JP3054323B2 - Developer supply container - Google Patents

Developer supply container

Info

Publication number
JP3054323B2
JP3054323B2 JP6278466A JP27846694A JP3054323B2 JP 3054323 B2 JP3054323 B2 JP 3054323B2 JP 6278466 A JP6278466 A JP 6278466A JP 27846694 A JP27846694 A JP 27846694A JP 3054323 B2 JP3054323 B2 JP 3054323B2
Authority
JP
Japan
Prior art keywords
shutter
supply container
developer supply
developer
opening
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP6278466A
Other languages
Japanese (ja)
Other versions
JPH08123175A (en
Inventor
京太 宮崎
一彦 小俣
長嶋  利明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Canon Inc
Original Assignee
Canon Inc
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Canon Inc filed Critical Canon Inc
Priority to JP6278466A priority Critical patent/JP3054323B2/en
Publication of JPH08123175A publication Critical patent/JPH08123175A/en
Application granted granted Critical
Publication of JP3054323B2 publication Critical patent/JP3054323B2/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Description

【発明の詳細な説明】DETAILED DESCRIPTION OF THE INVENTION

【0001】[0001]

【産業上の利用分野】本発明は、静電式複写機、プリン
タ等の画像形成装置の現像装置に現像剤を供給するため
に用いられる現像剤補給容器に関するものである。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a developer supply container for supplying a developer to a developing device of an image forming apparatus such as an electrostatic copying machine or a printer.

【0002】[0002]

【従来の技術】従来、静電式複写機、プリンタ等の画像
形成装置には現像剤として粉末トナーが使用されてい
る。装置本体のトナーが消費された場合には、トナー補
給容器を用いて装置本体へトナーを補給することが行わ
れている。このトナー補給容器は、一般に合成樹脂等で
作られた円筒状もしくは直方体等の容器本体と、容器本
体からトナーを現像装置に供給するために開口している
開口部と、開口部を封止するシールとによって構成され
ている。
2. Description of the Related Art Conventionally, powder toner is used as a developer in image forming apparatuses such as electrostatic copying machines and printers. When the toner in the apparatus main body is consumed, toner is supplied to the apparatus main body using a toner supply container. The toner replenishing container is generally a cylindrical or rectangular parallelepiped container body made of a synthetic resin or the like, an opening opening for supplying toner from the container body to the developing device, and sealing the opening. It is constituted by a seal.

【0003】従来のシールは大半がイージーピールタイ
プのフィルムであり、容器本体の開口部の周囲に接着剤
またはヒートシール等の手段で貼着されたフィルムの貼
着部を引き剥がして開封する方式を採っている。しかし
ながら、この方式ではトナーを排出した後に容器を密閉
することができないため、容器内に残ったトナーが落
下、飛散する場合があった。
[0003] Most conventional seals are easy peel type films, and a method of peeling off the sticking portion of the film stuck around the opening of the container body with an adhesive or a heat seal or the like to open it. Has been adopted. However, in this method, since the container cannot be closed after discharging the toner, the toner remaining in the container may fall or scatter.

