JPH0977137A - Laminated plastic bottle - Google Patents
Laminated plastic bottleInfo
- Publication number
- JPH0977137A JPH0977137A JP23546395A JP23546395A JPH0977137A JP H0977137 A JPH0977137 A JP H0977137A JP 23546395 A JP23546395 A JP 23546395A JP 23546395 A JP23546395 A JP 23546395A JP H0977137 A JPH0977137 A JP H0977137A
- Authority
- JP
- Japan
- Prior art keywords
- inner layer
- plastic bottle
- laminated plastic
- bottle
- outer layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
【0001】[0001]
【発明の属する技術分野】本発明は、内容物の減少に伴
って内側層が外側層から剥離し収縮する積層プラスチッ
クボトルに関するものである。BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a laminated plastic bottle in which an inner layer separates from an outer layer and shrinks as the content of the bottle decreases.
【0002】[0002]
【従来の技術】この種の積層プラスチックボトルとして
は、本出願人が先に出願を行い既に出願公開された特開
平4−339759号公報や特開平5−310265号
公報等に記載されたものがある。2. Description of the Related Art As laminated plastic bottles of this type, those disclosed in Japanese Patent Application Laid-Open No. 4-339759 and Japanese Patent Application Laid-Open No. 5-310265, which the applicant of the present application filed earlier and have already published. is there.
【0003】この積層プラスチックボトルは、外側層の
内側に内側層が剥離可能に積層されていて、外側層と内
側層の一部が接合されて構成されている。外側層と内側
層とを接合する接合部の設置位置については種々考えら
れているが、その一つの形態として、積層プラスチック
ボトルの軸線方向に沿って一直線に接合部を設けたもの
がある。In this laminated plastic bottle, an inner layer is releasably laminated inside an outer layer, and the outer layer and a part of the inner layer are joined together. Various installation positions of the joint portion for joining the outer layer and the inner layer have been considered, and as one form thereof, there is one in which the joint portion is provided in a straight line along the axial direction of the laminated plastic bottle.
【0004】[0004]
【発明が解決しようとする課題】図3は、軸線方向に沿
って直線的に延びる接合部33を1つだけ有する積層プ
ラスチックボトル30の横断面図である。この積層プラ
スチックボトルにおいて内側層32が外側層31から剥
離し収縮するためには、外側層31と内側層32の間に
空気を流入させなければならない。そのために、積層プ
ラスチックボトルの口筒部35の外側層31に空気孔3
4を設けている。FIG. 3 is a cross-sectional view of a laminated plastic bottle 30 having only one joint 33 extending linearly along the axial direction. In order for the inner layer 32 to separate from the outer layer 31 and contract in this laminated plastic bottle, air must be introduced between the outer layer 31 and the inner layer 32. Therefore, the air holes 3 are formed in the outer layer 31 of the mouth tube portion 35 of the laminated plastic bottle.
4 are provided.
【0005】ところで、この積層プラスチックボトルは
通常、以下に記載する方法で製造されている。初めに、
製造すべき積層プラスチックボトルに対応する積層構造
を備えた積層パリソンあるいは積層プリフォーム(以
下、積層パリソン等という)を押出成形等の手段で成形
し、この成形の際に、軸線方向に沿って延びる接合部を
所定の位置に設け、接合部以外では外側層と内側層とを
剥離可能にしておく。そして、この積層パリソン等を金
型にセットし、ブロー成形法によって所望のボトル形状
に成形する。そして、このようにボトル形状に成形した
後に、外側層31に空気孔34をパンチ等によって穿設
している。By the way, this laminated plastic bottle is usually manufactured by the method described below. at first,
A laminated parison or laminated preform (hereinafter referred to as laminated parison) having a laminated structure corresponding to the laminated plastic bottle to be manufactured is molded by means of extrusion molding or the like, and at the time of this molding, it extends along the axial direction. The joint portion is provided at a predetermined position so that the outer layer and the inner layer can be separated except for the joint portion. Then, this laminated parison or the like is set in a mold and molded into a desired bottle shape by a blow molding method. Then, after forming into a bottle shape in this manner, air holes 34 are punched in the outer layer 31.
