JP4342827B2 - Method for manufacturing active matrix light-emitting device - Google Patents

Method for manufacturing active matrix light-emitting device Download PDF

Info

Publication number
JP4342827B2
JP4342827B2 JP2003120650A JP2003120650A JP4342827B2 JP 4342827 B2 JP4342827 B2 JP 4342827B2 JP 2003120650 A JP2003120650 A JP 2003120650A JP 2003120650 A JP2003120650 A JP 2003120650A JP 4342827 B2 JP4342827 B2 JP 4342827B2
Authority
JP
Japan
Prior art keywords
electrode
layer
light
voltage
layers
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP2003120650A
Other languages
Japanese (ja)
Other versions
JP2004031335A5 (en
JP2004031335A (en
Inventor
康行 荒井
友幸 岩淵
舜平 山崎
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Semiconductor Energy Laboratory Co Ltd
Original Assignee
Semiconductor Energy Laboratory Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Semiconductor Energy Laboratory Co Ltd filed Critical Semiconductor Energy Laboratory Co Ltd
Priority to JP2003120650A priority Critical patent/JP4342827B2/en
Publication of JP2004031335A publication Critical patent/JP2004031335A/en
Publication of JP2004031335A5 publication Critical patent/JP2004031335A5/ja
Application granted granted Critical
Publication of JP4342827B2 publication Critical patent/JP4342827B2/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Description

【0001】
【発明の属する技術分野】
本発明は、一対の電極間に一つの層又は複数の層の積層体に発光体を含む発光素子を有する発光装置及びその作製方法に係り、特に発光素子の作製工程で発生するショートやリーク箇所を、簡便な方法で修復することのできる技術に関する。
【0002】
【従来の技術】
有機エレクトロルミネセンス材料と呼ばれる発光媒体を用いて形成される発光素子は、例えば、一対の電極間に有機アミン系のホール輸送層、電子導電性を示すと共に発光性を示すトリス−8−キノリノラトアルミニウム錯体(Alq3)等の有機化合物を含む層を積層した構成が有り、6〜8Vの直流電圧の印加により数百cd/cm2の輝度を得ることが可能である。
【0003】
発光素子において、直接的又は間接的に発光に寄与する層を機能的に表現すれば、発光層、正孔注入層、電子注入層、正孔輸送層、電子輸送層等と区別することもできる。これらの機能的表現は、それを層として明確に区別できる場合もあれば、混合体として形成され明瞭に区別できない場合もある。極めて簡単な構成としては、陽極/発光層/陰極が順に積層された構造であり、この構造に加えて、陽極/正孔注入層/発光層/陰極や、陽極/正孔注入層/発光層/電子輸送層/陰極等の順に積層した構造等もある。
【0004】
正常に動作する発光素子は整流性を示し、所謂ダイオードと同じ電流−電圧特性が観測される。即ち、順方向バイアスを印加すると、印加電圧に対して指数関数的に電流は増大し、逆方向バイアスを印加した場合には、降伏電圧に達するまで殆ど電流は流れない。発光させるには電荷を注入させる必要があり、順方向バイアスを印加することになる。
【0005】
このような発光素子を電界効果型トランジスタで制御するアクティブマトリクス駆動方式の発光装置が知られている(例えば、特許文献1参照。)。これは、多結晶シリコンを用いた薄膜トランジスタ(TFT)の上層に二酸化シリコンから成る絶縁膜を介して有機エレクトロルミネセンス層が形成された構成が開示されている。また、陽極上にテーパー形状に加工された端部を有するパッシベーション層は、有機エレクトロルミネセンス層の下層側に位置している。また、陰極は仕事関数が4eVより低い材料が選択され、Ag又はAlのような金属とMgとを合金化したものが適用される。
【0006】
ところで、このような発光素子に対し、発光に関与しない逆方向電圧を印加すると、素子寿命が延びることが経験的に知られている。この現象を利用して、入力映像データの同期タイミングに応じて、非発光期間に逆方向電圧を印加するアクティブマトリクス駆動方式の発光装置が開示されている(例えば、特許文献2参照。)。
【0007】
一方、半導体の薄膜でダイオードを形成する太陽電池等では、逆方向電圧を印加することにより短絡部分を修復する方法が種々試みられ、その技術の一例は米国特許6,365,825号等で開示されている。この発明は逆方向電圧の印加により、短絡部分には集中的に電流が流れ、ジュール熱による発熱でその部分を絶縁化させることで短絡不良を修復することを可能とするものである。
【0008】
図9(A)は、ピンホール14や異物15の混入により短絡欠陥を含む発光素子を模式的に示し、その逆方向電圧の効果を説明する図である。陽極11と陰極13とから成る一対の電極間に、整流接触若しくは整流接合を形成する薄膜12を有するダイオード素子10に短絡不良部14があると、逆方向電圧を印加した際にその部位を介して逆方向飽和電流以上の電流が流れる。
【0009】
このダイオード素子10の電流対電圧特性は図9(B)に模式的に示すように、逆方向電圧を印加した時に点線で示すポイントA、Bで示すように、ある電圧で急激に逆方向電流が増加する。例えば、ピンホールを含む短絡欠陥部14に起因するような短絡欠陥は、その部位に陰極材料が回り込んで比較的低い電圧で逆方向電流が流れることになる。また、微小な異物15が含まれている場合には耐圧が低くなり、絶縁破壊により降伏電圧以下で逆方向電流が増大するような短絡欠陥部15を形成する。
【0010】
この時、短絡欠陥部14、15に電流が集中して流れ、電流密度が増加することにより発熱して高温になりその部位が変質して絶縁化する。これにより2回目以降の電圧走査では正常なダイオード特性を得ることができるようになる。仮に1回の走査で短絡欠陥部が修復されなくとも電圧走査を複数回繰り返せば修復する確率を増すことができる。このように、所定の逆方向電圧を印加することにより短絡箇所を絶縁化して修復することができる。
【0011】
逆方向電圧の印加による短絡箇所の修理は、比較的簡便に行うことができるが、その原理は電流集中による発熱現象を利用するものであり、瞬間的に大電流を流す必要がある。従って、適用する電源にはそれに見合った電流供給能力を有する定電圧源が要求される。
【0012】
【特許文献1】
特開平8−234683号公報
【特許文献2】
特開2001−109432号公報
【0013】
【発明が解決しようとする課題】
しかしながら、アクティブマトリクス駆動方式で用いられるTFTのドレイン電流は、図10で示すようにゲート電圧が決まると、ドレイン電圧をいくら増加させても流れる電流はほぼ飽和してしまう。つまり、TFTの飽和領域で動作させている限りは定電流源に接続されている場合と同等である。また、線形領域で動作させたとしても同様であり、所詮飽和電流以上の電流を流すことはできない。結局TFTを介して逆方向電圧を印加しても、最大電流値が限定されるため、図9で示すような短絡不良を十分絶縁化させることができないことになる。
【0014】
本発明はこのような問題点を解決するためのものであり、TFTをマトリクス状に配列させて成るアクティブマトリクス駆動方式の表示装置において、逆方向電圧の印加による欠陥部分の修復を完全に行い、発光素子のショートやリーク箇所を修復することにより輝度の安定化及び使用時における劣化を防ぐことを目的とする。
【0015】
【課題を解決するための手段】
本発明は上記問題点を解決するために、各画素にTFTが備えられたアクティブマトリクス駆動方式の画素構造を有する発光装置において、発光素子にTFTを介さずに逆方向電圧を印加することに特徴を有している。本発明はそれを可能とする画素構成及びその作製方法を提供する。
【0016】
本発明に係る発光装置の作製方法は、TFTと接続する第1電極と帯状に延在する第2電極とを同一絶縁表面に形成し、その第2電極上に発光体を含む一つの層又は複数の層の積層体と、それを介して第2電極と交差する発光素子の第3電極を形成し、第2電極と第3電極とに電圧を印加して短絡不良箇所を修復した後、第3電極を第1電極と接続する個別の第3電極に分離加工する各段階を有するものである。この作製方法において、第1電極と第2電極とは同一材料で形成することが可能であり、第1電極及び第2電極上の開口部が形成され、その端部を被覆する隔壁層を形成し、第3電極はその隔壁層上に延設するように形成することを許容する。
【0017】
帯状に延在する第2電極と発光体を含む一つの層又は複数の層の積層体上に第2電極と交差する第3電極との間に電圧を印加することで、TFTを介さずに逆方向電圧を印加して欠陥部分の修復を完全に行い、発光素子のショートやリーク箇所を修復することができる。第2電極と第3電極とは、TFTの上層に位置する層間絶縁膜上に形成し、互いに交差するように形成することで、この両電極間に自由に逆方向電圧を印加することが可能である。第3電極はその後エッチングにより分離加工して個別電極とすれば良い。
【0018】
また、本発明に係る発光装置の作製方法は、TFTに接続する個別画素電極を形成し、個別画素電極上に発光体を含む一つの層又は複数の層の積層体と、それを介して個別画素電極と重畳し互いに分離された第1共通電極と第2共通電極を形成し、第1共通電極と第2共通電極との間に電圧を印加して短絡不良箇所を修復する各段階を有するものである。この作製方法において、個別画素電極上に開口部を有し、その端部を被覆する隔壁層を形成し、隔壁層上に延設し互いに分離された第1共通電極と第2共通電極を形成することを許容する。
【0019】
発光体を含む一つの層又は複数の層の積層体上に第1共通電極と第2共通電極とを並列的に配設して、この両電極間に電圧を印加することで、TFTを介さずに逆方向電圧を印加して欠陥部分の修復を完全に行い、発光素子のショートやリーク箇所を修復することができる。
【0020】
逆方向電圧の印加に際しては、電圧をパルス状に印加して短絡不良個所を修復する方法を適用することが可能であり、パルス状であり、且つ階段状に増減する電圧を印加して短絡不良個所を修復することが可能である。
【0021】
