JP6176967B2 - Roll paper and roll paper manufacturing method - Google Patents

Roll paper and roll paper manufacturing method Download PDF

Info

Publication number
JP6176967B2
JP6176967B2 JP2013070329A JP2013070329A JP6176967B2 JP 6176967 B2 JP6176967 B2 JP 6176967B2 JP 2013070329 A JP2013070329 A JP 2013070329A JP 2013070329 A JP2013070329 A JP 2013070329A JP 6176967 B2 JP6176967 B2 JP 6176967B2
Authority
JP
Japan
Prior art keywords
paper
layer
deodorant
roll
paper tube
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
JP2013070329A
Other languages
Japanese (ja)
Other versions
JP2014193212A (en
Inventor
哲平 森脇
哲平 森脇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Daio Paper Corp
Original Assignee
Daio Paper Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Daio Paper Corp filed Critical Daio Paper Corp
Priority to JP2013070329A priority Critical patent/JP6176967B2/en
Publication of JP2014193212A publication Critical patent/JP2014193212A/en
Application granted granted Critical
Publication of JP6176967B2 publication Critical patent/JP6176967B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Description

本発明は、帯状のキッチンペーパーやトイレットペーパーを紙管に巻いたロールペーパー、特に紙管に消臭剤が付与されたロールペーパーと、その製造方法に関する。   The present invention relates to a roll paper obtained by winding a strip-shaped kitchen paper or toilet paper around a paper tube, in particular, a roll paper in which a deodorant is applied to the paper tube, and a method for producing the same.

従来、トイレットロールの機能向上を目指して消臭機能を付与することが提案されている。例えば、紙管内面に消臭剤を塗布する方法(特許文献1)、トイレットペーパーの巻終わりを接着するテールシール糊に消臭剤を含ませる方法(特許文献2)等が提案されている。後者のものは使用開始と同時に消臭剤付与部分が使用されてしまうため、消臭効果の持続性という点において前者の態様のほうが望ましい。   Conventionally, it has been proposed to provide a deodorizing function with the aim of improving the function of a toilet roll. For example, a method of applying a deodorant to the inner surface of a paper tube (Patent Document 1), a method of adding a deodorant to a tail seal paste that bonds the end of toilet paper roll (Patent Document 2), and the like have been proposed. In the latter case, the deodorant-applied portion is used at the same time as the start of use, and therefore the former mode is more desirable in terms of durability of the deodorizing effect.

ところで、消臭剤の中には、活性炭など吸着機能の利用する粉体状のものがある。この粉体状消臭剤は、消臭性に優れるものの、紙管内面にバインダー等で付着させるようにしても、紙管内面の表面積が限られているため十分な付着量とすることが難しく、消臭効果の長期化が難しかった。また、使用時や加工時に剥がれ落ちやすく歩留まりが悪く、粉体状消臭剤の効果を十分に発現させることが困難であった。   By the way, some deodorizers are in the form of powder that uses an adsorption function such as activated carbon. Although this powdery deodorant is excellent in deodorizing properties, it is difficult to achieve a sufficient amount of adhesion even if it is attached to the inner surface of the paper tube with a binder or the like because the surface area of the inner surface of the paper tube is limited. It was difficult to extend the deodorizing effect. Moreover, it is easy to peel off at the time of use or processing, the yield is poor, and it has been difficult to fully express the effect of the powder deodorant.

ところで、トイレットロールは、使用時には常に開放環境に置かれるため、消臭成分の揮散により悪臭成分を化学的に消臭するものでは、消臭剤の効力が短時間で低下しやすい。消臭機能を長期化する方法として、例えば、フィルム状消臭剤を利用すること(特許文献3)や揮発性消臭剤をマイクロカプセルに封入して塗布する方法(特許文献4)が提案されているが、フィルムを接着したり、マイクロカプセルに揮発性消臭剤を封入する方法は、煩雑な操作を要し、生産工程も多いため、生産性に劣るとともにコストが高くなる。   By the way, since the toilet roll is always placed in an open environment at the time of use, if the deodorizing component is chemically deodorized by volatilization of the deodorizing component, the effectiveness of the deodorant tends to decrease in a short time. As a method for prolonging the deodorizing function, for example, a film-like deodorant (Patent Document 3) or a method of applying a volatile deodorant in a microcapsule (Patent Document 4) has been proposed. However, the method of adhering a film or encapsulating a volatile deodorant in a microcapsule requires a complicated operation and has many production steps, resulting in poor productivity and high cost.

実開昭62−197660Japanese Utility Model Sho 62-197660 実開平7−36887Real Kaihei 7-36887 実開昭63−142192Japanese Utility Model Sho 63-142192 特開2009−242065JP2009-242065 特開2009−242107JP2009-242107A 特許第4159061号Japanese Patent No. 4159061 特許第78192号Patent No. 78192 特許第5032398号Patent No. 5032398

そこで、本発明の主たる課題は、消臭効果が長期間維持されるロールペーパーと、このロールペーパーを容易に製造可能な製造方法を提供することにある。   Then, the main subject of this invention is providing the manufacturing method which can manufacture this roll paper easily, and the roll paper by which a deodorizing effect is maintained for a long period of time.

上記課題を解決した本発明とその効果は次記のとおりである。
〔請求項1記載の発明〕
帯状のペーパーシートが紙管に巻かれているロールペーパーであって、
前記紙管の内面は、紙管原紙からなる原紙層、原紙層上に形成された消臭剤層、消臭剤層上に形成されたコート層の層構造を有し、前記原紙層の表面に多数の凹部が形成され、
前記消臭剤層その凹部の深さを超える厚さを有しかつ凹部内に入り込んでいる
ことを特徴とするロールペーパー。
The present invention that has solved the above problems and the effects thereof are as follows.
[Invention of Claim 1]
A roll paper in which a strip-shaped paper sheet is wound around a paper tube,
The inner surface of the paper tube has a layer structure of a base paper layer made of a paper tube base paper, a deodorant layer formed on the base paper layer, and a coat layer formed on the deodorant layer, and the surface of the base paper layer A large number of recesses are formed in
The deodorant layer has a thickness that exceeds the depth of the recess and enters the recess ,
A roll paper characterized by that.

〔請求項2記載の発明〕
消臭剤層上に弱通気性のコート層が全面に形成されている、請求項1記載のロールペーパー。
[Invention of Claim 2]
The roll paper according to claim 1, wherein a weakly breathable coat layer is formed on the entire surface of the deodorant layer.

〔請求項3記載の発明〕
消臭剤層上に弱通気性もしくは非通気性であるコート層が部分的に形成されている、請求項1記載のロールペーパー。
[Invention of Claim 3]
The roll paper according to claim 1, wherein a coat layer that is weakly breathable or non-breathable is partially formed on the deodorant layer.

〔請求項4記載の発明〕
複数の紙管原紙のうち紙管内面に位置する紙管原紙の紙管内面側となる面に多数の凹部を形成する工程と、
その凹部を形成した面に消臭剤を塗工して前記凹部内に入り込みかつ凹部の深さを超える厚さの消臭剤層を形成する工程と、
消臭剤層の上にコート剤を塗工してコート層を形成する工程と、
複数の紙管原紙をマンドレルシャフトに螺旋状に巻いて連続的に筒状部分を形成し、その筒状に形成された部分をロールペーパーの複数倍幅以上の幅でカットして長尺の紙管を形成する紙管形成工程と、
長尺の紙管にロールペーパーの複数倍幅以上の幅のロールペーパー原紙を巻いてログを形成する工程と、
ログを切断して個々のロールペーパーにする工程と、
を有することを特徴とする、ロールペーパーの製造方法。
[Invention of Claim 4]
Forming a plurality of recesses on the surface of the paper tube base paper located on the inner surface of the paper tube among the plurality of paper tube base papers;
A step of applying a deodorant on the surface where the recess is formed and entering the recess and forming a deodorant layer having a thickness exceeding the depth of the recess;
Applying a coating agent on the deodorant layer to form a coating layer;
A plurality of paper tube base papers are spirally wound around a mandrel shaft to continuously form a cylindrical portion, and the cylindrical portion is cut with a width more than twice the width of roll paper to make a long paper A paper tube forming process for forming a tube;
A step of forming a log by winding a roll paper base paper having a width more than a multiple of the roll paper around a long paper tube;
Cutting logs into individual roll papers;
A method for producing roll paper, comprising:

〔請求項5記載の発明〕
原反ロールから紙管原紙を繰出して、消臭剤の塗工と、コート剤の塗工を行い、そのままマンドレルシャフトへの巻き付けを行なう、請求項4に記載のロールペーパーの製造方法。
[Invention of Claim 5]
The roll paper manufacturing method according to claim 4, wherein the paper tube base paper is fed out from the raw roll, coated with a deodorant and a coating agent, and wound around the mandrel shaft as it is.