【0006】ここで、空気孔34から確実に空気を流入
させるためには、空気孔34の位置を接合部33からず
らす必要がある。空気孔34の径が接合部33の横幅と
同寸法かあるいはそれよりも小さい場合に図4の平面図
に示すように接合部33と空気孔34とを重複させる
と、結果的に空気孔34が塞がれた状態になって、外側
層31と内側層32の間に空気が流入しなくなり、内側
層32を収縮せしめることができなくなるからである。Here, in order to ensure that the air flows in through the air holes 34, it is necessary to shift the positions of the air holes 34 from the joint portion 33. When the diameter of the air hole 34 is equal to or smaller than the lateral width of the joint portion 33 and the joint portion 33 and the air hole 34 are overlapped as shown in the plan view of FIG. This is because the air is blocked and air does not flow between the outer layer 31 and the inner layer 32, so that the inner layer 32 cannot be contracted.
【0007】しかしながら、従来の積層プラスチックボ
トルにおいては、特に接合部の位置を示すような目印は
なく、空気孔34を接合部33に重複させて穿設してし
まう場合があった。However, in the conventional laminated plastic bottle, there is no particular mark for indicating the position of the joint portion, and the air hole 34 may be formed so as to overlap the joint portion 33.
【0008】本発明はこのような従来の技術の問題点に
鑑みてなされたものであり、空気孔を接合部からずらし
た位置に確実に設けることができる積層プラスチックボ
トルを提供することを目的とする。The present invention has been made in view of the above problems of the prior art, and an object of the present invention is to provide a laminated plastic bottle in which air holes can be surely provided at positions displaced from the joint portion. To do.
【0009】[0009]
【課題を解決するための手段】本発明は前記課題を解決
するために、以下の手段を採用した。本発明は、互いに
剥離可能に積層された内側層と外側層の少なくとも2層
を備え、この内側層と外側層の一部が接着層によって接
合されており、外面には、ボトル形状に成形する際に形
成された凸部または凹部からなるマーキングが設けられ
ていることを特徴とする積層プラスチックボトルである
(請求項1に対応)。The present invention adopts the following means in order to solve the above problems. The present invention comprises at least two layers, an inner layer and an outer layer, which are releasably laminated to each other, a part of the inner layer and the outer layer are joined by an adhesive layer, and the outer surface is molded into a bottle shape. The laminated plastic bottle is provided with a marking formed of a convex portion or a concave portion formed at that time (corresponding to claim 1).
【0010】本発明の積層プラスチックボトルでは、内
容物の減少に伴って内側層が外側層から剥離し収縮す
る。内側層が収縮する際に空気孔から外側層と内側層と
の間に空気が流入し、これによって内側層はスムーズに
収縮することとなる。In the laminated plastic bottle of the present invention, the inner layer peels from the outer layer and shrinks as the content decreases. When the inner layer contracts, air flows from the air holes between the outer layer and the inner layer, whereby the inner layer contracts smoothly.
【0011】外面に設けたマーキングによって、積層プ
ラスチックボトルの周方向あるいは軸線方向の位置を確
実に認識でき、マーキングの位置を基準にして空気孔の
位置を設定することにより、接合部と空気孔の位置を確
実にずらして設けることが可能となる。The marking provided on the outer surface enables the position of the laminated plastic bottle in the circumferential direction or the axial direction to be surely recognized, and by setting the position of the air hole with reference to the position of the marking, the joint portion and the air hole can be separated from each other. It is possible to surely shift the position.
【0012】ボトル形状に成形する際にマーキングが形
成されるので、接合部とマーキングとの相互位置関係が
明確である。Since the marking is formed when molding into a bottle shape, the mutual positional relationship between the joint portion and the marking is clear.