本発明の発光装置は、TFTに接続する第1電極がマトリクス状に配置され、当該第1電極と帯状に延在する第2電極とが同一絶縁表面に形成され、第2電極上に発光体を含む一つの層又は複数の層の積層体と、それを介して第2電極と重畳して第1電極に接続する第3電極が配設されることで形成される発光素子が備えられているものである。この発明の構成において、第1電極及び第2電極上に開口部を有する隔壁層を有し、第2電極上に発光体を含む一つの層又は複数の層の積層体と、それを介して第2電極と重畳し隔壁層上に延設される第3電極を設けた構成としても良い。
【0022】
この発明の構成において、発光体を含む一つの層又は複数の層の積層体上に形成する第3電極を、第1電極と接続する構造とすることで、TFTを介さずに発光素子に逆方向電圧を印加することができ、欠陥部分の修復を完全に行い発光素子のショートやリーク箇所を修復することができる。
【0023】
本発明の発光装置は、TFTに接続する個別画素電極マトリクス状に配置され、当該個別画素電極は絶縁表面に形成され、個別画素電極上には、発光体を含む一つの層又は複数の層の積層体と、それを介して個別画素電極と重畳し、互いに交差することなく延設される、第1共通電極及び第2共通電極を有し、第1共通電極と第2共通電極とは発光時に同一の電位が印加され、非発光時には異なる電位が印加されるものである。この発明の構成において、個別画素電極上に開口部を有する隔壁層を有し、個別画素電極上の発光体を含む一つの層又は複数の層の積層体と、それを介して個別画素電極と重畳し、互いに交差することなく隔壁層上に延設される第1共通電極及び第2共通電極を有する構成としても良い。この第1共通電極と第2共通電極とは、互いに異なる電源に接続することでも、極性の異なる電圧印加を可能とし、容易とすることができる。
【0024】
この発明の構成により、発光体を含む一つの層又は複数の層の積層体上に第1共通電極と第2共通電極とを並列的に配設して、この両電極間に電圧を印加することで、TFTを介さずに逆方向電圧を印加して欠陥部分の修復を完全に行い、発光素子のショートやリーク箇所を修復することができる。
【0025】
【発明の実施の形態】
以下に、本発明の実施の形態について、図面を参照しながら詳細に説明する。
【0026】
(実施の形態1)
本実施の形態は、TFTに接続する第1電極と帯状に延在する発光素子の第2電極を同一絶縁表面に形成し、第2電極上に発光媒体の被膜を形成し、その上に第2電極と交差するように延設する発光素子の第3電極を形成し、短絡不良箇所を修復する逆方向電圧印加処理をした後、第3電極を個別電極に分離加工する発光装置について説明する。この形態の発光装置では、第2電極と第3電極とに電圧を印加して、短絡不良箇所を修復することが可能であり、逆方向電圧はパルス状に印加しても良いし、パルス状であり、且つ階段状に増減する電圧を印加して短絡不良個所を修復することもできる。
【0027】
まず、図2(A)に示すように第1絶縁膜102が形成された基板101上に、TFTのチャネル形成領域やソース・ドレイン領域等の不純物領域を形成する半導体膜103を形成する。基板101はガラス基板、石英基板等の絶縁性基板を適用する。第1絶縁膜102は、窒化珪素、酸化珪素、窒酸化珪素等の被膜又はそれらの積層体により50〜200nmの厚さで形成するものであり、基板101からの不純物をブロッキングする機能を有する被膜を用いる。半導体膜103は、好適にはプラズマCVD法又は減圧CVD法により30〜150nmの厚さに堆積形成した非晶質珪素膜を、熱又は光エネルギーの利用により結晶化させた結晶性珪素膜を適用する。第2絶縁膜104は、プラズマCVD法でTEOSで形成される酸化珪素、SiH4とN2Oを混合して形成する窒酸化珪素膜を用い、50〜150nmの厚さで形成する。また、他の材料として、窒酸化アルミニウム(AlOx1-x:x=0.01〜20原子%)、窒化アルミニウム、窒化シリコン等窒素を含む絶縁膜で形成することも可能である。ゲート電極105はAl、W、Ta、Ti、Mo等の金属材料うち少なくともいずれかを含むものとし、その断面形状は矩形、テーパー形状、或いは底部が上部よりも外側に凸設した異形としても良い。この場合、窒化物金属を第2絶縁膜104側に形成して密着性の向上と、選択加工を容易にさせても良い。
【0028】
図4はこの状態の上面図であり、A−A'線に対応する縦断面図が図2(A)に示されている。図4で示す上面図には、第2半導体膜20、ゲート電極を兼ねる走査信号線21、消去信号線22も同様に形成される。
【0029】
次に、図2(B)において第3絶縁膜106は窒化珪素を含むものとし、50〜200nmの厚さで形成する。第4絶縁膜107は酸化珪素又は窒酸化珪素膜で50〜100nmの厚さで形成する。半導体膜の水素化は第3絶縁膜106が含む水素を供給すれば足り、400〜450℃の加熱処理により行うことが可能である。
【0030】
図2(C)では、さらに第5絶縁膜108を形成する。第5絶縁膜108は感光性アクリル又は感光性ポリイミド等の有機化合物で形成し、厚さを0.5〜2μm程度として配線間の容量を低減させる。感光性材料を用いることにより、この第5絶縁膜108を形成すると同時に開口部110を形成することができる。開口部110は感光性材料を用いる場合、側壁が傾斜し、その上端部及び下端部が曲率をもって形成されるので、配線材料を被着させたときに被覆性よく形成することを可能としている。その後、開口部110の内側に開口部110'を形成するレジストマスク109を形成し、それをマスクとしてエッチング処理を行うことにより第2絶縁膜104、第3絶縁膜106及び第4絶縁膜107にコンタクトホールを形成する。
【0031】
図3(A)で示すように、TFTに接続する第1電極111と配線112(電源線)、配線113(データ線号線)はAl、W、Ta、Ti、Mo等の金属材料うち少なくともいずれかを含むものとして形成する。これらの配線はTiとAlの積層構造として、Tiを半導体膜と接触させることにより耐熱性を向上させる。画素領域において、帯状に延設する第2電極114は第1電極111と同じ材料で形成しても良いし、発光素子に対して正孔注入性又は電子注入性を考慮して、仕事関数の高い材料又は低い材料を選択して形成すれば良い。
【0032】
第2電極114を発光素子の陽極とする場合には仕事関数が4eV以上の材料を選択し、ITO(Indium Tin Oxide:酸化錫を混入した酸化インジウム)、酸化亜鉛、IZO((Indium Zinc Oxide:酸化亜鉛を混入した酸化インジウム)、窒化チタン、窒化タングステン等を用いる。また、第2電極114を陰極とする場合には仕事関数が4eV以下の材料を選択し、アルカリ金属又はアルカリ土類金属、或いはそれを含む合金又は化合物を用いる。例えば、AlLi、MgAg、LiF、CaF、CsF等を用いる。
【0033】
図5はこの状態の上面図であり、A−A'線に対応する縦断面図が図3(A)に示されている。また、図5で符号23は配線112等と同時に形成する画素内のTFTを接続する配線である。
【0034】
図3(B)に示すように第6絶縁層115は、第1電極111上に開口部117と第2電極114上に開口部116を有し、その端部を覆うように形成し、感光性樹脂材料を使うことにより側壁部を傾斜状とし、連続的な曲率を持たせて形成することができる。
【0035】
図3(C)に示すように、発光体を含む層118はこの第2電極114上及び第6絶縁層115の側壁部に沿って形成されるものであるから、この部位の連続的な曲面形状は発光体を含む層118の内部応力を緩和するのに適している。
【0036】
発光体を含む層118は、有機化合物又は無機化合物を含む電荷注入輸送媒体及び発光媒体であり、低分子系有機化合物、中分子系有機化合物、高分子系有機化合物から選ばれた一種又は複数種の層を含み、電子注入輸送性又は正孔注入輸送性の無機化合物と組み合わせても良い。発光体は、フェニルアントラセン誘導体、テトラアリールジアミン誘導体、キノリノール錯体誘導体、ジスチリルベンゼン誘導体などが適用可能でありこれをホスト物質として、クマリン誘導体、DCM、キナクリドン、ルブレン等が適用されるが、その他公知の材料を適用することが可能である。高分子系有機化合物としては、ポリパラフェニレンビニレン系、ポリパラフェニレン系、ポリチオフェン系、ポリフルオレン系などがあり、ポリ(パラフェニレンビニレン)(poly(p-phenylene vinylene)):(PPV)、ポリ(2,5−ジアルコキシ−1,4−フェニレンビニレン)(poly(2,5-dialkoxy-1,4-phenylene vinylene)):(RO−PPV)、ポリ(2−(2'−エチル−ヘキソキシ)−5−メトキシ−1,4−フェニレンビニレン)(poly[2-(2'-ethylhexoxy)-5-methoxy-1,4-phenylene vinylene]):(MEH−PPV)、ポリ(2−(ジアルコキシフェニル)−1,4−フェニレンビニレン)(poly[2-(dialkoxyphenyl)-1,4-phenylene vinylene]):(ROPh−PPV)、ポリパラフェニレン(poly[p-phenylene]):(PPP)、ポリ(2,5−ジアルコキシ−1,4−フェニレン)(poly(2,5-dialkoxy-1,4-phenylene)):(RO−PPP)、ポリ(2,5−ジヘキソキシ−1,4−フェニレン)(poly(2,5-dihexoxy-1,4-phenylene))、ポリチオフェン(polythiophene):(PT)、ポリ(3−アルキルチオフェン)(poly(3-alkylthiophene)):(PAT)、ポリ(3−ヘキシルチオフェン)(poly(3-hexylthiophene)):(PHT)、ポリ(3−シクロヘキシルチオフェン)(poly(3-cyclohexylthiophene)):(PCHT)、ポリ(3−シクロヘキシル−4−メチルチオフェン)(poly(3-cyclohexyl-4-methylthiophene)):(PCHMT)、ポリ(3,4−ジシクロヘキシルチオフェン)(poly(3,4-dicyclohexylthiophene)):(PDCHT)、ポリ[3−(4−オクチルフェニル)−チオフェン](poly[3-(4octylphenyl)-thiophene]):(POPT)、ポリ[3−(4−オクチルフェニル)−2,2ビチオフェン](poly[3-(4-octylphenyl)-2,2-bithiophene]):(PTOPT)、ポリフルオレン(polyfluorene):(PF)、ポリ(9,9−ジアルキルフルオレン)(poly(9,9-dialkylfluorene):(PDAF)、ポリ(9,9−ジオクチルフルオレン)(poly(9,9-dioctylfluorene):(PDOF)などが挙げられる。無機化合物材料としては、ダイヤモンドライクカーボン(DLC)、Si、Ge、及びこれらの酸化物又は窒化物であり、P、B、Nなどが適宜ドーピングされていても良い。またアルカリ金属又はアルカリ土類金属の、酸化物、窒化物又はフッ化物や、当該金属と少なくともZn、Sn、V、Ru、Sm、Inの化合物又は合金であっても良い。
【0037】
以上に掲げる材料は一例であり、これらを用いて正孔注入輸送層、正孔輸送層、電子注入輸送層、電子輸送層、発光層、電子ブロック層、正孔ブロック層などの機能性の各層を適宜積層することで発光素子を形成することができる。また、これらの各層を合わせた混合層又は混合接合を形成しても良い。
【0038】
カラーフィルターとの好適な組み合わせにおいては、白色発光を呈するものが好ましく、発光層に含まれる単一の色素で白色発光が得られない場合は、複数の色素を発光中心として使用し、同時に発光させて加法混色により白色化する。この場合には、異なる発光色を有する発光層を積層する方法や、一つ又は複数の発光層に複数の発光中心を含有させる方法などを適用することができる。白色発光を得る方法は光の3原色であるR(赤)G(緑)B(青)の各色を発光する発光層を積層して加法混色する方式と、2色の補色の関係を利用する方式とがある。補色を用いる場合には、青−黄色又は青緑−橙色の組み合わせが知られている。特に、後者の方が比較的視感度の高い波長領域の発光を利用できる点で有利であると考えられている。
