JP7382060B2 - Tile adhesion sheet and tile adhesion set - Google Patents

Tile adhesion sheet and tile adhesion set Download PDF

Info

Publication number
JP7382060B2
JP7382060B2 JP2019238072A JP2019238072A JP7382060B2 JP 7382060 B2 JP7382060 B2 JP 7382060B2 JP 2019238072 A JP2019238072 A JP 2019238072A JP 2019238072 A JP2019238072 A JP 2019238072A JP 7382060 B2 JP7382060 B2 JP 7382060B2
Authority
JP
Japan
Prior art keywords
sheet
tile
joint
base sheet
joint material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
JP2019238072A
Other languages
Japanese (ja)
Other versions
JP2021105314A (en
Inventor
伊織 藤垣
Original Assignee
藤垣窯業株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 藤垣窯業株式会社 filed Critical 藤垣窯業株式会社
Priority to JP2019238072A priority Critical patent/JP7382060B2/en
Publication of JP2021105314A publication Critical patent/JP2021105314A/en
Application granted granted Critical
Publication of JP7382060B2 publication Critical patent/JP7382060B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Description

本発明は、室内の壁面や家具の外表面等の被着面にタイルを貼着して装飾するためのタイル貼着シート及びタイル貼着セットに関する。 The present invention relates to a tile adhering sheet and a tile adhering set for adhering tiles to decorative surfaces such as indoor walls and the outer surfaces of furniture.

従来より、基材シートの表裏両面に粘着面を設けて両面粘着シートを形成し、その両面粘着シートの表面に複数のタイル片を接合すると共に裏面の粘着面を被着面に接合するようにしたタイル貼着シートがある(特許文献1参照)。
このタイル貼着シートは、タイル片の表面に透明シートが貼着されており、まず全部を被着面に貼り付けてから前記透明シートを剥がし、その後、タイル片の目地部に目地材を導入する、というものである。
Conventionally, adhesive surfaces are provided on both the front and back sides of a base sheet to form a double-sided adhesive sheet, and multiple tile pieces are bonded to the surface of the double-sided adhesive sheet, and the adhesive surface on the back side is bonded to the adhered surface. There is a tile adhesion sheet (see Patent Document 1).
This tile adhesive sheet has a transparent sheet pasted on the surface of the tile piece. First, the whole sheet is pasted on the surface to which it is attached, and then the transparent sheet is peeled off. Then, a grout material is introduced into the joint area of the tile piece. That is to do.

実登第3071347号公報(段落0019、図5)Jitto No. 3071347 (Paragraph 0019, Figure 5)

上記従来のタイル貼着シートは、被着面に貼り付けた後のタイル片の目地部に目地材を導入するようになっているが、従来の左官工事によるものと遜色のない仕上がりにするにはそれ相応の技量が必要である。目地部は、例えば幅約2mm、深さ約6mmというように、幅の割に奥行きがあり、そのような溝に目地材を均一に充填することが難しいためである。したがって、左官工事の経験のない一般需要者が綺麗な目地に仕上げることは困難であり、また、時間も掛かる。 The conventional tile adhesion sheet mentioned above is designed to introduce a joint material into the joints of the tile pieces after it is pasted on the surface to which it is attached, but it is difficult to achieve a finish that is comparable to that produced by conventional plastering. requires appropriate skill. This is because the joint portion has a depth relative to its width, for example, approximately 2 mm in width and approximately 6 mm in depth, and it is difficult to uniformly fill such a groove with the joint material. Therefore, it is difficult for general users with no experience in plastering to finish the joints neatly, and it also takes time.

本発明は、上記に鑑みなされたもので、その目的は、経験の浅い左官職人或は左官経験のない一般需要者でも本格的な目地を備えたタイルを簡単且つ綺麗に貼ることができるタイル貼着シート及びタイル貼着セットを提供することにある。 The present invention was made in view of the above, and its purpose is to provide a tile affixing method that allows even inexperienced plasterers or general users with no plastering experience to easily and neatly affix tiles with authentic joints. Our objective is to provide adhesive sheets and tile pasting sets.