【0013】積層プラスチックボトルの横断面形状には
特に限定はなく、円形、楕円形、矩形等、種々の形状が
採用可能である。The cross-sectional shape of the laminated plastic bottle is not particularly limited, and various shapes such as a circle, an ellipse and a rectangle can be adopted.
【0014】接合部は、積層プラスチックボトルの軸線
方向に沿って直線的に設けてもよいし(請求項2に対
応)、あるいは周方向に環状に設けてもよいし、ボトル
の胴部あるいは口筒部にスポット的に設けてもよい。The joint portion may be provided linearly along the axial direction of the laminated plastic bottle (corresponding to claim 2), or may be provided annularly in the circumferential direction, or the body or mouth of the bottle. It may be provided on the cylindrical portion as a spot.
【0015】空気孔は、積層プラスチックボトルの口筒
部、胴部、底部等、いずれの位置に設けても構わない。
マーキングは、接合部と一致する位置に設けてもよい
し、ずらした位置に設けてもよい。The air holes may be provided at any position such as the mouth cylinder, the body and the bottom of the laminated plastic bottle.
The marking may be provided at a position that coincides with the joining portion, or may be provided at a shifted position.
【0016】〈本発明の原材料〉外側層は例えば高密度
ポリエチレンで構成することができ、内側層は例えばナ
イロンで構成することができ、外側層と内側層を例えば
三井石油化学工業株式会社製の商品名「アドマー」で接
合することによって接合部を構成することができる。
尚、内側層にナイロンを採用した場合、ナイロンは水分
透過性が高いので、ナイロンの内側にガスバリヤ性に富
む他の樹脂からなる層(「アドマー」等)を積層して内
側層とし、内側層の水分透過性を減少せしめることも可
能である。<Raw material of the present invention> The outer layer can be made of, for example, high-density polyethylene, the inner layer can be made of, for example, nylon, and the outer layer and the inner layer can be made of, for example, Mitsui Petrochemical Industry Co., Ltd. The joint portion can be formed by joining with the product name “Admer”.
When nylon is used for the inner layer, nylon has a high water permeability, so a layer made of another resin with a high gas barrier property (such as "Admer") is laminated on the inner side of the nylon to form the inner layer. It is also possible to reduce the water permeability of the.
【0017】但し、接合部を形成するための接着剤、外
側層、内側層の原材料は上記の例に限るものではない。However, the raw materials for the adhesive, the outer layer, and the inner layer for forming the joint are not limited to the above examples.
【0018】[0018]
【発明の実施の形態】以下、本発明の実施の一形態を図
1及び図2の図面に基き、図3を援用して説明する。BEST MODE FOR CARRYING OUT THE INVENTION An embodiment of the present invention will be described below with reference to FIGS. 1 and 2 and with reference to FIG.
【0019】図1は本発明による積層プラスチックボト
ル(以下、ボトルと略称する)の外観斜視図であり、図
2は同平面図、図3は胴部の横断面図である。ボトル1
は、断面楕円形をなす胴部2と、胴部2の上部に連なる
肩部3と、肩部3の中央から上方に起立して延びる円筒
状の口筒部4とを備えている。ボトル1は、口筒部4か
ら胴部2の底部5に至るまでその全体が、外側層11と
内側層12とを積層して構成されている。外側層11と
内側層12は、1本の帯状の接合部13において互いに
接合されているが、接合部13以外の部位では外側層1
1と内側層12が当接しているだけで剥離可能になって
いる。図3は内側層12が外側層11から剥離する前の
状態を示している。FIG. 1 is an external perspective view of a laminated plastic bottle (hereinafter abbreviated as a bottle) according to the present invention, FIG. 2 is a plan view of the same, and FIG. 3 is a transverse sectional view of a body. Bottle 1
Includes a body portion 2 having an elliptical cross section, a shoulder portion 3 connected to the upper portion of the body portion 2, and a cylindrical mouth tube portion 4 extending upright from the center of the shoulder portion 3 to extend upward. The bottle 1 is entirely configured by laminating an outer layer 11 and an inner layer 12 from the mouth tube portion 4 to the bottom portion 5 of the body portion 2. The outer layer 11 and the inner layer 12 are bonded to each other at a single band-shaped bonding portion 13, but at portions other than the bonding portion 13, the outer layer 1
1 and the inner layer 12 are in contact with each other and can be peeled off. FIG. 3 shows a state before the inner layer 12 is separated from the outer layer 11.
