JPS5453155A - Method of sealing the inner surface of existing conduit - Google Patents
Method of sealing the inner surface of existing conduitInfo
- Publication number
- JPS5453155A JPS5453155A JP12074777A JP12074777A JPS5453155A JP S5453155 A JPS5453155 A JP S5453155A JP 12074777 A JP12074777 A JP 12074777A JP 12074777 A JP12074777 A JP 12074777A JP S5453155 A JPS5453155 A JP S5453155A
- Authority
- JP
- Japan
- Prior art keywords
- liquid
- sealant
- gas
- conduit
- parts
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: A fluid of gas-liquid mixed phase consisting of a liquid sealant and a conveying gas is passed through existing conduits under specific conditions, thereby enabling the easy and sure application of the sealant to the parts to be sealed and reducing the amount of the liquid sealant employed.
CONSTITUTION: Blowers 3, 4 are connected to existing conduits 1 having vertically curved parts. A liquid sealant is supplied from tank 5 to mixer 6 to form a fluid of gas-liquid mix phase consisting a conveying gas and the liquid sealant, which is passed through conduit 1 at such a high speed as to form circulating or spraying flows. The sealant is filled and accumulated on the depression parts such as cracks or holes to be sealed by roughening the inner surface of the conduit and the surface is smoothened. The excess shealant is recovered through a gas-liquid separator provided on the way of exhausting path or recycled through mixer 6
COPYRIGHT: (C)1979,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP52120747A JPS5811263B2 (en) | 1977-10-05 | 1977-10-05 | Internal sealing method for existing conduits |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP52120747A JPS5811263B2 (en) | 1977-10-05 | 1977-10-05 | Internal sealing method for existing conduits |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5453155A true JPS5453155A (en) | 1979-04-26 |
JPS5811263B2 JPS5811263B2 (en) | 1983-03-02 |
Family
ID=14793972
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP52120747A Expired JPS5811263B2 (en) | 1977-10-05 | 1977-10-05 | Internal sealing method for existing conduits |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5811263B2 (en) |
Cited By (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5640467A (en) * | 1979-09-07 | 1981-04-16 | Osaka Gas Co Ltd | Coating method of inner surface of arranged pipe |
JPS58193775A (en) * | 1982-04-30 | 1983-11-11 | Hakko Co Ltd | Repairing method of inside surface of installed pipe |
JPS58193776A (en) * | 1982-04-30 | 1983-11-11 | Hakko Co Ltd | Repairing method of inside surface of installed pipe |
JPS6012178A (en) * | 1983-06-29 | 1985-01-22 | Yonden Eng Kk | Method for blocking pinhole of pipe |
JPS63296868A (en) * | 1987-05-28 | 1988-12-02 | Osame Kogyo:Kk | Method for painting interior of permeable fine gap |
JP2006342337A (en) * | 2005-05-09 | 2006-12-21 | Osaka Gas Co Ltd | Sealing agent suppressing leakage and method for sealing |
JP2006342960A (en) * | 2005-05-09 | 2006-12-21 | Osaka Gas Co Ltd | Leakage preventing and sealing method |
JP2019163792A (en) * | 2018-03-19 | 2019-09-26 | 富士電機株式会社 | Leak mending method, light irradiation device for leak mending and photo-curing type resin |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP5796920B1 (en) * | 2015-05-18 | 2015-10-21 | 日本リニューアル株式会社 | Lining method |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5431622A (en) * | 1977-08-16 | 1979-03-08 | Osaka Gas Co Ltd | Treatment of inside surface of conduit installed |
-
1977
- 1977-10-05 JP JP52120747A patent/JPS5811263B2/en not_active Expired
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5431622A (en) * | 1977-08-16 | 1979-03-08 | Osaka Gas Co Ltd | Treatment of inside surface of conduit installed |
Cited By (11)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5640467A (en) * | 1979-09-07 | 1981-04-16 | Osaka Gas Co Ltd | Coating method of inner surface of arranged pipe |
JPS58193775A (en) * | 1982-04-30 | 1983-11-11 | Hakko Co Ltd | Repairing method of inside surface of installed pipe |
JPS58193776A (en) * | 1982-04-30 | 1983-11-11 | Hakko Co Ltd | Repairing method of inside surface of installed pipe |
JPH0139832B2 (en) * | 1982-04-30 | 1989-08-23 | Hatsukoo Kk | |
JPH0139833B2 (en) * | 1982-04-30 | 1989-08-23 | Hatsukoo Kk | |
JPS6012178A (en) * | 1983-06-29 | 1985-01-22 | Yonden Eng Kk | Method for blocking pinhole of pipe |
JPS63116B2 (en) * | 1983-06-29 | 1988-01-05 | Yonden Enjiniaringu Kk | |
JPS63296868A (en) * | 1987-05-28 | 1988-12-02 | Osame Kogyo:Kk | Method for painting interior of permeable fine gap |
JP2006342337A (en) * | 2005-05-09 | 2006-12-21 | Osaka Gas Co Ltd | Sealing agent suppressing leakage and method for sealing |
JP2006342960A (en) * | 2005-05-09 | 2006-12-21 | Osaka Gas Co Ltd | Leakage preventing and sealing method |
JP2019163792A (en) * | 2018-03-19 | 2019-09-26 | 富士電機株式会社 | Leak mending method, light irradiation device for leak mending and photo-curing type resin |
Also Published As
Publication number | Publication date |
---|---|
JPS5811263B2 (en) | 1983-03-02 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5453155A (en) | Method of sealing the inner surface of existing conduit | |
JPS5431622A (en) | Treatment of inside surface of conduit installed | |
ES8704249A1 (en) | Homogenizing device for a fluid transported in a conduit. | |
JPS523985A (en) | Cylinder using two kinds of fluid | |
JPS5275896A (en) | Means for mixing water and chemical for chemical extinguishing system | |
JPS52122901A (en) | Multi-functional circulation pump | |
JPS57177331A (en) | Removal of hydrogen sulfide | |
JPS5431623A (en) | Sealing-up of conduit installed | |
JPS5226623A (en) | Convering method of pipe | |
JPS5343149A (en) | Sealing method of guide vane of fluid machine | |
JPS51128707A (en) | Shaft sealing apparatus for turbo compressor | |
JPS5293803A (en) | Method of removing attachments from boilers and heat exchangers | |
JPS5344909A (en) | Fluid pressurizing apparatus | |
JPS55109439A (en) | Vapor-liquid contact apparatus | |
JPS52104464A (en) | Vapor-liquid contacting apparatus | |
JPS527787A (en) | Method for detecting leakage of tank or transportation pipe | |
JPS5232122A (en) | Increasing method of water tight efficiency in jointing parts of pipes in sea water | |
JPS5326384A (en) | Defoaming of aerobic cultivation tank | |
JPS531789A (en) | Sealing plug | |
JPS51129924A (en) | Apparatus for forming a branch pipe to main pipe | |
JPS5245727A (en) | Connecting method of liquid conduit | |
JPS5283990A (en) | Method and apparatus for separating bubbles from fermentation liquid | |
JPS5495317A (en) | Cooler for transformer cooler | |
JPS54138867A (en) | Gas-liquid contact apparatus | |
JPS5426503A (en) | Preventive method of cabitation and the device of same |