上記の目的を達成するため本発明は、請求項1に記載したように、
面に貼着層を有するベースシートと、
そのベースシートの表面に所定の目地空間を設けて配列され且つそのベースシートの表面に貼着される複数のタイル片と、
前記ベースシートの表面に貼着される軟質樹脂シートと、を備えており、
前記軟質樹脂シートは、
前記タイル片の厚みより小さく且つ外寸が前記ベースシートとほぼ同じであって、
前記ベースシートに配列される前記タイル片の形状と配置に合わせて象った貫通額孔を有すると共にその表面に植物繊維その他の繊維を膠着させてなる吸水性を有する紙シートを貼着してなり、
前記目地空間に前記軟質樹脂シートで嵩上げされ且つ前記紙シートが溝底に臨む目地溝が形成されるようにしたタイル貼着シートを提供する。
In order to achieve the above object, the present invention, as stated in claim 1,
a base sheet having an adhesive layer on the back side ;
a plurality of tile pieces arranged on the surface of the base sheet with predetermined joint spaces and adhered to the surface of the base sheet;
a soft resin sheet affixed to the surface of the base sheet,
The soft resin sheet is
smaller than the thickness of the tile piece and having approximately the same outer dimensions as the base sheet,
The base sheet has a through-frame hole shaped to match the shape and arrangement of the tile pieces arranged on the base sheet, and a water-absorbing paper sheet made of vegetable fibers or other fibers is adhered to the surface of the hole. Become,
To provide a tile sticking sheet in which a joint groove is formed in the joint space by raising the joint space with the soft resin sheet and in which the paper sheet faces the groove bottom.

また、請求項2に記載したように、
請求項1に記載のタイル貼着シートと、
そのタイル貼着シートの前記目地溝に充填する可塑性を有する目地材と、を一揃いにしてなるタイル貼着セットを提供する。
Furthermore, as stated in claim 2,
The tile adhesive sheet according to claim 1;
To provide a tile sticking set comprising a joint material having plasticity to be filled into the joint grooves of the tile sticking sheet.

また、請求項3に記載したように、
請求項1に記載のタイル貼着シートと、
そのタイル貼着シートの前記目地溝に充填する目地材と、を一揃いにしてなり、
前記目地材は、水を含むことで可塑性を発揮するものであって、水を含む前の状態になっているタイル貼着セットを提供する。
Furthermore, as stated in claim 3,
The tile adhesive sheet according to claim 1;
and a joint material to be filled into the joint grooves of the tile adhesive sheet,
The joint material exhibits plasticity when it contains water, and the tile sticking set is provided in a state before it contains water.

また、請求項4に記載したように、前記目地材に加える所要量の水を密閉容器に入れて一揃いにした請求項3記載のタイル貼着セットを提供する。 Moreover, as described in claim 4, there is provided a tile sticking set according to claim 3, wherein a required amount of water to be added to the joint material is placed in a sealed container.

本発明のタイル貼着シートは、目地溝が軟質樹脂シートで嵩上げされて浅くなっているため、目地材を充填することが比較的容易であり、しかも目地材の必要量が軟質樹脂シート相当量だけ少なくて済む。一方、目地溝を浅くすると目地材が剥がれやすくなるが、目地溝の底(溝底)には吸水性を有する紙シートが臨んでいてその紙シートに目地材がへばりつくため、浅い目地溝でも目地材が剥がれ難い。したがって、左官経験が無い若しくは浅い者でも本格的な目地を備えたタイルを簡単且つ綺麗に貼ることができる。 In the tile adhesive sheet of the present invention, the joint grooves are raised with a soft resin sheet and made shallow, so it is relatively easy to fill with joint material, and the required amount of joint material is equivalent to the soft resin sheet. Only less is required. On the other hand, if the grooves are made shallow, the joint material will easily peel off, but since the water-absorbing paper sheet faces the bottom of the groove (groove bottom) and the joint material clings to that paper sheet, even shallow grooves will cause the joint material to peel off. The material is difficult to peel off. Therefore, even a person with little or no experience in plastering can easily and neatly affix tiles with authentic joints.

また、請求項2のタイル貼着セットによれば、前記タイル貼着シートと、可塑性を有する目地材とが一揃いになっているため、左官経験の無い一般需要者が、自宅の例えば壁面にタイル貼着シートを貼着し、そのタイル貼着シートの目地溝にセットの目地材を充填して本格的な目地を備えたタイルが簡単且つ綺麗に貼れる。 Further, according to the tile pasting set of claim 2, since the tile pasting sheet and the joint material having plasticity are included in one set, general users without plastering experience can use the tile pasting sheet for example on the walls of their homes. Tiles with full-fledged joints can be easily and neatly pasted by pasting a tile pasting sheet and filling the joint grooves of the tile pasting sheet with a set of joint material.