以上のとおり本発明によれば、消臭効果が長期間維持されるロールペーパーと、このロールペーパーを容易に製造可能な製造方法が提供される。   As described above, according to the present invention, a roll paper whose deodorizing effect is maintained for a long period of time and a production method capable of easily producing this roll paper are provided.

本発明の実施形態に係るロールペーパーの斜視図である。It is a perspective view of the roll paper which concerns on embodiment of this invention. 本発明の実施形態に係る紙管の断面図である。It is sectional drawing of the paper tube which concerns on embodiment of this invention. 本発明の実施形態に係る他の紙管の断面図である。It is sectional drawing of the other paper tube which concerns on embodiment of this invention. 本発明の実施形態に係るロールペーパーの製造方法の概要を示す図であるIt is a figure which shows the outline | summary of the manufacturing method of the roll paper which concerns on embodiment of this invention. 本発明の実施形態に係る長尺紙管の製造方法を示す図である。It is a figure which shows the manufacturing method of the elongate paper tube which concerns on embodiment of this invention. 本発明の実施形態に係る紙管原紙に消臭剤層とコート層を設けた態様を示す図である。It is a figure which shows the aspect which provided the deodorizer layer and the coating layer in the paper tube base paper which concerns on embodiment of this invention. 本発明の実施形態に係る長尺紙管の製造方法を示す他の図である。It is another figure which shows the manufacturing method of the long paper tube which concerns on embodiment of this invention. 本発明の実施形態に係る紙管原紙に消臭剤層とコート層を設けた他の態様を示す図である。It is a figure which shows the other aspect which provided the deodorizer layer and the coating layer in the paper tube base paper which concerns on embodiment of this invention. 本発明の実施形態に係る長尺の紙管とマンドレルシャフトとの関係を示す断面図である。It is sectional drawing which shows the relationship between the elongate paper tube which concerns on embodiment of this invention, and a mandrel shaft.

本発明の実施形態を図1〜9を参照しながら以下に説明する。但し、本発明は、この実施形態に限られない。   Embodiments of the present invention will be described below with reference to FIGS. However, the present invention is not limited to this embodiment.

「ロールペーパー」
本発明に係るロールペーパー10は、図1に示すとおり、紙管11に帯状の家庭用薄葉紙であるペーパーシート12が巻かれたものである。係るロールペーパー10としては、トイレットロール、キッチンペーパーロールが例示できる。ロールペーパー10の大きさ等は、トイレットロールであれば、幅L1が100〜115mm、直径L2が100〜120mm、巻き長さ(トイレットペーパーの全長)が18〜70m、紙管内径L3が35〜50mmであるのが望ましい。この大きさであれば一般的なトイレットロール用のペーパーホルダーが利用でき、トイレットペーパーの長さも十分である。
"Roll paper"
As shown in FIG. 1, a roll paper 10 according to the present invention is obtained by winding a paper sheet 11, which is a strip-shaped household thin paper, around a paper tube 11. Examples of the roll paper 10 include a toilet roll and a kitchen paper roll. If the roll paper 10 is a toilet roll, the width L1 is 100 to 115 mm, the diameter L2 is 100 to 120 mm, the winding length (full length of the toilet paper) is 18 to 70 m, and the paper tube inner diameter L3 is 35 to 35 mm. 50 mm is desirable. With this size, a general toilet roll paper holder can be used, and the length of the toilet paper is sufficient.

また、キッチンペーパーロールであれば、幅L1が200〜400mm、直径L2が90〜140mm、巻き長さ(キッチンペーパーの全長)が10〜30m、紙管内径L3が35〜50mmであるのが望ましい。   In the case of a kitchen paper roll, it is desirable that the width L1 is 200 to 400 mm, the diameter L2 is 90 to 140 mm, the winding length (full length of the kitchen paper) is 10 to 30 m, and the paper tube inner diameter L3 is 35 to 50 mm. .

本実施形態のペーパーシート12は、微細な凹凸であるクレープを有する家庭用薄葉紙であるが、その具体的な組成・構成は限定されない。ペーパーシート12は、1プライから3プライのものが望ましい。紙厚は、トイレットペーパーであれば、100〜350μm、キッチンペーパーであれば、200〜450μmであるのが望ましい。また、1プライ当り米坪は、トイレットペーパーであれば、11.0〜25.0g/m2、キッチンペーパーであれば20.0〜45.0g/m2であるのが望ましい。この範囲であれば使用時の柔らかさや吸水性を確保できる。 The paper sheet 12 of the present embodiment is a household thin paper having a crepe which is fine unevenness, but its specific composition and configuration are not limited. The paper sheet 12 is preferably one to three plies. The paper thickness is preferably 100 to 350 μm for toilet paper and 200 to 450 μm for kitchen paper. Further, 1 ply per Beitsubo, if toilet paper, 11.0~25.0g / m 2, is preferably a 20.0~45.0g / m 2 if paper towels. If it is this range, the softness and water absorption at the time of use can be ensured.

なお、本発明に係る米坪とは、JIS P 8124(1998)の米坪測定方法によるものであり、紙厚とは、JIS P 8111(1998)の条件下で十分に調湿した後、同条件下でダイヤルシックネスゲージ(厚み測定器)「PEACOCK G型」(尾崎製作所製)を用いて5回測定した平均値をいう。なお、測定は1プライのものは1プライ、2プライのものは2プライ、3プライのものは3プライとして行なう。   In addition, the tsubo in accordance with the present invention is based on the tsubo tsubo measurement method of JIS P 8124 (1998), and the paper thickness is the same after the humidity is sufficiently adjusted under the conditions of JIS P 8111 (1998). The average value measured five times using a dial thickness gauge (thickness measuring instrument) “PEACOCK G type” (manufactured by Ozaki Seisakusho) under the conditions. The measurement is performed with 1 ply for 1 ply, 2 plies for 2 plies, and 3 plies for 3 plies.

本実施形態に係るロールペーパー10は、特徴的に、図2及び図3に紙管11の輪切り断面を示すように、紙管11の内面側が、紙管原紙からなる原紙層20、原紙層20上に形成された消臭剤層21、消臭剤層21上に形成されたコート層22の層構造を有しており、その原紙層20の表面に全体的に多数の凹部2,2…が形成されているとともに、前記消臭剤層21の厚さL4がその凹部2の深さL5を超える厚さとなっている。本実施形態に係るロールペーパー10は、消臭剤層21の厚さL4が原紙層20に形成した多数の凹部2,2…の深さL5より厚くすることで、凹部2,2…を設けない場合と比較して、特に凹部2,2…に入り込む分だけ消臭剤をより多く紙管に付着させることができ、さらに、それのみならず、原紙層20に形成された凹部2,2…に消臭剤層21が一部入り込むことによるアンカー効果によって消臭剤層21が原紙層20の表面からの離脱し難くなり、より一層厚みのある消臭剤層21を形成することができるようになる。   Characteristically, the roll paper 10 according to this embodiment has a base paper layer 20 and a base paper layer 20 made of a paper tube base paper on the inner surface side of the paper tube 11, as shown in FIGS. It has a layer structure of a deodorant layer 21 formed on the top and a coat layer 22 formed on the deodorant layer 21, and a large number of recesses 2, 2. And the thickness L4 of the deodorant layer 21 exceeds the depth L5 of the recess 2. The roll paper 10 according to the present embodiment is provided with the recesses 2, 2... By making the thickness L 4 of the deodorant layer 21 thicker than the depth L 5 of the numerous recesses 2, 2. More deodorant can be attached to the paper tube as much as it enters the recesses 2, 2..., And the recesses 2, 2 formed in the base paper layer 20. The deodorant layer 21 is not easily detached from the surface of the base paper layer 20 due to the anchor effect caused by the partial entry of the deodorant layer 21 into the deodorant layer 21, and a thicker deodorant layer 21 can be formed. It becomes like this.