【0039】
発光体を含む層118に低分子系有機発光媒体を用いる一例では、第2電極(陰極)114上に電子注入輸送層、赤色発光層、緑色発光層、正孔輸送層、青色発光層が順次積層された構造である。具体的には、正孔輸送層として1,2,4-トリアゾール誘導体(p−EtTAZ)を適用し3nmにすると、p−EtTAZ層中の正孔通過量が増えて緑色発光層として用いるトリス(8−キノリラト)アルミニウム(Alq3)にも正孔が注入されて発光が得られる。この構造においては青色発光層としてTPDの青色にAlq3の緑色が混ざった青緑色の発光が得られる。この発光に赤色を加え白色発光を実現するには赤色発光層としてAlq3かTPDのどちらかに赤色発光色素をドープすれば良い。赤色発光色素としてはナイルレッドなどを適用することができる。
【0040】
また、発光体を含む層118の他の構成として、第2電極(陰極)114側から、電子注入輸送層、電子輸送層、発光層、正孔輸送層、正孔注入輸送層とすることもできる。この場合適した材料の組み合わせは、電子注入輸送層としてAlq3を15nmの厚さで、電子輸送層としてフェニルアントラセン誘導体を20nmの厚さで形成する。発光層はテトラアリールベンジジン誘導体とフェニルアントラセン誘導体とが体積比1:3で混合し、且つスチリルアミン誘導体を3体積%含ませる25nmの第1発光層と、テトラアリールベンジジン誘導体と10,10'−ビス[2-ビフェニルイル]−9,9'−ビアンスリル(フェニルアントラセン誘導体)とを体積比1:3で混合し、且つナフタセン誘導体を3重量%含ませる40nmの第2発光層とを積層させた構成とする。正孔輸送層はN,N,N',N'−テトラキス−(3-ビフェニル-1-イル)ベンジジン(テトラアリールベンジジン誘導体)を20nmの厚さに形成し、正孔注入層としてN,N'−ジフェニル-N,N'−ビス[N-フェニル-N-4-トリル(4-アミノフェニル)]ベンジジンを30nmの厚さに形成する。
【0041】
上記構造において、電子注入輸送層を無機電子注入輸送層を用いても良い。無機電子輸送層としてはn型化したダイヤモンドライクカーボン(DLC)を適用することができる。DLC膜のn型化には燐などを適宜ドープすれば良い。その他に、アルカリ金属元素、アルカリ土類金属元素、及びランタノイド系元素から選択される一種の酸化物と、Zn、Sn、V、Ru、Sm、Inから選択される1種以上の無機材料を適用することができる。
【0042】
発光体を含む層118の上にITO、ZnO、SnO2等の酸化物導電性材料層119を10〜30nm程度の厚さで形成する。図示しないが、酸化物導電性材料層119と発光体を含む層118との間には、仕事関数が3eV以下である、アルカリ金属又はアルカリ土類金属を含む層を形成しておく。
【0043】
さらに、帯状に延設する第2電極114と交差するように形成され、同様に帯状の第3電極120を延設する。第3電極120は第1電極111と酸化物透明導電性材料119と接触するように形成する。第3電極120は第2電極114と極性が反対となる材料を選択して形成する。
【0044】
図6はこの状態の上面図であり、A−A'線に対応する縦断面図が図3(C)に示されている。よって、第2電極114と第3電極120との交差部において、発光体を含む層118と酸化物導電性材料層119とを介在させることにより電場を印加することことができる。
【0045】
この状態で、逆方向電圧を印加することが可能となる。即ち、第2電極114を陽極、第3電極を陰極とする極性に対しては、第3電極に正の電圧を印加する。また、第2電極114を陰極、第3電極を陽極とする極性に対しては、第3電極に負の電圧を印加する。電圧は直流電圧を印加しても良いし、パルス状の電圧(図19(A))を印加しても良いし、パルス状であり且つ階段状に増減する電圧(図19(B))を印加しても良い。
【0046】
図8は一つの層又は複数の層の積層体に発光体を含む発光素子を画素毎に設け、当該画素をマトリクス状に配列させた状態で逆方向電圧を印加する方法を示す上面図あり、帯状に形成した第2電極114と、第3電極120との間で定電圧電源125により逆方向電圧を印加する。この状態では第3電極120は共通電極である。第2電極114、第3電極120と定電圧源125との接続は、画素部の外部にてプローブを用いて接触コンタクトを形成すれば良い。各画素の下層には、TFTが設けられているが、この構成においてTFTは電気的に何ら関与しない。
【0047】
図9で説明したように、もし微小な短絡箇所があると、逆方向電圧を印加した場合に本来流れないはずの電流が短絡箇所に集中して流れ、その部分がジュール熱で発熱することにより変質し絶縁化を図ることができる。発光体を含む層118は主として有機化合物により形成され、炭素を主成分とする材料で大部分は形成される。短絡箇所の形態は様々であるが、概略、酸化物導電性材料層119や第3電極が空孔にしみ出す形で形成される。或いは、発光体を含む層118に異物が介在する形態となっていることが多い。逆方向電圧印加による発熱はこの部分において、第3電極の金属材料を変質させるが、酸化物導電性材料は酸素を供給して金属材料を酸化させ絶縁させるのに有効に作用する。
【0048】
逆方向電圧により短絡箇所を修復した後、図1に示すように第3電極上に第7絶縁膜122を形成して、さらに個別電極の形状に合わせたパターンとする。第7絶縁膜122は窒化珪素で形成し、このパターンをマスクとして、それと重ならない第3電極をエッチング加工して除去する。こうしてTFT150と接続する発光素子100を形成することができる。発光素子100は第2電極114、発光体を含む層118、酸化物導電性材料119、第3電極121が積層して形成されている。
【0049】
図7はこの状態の上面図であり、A−A'線に対応する縦断面図が図1に示されている。こうして個別電極となる第3電極121が形成される。さらに、全体を覆う第8絶縁膜122は保護膜として外部から水分等の侵入を防止する。
【0050】
このような製造方法により、アクティブマトリクス駆動方式の画素構成としても、TFTを介さずに逆方向電圧を印加することができ、欠陥個所がある場合には瞬間的に十分な電流を供給してその部分を変質させて絶縁化させることができる。
尚、本発明は上記形態に限定されるものではなく、その要旨を逸脱しない範囲で各種の変形を許容するものである。
【0051】
(実施の形態2)
本実施の形態は、TFTに接続する個別電極上に発光体を含む一つの層又は複数の層の積層体と、それを介して個別画素電極と重畳し互いに分離された第1共通電極と第2共通電極を形成し、第1共通電極と第2共通電極との間に電圧を印加して短絡不良箇所を修復するものである。
【0052】
図11は本実施の形態における画素部の等価回路図を示す。走査信号線305、消去信号線306、データ線307、電源線308、選択用TFT301、消去用TFT302、制御用TFT303が備えられた構成の一例を示している。発光素子304の一方の端子は制御用TFT303に接続されるが、他方の側は第1共通配線309と第2共通配線310とに分かれて接続している。
【0053】
第1共通電極309と第2共通電極310はそれぞれ異なる極性の定電圧源311と312に接続され、スイッチ313により適宜接続状態を変えることにより発光素子304に効果的に逆方向電圧を印加する仕組みとなっている。
【0054】
このような画素の構成において、第1共通配線と第2共通配線とは図12に示すような形態で実現される。第1共通配線123と第2共通配線124は画素部の外側において、それらに交差する形で形成される接続配線315、316により連結して、それぞれ異なる極性の定電圧源311と312に接続することで実現する。
【0055】
発光素子304と制御用TFT303の構成の一例として、その縦断面図を図14に示す。基板101、第1絶縁膜102、半導体膜103、第2絶縁膜104、ゲート電極105、第3絶縁膜106、第4絶縁膜107、第5絶縁膜108、第1電極111、配線(電源線)112、第6絶縁膜115の構成は実施の形態1と同様である。図15はこの状態の上面図であり、A−A'線に対応する縦断面図が図14に示されている。
【0056】
発光素子304は第5絶縁膜108上に形成される個別画素電極122と、発光体を含む層116、酸化物導電性材料117とが積層され、その上に第1共通電極123と第2共通電極124が形成された構成となっている。この共通電極は同じ材料で形成され、ダイオードとして見た場合には同じ方向に整流性を持つ。第1共通電極123と第2共通電極124は、逆方向電圧を印加する場合には異なる電位が付与され、その電位が交互に入替ることにより発光素子の修復を可能としている。
【0057】
図13は本実施の形態において発光素子の修復がどのように成されるのかを模式的に説明する回路図である。図13(A)は第1共通配線309が高電位、第2共通配線310が低電位に接続された状態であり、発光素子に短絡欠陥若しくはそれに近いリーク箇所が含まれていない正常な素子には、逆方向飽和電流以上の電流は流れない。一方、素子Aに短絡欠陥が内在するような場合には、その部分を通して電流が流れる(異常A)。この場合、短絡欠陥は修復可能である。しかし、素子Bに短絡欠陥があるような場合(異常B)には、このバイアス状態でその欠陥を修復することはできない。素子Aと素子Bとの両方に短絡欠陥がある場合(異常C)には、素子A、素子B共に欠陥の修復が可能であるが、素子Aの欠陥の修復が早く完了すると素子Bの欠陥の修復は不可能となる。
【0058】
素子Aと素子Bの欠陥を共に修復するには、図13(B)で示すように第1共通配線309と第2共通配線310とのバイアス状態を反転させれば良い。逆方向電圧の印加に際しては、電圧をパルス状に印加して短絡不良個所を修復する方法を適用することが可能であり、パルス状であり、且つ階段状に増減する電圧を印加して短絡不良個所を修復することが可能である。
【0059】
このような画素の構成により、アクティブマトリクス駆動方式の画素構成としても、TFTを介さずに逆方向電圧を印加することができ、欠陥個所がある場合には瞬間的に十分な電流を供給してその部分を変質させて絶縁化させることができる。
尚、本発明は上記形態に限定されるものではなく、その要旨を逸脱しない範囲で各種の変形を許容するものである。
【0060】
(実施の形態3)
逆方向電圧の印加による発光素子の修復の実際的な一例は図16〜図18に示されている。発光素子は一対の電極間に発光体を含む層として、CuPc、α−NPD、ドーパントとしてDCMを添加したAlq3、及びノンドープのAlq3を積層した構造である。図16では、順方向電圧から逆方向電圧まで±12Vの電圧を掃引した時の電流電圧特性を示している。順方向電圧を印加した時に、5V以下の領域において異常な順方向電流の増加が見られ、逆方向電圧を印加した時にも0〜−5Vの範囲において異常な逆方向電流の増加が見られる。この時逆方向電流は一旦急激に増加するが、その後すぐに元の電流値まで減少している。つまり、短絡箇所が修復された状態であり、局部的に高密度の電流が流れることによりその部位が発熱し、絶縁化することを意味している。しかしながら、その反応が十分でないと、或いは他に同様な短絡箇所が内在していると、図17に示すように2回目の電圧掃引においても同様な現象が観測されることがある。このような順方向から逆方向への電圧掃引又は逆方向の電圧掃引を、1回又は複数回繰り返すと図18に示すようにきれいな電流電圧特性を得ることができる。
【0061】
【発明の効果】
