JPS55148371A - Lead-acid battery with non-flowing electrolyte - Google Patents

Lead-acid battery with non-flowing electrolyte

Info

Publication number
JPS55148371A
JPS55148371A JP5728679A JP5728679A JPS55148371A JP S55148371 A JPS55148371 A JP S55148371A JP 5728679 A JP5728679 A JP 5728679A JP 5728679 A JP5728679 A JP 5728679A JP S55148371 A JPS55148371 A JP S55148371A
Authority
JP
Japan
Prior art keywords
electrode plate
active substance
small holes
electrode plates
electrolyte
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP5728679A
Other languages
Japanese (ja)
Inventor
Akio Watanabe
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Panasonic Holdings Corp
Original Assignee
Matsushita Electric Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Matsushita Electric Industrial Co Ltd filed Critical Matsushita Electric Industrial Co Ltd
Priority to JP5728679A priority Critical patent/JPS55148371A/en
Publication of JPS55148371A publication Critical patent/JPS55148371A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To enhance the utilization rate of active substance by improving the diffusion of electrolyte inside electrode plates by providing a great number of small holes in the surface of electrode plate in the direction of the right angle to the surface of the electrode plate. CONSTITUTION:The surface of the pasty active substance 4 filled in the lattice body 3 is provided with a great number of the small holes 5 drilled in the direction of the right angle to the surface, having a diameter of approximately 0.7mm., for example, to form an electrode plate. Then, the electrode plates are built up into a electrode plate group in such a manner that the distance between positive electrode plate and negative electrode plate is the same as or less than, or 1:1 or less, the thickness of the positive electrode plate. Thus, the electrolyte is secured within the small holes 5 and at the same time the diffusion effect toward the direction parallel with the electrode plates of electrolyte inside the electrode plates can also be secured, permitting the utilizing rate of the active substance to be raised.
JP5728679A 1979-05-10 1979-05-10 Lead-acid battery with non-flowing electrolyte Pending JPS55148371A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP5728679A JPS55148371A (en) 1979-05-10 1979-05-10 Lead-acid battery with non-flowing electrolyte

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP5728679A JPS55148371A (en) 1979-05-10 1979-05-10 Lead-acid battery with non-flowing electrolyte

Publications (1)

Publication Number Publication Date
JPS55148371A true JPS55148371A (en) 1980-11-18

Family

ID=13051293

Family Applications (1)

Application Number Title Priority Date Filing Date
JP5728679A Pending JPS55148371A (en) 1979-05-10 1979-05-10 Lead-acid battery with non-flowing electrolyte

Country Status (1)

Country Link
JP (1) JPS55148371A (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5935371A (en) * 1982-08-20 1984-02-27 Shin Kobe Electric Mach Co Ltd Retainer-type lead storage battery
JPS5935372A (en) * 1982-08-20 1984-02-27 Shin Kobe Electric Mach Co Ltd Retainer-type lead storage battery

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5935371A (en) * 1982-08-20 1984-02-27 Shin Kobe Electric Mach Co Ltd Retainer-type lead storage battery
JPS5935372A (en) * 1982-08-20 1984-02-27 Shin Kobe Electric Mach Co Ltd Retainer-type lead storage battery
JPH0328786B2 (en) * 1982-08-20 1991-04-22 Shin Kobe Electric Machinery
JPH0328785B2 (en) * 1982-08-20 1991-04-22 Shin Kobe Electric Machinery

Similar Documents

Publication Publication Date Title
GB884824A (en) Improvements in or relating to galvanic cells
JPS55148371A (en) Lead-acid battery with non-flowing electrolyte
JPS56143675A (en) Silver oxide battery
JPS5727570A (en) Lead battery
JPS57124866A (en) Closed type lead storage battery
GB1401837A (en) Electrochemical devices having solid electrolytes
JPS55133769A (en) Negative plate for lead-acid storage battery
GB1489730A (en) Electrochemical cell
JPS56156673A (en) Lithium solid battery
JPS5636863A (en) Lead storage battery
JPS55159571A (en) Lead-acid battery
JPS5787081A (en) Lead-acid battery
JPS5562672A (en) Nonaqueous electrolytic secondary cell
JPS55133768A (en) Battery
JPS5636871A (en) Battery
JPS56168368A (en) Lead acid battery
JPS55157870A (en) Solid electrolyte cell
GB1442945A (en) Primary cell
JPS5659463A (en) Battery
JPS56114282A (en) Pasted lead acid battery
JPS56141179A (en) Lead acid battery
JPS5439688A (en) Electrochemical cell
JPS566382A (en) Organic solvent cell
GB843367A (en) Improvements relating to galvanic cells
JPS55163778A (en) Solid electrolyte cell