JPH0789342A - Formation of molding for window glass and installation method thereof - Google Patents

Formation of molding for window glass and installation method thereof

Info

Publication number
JPH0789342A
JPH0789342A JP5214735A JP21473593A JPH0789342A JP H0789342 A JPH0789342 A JP H0789342A JP 5214735 A JP5214735 A JP 5214735A JP 21473593 A JP21473593 A JP 21473593A JP H0789342 A JPH0789342 A JP H0789342A
Authority
JP
Japan
Prior art keywords
molding
window glass
product
mold
simulated part
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP5214735A
Other languages
Japanese (ja)
Inventor
Tetsuji Tamura
哲持 田村
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Katayama Kogyo Co Ltd
Original Assignee
Katayama Kogyo Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Katayama Kogyo Co Ltd filed Critical Katayama Kogyo Co Ltd
Priority to JP5214735A priority Critical patent/JPH0789342A/en
Publication of JPH0789342A publication Critical patent/JPH0789342A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To install a molding onto the window glass of an automobile and the like so as not to generate any deformation and the like. CONSTITUTION:After forming a simulated part (s) with the same shape as a real window glass except one longer side (s1) among four surroundings, a push out mold 2 is engaged with the adequate place on one side (s1) of the periphery of this simulated part and a required molding product 1B is formed so that the push out mold can be moved along the periphery of the simulated part, while pushing out a molding raw material from this mold under this condition, and thereafter, this molded product is taken out from the simulated part and installed onto the real window glass after cutting off its excessive length.

Description

【発明の詳細な説明】Detailed Description of the Invention

【0001】[0001]

【産業上の利用分野】本発明は、特定形状となされた自
動車などの窓ガラスに対して実施される窓ガラス用モー
ルの成形及び装着方法に関する。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a method of molding and mounting a window glass molding, which is carried out on a window glass of an automobile or the like having a specific shape.

【0002】[0002]

【従来の技術】自動車の窓ガラスにモールを装着する場
合は、従来では一般に次のように行われている。
2. Description of the Related Art Conventionally, when a molding is attached to a window glass of an automobile, it is generally performed as follows.

【0003】即ち、直線状に成形された図3(a)に示
すようなモールの押し出し品1を適当長さとなるように
切断した後、これの両端1a、1bを同図(b)に示す
ように熱溶着させて閉鎖環となし、これを窓ガラスの周
縁に嵌着するようになしている。
That is, after extruding a molding 1 having a linear shape as shown in FIG. 3 (a) to a proper length, both ends 1a, 1b thereof are shown in FIG. 3 (b). As described above, it is heat-welded to form a closed ring, which is fitted to the peripheral edge of the window glass.

【0004】[0004]

【発明が解決しようとする課題】上記した従来の方法で
は、窓ガラスに装着されたモールがガラスコーナー部で
痩せを生じて図4中に符号aで示す巾寸法が小さくなっ
たり、また本来では同図中の仮想線kの位置にあるべき
リップ1cが図示の如く倒れを生じることがあるのであ
る。
According to the above-mentioned conventional method, the molding attached to the window glass becomes thin at the glass corner portion and the width dimension indicated by the symbol a in FIG. The lip 1c, which should be at the position of the imaginary line k in the figure, may collapse as shown.

【0005】これを解消させるため図5に示すように、
窓ガラスwの周縁に押し出し型2を位置させ、これを同
周縁に沿わせて移動させることによりモール1Aを成形
しつつ窓ガラスwへ直接に装着する方法が提案されてい
る。
In order to eliminate this, as shown in FIG.
A method has been proposed in which the extrusion die 2 is positioned on the peripheral edge of the window glass w and is moved along the peripheral edge to directly mount the molding die 1A on the window glass w while molding.

【0006】しかし、この方法では押し出し型2からの
モール原料の押し出し開始点であるモール端とその押し
出し終了点であるモール端とを誤差なく奇麗に接続させ
ることが難しく、また窓ガラスwの板厚や外形にばらつ
きの生じることは避けられず、これがために押し出し型
2からモール原料が漏れ出し、図6に示すような不良部
bが形成されるのである。
However, according to this method, it is difficult to cleanly and accurately connect the molding end, which is the starting point of the extrusion of the molding material from the extrusion die 2, and the molding end, which is the ending point of the extrusion, and the plate of the window glass w. Inevitably, variations in thickness and outer shape occur, which causes the molding material to leak from the extrusion die 2 and form a defective portion b as shown in FIG.

【0007】本発明は、上記した問題点を生じさせるこ
となく自動車などの窓ガラスにモールを装着することを
目的とする。
An object of the present invention is to mount a molding on a window glass of an automobile or the like without causing the above problems.

【0008】[0008]

【課題を解決するための手段】図1は本発明の実施の様
子を示す説明図である。図に示すように、先ず四周囲の
うちの一辺s1を長くしたほかは実物窓ガラスw(図2
参照)の形状と異ならない擬似品sを形成する。
FIG. 1 is an explanatory view showing a mode for carrying out the present invention. As shown in the figure, the actual window glass w (Fig.
The dummy product s having the same shape as the reference (see) is formed.

【0009】このさい、長く設定すべき前記一辺s1は
実物窓ガラスwの成るべく長い辺を選択するのがよい。
また模擬品sの材料はガラスに限るものではなく、モー
ルの成形に適するものであれば差し支えない。
At this time, it is preferable that the one side s1 to be set long is selected to be the long side of the actual window glass w.
The material of the simulated product s is not limited to glass, and any material suitable for molding a molding may be used.