【0004】一方、スライド式シャッターを有する現像
剤補給容器も種々考案されている。この容器は、往復運
動するスライド式シャッターと容器の開口部に取り付け
られたシャッターをガイドするキャップ部材と、容器の
密封性を保つためにシャッターとキャップの間に配置さ
れたシール部材とから構成されている。この種の現像剤
補給容器では、スライド式シャッターが移動することに
より、容器の開口が開放されて、容器内のトナーが装置
本体へ補給される。そして装置本体へのトナー補給後に
シャッターを閉めることによって容器の密封性が保た
れ、容器内にトナーが多少残っていても、イージーピー
ルタイプの容器に比べ、トナーの飛散は少ないものの、
近年の容器の大容量化に伴ない、開口部の大径化が進ん
でおり、容器の落下衝撃による開口のシール部からのト
ナー漏れ、汚れを防止するためにシール部材(発泡ポリ
ウレタン、発泡ポリエチレン、各種ゴム、ゴムスポンジ
等の弾性部材)を更に圧縮して使用しなければならな
い。その結果、シャッター開閉強度が上昇し、補給時の
操作性を犠牲にしている状況にある。
On the other hand, various developer supply containers having a sliding shutter have been devised. This container is composed of a sliding shutter that reciprocates, a cap member that guides the shutter attached to the opening of the container, and a seal member that is arranged between the shutter and the cap to maintain the hermeticity of the container. ing. In this type of developer supply container, the opening of the container is opened by moving the slide shutter, and the toner in the container is supplied to the apparatus main body. By closing the shutter after refilling the toner to the main body of the device, the tightness of the container is maintained, and even if some toner remains in the container, the scattering of toner is smaller than that of the easy peel type container,
With the recent increase in the capacity of containers, the diameter of the opening has been increasing. In order to prevent toner leakage and dirt from the sealing portion of the opening due to the impact of dropping the container, a sealing member (foamed polyurethane, foamed polyethylene) has been used. Elastic members such as various rubbers and rubber sponges) must be used after being further compressed. As a result, the shutter opening / closing strength is increased, and the operability during replenishment is sacrificed.

【0005】[0005]

【発明が解決しようとしている課題】近年、画質向上を
目的としたトナー粒径の極小化傾向があり、従来に比べ
トナーがより飛散しやすくなっているため、シャッター
部での高いシール性が要求されるようになってきてい
る。
In recent years, there has been a tendency for the toner particle size to be minimized for the purpose of improving image quality, and the toner is more easily scattered than in the prior art. It is becoming.

【0006】また、トナー補給に要するトナーボトル即
ち、現像剤補給容器の数を減らすというエコロジー問題
への対応のため、トナー補給回数を減らして操作性を向
上させるため、更にコストダウンを図るためにトナー容
器の容量が増大する傾向がある。これに伴い、トナー補
給性能を維持するために容器のトナー補給口を拡大する
傾向がある。しかし、補給口径が大きくなればなるほど
物流時、特に落下時のトナー漏れやトナー飛散が発生し
やすくなるため、シャッター部での更なる高いシール性
が要求されてきている。
In order to cope with the ecological problem of reducing the number of toner bottles required for toner replenishment, that is, the number of developer replenishing containers, the number of toner replenishments is reduced to improve operability, and further to reduce costs. The capacity of the toner container tends to increase. Accordingly, there is a tendency that the toner supply port of the container is expanded in order to maintain the toner supply performance. However, as the replenishment aperture becomes larger, toner leakage and toner scattering during distribution, particularly at the time of falling, are more likely to occur, so that a higher sealing property at the shutter portion is required.

【0007】従来のスライド式シャッターを備えた現像
剤補給容器において、前記シャッター部でのシール性を
向上させるために、前記シール部材の材質や圧縮率等を
変化させると、シャッターの開閉に要する開閉力即ちシ
ャッター開閉強度が異常に上昇し、操作性を悪化させて
しまうという問題があった。
In a conventional developer supply container provided with a sliding shutter, if the material or compression ratio of the seal member is changed in order to improve the sealability at the shutter portion, the opening and closing required for opening and closing the shutter is increased. There has been a problem that the force, that is, the shutter opening / closing strength is abnormally increased, and the operability is deteriorated.