以上説明したように、本発明によれば、発光体を含む一つの層又は複数の層の積層体上に第1共通電極と第2共通電極とを並列的に配設して、この両電極間に電圧を印加することで、TFTを介さずに逆方向電圧を印加して欠陥部分の修復を完全に行い、発光素子のショートやリーク箇所を修復することができる。
【0062】
それにより、発光装置の不要な消費電流を抑えることで発熱を抑えて、発光素子の非発光点の増加及び拡大等の劣化を低減することが可能となる。
【図面の簡単な説明】
【図1】 実施の形態1において画素の構成を説明する縦断面図。
【図2】 実施の形態1において画素の作製工程を説明する縦断面図。
【図3】 実施の形態1において画素の作製工程を説明する縦断面図。
【図4】 実施の形態1において画素の作製工程を説明する上面図。
【図5】 実施の形態1において画素の作製工程を説明する上面図。
【図6】 実施の形態1において画素の作製工程を説明する上面図。
【図7】 実施の形態1における画素の構造を示す上面図。
【図8】 実施の形態1における画素部に逆方向電圧を印加する状態を示す上面図。
【図9】 逆方向電圧の印加により欠陥個所が修復されることを模式的に説明する縦断面図とその電流対電圧特性を示すグラフ。
【図10】 TFTのドレイン電圧対ドレイン電流の関係を模式的に示すグラフ。
【図11】 実施の形態2における画素部の構成を示す等価回路図。
【図12】 実施の形態2における画素部の構成を示す上面図。
【図13】 実施の形態2において逆方向電圧により発光素子が修復される原理を説明する等価回路図。
【図14】 実施の形態2における画素の構造を示す縦断面図。
【図15】 実施の形態2における画素の構造を示す上面図。
【図16】 発光素子に1回目の電圧掃引を行った時の電流電圧特性を示すグラフ。
【図17】 発光素子に2回目の電圧掃引を行った時の電流電圧特性を示すグラフ。
【図18】 発光素子に3回目の電圧掃引を行った時の電流電圧特性を示すグラフ。
【図19】 本発明においてパルス状の逆方向電圧を印加するときの電圧波形を示す図。
[0001]
BACKGROUND OF THE INVENTION
The present invention relates to a light-emitting device having a light-emitting element including a light-emitting body in a single layer or a stack of a plurality of layers between a pair of electrodes, and a method for manufacturing the light-emitting device. It is related with the technique which can be repaired by a simple method.
[0002]
[Prior art]
A light-emitting element formed using a light-emitting medium called an organic electroluminescent material includes, for example, an organic amine-based hole transport layer between a pair of electrodes, Tris-8-quinolino that exhibits electronic conductivity and also emits light. Latoaluminum complex (Alq Three ) And other layers containing organic compounds, and several hundred cd / cm by applying a DC voltage of 6-8V 2 Can be obtained.
[0003]
In a light-emitting element, if a layer that directly or indirectly contributes to light emission is functionally expressed, it can be distinguished from a light-emitting layer, a hole injection layer, an electron injection layer, a hole transport layer, an electron transport layer, and the like. . These functional expressions may be clearly distinguishable as a layer or may be formed as a mixture and not clearly distinguishable. An extremely simple structure is a structure in which an anode / light emitting layer / cathode is laminated in order, and in addition to this structure, an anode / hole injection layer / light emitting layer / cathode and an anode / hole injection layer / light emitting layer. There is a structure in which / electron transport layer / cathode and the like are laminated in this order.
[0004]
A light-emitting element that operates normally exhibits rectification, and the same current-voltage characteristics as a so-called diode are observed. That is, when a forward bias is applied, the current increases exponentially with respect to the applied voltage, and when a reverse bias is applied, almost no current flows until the breakdown voltage is reached. In order to emit light, it is necessary to inject electric charge, and a forward bias is applied.
[0005]
An active matrix driving type light emitting device in which such a light emitting element is controlled by a field effect transistor is known (see, for example, Patent Document 1). This discloses a configuration in which an organic electroluminescence layer is formed on an upper layer of a thin film transistor (TFT) using polycrystalline silicon via an insulating film made of silicon dioxide. Further, the passivation layer having an end processed into a tapered shape on the anode is located on the lower layer side of the organic electroluminescence layer. For the cathode, a material having a work function lower than 4 eV is selected, and an alloy of a metal such as Ag or Al and Mg is used.
[0006]
By the way, it is empirically known that, when a reverse voltage not related to light emission is applied to such a light emitting element, the element life is extended. By utilizing this phenomenon, an active matrix driving type light emitting device is disclosed that applies a reverse voltage during a non-light emitting period in accordance with the synchronization timing of input video data (see, for example, Patent Document 2).
[0007]
On the other hand, in a solar cell or the like in which a diode is formed of a semiconductor thin film, various methods for repairing a short-circuited portion by applying a reverse voltage have been attempted, and an example of the technique is disclosed in US Pat. No. 6,365,825. According to the present invention, when a reverse voltage is applied, a current flows intensively in the short-circuit portion, and the short-circuit failure can be repaired by insulating the portion by heat generation due to Joule heat.
[0008]
FIG. 9A is a diagram schematically showing a light-emitting element including a short-circuit defect due to mixing of pinholes 14 and foreign matter 15 and explaining the effect of the reverse voltage. If there is a short-circuit defective portion 14 in the diode element 10 having the thin film 12 that forms a rectifying contact or a rectifying junction between a pair of electrodes composed of the anode 11 and the cathode 13, when a reverse voltage is applied, Current exceeding the reverse saturation current flows.