このような凹部2,2…を原紙層20の表面に形成するには、紙管原紙に対してエンボス加工を施すことにより形成することができる。原紙層20に形成する凹部2,2…の望ましい構成は、深さが0.1〜0.2mm、面積0.03〜1.0mm2の凹部を密度7〜100個/cm2で設けた構成である。ただし、凹部の深さは原紙の紙厚を超えない。この凹部2,2…の付与態様であれば、消臭剤の付与量増加効果とアンカー効果とを効果的に発揮させることができる。また、凹部の平面視での形状は限定されない。円形、楕円形、三角形、四角形、多角形など適宜の形状とすることができる。 In order to form such recesses 2, 2... On the surface of the base paper layer 20, it can be formed by embossing the paper tube base paper. A desirable configuration of the concave portions 2, 2... Formed in the base paper layer 20 is provided with concave portions having a depth of 0.1 to 0.2 mm and an area of 0.03 to 1.0 mm 2 at a density of 7 to 100 pieces / cm 2 . It is a configuration. However, the depth of the recess does not exceed the thickness of the base paper. If it is the application | coating aspect of this recessed part 2,2, ..., the application amount increase effect of a deodorizer and an anchor effect can be exhibited effectively. Further, the shape of the concave portion in plan view is not limited. An appropriate shape such as a circle, an ellipse, a triangle, a quadrangle, or a polygon can be used.

原紙層20を構成する紙管原紙20Aは、十分な強度を得るべく、米坪が120〜220g/m2、紙厚が150〜500μmであるのが望ましい。 The paper tube base paper 20A constituting the base paper layer 20 is preferably 120 to 220 g / m 2 in US basis and 150 to 500 μm in thickness in order to obtain sufficient strength.

他方、消臭剤層21は、消臭剤を有効成分として消臭機能を発揮する層である。この消臭剤層21は、図示のように紙管内面11Aの全面に形成するのが望ましい。係る消臭剤層21の有効成分である消臭剤としては、ポリフェノール系消臭剤、スギ、ヒノキ等から抽出された精油類、二酸化チタン、二酸化アルミニウム、ベタイン化合物、ジルコニウム化合物、銅化合物、ゼオライト、活性炭、イオン交換樹指の少なくとも1種を含むものであるのが望ましい。これらの消臭剤であれば、十分な消臭効果を得ることができる。   On the other hand, the deodorant layer 21 is a layer that exhibits a deodorizing function using the deodorant as an active ingredient. The deodorant layer 21 is preferably formed on the entire surface of the paper tube inner surface 11A as shown in the figure. Examples of the deodorant that is an active ingredient of the deodorant layer 21 include polyphenol deodorants, essential oils extracted from cedar, cypress, etc., titanium dioxide, aluminum dioxide, betaine compounds, zirconium compounds, copper compounds, zeolites It is desirable to contain at least one of activated carbon and ion exchange resin. With these deodorizers, a sufficient deodorizing effect can be obtained.

消臭剤層21は、消臭剤を紙管11の内面11Aに固着するためのバインダー成分が含まれていてもよい。バインダーとしては、消臭剤の効果を妨げないものであれば特に限定されない。例えば、空気中の悪臭成分を化学的に中和したり分解したり補足したりする消臭剤であれば、消臭剤の揮散を過度に妨げないバインダー、吸着を利用する消臭剤であれば消臭剤と外気との接触機会を過度に遮断しないバインダーを用いる。係るバインダーとしては、澱粉、カルボキシメチルセルロース、ポリビニルアルコールが例示できる。   The deodorant layer 21 may include a binder component for fixing the deodorant to the inner surface 11 </ b> A of the paper tube 11. The binder is not particularly limited as long as it does not interfere with the effect of the deodorant. For example, if it is a deodorant that chemically neutralizes, decomposes, or supplements bad odor components in the air, it should be a binder that does not excessively prevent the deodorant from volatilizing, or a deodorant that uses adsorption. For example, a binder that does not excessively block the contact between the deodorant and the outside air is used. Examples of the binder include starch, carboxymethyl cellulose, and polyvinyl alcohol.

特に、本実施形態に係るトイレットロールの構成は、二酸化チタン、二酸化アルミニウム、ベタイン化合物、ジルコニウム化合物、銅化合物、ゼオライト、活性炭、イオン交換樹指等のような粉状又は粒状の消臭剤をバインダーにより原紙層20上に付着させて消臭剤層21を形成するものに特に有用である。すなわち、これらの粉状又は粒状の消臭剤は、消臭効果が高いものの従来の凹部のない紙管内面には十分な量を付着させることが難しかった。これは、紙管内面は面積が限られること、粉状又は粒状であるとバインダーを用いても離脱しやすくなることが要因として大きい。本実施形態では、上述のとおり凹部内に入り込む分だけ消臭剤の担持量を増加させることができ、しかもアンカー効果により消臭剤層21の厚みを厚くすることができるため、係る粉状又は粒状の消臭剤を十分な量を付着させることができる。   In particular, the configuration of the toilet roll according to this embodiment includes a binder of powdery or granular deodorant such as titanium dioxide, aluminum dioxide, betaine compound, zirconium compound, copper compound, zeolite, activated carbon, ion exchange resin, etc. Is particularly useful for forming the deodorant layer 21 by adhering to the base paper layer 20. That is, although these powdery or granular deodorizers have a high deodorizing effect, it is difficult to attach a sufficient amount to the inner surface of a paper tube having no conventional recess. This is largely due to the fact that the inner surface of the paper tube has a limited area, and that it is easily separated even if a binder is used if it is powdery or granular. In the present embodiment, as described above, the amount of deodorant carried can be increased by the amount entering the recess, and the thickness of the deodorant layer 21 can be increased by the anchor effect. A sufficient amount of granular deodorant can be deposited.

本実施形態において特に望ましい粉状の平均粒子径は、0.5〜20μmである。この平均粒径であれば消臭剤層21を形成しやすく、また、十分に原紙層20上に付着させやすい。特に、上記の好ましい凹部2,2…の構成と組み合わせることで、一層の効果が発揮される。なお、ここでの平均粒子径とは、マイクロトラック法によるメジアン径を意味する。   A particularly desirable powdery average particle size in the present embodiment is 0.5 to 20 μm. With this average particle size, the deodorant layer 21 can be easily formed, and can be sufficiently deposited on the base paper layer 20. In particular, a further effect is exhibited by combining with the configuration of the above-mentioned preferable recesses 2, 2. Here, the average particle diameter means a median diameter by the microtrack method.

消臭剤の付与量は、用いる消臭剤の種類により適宜変更することができる。上記の粉状又は粒状の消臭剤であれば、好ましい担持量は0.1〜10g/m2である。 The amount of deodorant applied can be appropriately changed depending on the type of deodorant used. If it is said powdery or granular deodorant, a preferable load is 0.1-10 g / m < 2 >.

他方、本実施形態に係る消臭剤層21には、消臭剤の効果を妨げない範囲で、適宜の香料を含有することができる。香料は、例えば、レモン油、グレープフルーツ油、ローズマリー油、ペパーミント油、マンダリン油、ライム油、ユズ油、カモミール油、ラベンダー油、ローズ油、スペアミント油等の天然香料類;リナロール、シトロネロール、メントール、ゲラニオール等のアルコール類等の合成香料などが挙げられる。これらは単独で用いても、複数を組み合わせて調合香料として用いてもよい。香料の選択は、所望の香調によって決定すればよい。   On the other hand, the deodorant layer 21 according to the present embodiment can contain an appropriate fragrance as long as the effect of the deodorant is not hindered. Fragrances include, for example, natural fragrances such as lemon oil, grapefruit oil, rosemary oil, peppermint oil, mandarin oil, lime oil, yuzu oil, chamomile oil, lavender oil, rose oil, spearmint oil; linalool, citronellol, menthol, Synthetic fragrances such as alcohols such as geraniol. These may be used alone or in combination as a blended fragrance. The selection of the fragrance may be determined according to the desired fragrance tone.

