JP3227011B2 - Container - Google Patents

Container

Info

Publication number
JP3227011B2
JP3227011B2 JP7479393A JP7479393A JP3227011B2 JP 3227011 B2 JP3227011 B2 JP 3227011B2 JP 7479393 A JP7479393 A JP 7479393A JP 7479393 A JP7479393 A JP 7479393A JP 3227011 B2 JP3227011 B2 JP 3227011B2
Authority
JP
Japan
Prior art keywords
container
shrink film
recess
recesses
present
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP7479393A
Other languages
Japanese (ja)
Other versions
JPH06286743A (en
Inventor
伸治 嶋田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yoshino Kogyosho Co Ltd
Original Assignee
Yoshino Kogyosho Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yoshino Kogyosho Co Ltd filed Critical Yoshino Kogyosho Co Ltd
Priority to JP7479393A priority Critical patent/JP3227011B2/en
Publication of JPH06286743A publication Critical patent/JPH06286743A/en
Application granted granted Critical
Publication of JP3227011B2 publication Critical patent/JP3227011B2/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Description

【発明の詳細な説明】DETAILED DESCRIPTION OF THE INVENTION

【0001】[0001]

【産業上の利用分野】本発明は、外表面が熱収縮性を有
するシュリンクフィルムによって被覆される容器に関す
るものである。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a container whose outer surface is covered with a heat-shrinkable shrink film.

【0002】[0002]

【従来の技術】近年、液体食品用の容器には、ポリエチ
レンテレフタレート製プリフォームをブロー成形により
形成した所謂PETボトルが多用されている。
2. Description of the Related Art In recent years, so-called PET bottles formed by blow molding a polyethylene terephthalate preform have been frequently used as containers for liquid foods.

【0003】図6に示すように、一般にPETボトル1
の胴部10には、商品名やメーカー名等が印刷された、
熱収縮性を有する延伸フィルム、いわゆるシュリンクフ
ィルム2が装着されることが多い。
[0003] As shown in FIG.
The product name, the manufacturer name, etc. are printed on the body 10 of the
A stretched film having heat shrinkage, that is, a so-called shrink film 2 is often mounted.

【0004】このシュリンクフィルム2は、PETボト
ル1の胴部10よりも大径の筒状に形成されていて、予
めその表面に商品名等の印刷が施されており、このシュ
リンクフィルム2を胴部10に被せて熱を加え、収縮さ
せることにより、シュリンクフィルム2は胴部10に装
着される。
The shrink film 2 is formed in a cylindrical shape having a larger diameter than the body portion 10 of the PET bottle 1, and the surface of the shrink film 2 is printed with a trade name or the like in advance. The shrink film 2 is attached to the body 10 by applying heat and shrinking over the part 10.

【0005】[0005]

【発明が解決しようとする課題】前記シュリンクフィル
ム2は熱収縮する際に歪んで皺が寄る場合があった。こ
のようにシュリンクフィルム2に皺が寄っていると、表
面に印刷されていた商品名等が歪んで読み難くなるとい
う問題があった。
The shrink film 2 may be distorted and wrinkled when thermally contracted. If the shrink film 2 is wrinkled in this way, there is a problem that the product name or the like printed on the surface is distorted and difficult to read.

【0006】本発明はこのような従来の技術の問題点に
鑑みてなされたものであり、シュリンクフィルムを皺が
寄らないように装着できる容器を得ることを目的とす
る。
[0006] The present invention has been made in view of such problems of the conventional art, and has as its object to obtain a container in which a shrink film can be mounted without wrinkling.