[0009]
As shown schematically in FIG. 9B, the current-voltage characteristics of the diode element 10 are such that when a reverse voltage is applied, the reverse current suddenly increases at a certain voltage as indicated by points A and B indicated by dotted lines. Will increase. For example, a short-circuit defect such as that caused by the short-circuit defect portion 14 including a pinhole causes the cathode material to wrap around the portion, and a reverse current flows at a relatively low voltage. In addition, when the minute foreign matter 15 is included, the short-circuit defect portion 15 is formed such that the breakdown voltage is low, and the reverse current increases below the breakdown voltage due to dielectric breakdown.
[0010]
At this time, current concentrates and flows in the short-circuit defect portions 14 and 15, and when the current density increases, heat is generated and the temperature becomes high, and the portion is altered and insulated. As a result, normal diode characteristics can be obtained in the second and subsequent voltage scans. Even if the short-circuit defect portion is not repaired by one scan, the probability of repair can be increased by repeating the voltage scan a plurality of times. In this way, by applying a predetermined reverse voltage, the short-circuited portion can be insulated and repaired.
[0011]
Repair of a short-circuited portion by applying a reverse voltage can be performed relatively easily, but the principle is to use a heat generation phenomenon due to current concentration, and it is necessary to flow a large current instantaneously. Therefore, a constant voltage source having a current supply capability corresponding to the power supply to be applied is required.
[0012]
[Patent Document 1]
JP-A-8-234683
[Patent Document 2]
JP 2001-109432 A
[0013]
[Problems to be solved by the invention]
However, the drain current of the TFT used in the active matrix driving method is almost saturated when the gate voltage is determined as shown in FIG. 10, no matter how much the drain voltage is increased. That is, as long as the TFT is operated in the saturation region, it is equivalent to the case where it is connected to a constant current source. Moreover, even if it is operated in the linear region, the same is true, and it is impossible to pass a current exceeding the saturation current. Eventually, even if a reverse voltage is applied through the TFT, the maximum current value is limited, and therefore it is not possible to sufficiently insulate a short circuit defect as shown in FIG.
[0014]
The present invention is for solving such problems, and in an active matrix driving type display device in which TFTs are arranged in a matrix, a defective portion is completely repaired by applying a reverse voltage, An object is to stabilize luminance and prevent deterioration during use by repairing a short circuit or a leak portion of a light emitting element.
[0015]
[Means for Solving the Problems]
In order to solve the above problems, the present invention is characterized in that a reverse voltage is applied to a light emitting element without passing through a TFT in a light emitting device having an active matrix driving type pixel structure in which each pixel is provided with a TFT. have. The present invention provides a pixel configuration and a method for manufacturing the pixel configuration that enable this.
[0016]
In the method for manufacturing a light-emitting device according to the present invention, a first electrode connected to a TFT and a second electrode extending in a strip shape are formed on the same insulating surface, and a single layer including a light emitter on the second electrode or After forming a laminated body of a plurality of layers and a third electrode of the light emitting element intersecting with the second electrode through it, a voltage is applied to the second electrode and the third electrode to repair the short-circuit defective portion, Each step includes separating and processing the third electrode into individual third electrodes connected to the first electrode. In this manufacturing method, the first electrode and the second electrode can be formed of the same material, an opening on the first electrode and the second electrode is formed, and a partition layer that covers the end portion is formed. The third electrode is allowed to be formed so as to extend on the partition layer.
[0017]
By applying a voltage between the second electrode extending in a strip shape and the third electrode crossing the second electrode on a single layer or a stacked layer of a plurality of layers including the light emitter, without passing through the TFT By applying a reverse voltage, the defective portion can be completely repaired, and a short circuit or a leaked portion of the light emitting element can be repaired. The second electrode and the third electrode are formed on the interlayer insulating film located on the upper layer of the TFT and formed so as to cross each other, so that a reverse voltage can be freely applied between the two electrodes. It is. The third electrode may then be separated into individual electrodes by etching.
[0018]
In addition, in the method for manufacturing a light-emitting device according to the present invention, an individual pixel electrode connected to a TFT is formed, and a single layer or a stack of a plurality of layers including a light-emitting body is formed on the individual pixel electrode, and the individual body is interposed therebetween Forming a first common electrode and a second common electrode which are overlapped with the pixel electrode and separated from each other, and applying a voltage between the first common electrode and the second common electrode to repair a short-circuit defective portion; Is. In this manufacturing method, an opening is formed on an individual pixel electrode, a partition layer covering the end is formed, and a first common electrode and a second common electrode which are extended from the partition layer and separated from each other are formed. Allow to do.
[0019]
A first common electrode and a second common electrode are arranged in parallel on a single layer or a laminate of a plurality of layers including a light emitter, and a voltage is applied between the two electrodes so that the TFT is interposed. Without applying a reverse voltage, the defective portion can be completely repaired, and the short circuit or the leaked portion of the light emitting element can be repaired.
[0020]
When applying reverse voltage, it is possible to apply a method of applying voltage in a pulsed manner to repair a short-circuit defective part. Applying a voltage that is pulsed and increases or decreases stepwise applies a short-circuit failure. It is possible to repair the location.
[0021]
In the light emitting device of the present invention, the first electrode connected to the TFT is arranged in a matrix, the first electrode and the second electrode extending in a strip shape are formed on the same insulating surface, and the light emitter is formed on the second electrode. A light-emitting element formed by disposing a single electrode layer or a stacked layer of a plurality of layers, and a third electrode connected to the first electrode so as to overlap with the second electrode through the stacked body. It is what. In the structure of this invention, the first electrode and the second electrode have a partition layer having an opening, and the second electrode includes a single layer or a stack of a plurality of layers including the light emitter, A configuration may be employed in which a third electrode that overlaps with the second electrode and extends on the partition wall layer is provided.
[0022]
In the structure of the present invention, the third electrode formed over one layer including the light-emitting body or the stacked body of the plurality of layers is connected to the first electrode, so that the light-emitting element can be reversed without the TFT. A directional voltage can be applied, and the defective portion can be completely repaired to repair a short circuit or a leak portion of the light emitting element.
[0023]
The light-emitting device of the present invention is arranged in a matrix of individual pixel electrodes connected to TFTs, the individual pixel electrodes are formed on an insulating surface, and a single layer or a plurality of layers including a light emitter are formed on the individual pixel electrodes. The stacked body has a first common electrode and a second common electrode that overlap with the individual pixel electrode through the stacked body and extend without crossing each other, and the first common electrode and the second common electrode emit light. Sometimes the same potential is applied, and different potentials are applied when no light is emitted. In the configuration of the present invention, the individual pixel electrode includes a partition layer having an opening, and includes one layer or a plurality of layers including a light emitter on the individual pixel electrode, and the individual pixel electrode interposed therebetween. It is good also as a structure which has a 1st common electrode and a 2nd common electrode which overlap and are extended on a partition layer, without mutually crossing. By connecting the first common electrode and the second common electrode to different power sources, it is possible to easily apply voltages having different polarities.
[0024]
According to the configuration of the present invention, the first common electrode and the second common electrode are arranged in parallel on one layer or a stacked layer of a plurality of layers including the light emitter, and a voltage is applied between the two electrodes. Thus, it is possible to completely repair the defective portion by applying a reverse voltage without going through the TFT, and to repair the short circuit or the leak portion of the light emitting element.
[0025]
DETAILED DESCRIPTION OF THE INVENTION
Hereinafter, embodiments of the present invention will be described in detail with reference to the drawings.
[0026]
(Embodiment 1)
In the present embodiment, the first electrode connected to the TFT and the second electrode of the light-emitting element extending in a strip shape are formed on the same insulating surface, the film of the light-emitting medium is formed on the second electrode, and the first electrode is formed on the second electrode. A light-emitting device that forms a third electrode of a light-emitting element extending so as to intersect with two electrodes, performs reverse voltage application processing to repair a short-circuit defective portion, and then separates and processes the third electrode into individual electrodes will be described. . In the light-emitting device of this embodiment, it is possible to repair a short-circuit defective portion by applying a voltage to the second electrode and the third electrode, and the reverse voltage may be applied in a pulsed manner. In addition, it is possible to repair a short-circuit defective portion by applying a voltage that increases or decreases stepwise.
[0027]
First, as shown in FIG. 2A, a semiconductor film 103 for forming an impurity region such as a channel formation region or a source / drain region of a TFT is formed on a substrate 101 on which a first insulating film 102 is formed. As the substrate 101, an insulating substrate such as a glass substrate or a quartz substrate is used. The first insulating film 102 is formed of a film of silicon nitride, silicon oxide, silicon oxynitride or the like or a laminate thereof with a thickness of 50 to 200 nm, and has a function of blocking impurities from the substrate 101. Is used. The semiconductor film 103 is preferably a crystalline silicon film obtained by crystallizing an amorphous silicon film deposited to a thickness of 30 to 150 nm by plasma CVD or low pressure CVD using heat or light energy. To do. The second insulating film 104 is made of silicon oxide, SiH formed of TEOS by plasma CVD. Four And N 2 A silicon oxynitride film formed by mixing O is used to form a thickness of 50 to 150 nm. In addition, as other materials, aluminum oxynitride (AlO x N 1-x : X = 0.01 to 20 atomic%), and an insulating film containing nitrogen such as aluminum nitride or silicon nitride can also be used. The gate electrode 105 includes at least one of metal materials such as Al, W, Ta, Ti, and Mo, and the cross-sectional shape thereof may be a rectangle, a taper shape, or a deformed shape in which a bottom portion protrudes outward from the top. In this case, nitride metal may be formed on the second insulating film 104 side to improve adhesion and facilitate selective processing.