消臭剤層21上に部分的に形成されるコート層22は、図2に示すように消臭剤層21上に全面的に形成してもよいし、図3に示すように部分的に形成してもよい。全面的に形成する場合には、少なくとも消臭剤層21の消臭剤の効果を妨げないように少なくとも通気性を有する層とする。例えば、空気中の悪臭成分を化学的に中和したり分解したり補足したりする消臭剤を用いた場合には、消臭剤の揮散を過度に妨げないコート層、吸着を利用する消臭剤であれば消臭剤と外気との接触機会を過度の遮断しないコート層とする。部分的に形成する場合には、非通気性のコート層とすることができる。本実施形態のロールペーパー10は、このようにコート層22を設けられているため、消臭剤層と外気との接触機会が低減されており、消臭剤の効果の急激に低下することがなく、消臭効果の持続性に優れる。すなわち、消臭成分が揮散性のものであるならば、コート層22が設けられている部分からは消臭剤が揮散し難くなり、消臭効果が長持ちするようになる。また、消臭剤が吸着を利用するものであるならば、コート層22が設けられている部分からは悪臭成分が消臭剤層に取り込まれ難くなり、消臭剤層21の消臭効果が長持ちするようになる。   The coat layer 22 partially formed on the deodorant layer 21 may be formed entirely on the deodorant layer 21 as shown in FIG. 2, or partially as shown in FIG. It may be formed. In the case of forming the entire surface, at least a layer having air permeability is used so as not to interfere with the effect of the deodorant of the deodorant layer 21. For example, when a deodorant that chemically neutralizes, decomposes, or supplements bad odor components in the air is used, a coating layer that does not excessively prevent the deodorant from volatilizing, or an extinguishing that uses adsorption. If it is a odorant, it shall be a coat layer that does not excessively block contact opportunities between the deodorant and the outside air. When forming partially, it can be set as a non-breathable coat layer. Since the roll paper 10 of this embodiment is provided with the coat layer 22 in this way, the contact opportunity between the deodorant layer and the outside air is reduced, and the effect of the deodorant may be drastically reduced. No deodorant effect and excellent durability. That is, if the deodorant component is volatile, the deodorant is less likely to evaporate from the portion where the coat layer 22 is provided, and the deodorizing effect will last longer. In addition, if the deodorant uses adsorption, it is difficult for a malodorous component to be taken into the deodorant layer from the portion where the coat layer 22 is provided, and the deodorant effect of the deodorant layer 21 is reduced. It will last longer.

コート層22を、消臭剤層21上に部分的に形成する場合、本実施形態では、その形状までは限定されない。例えば、消臭剤層21上に網点状、円状、ブロック状など、適宜の形状・模様に形成することができる。コート層22の総付与面積及び単位付与面積は、消臭効果の維持期間により適宜調整すればよい。   In the case where the coat layer 22 is partially formed on the deodorant layer 21, in the present embodiment, the shape is not limited. For example, it can be formed on the deodorant layer 21 in an appropriate shape / pattern such as a dot shape, a circle shape, or a block shape. What is necessary is just to adjust the total provision area and unit provision area of the coat layer 22 suitably with the maintenance period of a deodorizing effect.

コート層22の厚みは、1〜100μm、より好ましくは1〜20μmとするのが望ましい。コート層22の厚みが1μm未満であると消臭剤層21と外気との接触機会を十分に低減できないおそれがあり、100μmを超えてもコスト高となるだけである。   The thickness of the coat layer 22 is preferably 1 to 100 μm, more preferably 1 to 20 μm. If the thickness of the coat layer 22 is less than 1 μm, the chance of contact between the deodorant layer 21 and the outside air may not be sufficiently reduced, and if it exceeds 100 μm, only the cost is increased.

本実施形態に係るコート層22は、コート剤の塗工により形成することができる。このコート剤としては、例えば、澱粉、カルボキシメチルセルロース、ポリビニルアルコール、パラフィン、酢酸ビニルの1種又は2種以上を混合して用いることができる。これらのコート剤は、表面が平滑なコート層22を形成でき、紙管製造時のシャフトとの摩擦を低減させて、生産性を向上させることができる。なお、これらのコート剤のうち、酢酸ビニルを用いた場合には、通気性が実質的にない非通気性のコート層となり、それ以外のコート剤であれば、通気性のコート層22となる。   The coat layer 22 according to the present embodiment can be formed by applying a coating agent. As this coating agent, for example, one or more of starch, carboxymethylcellulose, polyvinyl alcohol, paraffin, and vinyl acetate can be mixed and used. These coating agents can form a coating layer 22 having a smooth surface, reduce friction with the shaft during paper tube manufacture, and improve productivity. Of these coating agents, when vinyl acetate is used, it becomes a non-breathable coating layer having substantially no breathability, and if it is other coating agent, it becomes a breathable coating layer 22. .

以上の本実施形態に係るロールペーパー10は、下記のロールペーパーの製造方法で述べるとおり製造性に優れるという利点がある。   The roll paper 10 according to the above embodiment has an advantage that it is excellent in manufacturability as described in the following roll paper manufacturing method.

「ロールペーパーの製造方法」
次に、本発明の実施形態に係るロールペーパー10の製造方法例を特に図4〜図8を参照しながら説明する。但し、本発明のロールペーパーの製造方法は、この方法に必ずしも限定されるわけではない。
"Method for manufacturing roll paper"
Next, an example of a method for manufacturing the roll paper 10 according to the embodiment of the present invention will be described with particular reference to FIGS. However, the method for producing the roll paper of the present invention is not necessarily limited to this method.

本実施形態のロールペーパー10の製造方法は、図4に示すように、長尺のスパイラル紙管30を製造する工程(A)と、その長尺のスパイラル紙管を用いてログを製造するログ製造工程(B)と、ログを裁断して個々のロールペーパーにする裁断工程(C)を有している。   As shown in FIG. 4, the manufacturing method of the roll paper 10 of this embodiment includes a step (A) for manufacturing a long spiral paper tube 30 and a log for manufacturing a log using the long spiral paper tube. It has a manufacturing process (B) and a cutting process (C) for cutting the log into individual roll papers.

〔紙管製造工程(A)〕
本実施形態の紙管製造工程は、図4中(A)、図5に示すように、原反ロール31A,32Aから繰出された二枚の帯状の紙管原紙31,32のうち一方の紙管原紙31の一方面に糊付けロール51により糊44を付与した後、前記一方の紙管原紙31の糊付けされた面に他方の紙管原紙32を幅方向に一部重ね、前記他方の紙管原紙32の糊付け面と接しない面をマンドレルシャフト52に対向する面、すなわち紙管内面となる面にして、各紙管原紙31,32をマンドレルシャフト52に螺旋状に巻き付けて連続的に筒状部分29を形成し、その筒状部分29をトイレットロールの複数倍幅以上の幅でカッター58によりカットして長尺のスパイラル紙管30(スパイラル式紙管とも称される)を形成する。このスパイラル紙管は、一方の紙管原紙31が紙管外面側、他方の紙管原紙32が紙管内面側となる態様の二層積層構造となる。なお、本実施形態では、2枚の紙管原紙31,32をスパイラル巻きしているが、3枚以上の紙管原紙をスパイラル巻きして長尺の紙管を形成してもよい。
[Paper tube manufacturing process (A)]
In the paper tube manufacturing process of the present embodiment, as shown in FIG. 4A and FIG. 5, one of the two strip-shaped paper tube base papers 31 and 32 fed out from the raw rolls 31A and 32A. After the paste 44 is applied to one surface of the tube base paper 31 by the glue roll 51, the other paper tube base paper 32 is partially overlapped in the width direction on the surface of the one paper tube base paper 31, and the other paper tube The surface of the base paper 32 that does not contact the gluing surface is the surface facing the mandrel shaft 52, that is, the surface that becomes the inner surface of the paper tube, and the paper tube base papers 31 and 32 are spirally wound around the mandrel shaft 52 to continuously form a cylindrical portion. 29 is formed, and the cylindrical portion 29 is cut by a cutter 58 with a width more than a multiple of the toilet roll to form a long spiral paper tube 30 (also referred to as a spiral paper tube). This spiral paper tube has a two-layer laminated structure in which one paper tube base paper 31 is on the outer surface side of the paper tube and the other paper tube base paper 32 is on the inner surface side of the paper tube. In this embodiment, two paper tube base papers 31 and 32 are spirally wound. However, a long paper tube may be formed by spirally winding three or more paper tube base papers.

紙管原紙31に対する糊44の付与量は特に限定されないが、概ね1〜25.0g/m2程度である。また、糊は、本発明の効果を妨げない範囲で既知の紙管用のものを用いることができ、アクリル系接着剤、ホットメルト接着剤、澱粉糊、ポリビニルアルコール等が例示できる。 The amount of paste 44 applied to the paper tube base 31 is not particularly limited, but is approximately 1 to 25.0 g / m 2 . Further, as the glue, those for known paper tubes can be used as long as the effects of the present invention are not hindered, and examples thereof include acrylic adhesives, hot melt adhesives, starch glues, and polyvinyl alcohol.