【0007】[0007]

【課題を解決するための手段】本発明は前記課題を解決
するために、以下の構成を採用した。即ち、本発明の容
器は、その外表面に、容器の周方向に間隔を置いて容器
の厚さ方向に凹む凹部を容器の軸線方向に複数列設け、
互いに隣接する列の凹部が互い違いになるように配置さ
れていることを特徴とする。凹部は、その幅を1〜10
mmとするのが好ましく、長さを10〜100mmとするの
が好ましく、深さを1〜5mmとするのが好ましい。
The present invention has the following features to attain the object mentioned above. That is, the container of the present invention, on its outer surface, provided in a plurality of rows in the axial direction of the container, concave portions that are recessed in the thickness direction of the container at intervals in the circumferential direction of the container,
It is characterized in that the recesses of the rows adjacent to each other are arranged alternately. The recess has a width of 1 to 10
mm, the length is preferably 10 to 100 mm, and the depth is preferably 1 to 5 mm.

【0008】シュリンクフィルムは1軸配向と2軸配向
のいずれのものも使用可能であるが、容器の凹部の長手
方向とフィルムの収縮方向とを一致させるのが好まし
い。容器はPETボトルに限定されるものではなく、種
々の形状、材質のものに適用可能である。
The shrink film may be either uniaxially oriented or biaxially oriented, but it is preferable that the longitudinal direction of the concave portion of the container and the shrinking direction of the film coincide. The container is not limited to PET bottles, but can be applied to containers of various shapes and materials.

【0009】[0009]

【作用】シュリンクフィルムを容器に被せて熱収縮させ
た際に、シュリンクフィルムに皺を生じさせるような力
が働いても、シュリンクフィルムにおいて凹部の上に配
された部分が皺を吸収する。したがって、シュリンクフ
ィルムを皺なく綺麗に容器の外表面に被覆することがで
きる。その結果、熱収縮前のシュリンクフィルムに予め
商品名等の印刷を施しておいても、容器へ装着後にその
印刷文字等が歪むことがなく、見栄えがよくなり、品質
が向上する。
When a shrink film is placed on a container and thermally shrunk, even if a force that causes wrinkles acts on the shrink film, the portion of the shrink film disposed above the recess absorbs the wrinkles. Therefore, the shrink film can be coated on the outer surface of the container neatly without wrinkles. As a result, even if the shrink film before heat shrinking is printed in advance with a product name or the like, the printed characters and the like do not become distorted after being attached to the container, the appearance is improved, and the quality is improved.

【0010】又、容器はその断面形状が複雑になるた
め、凹部を有さない従来の容器よりも機械的強度が大き
くなる。
[0010] Further, since the cross-sectional shape of the container is complicated, the mechanical strength is higher than that of a conventional container having no concave portion.

【0011】[0011]

【実施例】以下、本発明の実施例を図1から図6の図面
に基いて説明する。図1は本発明の第1実施例における
容器の要部拡大正面図であり、図2は図1のA−A矢視
断面図であり、図3は図1のB−B矢視断面図である。
尚、シュリンクフィルムが装着された容器の全体外観図
については図6を援用する。
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS An embodiment of the present invention will be described below with reference to FIGS. 1 is an enlarged front view of a main part of a container according to a first embodiment of the present invention, FIG. 2 is a sectional view taken along the line AA of FIG. 1, and FIG. 3 is a sectional view taken along the line BB of FIG. It is.
FIG. 6 is referred to for an overall external view of the container provided with the shrink film.

【0012】容器としてのPETボトル1の胴部10の
外表面には多数の凹部11が規則的に散在配置されてい
る。凹部11は内側に凹んでおり、各凹部11は胴部1
0の周方向に沿って細長く形成されている。この凹部1
1の幅Wは1〜10mmにするのが好ましく、長さLは1
0〜100mmにするのが好ましく、深さDは1〜5mmに
するのが好ましい。
On the outer surface of the body 10 of the PET bottle 1 as a container, a large number of recesses 11 are regularly scattered. The recesses 11 are recessed inward, and each recess 11 is
It is formed to be elongated along the circumferential direction of 0. This recess 1
The width W of one is preferably 1 to 10 mm, and the length L is 1
The depth D is preferably 0 to 100 mm, and the depth D is preferably 1 to 5 mm.