[0028]
FIG. 4 is a top view of this state, and a longitudinal sectional view corresponding to the line AA ′ is shown in FIG. In the top view shown in FIG. 4, the second semiconductor film 20, the scanning signal line 21 also serving as the gate electrode, and the erasing signal line 22 are formed in the same manner.
[0029]
Next, in FIG. 2B, the third insulating film 106 includes silicon nitride and is formed to a thickness of 50 to 200 nm. The fourth insulating film 107 is formed of a silicon oxide or silicon oxynitride film with a thickness of 50 to 100 nm. Hydrogenation of the semiconductor film only needs to be performed by supplying hydrogen contained in the third insulating film 106, and can be performed by heat treatment at 400 to 450 ° C.
[0030]
In FIG. 2C, a fifth insulating film 108 is further formed. The fifth insulating film 108 is formed of an organic compound such as photosensitive acrylic or photosensitive polyimide, and has a thickness of about 0.5 to 2 μm to reduce the capacitance between the wirings. By using a photosensitive material, the opening 110 can be formed simultaneously with the formation of the fifth insulating film 108. When the photosensitive material is used for the opening 110, the side wall is inclined and the upper end and the lower end thereof are formed with a curvature, so that the opening 110 can be formed with good coverage when the wiring material is deposited. Thereafter, a resist mask 109 for forming an opening 110 ′ is formed inside the opening 110, and etching is performed using the resist mask 109 as a mask to form the second insulating film 104, the third insulating film 106, and the fourth insulating film 107. A contact hole is formed.
[0031]
As shown in FIG. 3A, the first electrode 111 connected to the TFT, the wiring 112 (power supply line), and the wiring 113 (data line number line) are at least one of metal materials such as Al, W, Ta, Ti, and Mo. It is formed as including. These wirings have a laminated structure of Ti and Al, and improve heat resistance by bringing Ti into contact with the semiconductor film. In the pixel region, the second electrode 114 extending in a strip shape may be formed of the same material as the first electrode 111, and the work function of the light emitting element is considered in consideration of hole injection property or electron injection property. A high material or a low material may be selected and formed.
[0032]
When the second electrode 114 is used as an anode of the light emitting element, a material having a work function of 4 eV or more is selected, and ITO (Indium Tin Oxide: indium oxide mixed with tin oxide), zinc oxide, IZO ((Indium Zinc Oxide: Indium oxide mixed with zinc oxide), titanium nitride, tungsten nitride, etc. Further, when the second electrode 114 is used as a cathode, a material having a work function of 4 eV or less is selected, and an alkali metal or alkaline earth metal, Alternatively, an alloy or a compound containing the same is used, for example, AlLi, MgAg, LiF, CaF, CsF, or the like.
[0033]
FIG. 5 is a top view of this state, and a longitudinal sectional view corresponding to the line AA ′ is shown in FIG. In FIG. 5, reference numeral 23 denotes a wiring for connecting TFTs in a pixel formed simultaneously with the wiring 112 and the like.
[0034]
As shown in FIG. 3B, the sixth insulating layer 115 has an opening 117 on the first electrode 111 and an opening 116 on the second electrode 114, and is formed so as to cover the end thereof. By using a conductive resin material, the side wall portion can be inclined and formed with a continuous curvature.
[0035]
As shown in FIG. 3C, the layer 118 containing a light emitter is formed on the second electrode 114 and along the side wall of the sixth insulating layer 115. The shape is suitable for relieving the internal stress of the layer 118 containing a light emitter.
[0036]
The layer 118 containing a light emitter is a charge injecting and transporting medium and a light emitting medium containing an organic compound or an inorganic compound, and one or more kinds selected from a low molecular organic compound, a medium molecular organic compound, and a high molecular organic compound. These layers may be combined with an inorganic compound having electron injection / transport properties or hole injection / transport properties. The phosphor can be a phenylanthracene derivative, a tetraaryldiamine derivative, a quinolinol complex derivative, a distyrylbenzene derivative, etc., and a coumarin derivative, DCM, quinacridone, rubrene, etc. can be used as a host substance. It is possible to apply these materials. High molecular organic compounds include polyparaphenylene vinylene, polyparaphenylene, polythiophene, polyfluorene, and the like. Poly (p-phenylene vinylene): (PPV), poly (2,5-dialkoxy-1,4-phenylene vinylene) (RO-PPV), poly (2- (2′-ethyl-hexoxy) ) -5-methoxy-1,4-phenylene vinylene (poly [2- (2'-ethylhexoxy) -5-methoxy-1,4-phenylene vinylene]): (MEH-PPV), poly (2- (di (Alkoxyphenyl) -1,4-phenylene vinylene) (poly [2- (dialkoxyphenyl) -1,4-phenylene vinylene]): (ROPh-PPV), polyparaphenylene (poly [p-phenylene]): (PPP) , Poly (2,5-dialkoxy-1,4-phenylene) (poly (2,5-dialkoxy-1,4-ph enylene)): (RO-PPP), poly (2,5-dihexoxy-1,4-phenylene) (poly (2,5-dihexoxy-1,4-phenylene)), polythiophene: (PT), Poly (3-alkylthiophene): (PAT), poly (3-hexylthiophene): (PHT), poly (3-cyclohexylthiophene) (poly ( 3-cyclohexylthiophene)): (PCHT), poly (3-cyclohexyl-4-methylthiophene): (PCHMT), poly (3,4-dicyclohexylthiophene) (poly ( 3,4-dicyclohexylthiophene)): (PDCHT), poly [3- (4-octylphenyl) -thiophene]: (POPT), poly [3- (4-octyl) Phenyl) -2,2-bithiophene] (poly [3- (4-octylphenyl) -2,2-bithi ophene]): (PTOPT), polyfluorene: (PF), poly (9,9-dialkylfluorene) (poly (9,9-dialkylfluorene): (PDAF), poly (9,9-dioctylfluorene) (poly (9,9-dioctylfluorene): (PDOF)) and the like. As the inorganic compound material, diamond-like carbon (DLC), Si, Ge, and oxides or nitrides thereof may be appropriately doped with P, B, N, or the like. Alternatively, an oxide, nitride, or fluoride of an alkali metal or an alkaline earth metal, or a compound or alloy of the metal and at least Zn, Sn, V, Ru, Sm, or In may be used.
[0037]
The materials listed above are examples, and functional layers such as a hole injecting and transporting layer, a hole transporting layer, an electron injecting and transporting layer, an electron transporting layer, a light emitting layer, an electron blocking layer, and a hole blocking layer using these materials. A light-emitting element can be formed by appropriately stacking layers. Moreover, you may form the mixed layer or mixed junction which combined these each layer.
[0038]
In a preferred combination with a color filter, a material that emits white light is preferable. When white light cannot be obtained with a single dye contained in the light-emitting layer, a plurality of dyes are used as light emission centers to emit light simultaneously. To whiten by additive color mixing. In this case, a method of stacking light emitting layers having different emission colors, a method of incorporating a plurality of light emission centers in one or a plurality of light emitting layers, and the like can be applied. The method for obtaining white light emission utilizes the relationship between the additive color mixture by laminating light emitting layers emitting light of the three primary colors R (red), G (green), and B (blue), and the complementary colors of the two colors. There is a method. When complementary colors are used, combinations of blue-yellow or blue-green-orange are known. In particular, the latter is considered advantageous in that it can utilize light emission in a wavelength region with relatively high visibility.
[0039]
In an example in which a low molecular weight organic light emitting medium is used for the layer 118 containing a light emitter, an electron injecting and transporting layer, a red light emitting layer, a green light emitting layer, a hole transporting layer, and a blue light emitting layer are sequentially formed on the second electrode (cathode) 114. It is a laminated structure. Specifically, when 1,2,4-triazole derivative (p-EtTAZ) is applied to the hole transport layer to 3 nm, the amount of holes passing through the p-EtTAZ layer increases, and tris ( 8-quinolinolato) aluminum (Alq Three ) Also injects holes and emits light. In this structure, as the blue light emitting layer, the blue color of TPD is changed to Alq. Three Blue-green light emission in which the green color is mixed is obtained. In order to realize white light emission by adding red to this light emission, Alq is used as a red light emitting layer. Three Or TPD may be doped with a red luminescent dye. Nile red or the like can be applied as the red light emitting pigment.
[0040]
As another structure of the layer 118 including a light emitter, an electron injecting and transporting layer, an electron transporting layer, a light emitting layer, a hole transporting layer, and a hole injecting and transporting layer may be formed from the second electrode (cathode) 114 side. it can. In this case, a suitable material combination is Alq as the electron injection transport layer. Three Is formed with a thickness of 15 nm and a phenylanthracene derivative with a thickness of 20 nm as an electron transport layer. The light-emitting layer is a 25 nm first light-emitting layer in which a tetraarylbenzidine derivative and a phenylanthracene derivative are mixed at a volume ratio of 1: 3 and 3% by volume of a styrylamine derivative is contained, a tetraarylbenzidine derivative and 10,10′- Bis [2-biphenylyl] -9,9′-bianthryl (phenylanthracene derivative) was mixed at a volume ratio of 1: 3, and a 40 nm second light emitting layer containing 3% by weight of naphthacene derivative was laminated. The configuration. The hole transport layer is formed by forming N, N, N ′, N′-tetrakis- (3-biphenyl-1-yl) benzidine (tetraarylbenzidine derivative) to a thickness of 20 nm, and N, N '-Diphenyl-N, N'-bis [N-phenyl-N-4-tolyl (4-aminophenyl)] benzidine is formed to a thickness of 30 nm.