図示の形態では、各紙管原紙31,32のマンドレルシャフト52への巻き付けは、一対のプーリー53,53間に巻き掛けられた平ベルト54により、マンドレルシャフト52上の所定部分に位置する筒状部分29に回転力を与え、その回転により紙管原紙31,32をマンドレルシャフト52の軸心に対して所定角度で引き込んで、螺旋状に巻くようにしている。図示例では、一対のプーリー53,53を二機配置して二つの平ベルト54,54により、筒状部分29に回転力を与えているが、一機の一対のプーリーと平ベルトにより筒状部分に回転力を与えるようにしてもよい。また、図示しないが、筒状部分29に平ベルト54ではなくロールを当接させて回転力を与えるようにしても、各紙管原紙31,32をマンドレルシャフト52に巻き付けることができる。   In the form shown in the drawing, each of the paper tube base papers 31 and 32 is wound around the mandrel shaft 52 by a flat belt 54 wound between a pair of pulleys 53 and 53 and a cylindrical portion located at a predetermined portion on the mandrel shaft 52. A rotational force is applied to 29, and the paper tube base papers 31 and 32 are drawn at a predetermined angle with respect to the axis of the mandrel shaft 52 by the rotation, and are wound spirally. In the illustrated example, two pairs of pulleys 53, 53 are arranged and rotational force is applied to the tubular portion 29 by two flat belts 54, 54. However, the pair of pulleys 53 and the flat belt form a tubular shape. You may make it give rotational force to a part. Although not shown, the paper tube base papers 31 and 32 can be wound around the mandrel shaft 52 even when a roll is applied to the tubular portion 29 instead of the flat belt 54 to apply a rotational force.

ここで、紙管原紙31,32をマンドレルシャフト52に巻き付けてスパイラル紙管の形成するにあたっては、図示例からも理解されるように、紙管原紙31,32が連続的にマンドレルシャフト52に送り込まれることにより筒状部分29が長くなり、その筒状部分29が連続的に形成されてマンドレルシャフト52の先端方向に伸びていく。そして、その過程では、筒状部分29の内面がマンドレルシャフト52の周面に摺接しながら、マンドレルシャフト52の先端方向に向かって移動していくことになる。   Here, when the paper tube base papers 31 and 32 are wound around the mandrel shaft 52 to form a spiral paper tube, the paper tube base papers 31 and 32 are continuously fed into the mandrel shaft 52 as understood from the illustrated example. As a result, the tubular portion 29 becomes longer, and the tubular portion 29 is formed continuously and extends in the direction of the distal end of the mandrel shaft 52. In this process, the inner surface of the cylindrical portion 29 moves toward the distal end of the mandrel shaft 52 while being in sliding contact with the peripheral surface of the mandrel shaft 52.

本実施形態では、このように長尺の紙管30を形成するにあたって、二枚の紙管原紙31,32のうち他方の紙管原紙32、すなわちマンドレルシャフト52にスパイラル巻きした際に長尺紙管30の内面側になる面を有する紙管原紙32に対して、接着糊44を付与した一方の紙管原紙31と重ね合わせるよりも前段において、図6に示すように、原紙層となる紙管原紙32に対する凹部40,40…の形成と、消臭剤層41の形成と、コート層42の形成を行なう。なお、図6は、原紙層となる紙管原紙32に凹部40,40…を設けさらに消臭剤層41とコート層42を形成したものの断面図である。   In the present embodiment, when the long paper tube 30 is formed in this manner, the long paper tube 30 is spirally wound around the other paper tube base paper 32, that is, the mandrel shaft 52, of the two paper tube base papers 31 and 32. As shown in FIG. 6, the paper serving as the base paper layer before the paper tube base paper 31 having the surface that becomes the inner surface side of the pipe 30 is overlaid with the one paper base paper 31 provided with the adhesive paste 44. .. Are formed on the tube base paper 32, the deodorant layer 41 is formed, and the coat layer 42 is formed. FIG. 6 is a cross-sectional view of a paper tube base paper 32 that is a base paper layer provided with recesses 40, 40... And a deodorant layer 41 and a coat layer 42 formed thereon.

他方の紙管原紙32としては、米坪が120〜220g/m2、紙厚が150〜500μmであるのが望ましい。消臭剤及びコート剤の塗工がしやすく、また、凹部40,40…を形成しても紙管となった際に十分な強度を確保することができる。なお、長尺紙管30の形成するにあたって、この他方の紙管原紙32と対となるもう一方の紙管原紙31は、違う原反を使用してもよく、例えば、米坪を変えたりしてもよい。但し、双方ともに上記範囲であるのが望ましい。 As the other paper tube base paper 32, it is desirable that the US basis weight is 120 to 220 g / m 2 and the paper thickness is 150 to 500 μm. It is easy to apply the deodorant and the coating agent, and even if the recesses 40, 40... Are formed, sufficient strength can be secured when the paper tube is formed. When the long paper tube 30 is formed, the other paper tube base paper 31 that is paired with the other paper tube base paper 32 may use a different raw material. May be. However, it is desirable that both are in the above range.

原紙層20となる他方の紙管原紙32の一方面の全体に多数の凹部40,40…を形態するには、図7に示すように、消臭剤やコート剤が無塗工の紙管原紙32が巻かれた原反ロール32aから当該紙管原紙32を繰出し、エンボス加工機60でエンボス加工することで形成することができる。図示のエンボス加工機は、表面に凹部の形成パターンに対応する多数の凸部が形成されたエンボスロール60Aとこれと対になる受けロール60Bとからなり、これらエンボスロールと受けロールとの間にシートを通してエンボスロール表面に形成された凸部のパターンを型押しする。受けロール60Bは、その表面が金属製の硬質なものであってもゴム製の弾性のものであってもよい。エンボスロール60Aとの関係で適宜選択することができる。エンボスロール60Aと受けロール60Bの線厚(ニップ圧)は、凹部の深さ、及び紙管原紙32の紙質により適宜調整すればよい。   In order to form a large number of recesses 40, 40... On the entire one surface of the other paper tube base paper 32 to be the base paper layer 20, as shown in FIG. It can be formed by feeding the paper tube base paper 32 from the raw roll 32 a around which the base paper 32 is wound and embossing it with the embossing machine 60. The embossing machine shown in the drawing is composed of an embossing roll 60A having a large number of convex portions corresponding to the formation pattern of the concave portions on the surface and a receiving roll 60B paired therewith, and between these embossing rolls and the receiving roll. The pattern of the convex part formed on the embossing roll surface is embossed through the sheet. The receiving roll 60B may have a hard surface made of metal or an elastic material made of rubber. It can be selected as appropriate in relation to the embossing roll 60A. The line thickness (nip pressure) of the embossing roll 60A and the receiving roll 60B may be adjusted as appropriate depending on the depth of the recess and the paper quality of the paper tube base paper 32.

本実施形態で紙管原紙32に付与する好ましい凹部40,40…の構成は、上記「ロールペーパー」の欄で述べたのと同様であり、深さが0.1〜0.2mm、面積0.03〜1.0mm2の凹部を密度7〜100個/cm2で設けるのが望ましい。この凹部40,40…の付与態様であれば、消臭剤の付与量増加効果とアンカー効果とを効果的に発揮させることができる。 The configuration of the preferable concave portions 40, 40... Imparted to the paper tube base paper 32 in the present embodiment is the same as that described in the above-mentioned “roll paper” column, the depth is 0.1 to 0.2 mm, and the area 0. It is desirable to provide recesses of 0.03 to 1.0 mm 2 at a density of 7 to 100 / cm 2 . If it is the application | coating aspect of this recessed part 40, 40 ..., the application amount increase effect of a deodorizer and an anchor effect can be exhibited effectively.

このようにして紙管原紙32の紙管内面となる面に、多数の凹部40,40…を形成した後には、この面に塗工機61で消臭剤を塗工して消臭剤層41を形成する。消臭剤の塗工は、適宜のバインダーや溶媒に対して消臭剤を混合した消臭液を、既知の印刷機、塗工機を用いて行なうことができる。消臭液の塗工量は、5〜80g/m2となるようにするのが望ましい。この範囲であれば、生産性よく消臭液を十分に塗工することができ、また、十分な量の消臭剤を付与することができる。 In this way, after forming a large number of recesses 40, 40... On the surface that becomes the inner surface of the paper tube base paper 32, a deodorant is applied to the surface by the coating machine 61 and the deodorant layer is formed. 41 is formed. Deodorant coating can be performed using a known printing machine and coating machine with a deodorizing liquid obtained by mixing a deodorant with an appropriate binder or solvent. The coating amount of the deodorant liquid is desirably 5 to 80 g / m 2 . If it is this range, a deodorizing liquid can fully be applied with sufficient productivity, and a sufficient amount of deodorant can be applied.