【0020】接合部13は口筒部4の先端から胴部2の
下縁に至るまでボトル1の軸線方向に沿って直線的に延
び、底部5の中心まで延びている。ボトル1の口筒部4
における外側層11には、接合部13から周方向180
度離れた部位に空気孔14が設けられている。空気孔1
4は外側層11だけを貫通しており、内側層12には貫
通していない。The joint portion 13 extends linearly along the axial direction of the bottle 1 from the tip of the mouth tube portion 4 to the lower edge of the body portion 2, and extends to the center of the bottom portion 5. Mouth tube part 4 of bottle 1
The outer layer 11 in the
An air hole 14 is provided at a position apart from each other. Air hole 1
4 penetrates only the outer layer 11 and does not penetrate the inner layer 12.
【0021】又、肩部3の外面には、接合部13及び空
気孔14から周方向に90度離れた位置に、周方向位置
決め用マーキングとしての3つの小さな突起(凸部)1
5が並んで形成されている。換言すると、平面的に見た
場合に、突起15に対して周方向に右90度離れた位置
に接合部13が設けられ、突起15に対して周方向に左
90度離れた位置に空気孔14が設けられている。Further, on the outer surface of the shoulder portion 3, three small protrusions (projections) 1 as circumferential positioning markings are provided at positions 90 degrees apart from the joint portion 13 and the air holes 14 in the circumferential direction.
5 are formed side by side. In other words, when viewed two-dimensionally, the joint portion 13 is provided at a position that is 90 degrees to the right in the circumferential direction with respect to the protrusion 15, and the air hole is 90 degrees to the left in the circumferential direction with respect to the protrusion 15. 14 are provided.
【0022】このボトル1では、口筒部4に図示しない
注出ポンプを装着し、注出ポンプの吸い上げ管を口筒部
4から内側層12内に挿入して、内側層12の内部に収
容した内容物をポンプアップし注出する。In this bottle 1, a spout pump (not shown) is attached to the mouth cylinder part 4, and a suction pipe of the spout pump is inserted from the mouth cylinder part 4 into the inner layer 12 so as to be housed inside the inner layer 12. Pump up and pour out the contents.
【0023】内側層12内の内容物の減少に伴い、内側
層12が外側層11から剥離し収縮する。内側層12の
いずれの部位から剥離、収縮が始まるかは内側層12の
肉厚分布によって決まるが、通常は接合部13から離れ
た位置から始まる。内側層12が収縮する際には、空気
孔14から外側層11と内側層12との間に空気が流入
し、内側層12の収縮を確実且つスムーズにする。As the content in the inner layer 12 decreases, the inner layer 12 separates from the outer layer 11 and shrinks. From which portion of the inner layer 12 the peeling and shrinkage start depends on the thickness distribution of the inner layer 12, but usually it starts from a position away from the joint 13. When the inner layer 12 contracts, air flows from the air holes 14 between the outer layer 11 and the inner layer 12 to surely and smoothly contract the inner layer 12.