【0008】また、シャッターとキャップ部材の間に配
置されるシール部材は、トナー補給口を囲むようにキャ
ップ部材に貼着されるのが一般的であった。しかしなが
らこの構成では、キャップ部材のフランジにシール部材
の貼着部とシャッターのガイド部を設ける必要があり、
キャップ部材全体が大きくなる傾向があった。画像形成
装置本体の現像ホッパーに余裕がある場合には問題ない
が、最近画像形成装置本体のコンパクト化が要求される
傾向にあり、現像ホッパー自体も小さくなっている。そ
のため、シール部材の貼着部とシャッターガイド部とを
除いたスペースに設置する現像剤補給容器の開口部が小
さくなってしまう。この容器の開口部が小さくなるとト
ナーの排出性が悪くなるだけでなく、容器の開口部がト
ナー充填口を兼ねる場合が多いため、トナー充填性能も
悪化する。このため、充填量を減らさざるを得なかった
り、充填タクトが長くなりコストアップしてしまう問題
があった。
Further, a seal member disposed between the shutter and the cap member is generally attached to the cap member so as to surround the toner supply port. However, in this configuration, it is necessary to provide the sticking portion of the seal member and the guide portion of the shutter on the flange of the cap member,
The entire cap member tended to be large. Although there is no problem if the developing hopper of the image forming apparatus main body has a margin, the size of the image forming apparatus main body has recently tended to be reduced, and the developing hopper itself has become smaller. For this reason, the opening of the developer supply container installed in the space excluding the sticking portion of the seal member and the shutter guide portion becomes small. If the opening of the container becomes smaller, not only does the toner discharge property deteriorate, but also the toner filling performance deteriorates because the opening of the container often serves also as a toner filling port. For this reason, there has been a problem that the filling amount has to be reduced, and the filling tact becomes long and the cost increases.

【0009】更に、シール部材をキャップ部材のフラン
ジ部に貼着する場合には、組み立て性を考慮すると、シ
ャッターガイド部を逃がす必要がある。しかしながら、
シール部材を圧縮するシャッターはガイドによって抑え
られているため、シャッターガイド部にシール部材が存
在しないと確実にシール部材を圧縮することが困難にな
り、あるいはシャッターが撓み、シール性に安定性がな
くなる問題があった。
Further, when the sealing member is attached to the flange portion of the cap member, it is necessary to release the shutter guide portion in consideration of assemblability. However,
Since the shutter for compressing the seal member is suppressed by the guide, it is difficult to reliably compress the seal member if the seal member is not present in the shutter guide portion, or the shutter bends, and the sealing performance becomes unstable. There was a problem.

【0010】本発明の目的は、物流時の落下衝撃あるい
は画像形成装置本体へ現像剤を補給する際に現像剤の外
部へのはみ出しによる汚れが発生せず、シャッターの開
閉動作に必要な操作力を低減させた易開閉性を実現さ
せ、しかも画像形成装置のコンパクト化に対応した現像
剤補給容器を提供するものである。
SUMMARY OF THE INVENTION It is an object of the present invention to prevent the occurrence of dirt due to a drop impact during distribution or a protrusion of the developer to the outside when the developer is supplied to the image forming apparatus main body, and an operating force required for opening and closing the shutter. It is intended to provide a developer supply container that realizes easy opening and closing with reduced image quality and that can be made compact in size of an image forming apparatus.

【0011】[0011]

【課題を解決するための手段】本発明の第1の発明は
像形成装置の本体に現像剤を補給する現像剤補給容器で
あって、現像剤を補給する開口部を備え、現像剤を収納
する容器本体と、前記開口部を閉鎖するシャッターと、
前記シャッターを、前記開口部を閉鎖する閉鎖位置と、
前記開口部を開放する開放位置と、に移動可能にガイド
するガイド部であって、前記シャッターの移動方向と直
角方向において前記シャッターの端部に設けられ、前記
移動方向に沿って延びて設けられたガイド部と、を有す
る現像剤補給容器において、前記シャッターの現像剤が
収納される側の表面であって、前記開口部に対応する領
域と前記ガイド部に対応する領域にまたがって設けら
れ、前記シャッターと前記ガイド部との間で圧縮される
弾性シール部材と、前記弾性シール部材表面に設けられ
前記ガイド部と摺動する可撓性フィルムと、を有し、こ
の可撓性フィルムはその表面にシリコン系材料のコーテ
ィング層を備えることを特徴とする現像剤補給容器であ
Means for Solving the Problems The first invention of the present invention is an image
In a developer supply container that supplies developer to the main body of the image forming apparatus
There is an opening to supply the developer and stores the developer
Container body, and a shutter that closes the opening,
The shutter, a closed position to close the opening,
An open position to open the opening, and a guide movably to
Guide section, which is directly in the moving direction of the shutter.
Provided at an end of the shutter in an angular direction,
A guide portion extending along the moving direction.
In the developer supply container, the developer of the shutter is
A surface corresponding to the opening on the surface to be stored.
Area and an area corresponding to the guide portion.
Is compressed between the shutter and the guide portion.
An elastic seal member, provided on a surface of the elastic seal member;
A flexible film slidable with the guide portion.
Flexible film has a silicon-based material coating on its surface.
A developer supply container having a developing layer.
You .