本実施形態で用いる消臭剤の種類は、上記「ロールペーパー」の欄で述べたのと同様であり、ポリフェノール系消臭剤、スギ、ヒノキ等から抽出された精油類、二酸化チタン、二酸化アルミニウム、ベタイン化合物、ジルコニウム化合物、銅化合物、ゼオライト、活性炭、イオン交換樹指の少なくとも1種を含むものであるのが望ましい。粉状又は粒状のものを用いるのであれば、その平均粒子径は、0.5〜20μmであるのが望ましい。なお、ここでの平均粒子径も、マイクロトラック法によるメジアン径を意味する。また、粉状又は粒状の消臭剤であれば、好ましい担持量は0.1〜10g/m2である。 The type of deodorant used in the present embodiment is the same as described in the above-mentioned “roll paper” column, essential oils extracted from polyphenol deodorant, cedar, cypress, etc., titanium dioxide, aluminum dioxide , Betaine compounds, zirconium compounds, copper compounds, zeolites, activated carbons, and ion exchange resins are desirable. If a powdery or granular material is used, the average particle size is preferably 0.5 to 20 μm. Here, the average particle diameter also means the median diameter by the microtrack method. Moreover, if it is a powdery or granular deodorant, a preferable load is 0.1-10 g / m < 2 >.

また、本実施形態で用いるバインダーの種類は、上記「ロールペーパー」の欄で述べたのと同様であり、澱粉、カルボキシメチルセルロース、ポリビニルアルコールが例示できる。バインダーと消臭剤との混合割合は、消臭剤の効力やその性状が粉末状であるか液体状であるか等に応じて適宜調整すればよい。   Moreover, the kind of binder used by this embodiment is the same as having described in the column of the said "roll paper", and can illustrate starch, carboxymethylcellulose, and polyvinyl alcohol. What is necessary is just to adjust suitably the mixing ratio of a binder and a deodorizer according to the efficacy of the deodorizer, whether the property is a powder form, or a liquid form.

本実施形態に係る消臭剤の塗工に用いる塗工機61は、ロッドコーター、フレキソコーター、グラビアコーター、インクジェット印刷機、スプレー塗布装置等の既知の塗工機、印刷機のなかから、消臭液の性状に応じて適宜選択することができる。なかでも、多くの液体を対象物に均一に塗工することができ、また、粉状や粒状の消臭剤を含む粘度の高い消臭液にも十分に対応できることから、本実施形態に係る消臭剤層の塗工には、ロッドコーター、グラビアコーターが特に適する。グラビアコーターを用いる場合には、特に、線数15〜100線/インチ、面積率30%以上とするのが望ましい。紙管内面の全面に十分に消臭剤を付与することができる。   The coating machine 61 used for coating the deodorant according to the present embodiment includes a rod coater, a flexo coater, a gravure coater, an inkjet printing machine, a known coating machine such as a spray coating apparatus, and a printing machine. It can select suitably according to the property of a odor liquid. Among them, it is possible to uniformly apply a lot of liquids to an object, and it can sufficiently deal with a high-viscosity deodorant liquid containing powdery or granular deodorant, and thus according to this embodiment. A rod coater and a gravure coater are particularly suitable for coating the deodorant layer. When a gravure coater is used, it is particularly desirable that the number of lines is 15 to 100 lines / inch and the area ratio is 30% or more. A deodorant can be sufficiently applied to the entire inner surface of the paper tube.

他方、図示の本実施形態では、紙管原紙32上に消臭剤を塗工した後、好ましく、次段のコート剤の塗工を行なう前にヒーター(乾燥機)62及びヒートロール63を介して消臭剤の塗工部分の乾燥を行なうようにして、コート剤の塗工の前に乾燥された消臭剤層41が形成されるようにしている。この乾燥工程により、未乾燥の消臭液層上にコート剤が塗工されて所望のコート層42が形成されにくくなることや、後工程で濡れによるはり付きが生じたりすることが防止される。   On the other hand, in the illustrated embodiment, after applying the deodorant on the paper tube base paper 32, it is preferable to pass the heater (dryer) 62 and the heat roll 63 before applying the next coating agent. Thus, the deodorant coating portion is dried, so that the deodorant layer 41 dried before the coating of the coating agent is formed. This drying step prevents the coating agent from being coated on the undried deodorant liquid layer, making it difficult to form the desired coating layer 42, and preventing sticking due to wetting in subsequent steps. .

このようにして消臭剤層41を形成した後には、この消臭剤層41上に、塗工機64によりコート剤を塗工して、コート層42を形成する。このコート層42の形成により、本実施形態に係るロールペーパー10は、消臭剤層41の露出部分が低減され、消臭剤と外気との接触機会を低下されて、消臭剤の消臭機能が急速に低下することが防止されるようになる。   After the deodorant layer 41 is formed in this way, a coating agent is applied onto the deodorant layer 41 by the coating machine 64 to form the coat layer 42. By forming this coat layer 42, the exposed portion of the deodorant layer 41 is reduced in the roll paper 10 according to the present embodiment, the opportunity for contact between the deodorant and the outside air is reduced, and the deodorant of the deodorant is reduced. The function is prevented from rapidly decreasing.

また、消臭剤層41上にコート層42を形成するとことにより、長尺紙管30にカットされる前の筒状部分29の内面がマンドレルシャフト52と摺接する際に、消臭剤層41がマンドレルシャフト52と接し難くなり、その際の摩擦によって消臭剤41が剥がれ落ちることが防止される。さらに、マンドレルシャフトは、紙管原紙を単に巻き付けただけでは、その際の摩擦熱によってマンドレルシャフト上の温度が80〜100℃と高温になることがある。本実施形態では、マンドレルシャフト52に接する面にコート層42が存在しているので、摩擦熱自体の発生が抑制され、また摩擦熱による消臭剤層41の性能劣化も抑制される。このため長尺紙管30の形成速度を早めることができ、長尺紙管30の製造性を高めることができる。これにより、ロールペーパー10の生産効率を高めることができる。   Further, by forming the coat layer 42 on the deodorant layer 41, when the inner surface of the cylindrical portion 29 before being cut into the long paper tube 30 comes into sliding contact with the mandrel shaft 52, the deodorant layer 41. However, the deodorant 41 is prevented from peeling off due to friction at that time. Furthermore, when the mandrel shaft is simply wound around the paper tube base paper, the temperature on the mandrel shaft may be as high as 80 to 100 ° C. due to frictional heat at that time. In this embodiment, since the coat layer 42 exists on the surface in contact with the mandrel shaft 52, the generation of frictional heat itself is suppressed, and the performance deterioration of the deodorant layer 41 due to the frictional heat is also suppressed. For this reason, the formation speed of the long paper tube 30 can be increased, and the productivity of the long paper tube 30 can be improved. Thereby, the production efficiency of the roll paper 10 can be improved.

本実施形態に係るコート層42は、図6に示すように消臭剤層41上に全面的に設ける態様のほか、図8に示すように消臭剤層41上にコート層を部分的に設けてもよい。なお、図8中(a)は、紙管原紙32に消臭剤層41とコート層42を設けたものの部分平面図であり、(b)は(a)のb-b断面図である。このようにコート層42を部分的に形成すると、特に、図9に示すように、マンドレルシャフト52との当該面の接触部分がより低減され、紙管内面とマンドレルシャフト52との摩擦をより低減することができる。   As shown in FIG. 6, the coat layer 42 according to the present embodiment is partially provided on the deodorant layer 41 as shown in FIG. 6, and the coat layer is partially formed on the deodorant layer 41 as shown in FIG. It may be provided. 8A is a partial plan view of the paper tube base paper 32 provided with the deodorant layer 41 and the coat layer 42, and FIG. 8B is a cross-sectional view taken along the line bb of FIG. 8A. When the coat layer 42 is partially formed in this way, particularly, as shown in FIG. 9, the contact portion of the surface with the mandrel shaft 52 is further reduced, and the friction between the inner surface of the paper tube and the mandrel shaft 52 is further reduced. can do.