[0041]
In the above structure, an inorganic electron injecting and transporting layer may be used as the electron injecting and transporting layer. As the inorganic electron transport layer, n-type diamond-like carbon (DLC) can be applied. Phosphorus or the like may be appropriately doped to make the DLC film n-type. In addition, one kind of oxide selected from alkali metal elements, alkaline earth metal elements, and lanthanoid elements and one or more inorganic materials selected from Zn, Sn, V, Ru, Sm, and In are applied. can do.
[0042]
ITO, ZnO, SnO on the layer 118 containing the phosphor. 2 An oxide conductive material layer 119 such as 10 to 30 nm is formed. Although not illustrated, a layer containing an alkali metal or an alkaline earth metal having a work function of 3 eV or less is formed between the oxide conductive material layer 119 and the layer 118 containing a light emitter.
[0043]
Furthermore, it is formed so as to intersect with the second electrode 114 extending in a strip shape, and the strip-shaped third electrode 120 is similarly extended. The third electrode 120 is formed in contact with the first electrode 111 and the oxide transparent conductive material 119. The third electrode 120 is formed by selecting a material having a polarity opposite to that of the second electrode 114.
[0044]
FIG. 6 is a top view of this state, and a longitudinal sectional view corresponding to the line AA ′ is shown in FIG. Therefore, an electric field can be applied by interposing the layer 118 including a light emitter and the oxide conductive material layer 119 at the intersection of the second electrode 114 and the third electrode 120.
[0045]
In this state, a reverse voltage can be applied. That is, a positive voltage is applied to the third electrode for the polarity with the second electrode 114 as an anode and the third electrode as a cathode. In addition, a negative voltage is applied to the third electrode for the polarity in which the second electrode 114 is a cathode and the third electrode is an anode. As the voltage, a DC voltage may be applied, a pulsed voltage (FIG. 19A) may be applied, or a voltage that is pulsed and increases or decreases stepwise (FIG. 19B). You may apply.
[0046]
FIG. 8 is a top view illustrating a method of applying a reverse voltage in a state where a light emitting element including a light emitter is provided for each pixel in a single layer or a stack of a plurality of layers, and the pixels are arranged in a matrix. A reverse voltage is applied between the second electrode 114 formed in a strip shape and the third electrode 120 by a constant voltage power source 125. In this state, the third electrode 120 is a common electrode. The second electrode 114, the third electrode 120, and the constant voltage source 125 may be connected by forming a contact contact using a probe outside the pixel portion. A TFT is provided below each pixel, but the TFT is not electrically involved in this configuration.
[0047]
As explained in FIG. 9, if there is a minute short-circuited part, when a reverse voltage is applied, the current that should not flow originally flows in the short-circuited part, and that part generates heat due to Joule heat. It can be altered and insulated. The layer 118 including a luminescent material is mainly formed of an organic compound, and is mostly formed of a material containing carbon as a main component. Although there are various forms of the short-circuited portion, the oxide conductive material layer 119 and the third electrode are generally formed so as to ooze out into the holes. Alternatively, in many cases, foreign matter is interposed in the layer 118 containing a light emitter. The heat generated by the reverse voltage application alters the metal material of the third electrode in this portion, but the oxide conductive material effectively acts to supply oxygen and oxidize and insulate the metal material.
[0048]
After repairing the short-circuited portion with the reverse voltage, a seventh insulating film 122 is formed on the third electrode as shown in FIG. 1, and the pattern is further matched to the shape of the individual electrode. The seventh insulating film 122 is formed of silicon nitride, and the third electrode that does not overlap with this pattern is removed by etching using this pattern as a mask. Thus, the light emitting element 100 connected to the TFT 150 can be formed. The light-emitting element 100 is formed by stacking a second electrode 114, a layer 118 including a light emitter, an oxide conductive material 119, and a third electrode 121.
[0049]
FIG. 7 is a top view of this state, and a longitudinal sectional view corresponding to the line AA ′ is shown in FIG. Thus, the third electrode 121 serving as an individual electrode is formed. Further, the eighth insulating film 122 covering the whole prevents the entry of moisture and the like from the outside as a protective film.
[0050]
With such a manufacturing method, even in an active matrix driving type pixel configuration, a reverse voltage can be applied without going through a TFT, and if there is a defect, a sufficient current is instantaneously supplied to The part can be altered and insulated.
In addition, this invention is not limited to the said form, A various deformation | transformation is accept | permitted in the range which does not deviate from the summary.
[0051]
(Embodiment 2)
In this embodiment, a single layer or a stacked layer of a plurality of layers including a light emitter on an individual electrode connected to a TFT, and a first common electrode and a first layer separated from each other are overlapped with the individual pixel electrode through the layer. Two common electrodes are formed, and a voltage is applied between the first common electrode and the second common electrode to repair a short-circuit defective portion.
[0052]
FIG. 11 is an equivalent circuit diagram of the pixel portion in this embodiment. An example of a configuration including a scanning signal line 305, an erasing signal line 306, a data line 307, a power supply line 308, a selection TFT 301, an erasing TFT 302, and a control TFT 303 is shown. One terminal of the light emitting element 304 is connected to the control TFT 303, but the other side is divided and connected to a first common wiring 309 and a second common wiring 310.
[0053]
The first common electrode 309 and the second common electrode 310 are connected to the constant voltage sources 311 and 312 having different polarities, respectively, and the reverse voltage is effectively applied to the light emitting element 304 by changing the connection state appropriately by the switch 313. It has become.
[0054]
In such a pixel configuration, the first common wiring and the second common wiring are realized in a form as shown in FIG. The first common wiring 123 and the second common wiring 124 are connected to the constant voltage sources 311 and 312 having different polarities by connecting them with connection wirings 315 and 316 formed so as to intersect with each other outside the pixel portion. It will be realized.
[0055]
As an example of the structure of the light emitting element 304 and the control TFT 303, a longitudinal sectional view thereof is shown in FIG. Substrate 101, first insulating film 102, semiconductor film 103, second insulating film 104, gate electrode 105, third insulating film 106, fourth insulating film 107, fifth insulating film 108, first electrode 111, wiring (power line) ) 112 and the sixth insulating film 115 are the same as those in the first embodiment. FIG. 15 is a top view of this state, and FIG. 14 shows a longitudinal sectional view corresponding to the line AA ′.
[0056]
In the light emitting element 304, the individual pixel electrode 122 formed on the fifth insulating film 108, the layer 116 including the light emitter, and the oxide conductive material 117 are stacked, and the first common electrode 123 and the second common electrode are stacked thereon. The electrode 124 is formed. The common electrode is formed of the same material and has a rectifying property in the same direction when viewed as a diode. The first common electrode 123 and the second common electrode 124 are applied with different potentials when a reverse voltage is applied, and the potentials are alternately switched to allow the light emitting element to be repaired.
[0057]
FIG. 13 is a circuit diagram schematically illustrating how the light emitting element is repaired in the present embodiment. FIG. 13A shows a state in which the first common wiring 309 is connected to a high potential and the second common wiring 310 is connected to a low potential, and the light emitting element is a normal element that does not include a short-circuit defect or a leak point close thereto. No current exceeding the reverse saturation current flows. On the other hand, when a short-circuit defect is inherent in the element A, a current flows through that portion (abnormality A). In this case, the short-circuit defect can be repaired. However, when the element B has a short-circuit defect (abnormal B), the defect cannot be repaired in this bias state. When both the element A and the element B have a short-circuit defect (abnormal C), both the element A and the element B can be repaired. However, when the defect repair of the element A is completed quickly, the defect of the element B Repair is impossible.
[0058]
In order to repair both the defects of the element A and the element B, the bias states of the first common wiring 309 and the second common wiring 310 may be reversed as shown in FIG. When applying reverse voltage, it is possible to apply a method of applying voltage in a pulsed manner to repair a short-circuit defective part. Applying a voltage that is pulsed and increases or decreases stepwise applies a short-circuit failure. It is possible to repair the location.
[0059]
With such a pixel configuration, even in an active matrix drive type pixel configuration, a reverse voltage can be applied without going through a TFT, and if there is a defective part, a sufficient current is instantaneously supplied. The portion can be altered and insulated.
In addition, this invention is not limited to the said form, A various deformation | transformation is accept | permitted in the range which does not deviate from the summary.
[0060]
(Embodiment 3)
A practical example of repairing a light emitting element by applying a reverse voltage is shown in FIGS. The light-emitting element is an Alq layer in which CuPc, α-NPD, and DCM are added as a layer including a light emitter between a pair of electrodes. Three And non-doped Alq Three It is the structure which laminated | stacked. FIG. 16 shows current-voltage characteristics when a voltage of ± 12 V is swept from the forward voltage to the reverse voltage. When a forward voltage is applied, an abnormal increase in the forward current is observed in the region of 5 V or less, and when the reverse voltage is applied, an abnormal increase in the reverse current is observed in the range of 0 to -5V. At this time, the reverse current once increases rapidly, but then immediately decreases to the original current value. That is, it means that the short-circuited portion has been repaired, and when the high-density current flows locally, the portion generates heat and is insulated. However, if the reaction is not sufficient, or if another similar short-circuited part is present, the same phenomenon may be observed in the second voltage sweep as shown in FIG. When such a voltage sweep from the forward direction to the reverse direction or a voltage sweep in the reverse direction is repeated once or a plurality of times, a clean current-voltage characteristic can be obtained as shown in FIG.
[0061]
【The invention's effect】
As described above, according to the present invention, the first common electrode and the second common electrode are arranged in parallel on one layer or a laminate of a plurality of layers including the light emitter, and both the electrodes are arranged. By applying a voltage in between, a reverse voltage can be applied without going through the TFT to completely repair the defective portion, and a short circuit or a leaked portion of the light emitting element can be repaired.
[0062]
Accordingly, it is possible to suppress heat generation by suppressing unnecessary current consumption of the light emitting device, and to reduce deterioration such as increase and enlargement of the non-light emitting point of the light emitting element.