【0013】凹部11は、胴部10の同一高さ位置にお
いて、周方向等間隔に複数形成されている。又、凹部1
1は、胴部10の高さ方向(軸線方向)に対しても等間
隔に離間して配されている。更に、上下に隣接して位置
する凹部11同士はその端部を周方向に若干重複させて
いる。
A plurality of recesses 11 are formed at equal intervals in the circumferential direction at the same height position of the body 10. Also, recess 1
Numerals 1 are arranged at equal intervals in the height direction (axial direction) of the body 10. Further, the recesses 11 located vertically adjacent to each other have their ends slightly overlapped in the circumferential direction.

【0014】一方、前記胴部10に装着されるシュリン
クフィルム2は筒状をなしている。このシュリンクフィ
ルム2は1軸配向にされており、周方向にだけ収縮し、
軸線方向には収縮しないようになっている。
On the other hand, the shrink film 2 mounted on the body 10 has a cylindrical shape. This shrink film 2 is uniaxially oriented, shrinks only in the circumferential direction,
It does not shrink in the axial direction.

【0015】このシュリンクフィルム2をPETボトル
1の胴部10に被せ、熱収縮させた時に、シュリンクフ
ィルム2に皺を生じさせるような力が働いても、シュリ
ンクフィルム2において凹部11の上に配された部分に
よって、皺が吸収される。その結果、シュリンクフィル
ム2を皺なく綺麗に胴部10に装着することができる。
When the shrink film 2 is put on the body 10 of the PET bottle 1 and thermally shrunk, even if a force that causes wrinkles is applied to the shrink film 2, the shrink film 2 is arranged on the recess 11 in the shrink film 2. The wrinkles are absorbed by the cut portion. As a result, the shrink film 2 can be attached to the body 10 neatly without wrinkles.

【0016】したがって、熱収縮前のシュリンクフィル
ム2に予め商品名等の印刷を施しておいても、PETボ
トル1装着後にその印刷文字等が歪むことがなく、見栄
えがよくなり、品質が向上する。
Therefore, even if the shrink film 2 before heat shrinking is printed in advance with a product name or the like, the printed characters and the like are not distorted after the PET bottle 1 is attached, the appearance is improved, and the quality is improved. .

【0017】又、PETボトル1はその胴部10の断面
形状が複雑であるために、凹部11を有さない従来のP
ETボトルよりも機械的強度が大きくなる。図4は本発
明に係るPETボトル1の第2実施例における図1に対
応する正面図である。このPETボトル1が前記第1実
施例のものと相違する点は、上下に隣接して位置する凹
部11同士の端部が周方向に重複せず、離間している点
にある。そのほかの点については前述第1実施例のもの
と同様であるので、説明は省略する。
Further, since the cross section of the body 10 of the PET bottle 1 is complicated, a conventional P bottle having no recess 11 is used.
Higher mechanical strength than ET bottle. FIG. 4 is a front view corresponding to FIG. 1 of a second embodiment of the PET bottle 1 according to the present invention. The difference of this PET bottle 1 from that of the first embodiment is that the ends of the recesses 11 located vertically adjacent to each other are not overlapped in the circumferential direction and are separated. The other points are the same as those of the first embodiment, and the description is omitted.

【0018】図5は本発明に係るPETボトル1の第3
実施例における図1に対応する正面図である。このPE
Tボトル1が前記第1実施例のものと相違する点は、各
凹部11の長手方向が胴部10の高さ方向(軸線方向)
に沿って延びている点にある。そのほかの点については
前述第1実施例のものと同様であるので、説明は省略す
る。
FIG. 5 shows a third embodiment of the PET bottle 1 according to the present invention.
It is a front view corresponding to FIG. 1 in an Example. This PE
The point that the T bottle 1 is different from that of the first embodiment is that the longitudinal direction of each recess 11 is the height direction (axial direction) of the body 10.
It extends along the point. The other points are the same as those of the first embodiment, and the description is omitted.