また、請求項3のタイル貼着セットによれば、前記タイル貼着シートと、水を含んで可塑性を発揮する目地材が、水を含む前の状態で一揃いになっているため、保管時に目地材が固化してしまうおそれがなく、しかも作業前に水を加えて混練するだけで可塑性を有する目地材ができるため、目地を備えたタイルが簡単且つ綺麗に貼れる。しかも、請求項4のタイル貼着セットでは、目地材に加える所要量の水が密閉容器に入れて一緒に揃えられているため、水の計量ミスによる目地材の硬軟に関する不良が起きにくい。 Further, according to the tile adhesion set of claim 3, the tile adhesion sheet and the joint material that contains water and exhibits plasticity are assembled together in a state before containing water, so that when stored, There is no risk of the joint material solidifying, and the joint material having plasticity can be created by simply adding water and kneading before work, so tiles with joints can be easily and neatly pasted. Moreover, in the tile sticking set of claim 4, since the required amount of water to be added to the joint material is placed together in a sealed container, defects related to hardness and softness of the joint material due to mistakes in measuring water are less likely to occur.

目地溝に目地材を充填した状態を示すタイル貼りシートの一部拡大図を含む全体斜視図である。FIG. 2 is an overall perspective view including a partially enlarged view of the tiled sheet showing a state in which the joint grooves are filled with a joint material. タイル貼りシートの分解斜視図である。FIG. 2 is an exploded perspective view of a tiled sheet. 図2のZ1、Z2、Z3の拡大図である。3 is an enlarged view of Z1, Z2, and Z3 in FIG. 2. FIG. 被着面に貼着して目地材を充填した状態を示す中間を省略したタイル貼りシートの拡大断面図である。FIG. 2 is an enlarged cross-sectional view of a tiled sheet with the middle portion omitted, showing a state in which it is adhered to a surface to be adhered and filled with a joint material. タイル貼着セットを示す斜視図である。It is a perspective view showing a tile pasting set.

以下に、本発明の実施の形態を図面を参照しつつ説明する。
実施形態のタイル貼着シート1は、ベースシート2と、複数のタイル片3,3…と、軟質樹脂シート4と、から概略構成され、タイル片3,3…同士の間に目地溝5を有する。
Embodiments of the present invention will be described below with reference to the drawings.
The tile sticking sheet 1 of the embodiment is roughly composed of a base sheet 2, a plurality of tile pieces 3, 3..., and a soft resin sheet 4, and has joint grooves 5 between the tile pieces 3, 3... have

[1.ベースシート]
前記ベースシート2は、例えば約150mm×150mmの四角い紙又は合成樹脂製の薄いシートであり、図4の拡大図に示したように、裏面と表面に粘着剤又は接着剤を塗布してなる貼着層6r,6fを有する。
[1. Base sheet]
The base sheet 2 is a thin sheet made of square paper or synthetic resin, for example, about 150 mm x 150 mm, and as shown in the enlarged view of FIG. It has deposited layers 6r and 6f.

[2.タイル片]
タイル片3は、陶磁器、ガラス、合成樹脂、金属、竹、木、石などで形成されている。また、タイル片3は、表面が装飾面で、裏面がほぼ平らな接合面になっており、前記べースシート2の表面に所定の目地空間7を設けて配列され且つそのベースシート2の表面に前記貼着層6fを介して貼着される。
実施形態のタイル片3は、表面に釉薬を施して焼成した陶磁製で、約23mm×23mm×6mmの四角い板状であり、前記ベースシート2の表面に約2mmの幅の目地空間7を設けて12個×12個配列されている。
なお、タイル片3,3…の目地空間7は、ベースシート2の角を挟んで隣合う二辺(図において右辺と上辺)にはない。これにより、複数のタイル貼着シート1,1…を横や上下に並べて連続させた場合に、タイル貼着シート1,1…同士の継ぎ目の目地空間7が二本分に連なる(太くなる)不具合を回避することができる。
[2. tile piece]
The tile piece 3 is made of ceramics, glass, synthetic resin, metal, bamboo, wood, stone, or the like. The tile pieces 3 have a decorative surface on the front surface and a substantially flat joint surface on the back surface, and are arranged with predetermined joint spaces 7 on the surface of the base sheet 2. It is attached via the adhesive layer 6f.
The tile piece 3 of the embodiment is made of ceramic whose surface is glazed and fired, and has a square plate shape of approximately 23 mm x 23 mm x 6 mm, and a joint space 7 of approximately 2 mm width is provided on the surface of the base sheet 2. 12 x 12 pieces are arranged.
Note that the joint spaces 7 of the tile pieces 3, 3, . As a result, when a plurality of tile-attached sheets 1, 1... are arranged horizontally or vertically in series, the joint space 7 at the joint between the tile-attached sheets 1, 1... becomes two lines long (thick). Problems can be avoided.

