughness | |
JPS54109041A (en) | Electroslag welding method for thick metal | |
JPS54139844A (en) | Construction welding method for tank base plate | |
JPS53106355A (en) | Welding method for stainless steel material | |
JPS5775204A (en) | Preventing method for edge crack of austeniteferrite double phase stainless steel during hot process | |
JPS5666391A (en) | Manufacture of hard titanium clad steel by explosive cladding | |
Drews et al. | D. C. Plasma Welding of AlMg 4. 5 Mn | |
JPS5619994A (en) | Welding method of silicon steel strip | |
JPS56158295A (en) | Electrode for welding excellent in arc stability | |
JPS5492536A (en) | Submerged arc welding method | |
Artemov | Electron Beam Welding of 12 Kh 2 N 4 MA Steel Gears | |
JPS5636384A (en) | Welding method of spheroidal graphite cast iron | |
JPS5250907A (en) | Tool attached with super hard alloy and process for producing the tool |