【0019】[0019]

【発明の効果】以上説明したように、本発明によれば、
容器の外表面に、容器の周方向に間隔を置いて容器の厚
さ方向に凹む凹部を容器の軸線方向に複数列設け、互い
に隣接する列の凹部を互い違いになるように配置したこ
とにより、この容器にシュリンクフィルムを被せ熱収縮
させて装着した時に、シュリンクフィルムが歪まないよ
うになるという優れた効果が奏される。
As described above, according to the present invention,
On the outer surface of the container, by providing a plurality of recesses in the container axial direction at intervals in the circumferential direction of the container at intervals in the circumferential direction of the container, and by arranging the recesses in adjacent rows alternately, When the container is covered with a shrink film and heat shrunk, the shrink film is prevented from being distorted.

【図面の簡単な説明】[Brief description of the drawings]

【図1】本発明に係る容器の第1実施例における要部拡
大正面図である。
FIG. 1 is an enlarged front view of a main part of a container according to a first embodiment of the present invention.

【図2】図1のA−A矢視拡大断面図である。FIG. 2 is an enlarged sectional view taken on line AA of FIG. 1;

【図3】図1のB−B矢視拡大断面図である。FIG. 3 is an enlarged sectional view taken on line BB of FIG. 1;

【図4】本発明に係る容器の第2実施例における要部拡
大正面図である。
FIG. 4 is an enlarged front view of a main part of a container according to a second embodiment of the present invention.

【図5】本発明に係る容器の第3実施例における要部拡
大正面図である。
FIG. 5 is an enlarged front view of a main part of a third embodiment of the container according to the present invention.

【図6】シュリンクフィルムが装着された容器の正面図
である。
FIG. 6 is a front view of the container on which the shrink film is mounted.

【符号の説明】[Explanation of symbols]

1 PETボトル(容器) 2 シュリンクフィルム 10 胴部 11 凹部 DESCRIPTION OF SYMBOLS 1 PET bottle (container) 2 Shrink film 10 Body 11 Recess

───────────────────────────────────────────────────── フロントページの続き (58)調査した分野(Int.Cl.7,DB名) B65D 1/02 B65D 23/08 ──────────────────────────────────────────────────続 き Continued on front page (58) Field surveyed (Int.Cl. 7 , DB name) B65D 1/02 B65D 23/08

Claims (3)

(57)【特許請求の範囲】(57) [Claims] 【請求項1】 外表面が熱収縮性を有するシュリンクフ
ィルムによって被覆される容器において、該容器の外表
面に、容器の周方向に間隔を置いて容器の厚さ方向に凹
む凹部を容器の軸線方向に複数列設け、互いに隣接する
列の凹部が互い違いになるように配置されていることを
特徴とすることを特徴とする容器。
1. A container whose outer surface is covered with a heat-shrinkable shrink film, wherein the outer surface of the container is provided with a concave portion which is recessed in a thickness direction of the container at intervals in a circumferential direction of the container. A container characterized in that a plurality of rows are provided in the direction, and the recesses of rows adjacent to each other are arranged alternately.
【請求項2】 前記凹部の幅が1〜10mmの範囲にあ
り、凹部の長さが10〜100mmの範囲にあり、凹部の
深さが1〜5mmの範囲にあることを特徴とする請求項1
に記載の容器。
2. The method according to claim 1, wherein the width of the recess is in the range of 1 to 10 mm, the length of the recess is in the range of 10 to 100 mm, and the depth of the recess is in the range of 1 to 5 mm. 1
A container according to claim 1.
【請求項3】 前記凹部の長手方向を前記シュリンクフ
ィルムの収縮方向に一致させたことを特徴とする請求項
1または2に記載の容器。
3. The container according to claim 1, wherein a longitudinal direction of the recess is made to coincide with a shrinking direction of the shrink film.
JP7479393A 1993-03-31 1993-03-31 Container Expired - Lifetime JP3227011B2 (en)