[3.軟質樹脂シート]
軟質樹脂シート4は、例えば軟質の塩化ビニル樹脂を主成分とする白色系のものであり、耐水性と適度な弾性を有する。この軟質樹脂シート4は、厚みがタイル片3の厚みより小さく、実施形態ではタイル片3の厚みのほぼ半分強(約3.5mm)である。軟質樹脂シート4は、外寸が前記ベースシート2とほぼ同じで、ベースシート2に配列される前記タイル片3,3…の形状と配置に合わせて象った貫通額孔9,9…を有しており、前記目地空間7の深さのほぼ半分強を埋める状態でベースシート2の表面の貼着層6f 貼着されている。
また、軟質樹脂シート4の表面には、図2に分解して示したように、植物繊維その他の繊維を膠着させてなる紙シート4Pが、例えば、エポキシ樹脂系、ウレタン樹脂系等の非水溶性の接着剤で貼着されている。この紙シート4Pは、植物繊維からなる一般的な紙はもちろん、合成樹脂繊維からなる不織布をも含むものであり、要は表面に繊維による微細な起伏と吸水性があればよい。
[3. Soft resin sheet]
The soft resin sheet 4 is, for example, a white sheet whose main component is soft vinyl chloride resin, and has water resistance and appropriate elasticity. The thickness of the soft resin sheet 4 is smaller than the thickness of the tile piece 3, and in the embodiment, it is approximately half the thickness of the tile piece 3 (approximately 3.5 mm). The soft resin sheet 4 has approximately the same outer dimensions as the base sheet 2, and has through-frame holes 9, 9 shaped to match the shape and arrangement of the tile pieces 3, 3, arranged on the base sheet 2. The adhesive layer 6f is attached to the surface of the base sheet 2 so as to fill approximately half of the depth of the joint space 7.
In addition, on the surface of the soft resin sheet 4, as shown in the exploded view in FIG. It is attached with adhesive. The paper sheet 4P includes not only general paper made of vegetable fibers but also nonwoven fabric made of synthetic resin fibers, and the important thing is that the surface has fine undulations and water absorption due to the fibers.

[4.目地溝]
目地溝5は、前記のようにタイル片3,3…同士の間の目地空間7に形成されており、深さが、前記軟質樹脂シート4により嵩上げされたことでタイル片3の厚みのほぼ半分弱(約2.5mm)程度になっている。また、目地溝5の溝底には、軟質樹脂シート4の表面に貼着された紙シート4Pが一面に臨んでおり、したがって目地溝5の溝底はほぼ紙シート4Pで覆われている。
[4. Grasshopper]
The joint grooves 5 are formed in the joint spaces 7 between the tile pieces 3, 3, . It is about a little less than half (approximately 2.5 mm). In addition, a paper sheet 4P stuck to the surface of the soft resin sheet 4 faces the bottom of the joint groove 5, so that the bottom of the joint groove 5 is almost covered with the paper sheet 4P.

[5.製造方法]
次に、実施形態のタイル貼着シート1の製造方法について説明する。なお、軟質樹脂シート4の表面には、図2の分解斜視図に示した紙シート4Pが予め接着されている。
[5. Production method]
Next, a method for manufacturing the tile adhesive sheet 1 of the embodiment will be described. Note that a paper sheet 4P shown in the exploded perspective view of FIG. 2 is adhered to the surface of the soft resin sheet 4 in advance.