【0010】次に、この模擬品sの周縁の前記一辺s1
の適当個所に押し出し型2を係合させるのであり、通常
ではこの押し出し型2は同辺s1の概ね中央に位置され
る。
Next, the one side s1 of the periphery of the simulated product s
The extrusion die 2 is engaged with an appropriate portion of the extrusion die 2. Normally, the extrusion die 2 is located at the approximate center of the same side s1.

【0011】続いてこの状態の下で押し出し型2を、こ
れからモール原料を押し出しつつ模擬品sの周縁に沿っ
て移動させるようにする。このさい、押し出し型2は固
定しておいて模擬品sを回転変位させるようにするか若
しくはこれとは逆に模擬品sを固定しておいて押し出し
型2を周回変位させるようにするか、或いは押し出し型
2と模擬品sの双方を変位させるようにする。
Then, under this condition, the extrusion die 2 is moved along the peripheral edge of the imitation product s while extruding the molding raw material therefrom. At this time, the extrusion die 2 is fixed and the simulated product s is rotationally displaced, or conversely, the imitation product s is fixed and the extrusion die 2 is orbitally displaced. Alternatively, both the extrusion mold 2 and the simulated product s are displaced.

【0012】このようにして押し出し型2が模擬品sの
周縁をほぼ一周されると、所要のモール製品1Bが形成
されるのである。
In this way, when the extrusion die 2 is made to go around the periphery of the imitation product s almost once, the required molding product 1B is formed.

【0013】この後、このモール製品1Bを模擬品sか
ら取り外してその余分長部分を切り除き、その両端1
B’、1B”を従来同様に熱融着させて閉鎖環となし、
これを図2に示すように実物窓ガラスwに装着する。
After this, the molding product 1B is removed from the imitation product s, the extra long portion is cut off, and both ends 1 thereof are removed.
B'and 1B "are heat-fused as in the conventional case to form a closed ring,
This is attached to the actual window glass w as shown in FIG.

【0014】[0014]

【発明の効果】本発明によれば、モール製品は実物窓ガ
ラスに適合するように曲がった状態で一様断面に成形さ
れるものとなり、したがって実物窓ガラスに装着するさ
いに大きな変形を伴うことのないものとなって従来のよ
うな痩せとか、リップの倒れを生じるものとならない。
According to the present invention, the molding product is formed into a uniform cross-section in a bent state so as to fit the actual window glass, and therefore, a large deformation is involved when it is attached to the actual window glass. It doesn't cause the skin to lose weight and the lip collapses as in the past.

【0015】またモール製品の成形において模擬品を使
用することは、実物窓ガラスの板厚や外形のばらつきが
モール製品の成形に影響を及ぼすことを回避させ、確実
に良好な品質のモール製品と得ることを可能となす。
Further, the use of the simulated product in the molding of the molding product prevents the molding of the molding product from being affected by the variation in the plate thickness and the outer shape of the actual window glass, and ensures that the molding product has good quality. Makes it possible to obtain.

【図面の簡単な説明】[Brief description of drawings]

【図1】本発明の実施の様子を示す説明図である。FIG. 1 is an explanatory diagram showing how the present invention is implemented.

【図2】本発明を実施された実物窓ガラスである。FIG. 2 is a real window glass in which the present invention is implemented.

【図3】従来のモールを示す図である。FIG. 3 is a diagram showing a conventional molding.

【図4】従来例に係り、窓ガラスに装着された状態のモ
ールの断面図てある。
FIG. 4 is a cross-sectional view of a molding according to a conventional example, which is mounted on a window glass.

【図5】本発明に関連した技術に係り、モールの装着方
法を示す説明図である。
FIG. 5 is an explanatory diagram showing a method of mounting a mall according to a technique related to the present invention.

【図6】図5に示す装着方法で成形されたモールの断面
図である。
6 is a cross-sectional view of a molding formed by the mounting method shown in FIG.

【符号の説明】[Explanation of symbols]

s 擬似品 s1 一辺 w 窓ガラス 1B モール製品 2 押し出し型 s Fake product s1 Side w Window glass 1B Mall product 2 Extrusion type

Claims (1)

【特許請求の範囲】[Claims] 【請求項1】 四周囲のうちの一辺(s1)を長くした
ほかは実物窓ガラス(w)の形状と異ならない擬似品
(s)を形成した後、この模擬品(s)の周縁の前記一
辺(s1)の適当個所に押し出し型(2)を係合させ、
この状態の下で押し出し型(2)をこれからモール原料
を押し出しつつ模擬品(s)の周縁に沿って移動させる
ようにして所要のモール製品(1B)を成形し、その
後、このモール製品(1B)を模擬品(s)から取り外
してその余分長部分を切除し、これを実物窓ガラス
(w)に装着することを特徴とする窓ガラス用モールの
成形及び装着方法。
1. After forming a dummy product (s) which is not different from the shape of the actual window glass (w) except that one side (s1) of the four peripheries is elongated, the peripheral portion of the dummy product (s) is Engage the extrusion die (2) at an appropriate point on one side (s1),
Under this condition, the extrusion mold (2) is moved along the peripheral edge of the imitation product (s) while extruding the molding raw material from this, to mold the required molding product (1B), and then this molding product (1B). ) Is removed from the imitation product (s), the extra long portion is cut off, and this is attached to the actual window glass (w).
JP5214735A 1993-06-30 1993-06-30 Formation of molding for window glass and installation method thereof Pending JPH0789342A (en)