【0024】〔ボトル本体の製造方法〕ボトル1は次の
ようにして製造する。初めに、製造すべきボトルに対応
する積層構造を備えた積層パリソンあるいは積層プリフ
ォーム(以下、積層パリソン等という)を押出成形等の
手段で成形する。積層パリソン等を成形する際に、軸線
方向に沿って延びる接合部を所定の位置にその全長に亙
って設け、接合部以外では外側層と内側層とを剥離可能
にしておく。[Manufacturing Method of Bottle Main Body] The bottle 1 is manufactured as follows. First, a laminated parison or laminated preform (hereinafter, referred to as laminated parison) having a laminated structure corresponding to the bottle to be manufactured is molded by means of extrusion molding or the like. When molding a laminated parison or the like, a joint portion extending along the axial direction is provided at a predetermined position over the entire length thereof, and the outer layer and the inner layer can be separated except for the joint portion.
【0025】そして、この積層パリソン等をブロー成形
金型にセットし、ブロー成形法によって所望のボトル形
状に成形する。ブロー成形金型には、平面視楕円形をな
すボトル1の肩部3の成形面の短軸側に3つの小さな凹
部を設けておく。この凹部は周方向位置決めマーキング
用の突起15を成形するためのものであり、ブロー成形
時に外側層がこの凹部に押し込まれることにより突起1
5が形成される。Then, the laminated parison and the like are set in a blow molding die and molded into a desired bottle shape by a blow molding method. The blow molding die is provided with three small recesses on the minor axis side of the molding surface of the shoulder portion 3 of the bottle 1 having an elliptical shape in plan view. This concave portion is for molding the projection 15 for circumferential positioning marking, and the outer layer is pushed into this concave portion during blow molding, so that the projection 1 is formed.
5 is formed.
【0026】そして、積層パリソン等を金型にセットす
る際に、積層パリソン等の接合部が楕円形をなす肩部3
の成形面の長軸側に位置するようにセットすると、突起
15を接合部13から周方向に90度離れた位置に成形
することができる。When the laminated parison or the like is set in the mold, the shoulder portion 3 in which the joint of the laminated parison or the like has an elliptical shape.
When the protrusion 15 is set so as to be positioned on the long axis side of the molding surface, the protrusion 15 can be molded at a position separated from the joint portion 13 by 90 degrees in the circumferential direction.
【0027】このようにボトル形状にブロー成形した後
に、パンチ等の手段により口筒部4における外側層11
に空気孔14を穿設する。その際に、平面的に見て突起
15を手前側にし、突起15から周方向に左90度離れ
た位置の口筒部4に空気孔14を穿設すると、空気孔1
4を接合部13とは反対側(周方向に180度離れた位
置)に位置せしめることができ、接合部13と空気孔1
4とが重複して位置するのを確実に回避することができ
る。After blow molding into a bottle shape in this way, the outer layer 11 in the mouth tube portion 4 is punched or otherwise.
An air hole 14 is formed in the hole. At that time, when the projection 15 is located on the front side when viewed two-dimensionally and the air hole 14 is formed in the mouth tube portion 4 at a position left 90 degrees from the projection 15 in the circumferential direction, the air hole 1
4 can be located on the side opposite to the joint portion 13 (position 180 degrees apart in the circumferential direction).
It is possible to surely avoid overlapping of 4 and 4.
【0028】即ち、肩部3の突起15の位置が確認でき
れば、接合部13の位置が判別でき、突起15を基準に
して空気孔14の穿設位置を決定すると、接合部13と
空気孔14の設置位置を確実に離間せしめることができ
る。That is, if the position of the protrusion 15 of the shoulder portion 3 can be confirmed, the position of the joint portion 13 can be discriminated. If the position of the air hole 14 is determined with reference to the protrusion 15, the joint portion 13 and the air hole 14 are determined. The installation positions of can be reliably separated.
【0029】又、突起15を光センサ等によって検知す
るようにすれば、ボトル1を穿設装置にセットする際に
センサの検出信号に基づいてボトル1の姿勢を制御した
り、向きを制御することができ、自動生産ラインへの対
応も可能である。Further, if the projection 15 is detected by an optical sensor or the like, when the bottle 1 is set in the punching device, the attitude and orientation of the bottle 1 are controlled based on the detection signal of the sensor. It is also possible to support automatic production lines.