まず、ベースシート2の表裏両面の貼着層6r,6fは、剥離可能な剥離紙(図示せず)で保護されている。そのため、表面の剥離紙を剥がしてその表面の貼着層6fに軟質樹脂シート4を貼着する。
次に、その軟質樹脂シート4の貫通額孔9,9…にタイル片3,3…を嵌めてベースシート2の貼着層6fに押し付ける。これによりタイル片3がベースシート2の表面に貼着層6fを介して貼着される。
こうして製造されたタイル貼着シート1は、ベースシート2の表面に貼着された全てのタイル片3,3…が軟質樹脂シート4の貫通額孔9,9…に殆ど隙間なく嵌っており、溝底に紙シート4Pが臨む浅い目地溝5がタイル片3,3…同士の間に開口している。
First, the adhesive layers 6r and 6f on both the front and back surfaces of the base sheet 2 are protected with peelable release paper (not shown). Therefore, the release paper on the surface is peeled off and the soft resin sheet 4 is adhered to the adhesive layer 6f on the surface.
Next, the tile pieces 3, 3... are fitted into the through-frame holes 9, 9... of the soft resin sheet 4 and pressed against the adhesive layer 6f of the base sheet 2. As a result, the tile piece 3 is adhered to the surface of the base sheet 2 via the adhesive layer 6f.
In the tile adhesion sheet 1 manufactured in this way, all the tile pieces 3, 3... adhered to the surface of the base sheet 2 fit into the through-frame holes 9, 9... of the soft resin sheet 4 with almost no gaps. A shallow joint groove 5 with a paper sheet 4P facing the groove bottom is opened between the tile pieces 3, 3....

[6.施工方法]
実施形態のタイル貼着シート1は、以上のような構成よりなるため、例えば建物室内の壁面等の被着面8に対して、ベースシート2の裏面の剥離紙を剥がして貼着層6rにより貼り付けることができる。
そして、水を含んだ状態で可塑性を有する周知のモルタル等の目地材10を、タイル貼着シート1の目地溝5に充填する。その際、目地溝5が軟質樹脂シート4による嵩上げ効果で浅くなっているため、目地材10を均一に且つ素早く充填することが可能であり、したがって従来に比べて格段に作業性がよい。
一方、目地溝5が浅いと、乾燥して固化した目地材10が剥がれやすくなるが、実施形態のタイル貼着シート1では、溝底に吸水性を有する紙シート4Pが臨んでいて、その紙シート4Pに目地材10がへばりつくため、浅い目地溝5でも剥がれ難い。紙シート4Pに接触した目地材10が繊維の起伏に馴染みつつ水分が紙シート4Pに吸収されていち早く固化するものと推測される。したがって、経験の浅い左官職人等でも本格的な目地を備えたタイルを簡単且つ綺麗に貼ることができる。
[6. Construction method】
Since the tile adhesion sheet 1 of the embodiment has the above-described configuration, the release paper on the back side of the base sheet 2 is peeled off and the adhesive layer 6r is applied to the adhesion surface 8 such as a wall inside a building. Can be pasted.
Then, the joint grooves 5 of the tile adhesive sheet 1 are filled with a water-containing joint material 10 such as well-known mortar that has plasticity. At this time, since the joint groove 5 is shallow due to the raising effect of the soft resin sheet 4, it is possible to fill the joint material 10 uniformly and quickly, and therefore the workability is much better than in the past.
On the other hand, if the joint groove 5 is shallow, the dried and solidified joint material 10 will easily peel off, but in the tile sticking sheet 1 of the embodiment, the water-absorbing paper sheet 4P faces the groove bottom, and the paper Since the joint material 10 sticks to the sheet 4P, it is difficult to peel off even in shallow joint grooves 5. It is presumed that the joint material 10 in contact with the paper sheet 4P adapts to the undulations of the fibers, absorbs moisture into the paper sheet 4P, and quickly solidifies. Therefore, even inexperienced plasterers can easily and neatly affix tiles with authentic joints.