本実施形態に係るコート層を形成するコート剤は、上記「ロールペーパー」の欄で述べたものと同様であり、澱粉、カルボキシメチルセルロース、ポリビニルアルコール、パラフィン、酢酸ビニルの1種又は2種以上を混合して用いることができる。但し、酢酸ビニルにより形成されるコート層は、通気性が非常に低いものとなるので、消臭剤層上に全面に塗工するには適さず、部分的に形成する場合に用いるのが望ましい。これらのコート剤は、塗工性に優れ、塗工機によって効率よくコート層42を形成することができるとともに、表面の平滑性の高いコート層42を形成することができる。したがって、マンドレルシャフト52と筒状部分29の内面が摺接する際の摩擦熱が低減され、消臭剤の熱による劣化を低減することができる。加えて、長尺紙管30の製造性を高め、ロールペーパー10の生産効率を高めることができる。なお、これらのコート剤は、塗工に適するようにするために水や適宜の溶媒で粘度調整をすることができる。   The coating agent that forms the coating layer according to this embodiment is the same as that described in the above-mentioned “roll paper” column, and includes one or more of starch, carboxymethyl cellulose, polyvinyl alcohol, paraffin, and vinyl acetate. It can be used by mixing. However, since the coating layer formed of vinyl acetate has very low air permeability, it is not suitable for coating on the entire surface of the deodorant layer, and is preferably used when partially formed. . These coating agents are excellent in coating property, and can form the coating layer 42 efficiently with a coating machine, and can form the coating layer 42 with high surface smoothness. Therefore, frictional heat generated when the mandrel shaft 52 and the inner surface of the cylindrical portion 29 are in sliding contact with each other is reduced, and deterioration of the deodorant due to heat can be reduced. In addition, the productivity of the long paper tube 30 can be improved, and the production efficiency of the roll paper 10 can be increased. In addition, in order to make these coating agents suitable for coating, the viscosity can be adjusted with water or an appropriate solvent.

本実施形態に係るコート剤の塗工に用いる塗工機64は、フレキソコーター、グラビアコーター、インクジェット印刷機、スプレー塗布装置等の既知の塗工機、印刷機のなかから、コート剤の性状に応じて適宜選択することができる。部分的なコート層を形成する場合には、塗工機64は、十分な量のコート剤を簡易にパターン塗工することができるフレキソコーター、グラビアコーターが適する。コート層42を部分的に形成する場合の付与パターンは、特に限定されない。図6に示すような線状に配する態様のほか、例えば、網点状、円状、ブロック状など適宜の形状・模様に形成することができる。コート層42を部分的に形成する場合の、コート剤の総付与面積及び単位付与面積は、消臭効果の維持期間、マンドレルシャフト52との摩擦の低減効果などにより適宜調整する   The coating machine 64 used for the coating of the coating agent according to the present embodiment has a coating agent property from known coating machines and printing machines such as a flexo coater, a gravure coater, an ink jet printer, and a spray coating device. It can be appropriately selected depending on the case. When forming a partial coat layer, the coating machine 64 is suitably a flexo coater or a gravure coater that can easily apply a sufficient amount of a coating agent to a pattern. The application pattern when the coat layer 42 is partially formed is not particularly limited. In addition to the linear arrangement as shown in FIG. 6, for example, it can be formed in an appropriate shape / pattern such as a halftone dot shape, a circular shape, or a block shape. When the coat layer 42 is partially formed, the total application area and unit application area of the coating agent are adjusted as appropriate depending on the maintenance period of the deodorizing effect, the effect of reducing friction with the mandrel shaft 52, and the like.

他方、コート剤を塗工するにあたっては、コート層42の厚みが1〜100μm、より好ましくは1〜20μmとなるようにするのが望ましい。コート層42の厚みが1μm未満であると均一なコート層を形成するのが難しく、消臭剤層41と外気との接触機会を十分に低減できないおそれがあり、100μmを超えてもコスト高となるだけである。また、厚みが1μm未満であると、特に部分的にコート層42を形成した場合、筒状部分29がマンドレルシャフト52上を移動し、筒状部分29の内面とが摺接する際に、シャフト52と紙管内面に形成した消臭剤層41とが接触して、消臭剤層41を傷めるおそれが高まる。   On the other hand, when coating the coating agent, it is desirable that the thickness of the coating layer 42 be 1 to 100 μm, more preferably 1 to 20 μm. If the thickness of the coat layer 42 is less than 1 μm, it is difficult to form a uniform coat layer, and there is a possibility that the opportunity for contact between the deodorant layer 41 and the outside air cannot be sufficiently reduced. It only becomes. Further, when the thickness is less than 1 μm, particularly when the coat layer 42 is partially formed, when the tubular portion 29 moves on the mandrel shaft 52 and the inner surface of the tubular portion 29 comes into sliding contact, the shaft 52 And the deodorant layer 41 formed on the inner surface of the paper tube come into contact with each other, and the risk of damaging the deodorant layer 41 is increased.

他方、図示の本実施形態では、消臭剤層41上にコート剤を塗工した後、好ましく、次段の工程として、ヒーター(乾燥機)65及びヒートロール66によりコート剤の乾燥を行なうようにしている。この乾燥工程により、後工程で濡れによるはり付きが生じたりすることが防止される。   On the other hand, in the illustrated embodiment, the coating agent is preferably coated on the deodorant layer 41, and the coating agent is dried by the heater (dryer) 65 and the heat roll 66 as the next step. I have to. This drying process prevents sticking due to wetting in a subsequent process.

このようにして、他方の紙管原紙32の一方面に多数の凹部40,40…、消臭剤層41、コート層42を形成した後には、その他方の紙管原紙32を一旦巻き取って原反ロール32Aとしてもよいし、そのままマンドレルシャフト52に巻き付けるようにしてもよい。すなわち、図7において、消臭剤層41とコート層42とを形成した紙管原紙を巻き取った原反ロール32A’を図4の原反ロール32Aとして用いるようにしてもよいし、図7のP工程を図4のP部分に組み込むようにしてもよい。後者の場合には、紙管原紙の掛け替えの手間がなく、高速に消臭剤層41及びコート層42が形成された長尺の紙管30を生産することが可能となる。   In this way, after forming a large number of recesses 40, 40..., Deodorant layer 41, and coat layer 42 on one surface of the other paper tube base paper 32, the other paper tube base paper 32 is once wound up. The raw roll 32A may be used, or may be wound around the mandrel shaft 52 as it is. That is, in FIG. 7, the raw roll 32A ′ obtained by winding the paper tube base paper on which the deodorant layer 41 and the coat layer 42 are wound may be used as the raw roll 32A in FIG. The P process may be incorporated into the P portion of FIG. In the latter case, it is possible to produce a long paper tube 30 in which the deodorant layer 41 and the coating layer 42 are formed at high speed without the trouble of changing the paper tube base paper.

他方、本実施形態では、上記の長尺紙管30の製造と平行して又はその後において、ログ製造工程(図3中(B)にて、ログ70を製造する。なお、ログ70とは、業界においての一般用語であり、最終製品であるロールペーパー10の径と同径でありかつ幅が最終製品の複数個分ある中間製品である。   On the other hand, in the present embodiment, the log 70 is manufactured in the log manufacturing step ((B) in FIG. 3) in parallel with or after the manufacture of the long paper tube 30. It is a general term in the industry, and is an intermediate product that has the same diameter as the roll paper 10 that is the final product and has a width corresponding to a plurality of final products.

このログ70の製造は、連続的に又は段階的に、長尺紙管30と実質的に同幅のペーパーシート原紙71,71を、ロール71A,71Aから繰り出すとともに巻き付けてログ70を形成する。この巻き付けは、既知のワインダー装置X2が利用できる。なお、図示例は、二つのロール71A,71Aからペーパーシート原紙71,71を繰り出して、重ね合わせ部81にて2プライのペーパーシート原紙72とした後、ミシン目線形成装置82にてミシン目線の形成を行なった後、巻き取り装置83にて巻き取り2プライ構造となるようにしている。なお、図示の形態では、2つのロール71A、71Aからトイレットペーパー原紙71、71を繰り出し、積層構造とした2プライ構造のトイレットペーパー原紙72としているが、本発明に係るペーパーシート原紙は、この2プライに限定されず、1プライ若しくは3プライ以上であってもよい。さらには、複数プライ構造とする場合には、各原紙の米坪や物性等は同じである必要もない。また、予め積層されたシートを巻き取ったロールから積層シートを繰出して長尺紙管30に巻き付けてログ70を形成すようにしてもよい。   In manufacturing the log 70, paper sheets 71 and 71 having substantially the same width as the long paper tube 30 are unwound from the rolls 71 </ b> A and 71 </ b> A and wound to form the log 70 continuously or stepwise. A known winder device X2 can be used for this winding. In the illustrated example, the paper sheet base papers 71 and 71 are fed out from the two rolls 71A and 71A to form a two-ply paper sheet base paper 72 by the overlapping unit 81, and then the perforation line forming device 82 After the formation, the take-up device 83 has a take-up 2-ply structure. In the illustrated embodiment, toilet paper base sheets 71 and 71 are fed out from two rolls 71A and 71A to form a two-ply structure toilet paper base paper 72, but the paper sheet base paper according to the present invention is the two-sheet paper base paper. The ply is not limited and may be 1 ply or 3 plies or more. Furthermore, in the case of a multi-ply structure, it is not necessary for the base paper and physical properties of each base paper to be the same. Alternatively, the log 70 may be formed by feeding the laminated sheet from a roll obtained by winding a previously laminated sheet and winding it around the long paper tube 30.