[Brief description of the drawings]
FIG. 1 is a vertical cross-sectional view illustrating a structure of a pixel in Embodiment 1;
2 is a longitudinal cross-sectional view illustrating a manufacturing process of a pixel in Embodiment 1. FIG.
3 is a vertical cross-sectional view illustrating a manufacturing process of a pixel in Embodiment 1. FIG.
4 is a top view illustrating a manufacturing process of a pixel in Embodiment 1. FIG.
5 is a top view illustrating a manufacturing process of a pixel in Embodiment 1. FIG.
6 is a top view illustrating a manufacturing process of a pixel in Embodiment 1. FIG.
7 is a top view illustrating a structure of a pixel in Embodiment 1. FIG.
8 is a top view illustrating a state in which a reverse voltage is applied to the pixel portion in Embodiment 1. FIG.
FIG. 9 is a longitudinal sectional view schematically explaining that a defective portion is repaired by applying a reverse voltage, and a graph showing its current-voltage characteristics.
FIG. 10 is a graph schematically showing a relationship between a drain voltage and a drain current of a TFT.
11 is an equivalent circuit diagram illustrating a configuration of a pixel portion in Embodiment 2. FIG.
12 is a top view illustrating a structure of a pixel portion in Embodiment 2. FIG.
13 is an equivalent circuit diagram illustrating the principle of repairing a light-emitting element by reverse voltage in Embodiment 2. FIG.
14 is a vertical cross-sectional view illustrating the structure of a pixel in Embodiment 2. FIG.
15 is a top view illustrating a structure of a pixel in Embodiment 2. FIG.
FIG. 16 is a graph showing current-voltage characteristics when a first voltage sweep is performed on a light-emitting element.
FIG. 17 is a graph showing current-voltage characteristics when a second voltage sweep is performed on a light-emitting element.
FIG. 18 is a graph showing current-voltage characteristics when a third voltage sweep is performed on a light-emitting element.
FIG. 19 is a diagram showing a voltage waveform when a pulsed reverse voltage is applied in the present invention.

Claims (8)

同一絶縁表面にTFTと接続された第1電極と、帯状の第2電極とを形成し、
前記第2電極上に、発光体を含む一つの層又は複数の層の積層体を形成し、
前記発光体を含む一つの層又は複数の層の積層体を介して、前記第2電極と交差するように重畳し、前記第1電極と電気的に接続する第3電極を形成し、
前記第2電極と前記第3電極との間に電圧を印加して、前記第2電極と前記第3電極との短絡欠陥を修復し、
前記第3電極を複数の第3電極に分離して、前記第2電極と、前記発光体を含む一つの層又は複数の層の積層体と、前記分離された第3の電極とを有する発光素子を形成することを特徴とするアクティブマトリクス型発光装置の作製方法。
Forming a first electrode connected to the TFT on the same insulating surface and a strip-shaped second electrode;
On the second electrode, a single layer including a light emitter or a laminate of a plurality of layers is formed,
Forming a third electrode that is electrically connected to the first electrode by overlapping with the second electrode through a single layer or a stack of a plurality of layers including the light emitter;
A voltage is applied between the second electrode and the third electrode to repair a short-circuit defect between the second electrode and the third electrode,
Light emission having the third electrode separated into a plurality of third electrodes, the second electrode, a single layer including the light emitter or a laminate of a plurality of layers, and the separated third electrode A method for manufacturing an active matrix light-emitting device, wherein an element is formed.
同一絶縁表面にTFTと接続された第1電極と、帯状の第2電極とを形成し、
前記第1電極と、前記第2電極の端部とを被覆する隔壁層を形成し、
前記第2電極上の前記隔壁層に帯状の開口部を形成し、
前記開口部における第2電極上に、発光体を含む一つの層又は複数の層の積層体を形成し、
前記発光体を含む一つの層又は複数の層の積層体を介して、前記第2電極と交差するように重畳し、前記第1電極と電気的に接続する第3電極を、前記帯状の開口部が形成された隔壁層の端部を被覆するように形成し、
前記第2電極と前記第3電極との間に電圧を印加して、前記第2電極と前記第3電極との短絡欠陥を修復し、
前記第3電極を複数の第3電極に分離して、前記第2電極と、前記発光体を含む一つの層又は複数の層の積層体と、前記分離された第3の電極とを有する発光素子を形成することを特徴とするアクティブマトリクス型発光装置の作製方法。
Forming a first electrode connected to the TFT on the same insulating surface and a strip-shaped second electrode;
Forming a partition layer covering the first electrode and an end of the second electrode;
Forming a band-shaped opening in the partition layer on the second electrode;
On the second electrode in the opening, a single layer including a light emitter or a laminate of a plurality of layers is formed,
A third electrode that overlaps the second electrode and is electrically connected to the first electrode through one layer or a stacked layer of a plurality of layers including the light emitter is formed in the band-shaped opening. Formed so as to cover the edge of the partition wall layer formed,
A voltage is applied between the second electrode and the third electrode to repair a short-circuit defect between the second electrode and the third electrode,
Light emission having the third electrode separated into a plurality of third electrodes, the second electrode, a single layer including the light emitter or a laminate of a plurality of layers, and the separated third electrode A method for manufacturing an active matrix light-emitting device, wherein an element is formed.
請求項1又は2において、前記第1電極と前記第2電極とは同一材料で形成することを特徴とするアクティブマトリクス型発光装置の作製方法。3. The method for manufacturing an active matrix light-emitting device according to claim 1, wherein the first electrode and the second electrode are formed of the same material. 縁表面にTFTと接続された画素電極を形成し、
前記画素電極上に、発光体を含む一つの層又は複数の層の積層体を形成し、
前記発光体を含む一つの層又は複数の層の積層体を介して、互いに分離され、前記画素電極にそれぞれ重畳する第1共通電極と第2共通電極とを形成し、
前記第1共通電極と前記第2共通電極とのに電圧を印加し、前記電圧を交互に入れ替えることにより、短絡欠陥を修復し、
前記画素電極と、前記発光体を含む一つの層又は複数の層の積層体と、前記第1共通電極及び前記第2共通電極とを有する発光素子を形成することを特徴とするアクティブマトリクス型発光装置の作製方法。
Forming a pixel electrode connected to the TFT on insulation surface,
On the pixel electrode, a single layer including a light emitter or a laminate of a plurality of layers is formed,
Forming a first common electrode and a second common electrode that are separated from each other via a single layer or a stacked body of a plurality of layers including the light emitter and overlap with the pixel electrode, respectively;
The voltage is applied between the second common electrode and the first common electrode, by interchanging the voltages alternately to repair short defect,
An active matrix type light emitting device comprising: a light emitting element having the pixel electrode, a single layer or a stacked layer of a plurality of layers including the light emitter, and the first common electrode and the second common electrode. Device fabrication method.
縁表面にTFTと接続された画素電極を形成し、
前記画素電極の端部を被覆する隔壁層を形成し、
前記画素電極上の前記隔壁層に開口部を形成し、
前記開口部における前記画素電極上に、発光体を含む一つの層又は複数の層の積層体を形成し、
前記発光体を含む一つの層又は複数の層の積層体を介して、互いに分離され、前記画素電極にそれぞれ重畳する第1共通電極と第2共通電極とを、前記開口部が形成された隔壁層のそれぞれの端部を被覆するように形成し、
前記第1共通電極と前記第2共通電極とのに電圧を印加し、前記電圧を交互に入れ替えることにより、短絡欠陥を修復し、
前記画素電極と、前記発光体を含む一つの層又は複数の層の積層体と、前記第1共通電極及び前記第2共通電極とを有する発光素子を形成することを特徴とするアクティブマトリクス型発光装置の作製方法。
Forming a pixel electrode connected to the TFT on insulation surface,
Forming a partition layer covering an end of the pixel electrode;
Forming an opening in the partition layer on the pixel electrode;
On the pixel electrode in the opening, a single layer including a light emitter or a laminate of a plurality of layers is formed,
A first common electrode and a second common electrode that are separated from each other and overlap with the pixel electrode via a single layer or a stacked layer of a plurality of layers including the light emitter, and a partition wall in which the opening is formed Forming to cover each end of the layer,
The voltage is applied between the second common electrode and the first common electrode, by interchanging the voltages alternately to repair short defect,
An active matrix type light emitting device comprising: a light emitting element having the pixel electrode, a single layer or a stacked layer of a plurality of layers including the light emitter, and the first common electrode and the second common electrode. Device fabrication method.
請求項1乃至5のいずれか一項において、前記電圧をパルス状に印加して短絡不良個所を修復することを特徴とするアクティブマトリクス型発光装置の作製方法。6. The method for manufacturing an active matrix light-emitting device according to claim 1, wherein the voltage is applied in a pulse shape to repair a short-circuit defective portion. 請求項1乃至6のいずれか一項において、前記電圧はパルス状であり、且つ階段状に増減するように印加して短絡欠陥を修復することを特徴とするアクティブマトリクス型発光装置の作製方法。7. The method for manufacturing an active matrix light-emitting device according to claim 1, wherein the voltage is pulsed and applied so as to increase or decrease stepwise to repair a short-circuit defect. 請求項1乃至7のいずれか一項において、前記積層体の複数の層のうち少なくとも一つの層は、酸化物導電性材料を用いて形成されていることを特徴とするアクティブマトリクス型発光装置の作製方法。8. The active matrix light-emitting device according to claim 1, wherein at least one of the plurality of layers of the stacked body is formed using an oxide conductive material. Manufacturing method.
JP2003120650A 2002-04-30 2003-04-24 Method for manufacturing active matrix light-emitting device Expired - Fee Related JP4342827B2 (en)