[7.タイル貼着セット]
以上のように実施形態のタイル貼着シート1によれば、本格的な目地を備えたタイルを簡単且つ綺麗に貼ることができるが、図5に示したように、タイル貼着シート1と目地材10とを一揃いにしてタイル貼着セット11とすれば、手元に目地材10がない一般需要者でも、本格的な目地を備えたタイルを簡単且つ綺麗に貼ることができる。
このタイル貼着セット11の目地材10は、水を含んだ粘土のように、当初から可塑性を有する状態でタイル貼着シート1に添付しておけば、タイルの貼着及び目地溝5への目地材10の充填が最も手間なく行える。
しかし一方、当初から水を含ませた目地材10では、時間の経過と共に固化する可能性があるため、例えば乾燥させた粉末状の粘土を目地材10としてタイル貼着シート1に添付し、使用する直前に水を含ませるようにするとよい。この場合、目地材10に所要量の水を加えて混練する作業が別途必要になるが、流通・保管の段階で目地材10が固化するおそれがないため、長期間安定した品質を保つことができる。なお、目地材10を入れた容器は、そのまま目地材10を混練する容器としても使えるようになっている。
さらに、上記したタイル貼着セット11に、乾燥させた目地材10に加える所要量の水10wを密閉容器に入れて同梱するとよい。そうすることにより、目地材10に加える水10wの量が正確になるため、計量ミス等による目地材10の硬軟に関する不良が防止でき、目地材10の充填が失敗なく行える。
[7. Tile pasting set]
As described above, according to the tile sticking sheet 1 of the embodiment, tiles with full-scale joints can be easily and neatly pasted, but as shown in FIG. By combining the materials 10 and 10 to form a tile pasting set 11, even general users who do not have the joint material 10 on hand can easily and neatly paste tiles with full-fledged joints.
If the joint material 10 of this tile sticking set 11 is attached to the tile sticking sheet 1 in a plastic state from the beginning like water-containing clay, it will be easier to stick the tiles and fill the joint grooves 5. Filling of the joint material 10 can be performed with the least effort.
However, on the other hand, if the joint material 10 is moistened with water from the beginning, there is a possibility that it will harden over time. It is best to soak it in water just before cooking. In this case, it is necessary to separately add the required amount of water to the joint material 10 and knead it, but since there is no risk of the joint material 10 solidifying during distribution and storage, it is possible to maintain stable quality for a long period of time. can. Note that the container containing the joint material 10 can also be used as a container for kneading the joint material 10 as is.
Furthermore, it is preferable to package the above-described tile sticking set 11 with the required amount of water 10w to be added to the dried joint material 10 in a sealed container. By doing so, the amount of water 10w added to the joint filler 10 becomes accurate, so defects in hardness and softness of the joint filler 10 due to measurement errors can be prevented, and filling of the joint filler 10 can be performed without failure.

ところで、実施形態のタイル貼着シート1は、前記のように右辺と上辺に目地空間7が設けられていない。そのため、例えばこれを被着面8の右の縁や上の縁に配置する場合には、図4の断面図に示したように被着面8とタイル片3とのコーナー部分に目地材10を塗布して斜めに成形するとよい。 By the way, the tile sticking sheet 1 of the embodiment does not have the joint spaces 7 on the right side and the top side as described above. Therefore, for example, when placing this on the right edge or upper edge of the adherend surface 8, the joint material 10 is placed at the corner of the adherend surface 8 and the tile piece 3, as shown in the cross-sectional view of FIG. It is best to apply it and shape it diagonally.

以上本発明を実施の形態について説明したが、もちろん本発明は上記実施形態に限定されるものではない。
例えば、実施形態では、軟質樹脂シート4の貫通額孔9を貫通方向に真っ直ぐな直孔状にしたが、図示しないが前記貫通額孔9を貫通方向の表面に向かって拡大するテーパ孔状にしてもよい。そうすることにより貫通額孔9の内周面とタイル片3の側壁との間に、奥に向かってくさび状に狭まる微細な隙間ができ、その微細な隙間に可塑性を有する目地材10が染みこんで固化する。したがって、目地材10の目地溝5からの剥離がさらに強く防止できる。
また、実施形態では、ベースシート2の表面に貼着層6fを設けて軟質樹脂シート4とタイル片3を貼着するようにしたが、軟質樹脂シート4とタイル片3の裏面に貼着層を設けるようにしてもよい。
また、実施形態ではタイル片3を正方形の板状に形成したが、長方形はもちろん、円形や三角形等の多角形にしてもよい。
Although the present invention has been described above with reference to the embodiments, the present invention is of course not limited to the above embodiments.
For example, in the embodiment, the through forehead hole 9 of the soft resin sheet 4 is made into a straight hole shape in the penetration direction, but although not shown, the through forehead hole 9 is made into a tapered hole shape that expands toward the surface in the penetration direction. It's okay. By doing so, a minute gap is created between the inner circumferential surface of the through-frame hole 9 and the side wall of the tile piece 3, narrowing in a wedge shape toward the back, and the plastic joint material 10 stains the minute gap. It will harden. Therefore, peeling of the joint material 10 from the joint groove 5 can be further prevented.
Further, in the embodiment, the adhesive layer 6f is provided on the surface of the base sheet 2 to adhere the soft resin sheet 4 and the tile piece 3, but the adhesive layer 6f is provided on the back surface of the soft resin sheet 4 and the tile piece 3. may be provided.
Further, in the embodiment, the tile piece 3 is formed into a square plate shape, but it may be formed into a polygonal shape such as a circle or a triangle as well as a rectangle.