【0012】本発明の第2の発明は前記ガイド部は、前
記シャッター、前記弾性シール部材及び前記可撓性フィ
ルムを挟む、一体成形された凹部を備えることを特徴と
する第1の発明の現像剤補給容器である。
According to a second aspect of the present invention, in the developing method of the first aspect, the guide portion includes an integrally formed concave portion sandwiching the shutter, the elastic seal member and the flexible film. It is a medicine supply container.

【0013】本発明の第3の発明は前記弾性シール部材
は発泡体であることを特徴とする第1又は第2の発明の
現像剤補給容器である。
According to a third aspect of the present invention, there is provided the elastic sealing member.
Is a developer supply container according to the first or second invention, which is a foam .

【0014】本発明の4の発明は前記可撓性フィルムの
基材の厚さは4μm〜100μmであることを特徴とす
る第1乃至第3いずれかの発明の現像剤補給容器。
According to a fourth aspect of the present invention, the flexible film is
The thickness of the substrate is 4 μm to 100 μm.
The developer supply container according to any one of the first to third inventions .

【0015】本発明の5の発明は前記コーティング層の
厚さは0.05μm〜2μmであることを特徴とする第
1乃至第4のいずれかの発明の現像剤補給容器である。
According to a fifth aspect of the present invention, the coating layer
The thickness is 0.05 μm to 2 μm.
A developer supply container according to any one of the first to fourth inventions .

【0016】本発明の6の発明は前記弾性シール部材は
前記シャッターと2色成型したものであることを特徴と
する第1乃至第5のいずれかの発明の現像剤補給容器で
ある。
According to a sixth aspect of the present invention, the elastic sealing member is
Characterized in that the shutter is molded in two colors.
A developer supply container according to any one of the first to fifth aspects of the present invention .

【0017】本発明の第7の発明は前記シール部材は硬
度20〜70°、圧縮永久歪み4%以下、セルサイズ6
0〜300μm、比重が0.2〜0.5の発泡ポリウレ
タンであって、前記シール部材を5〜50%圧縮して用
いることを特徴とする第1乃至第6のいずれかの発明の
現像剤補給容器である。
According to a seventh aspect of the present invention, the sealing member is hard.
Degree 20-70 °, compression set 4% or less, cell size 6
0-300 μm, specific gravity 0.2-0.5 foamed polyurethane
A tongue for compressing the seal member by 5 to 50%
The developer supply container according to any one of the first to sixth aspects of the present invention .

【0018】本発明の第8の発明は前記シール部材の圧
縮応力が0.1kg/cm 2 〜2.0kg/cm 2 である
ことを特徴とする第7の発明の現像剤補給容器。
According to an eighth aspect of the present invention, the pressure of the sealing member is reduced.
Shrinkage stress is at 0.1kg / cm 2 ~2.0kg / cm 2
A developer supply container according to the seventh aspect of the present invention .

【0019】本発明の第9の発明は前記シャッターの曲
げ弾性率が20000kg/cm 2 〜100000kg
/cm 2 であることを特徴とする第1乃至第8のいずれ
かの発明の現像剤補給容器である。
According to a ninth aspect of the present invention, a tune of the shutter is provided.
The lower elastic modulus is 20000kg / cm 2 ~100000kg
/ Any of the first to eighth characterized in that it is a cm 2
A developer supply container according to the invention.

【0020】本発明の第10の発明は前記シャッターの
前記弾性シール部材が設けられた面とは反対側の面に、
低摩擦抵抗材料が塗布されていることを特徴とする第1
乃至第9のいずれかの発明の現像剤補給容器である。
According to a tenth aspect of the present invention, the shutter
On the surface opposite to the surface on which the elastic seal member is provided,
The first feature is that a low friction resistance material is applied.
A developer supply container according to any one of the first to ninth aspects .