【0030】[0030]
【実施例】外側層11をポリエチレンで構成し、内側層
12をナイロンで構成し、外側層11と内側層12とを
アドマー(商品名、三井石油化学工業株式会社製)で接
合して接合部13を形成して、ボトル1を製造したとこ
ろ、良好な結果が得られた。EXAMPLE The outer layer 11 is made of polyethylene, the inner layer 12 is made of nylon, and the outer layer 11 and the inner layer 12 are joined by Admer (trade name, manufactured by Mitsui Petrochemical Industry Co., Ltd.). 13 was formed and bottle 1 was manufactured, and good results were obtained.
【0031】又、内側層12の水分透過性を減少せしめ
るために、ナイロン層の内側にアドマー層を積層して内
側層12を構成し、ボトル1を製造したところ、この場
合にも良好な結果が得られた。Further, in order to reduce the water permeability of the inner layer 12, the inner layer 12 was formed by laminating the Admer layer on the inner side of the nylon layer, and the bottle 1 was manufactured. In this case as well, good results were obtained. was gotten.
【0032】[0032]
【発明の効果】以上説明したように、本発明によれば、
積層プラスチックボトルの外面にマーキングを設けたの
で、マーキングの位置を基準にして空気孔の位置を設定
することにより、接合部と空気孔の位置を確実にずらし
て設けることができるという優れた効果が奏される。As described above, according to the present invention,
Since the marking is provided on the outer surface of the laminated plastic bottle, by setting the position of the air hole based on the position of the marking, the excellent effect that the position of the joint and the air hole can be surely shifted Played.
【0033】マーキングはボトル形状に成形する際に形
成されたものであるので、接合部とマーキングとの相互
位置関係が明確である。Since the marking is formed when molding into a bottle shape, the mutual positional relationship between the joint and the marking is clear.
【図1】 本発明の実施の一形態における積層プラスチ
ックボトルの外観斜視図である。FIG. 1 is an external perspective view of a laminated plastic bottle according to an embodiment of the present invention.
【図2】 本発明の実施の一形態における積層プラスチ
ックボトルの平面図である。FIG. 2 is a plan view of a laminated plastic bottle according to an embodiment of the present invention.
【図3】 本発明の実施の一形態における積層プラスチ
ックボトルの内側層収縮前を示す横断面図である。FIG. 3 is a cross-sectional view showing the laminated plastic bottle before shrinking the inner layer according to the embodiment of the present invention.
【図4】 接合部と空気孔とを重複した位置に設けた積
層プラスチックボトルの平面図である。FIG. 4 is a plan view of a laminated plastic bottle in which a joint portion and an air hole are provided at overlapping positions.
1 積層プラスチックボトル 11 外側層 12 内側層 13 接合部 14 空気孔 15 突起(マーキング) 1 Laminated plastic bottle 11 Outer layer 12 Inner layer 13 Joint part 14 Air hole 15 Protrusion (marking)
Claims (2)
側層の少なくとも2層を備え、この内側層と外側層の一
部が接着層によって接合されており、外面には、ボトル
形状に成形する際に形成された凸部または凹部からなる
マーキングが設けられていることを特徴とする積層プラ
スチックボトル。1. A laminate comprising at least two layers, an inner layer and an outer layer, which are releasably laminated to each other, wherein the inner layer and the outer layer are partially bonded by an adhesive layer, and the outer surface is molded into a bottle shape. A laminated plastic bottle, which is provided with a marking formed of a convex portion or a concave portion formed when the laminated plastic bottle is formed.
ることを特徴とする請求項1に記載の積層プラスチック
ボトル。2. The laminated plastic bottle according to claim 1, wherein the adhesive layer extends along the axial direction.