1 …タイル貼着シート
2 …ベースシート
3 …タイル片
4 …軟質樹脂シート
4P …紙シート
5 …目地溝
6r,6f …貼着層
7 …目地空間
8 …被着面
9 …貫通額孔
10 …目地材
10w …水
11 …タイル貼着セット
1... Tile adhesion sheet 2... Base sheet 3... Tile piece 4... Soft resin sheet 4P... Paper sheet 5... Joint groove 6r, 6f... Adhesive layer 7... Joint space 8... Adhering surface 9... Through forehead hole 10... Grout material 10w...Water 11...Tile adhesion set

Claims (4)

面に貼着層を有するベースシートと、
そのベースシートの表面に所定の目地空間を設けて配列され且つそのベースシートの表面に貼着される複数のタイル片と、
前記ベースシートの表面に貼着される軟質樹脂シートと、を備えており、
前記軟質樹脂シートは、
前記タイル片の厚みより小さく且つ外寸が前記ベースシートとほぼ同じであって、
前記ベースシートに配列される前記タイル片の形状と配置に合わせて象った貫通額孔を有すると共にその表面に植物繊維その他の繊維を膠着させてなる吸水性を有する紙シートを貼着してなり、
前記目地空間に前記軟質樹脂シートで嵩上げされ且つ前記紙シートが溝底に臨む目地溝が形成されるようにしたことを特徴とするタイル貼着シート。
a base sheet having an adhesive layer on the back side ;
a plurality of tile pieces arranged on the surface of the base sheet with predetermined joint spaces and adhered to the surface of the base sheet;
a soft resin sheet affixed to the surface of the base sheet,
The soft resin sheet is
smaller than the thickness of the tile piece and having approximately the same outer dimensions as the base sheet,
The base sheet has a through-frame hole shaped to match the shape and arrangement of the tile pieces arranged on the base sheet, and a water-absorbing paper sheet made of vegetable fibers or other fibers is adhered to the surface of the hole. Become,
A tile adhering sheet characterized in that a joint groove is formed in the joint space, the joint groove being raised by the soft resin sheet and in which the paper sheet faces the groove bottom.
請求項1に記載のタイル貼着シートと、
そのタイル貼着シートの前記目地溝に充填する可塑性を有する目地材と、を一揃いにしてなることを特徴とするタイル貼着セット。
The tile adhesive sheet according to claim 1;
A tile adhering set comprising: a plastic joint material to be filled into the joint grooves of the tile adhering sheet.
請求項1に記載のタイル貼着シートと、
そのタイル貼着シートの前記目地溝に充填する目地材と、を一揃いにしてなり、
前記目地材は、水を含むことで可塑性を発揮するものであって、水を含む前の状態になっていることを特徴とするタイル貼着セット。
The tile adhesive sheet according to claim 1;
and a joint material to be filled into the joint grooves of the tile adhesive sheet,
The tile sticking set is characterized in that the joint material exhibits plasticity when it contains water, and is in a state before it contains water.
前記目地材に加える所要量の水を密閉容器に入れて一揃いにしたことを特徴とする請求項3記載のタイル貼着セット。 4. The tile sticking set according to claim 3, wherein a required amount of water to be added to the joint material is placed in a sealed container.
JP2019238072A 2019-12-27 2019-12-27 Tile adhesion sheet and tile adhesion set Active JP7382060B2 (en)