なお、図示の本実施形態では、ミシン目線形成装置82を設けてミシン目線を付与する形態を示しているが、本発明では必ずしもミシン目線形成装置及びミシン目線の付与は必須ではない。また、本実施形態において、図示はしないが、ミシン目線付与装置82の前段に既知のコンタクトエンボス付与装置を設けてコンタクトエンボスを付与してもよいし、重ね合わせ部81の前段で各ペーパーシート71,71にエンボスロールでエンボスを付与するようにしてもよいし、その付与したエンボスの凸部頭頂に接着剤を付与して係る接着剤でシート同士を積層一体化するようにしてもよい。   In the illustrated embodiment, the perforated line forming device 82 is provided and the perforated line is provided. However, in the present invention, the perforated line forming device and the perforated line are not necessarily provided. In the present embodiment, although not shown, a known contact embossing device may be provided at the front stage of the perforation line giving device 82 to provide contact embossing, or each paper sheet 71 may be provided at the front stage of the overlapping portion 81. , 71 may be embossed with an embossing roll, or an adhesive may be applied to the top of the convex portion of the embossed surface, and the sheets may be laminated and integrated with the adhesive.

以上のように、ログ70を製造したならば、このログ70を既知のログアキュームレーターX3で複数本をストックしつつ後段のログカッター設備X4へと移動させる。そして、その後に図3中(C)に示すように、既知のログカッター91でログ70を製品幅に裁断し、個々のロールペーパー10,10…とする。このログの切断と同時に、長尺の紙管も裁断され、長尺の紙管も個々の紙管となるため、本実施形態により、上記「ロールペーパー」の欄で説明したロールペーパー10が製造される。   As described above, when the log 70 is manufactured, the log 70 is moved to the subsequent log cutter facility X4 while stocking a plurality of logs by the known log accumulator X3. And after that, as shown to (C) in FIG. 3, the log 70 is cut | judged to a product width with the known log cutter 91, and it is set as each roll paper 10,10 .... Simultaneously with the cutting of the log, the long paper tube is also cut, and the long paper tube becomes an individual paper tube. Thus, according to the present embodiment, the roll paper 10 described in the above-mentioned “roll paper” column is manufactured. Is done.

2…凹部、10…ロールペーパー、11…紙管、11A…紙管内面、12…ペーパーシート、L1…ロールペーパーの幅、L2…ロールペーパーの直径、L3…紙管内径、20…原紙層、21…消臭剤層、22…コート層、30…長尺の紙管、30A…長尺の紙管の内面、31,32…紙管原紙、31A,32A,32a…原反ロール、41…消臭剤層、42…コート層、51…糊付けロール、52…マンドレルシャフト、53…プーリー、54…平ベルト、58…カッター、61,64…塗工機、62,65…ヒーター、63,66…ヒーターロール、70…ログ、71…ペーパーシート原紙、71A…ロール、72…2プライのペーパーシート原紙、81…重ね合わせ部、82…ミシン目線形成装置、83…巻き取り手段、91…ログカッター、L4…消臭剤層の厚さ、L5…凹部の深さ、40…凹部、60…エンボス加工機、60A…エンボスロール、60B…受けロール。   2 ... concave portion, 10 ... roll paper, 11 ... paper tube, 11A ... paper tube inner surface, 12 ... paper sheet, L1 ... width of roll paper, L2 ... diameter of roll paper, L3 ... inner diameter of paper tube, 20 ... base paper layer, DESCRIPTION OF SYMBOLS 21 ... Deodorant layer, 22 ... Coat layer, 30 ... Long paper tube, 30A ... Inner surface of a long paper tube, 31, 32 ... Paper tube base paper, 31A, 32A, 32a ... Original fabric roll, 41 ... Deodorant layer, 42 ... coat layer, 51 ... gluing roll, 52 ... mandrel shaft, 53 ... pulley, 54 ... flat belt, 58 ... cutter, 61, 64 ... coating machine, 62, 65 ... heater, 63, 66 ... Heater roll, 70 ... Log, 71 ... Paper sheet base paper, 71A ... Roll, 72 ... Two-ply paper sheet base paper, 81 ... Overlapping part, 82 ... Perforation forming device, 83 ... Winding means, 91 ... Logger Tha, L4 ... deodorant layer thickness, L5 ... recess depth, 40 ... recess, 60 ... embosser, 60A ... embossing roll, 60B ... receiving roll.

Claims (5)

帯状のペーパーシートが紙管に巻かれているロールペーパーであって、
前記紙管の内面は、紙管原紙からなる原紙層、原紙層上に形成された消臭剤層、消臭剤層上に形成されたコート層の層構造を有し、前記原紙層の表面に多数の凹部が形成され、
前記消臭剤層その凹部の深さを超える厚さを有しかつ凹部内に入り込んでいる
ことを特徴とするロールペーパー。
A roll paper in which a strip-shaped paper sheet is wound around a paper tube,
The inner surface of the paper tube has a layer structure of a base paper layer made of a paper tube base paper, a deodorant layer formed on the base paper layer, and a coat layer formed on the deodorant layer, and the surface of the base paper layer A large number of recesses are formed in
The deodorant layer has a thickness that exceeds the depth of the recess and enters the recess ,
A roll paper characterized by that.
消臭剤層上に弱通気性のコート層が全面に形成されている、請求項1記載のロールペーパー。   The roll paper according to claim 1, wherein a weakly breathable coat layer is formed on the entire surface of the deodorant layer. 消臭剤層上に弱通気性もしくは非通気性であるコート層が部分的に形成されている、請求項1記載のロールペーパー。   The roll paper according to claim 1, wherein a coat layer that is weakly breathable or non-breathable is partially formed on the deodorant layer. 複数の紙管原紙のうち紙管内面に位置する紙管原紙の紙管内面側となる面に多数の凹部を形成する工程と、
その凹部を形成した面に消臭剤を塗工して前記凹部内に入り込みかつ凹部の深さを超える厚さの消臭剤層を形成する工程と、
消臭剤層の上にコート剤を塗工してコート層を形成する工程と、
複数の紙管原紙をマンドレルシャフトに螺旋状に巻いて連続的に筒状部分を形成し、その筒状に形成された部分をロールペーパーの複数倍幅以上の幅でカットして長尺の紙管を形成する紙管形成工程と、
長尺の紙管にロールペーパーの複数倍幅以上の幅のロールペーパー原紙を巻いてログを形成する工程と、
ログを切断して個々のロールペーパーにする工程と、
を有することを特徴とする、ロールペーパーの製造方法。
Forming a plurality of recesses on the surface of the paper tube base paper located on the inner surface of the paper tube among the plurality of paper tube base papers;
A step of applying a deodorant on the surface where the recess is formed and entering the recess and forming a deodorant layer having a thickness exceeding the depth of the recess;
Applying a coating agent on the deodorant layer to form a coating layer;
A plurality of paper tube base papers are spirally wound around a mandrel shaft to continuously form a cylindrical portion, and the cylindrical portion is cut with a width more than twice the width of roll paper to make a long paper A paper tube forming process for forming a tube;
A step of forming a log by winding a roll paper base paper having a width more than a multiple of the roll paper around a long paper tube;
Cutting logs into individual roll papers;
A method for producing roll paper, comprising:
原反ロールから紙管原紙を繰出して、消臭剤の塗工と、コート剤の塗工を行い、そのままマンドレルシャフトへの巻き付けを行なう、請求項4に記載のロールペーパーの製造方法。   The roll paper manufacturing method according to claim 4, wherein the paper tube base paper is fed out from the raw roll, coated with a deodorant and a coating agent, and wound around the mandrel shaft as it is.
JP2013070329A 2013-03-28 2013-03-28 Roll paper and roll paper manufacturing method Active JP6176967B2 (en)