【0021】本発明の第11の発明は前記低摩擦抵抗材
料はシリコンオイルであることを特徴とする第10の発
明の現像剤補給容器である。
According to an eleventh aspect of the present invention, the low friction resistance material is
The tenth aspect characterized in that the material is silicone oil
This is a bright developer supply container.

【0022】本発明の第12の発明は前記シリコンオイ
ルの粘度は100cSt〜10000cStであること
を特徴とする第11の発明の現像剤補給容器である。
According to a twelfth aspect of the present invention, the silicon oil
The viscosity of the oil must be 100 cSt to 10,000 cSt
An eleventh aspect of the present invention is the developer supply container according to the eleventh aspect .

【0023】本発明の第13の発明は前記シリコンオイ
ルの塗布量は0.01mg/cm 2 〜0.5mg/cm 2
であることを特徴とする第11又は第12の発明の現像
剤補給容器である。
According to a thirteenth aspect of the present invention, the silicon oil
Is 0.01 mg / cm 2 to 0.5 mg / cm 2
A developer supply container according to the eleventh or twelfth aspect, characterized in that:

【0024】[0024]

【0025】[0025]

【0026】[0026]

【0027】[0027]

【0028】[0028]

【0029】[0029]

【0030】[0030]

【0031】[0031]

【0032】[0032]

【0033】[0033]

【0034】[0034]

【0035】[0035]

【0036】[0036]

【0037】[0037]

【0038】[0038]

【0039】[0039]

【0040】[0040]

【0041】[0041]

【0042】[0042]

【0043】[0043]

【0044】[0044]

【実施例】以下、本発明の実施例を図面を基いて説明す
る。
Embodiments of the present invention will be described below with reference to the drawings.

【0045】「実施例1」本発明の実施例を適用した現
像剤補給容器及び前記容器の組立方法について図1〜図
4に基づいて説明する。
Embodiment 1 A developer supply container to which an embodiment of the present invention is applied and a method for assembling the container will be described with reference to FIGS.

【0046】符号Cは、本実施例におけるスライドシャ
ッター式現像剤補給容器である。図1に示すように、縁
部がシャッター3のキャップ部材2との間に配置され、
表面に可撓性フィルム5が貼着されたシール部材4をシ
ャッター3の現像剤補給用の開口1aに対する面3aに
貼着する。可撓性フィルム5を貼着したシール部材4を
可撓性フィルム5を該開口1aに面する側にしてシャッ
ター3の面3aに貼着することで、キャップ部材2の
示凹部となったシャッターガイド部2cに、可撓性フィ
ルム5を貼着したシール部材4を配置することが可能に
なり、シール性の安定性を図ることができる。
Reference numeral C denotes a slide shutter type developer supply container in this embodiment. As shown in FIG. 1, the edge is disposed between the shutter 3 and the cap member 2 of the shutter 3,
A sealing member 4 having a flexible film 5 adhered to the surface is adhered to the surface 3a of the shutter 3 corresponding to the developer supply opening 1a. The seal member 4 to which the flexible film 5 has been attached is attached to the surface 3a of the shutter 3 with the flexible film 5 facing the opening 1a, so that the cap member 2 is shown in FIG.
The seal member 4 to which the flexible film 5 is adhered can be arranged on the shutter guide portion 2c that is the concave portion, and the sealing performance can be stabilized.

【0047】図1〜図4に示す通り、本実施例における
現像剤補給容器Cは、複写機本体Pに設けられた現像ホ
ッパー7に現像剤を供給するための開口1aを有し、現
像剤6を収納可能な容器本体1と、前記開口1aを閉鎖
するためのシャッター3と、前記開口1aを閉鎖する閉
鎖位置と、該閉鎖位置から退避して前記開口1aを開放
する開放位置とを取り得るよう、前記シャッター3を支
持するキャップ部材2とを有しており、前記シャッター
3の前記開口1a側の面3aには可撓性フィルム5を貼
着したシール部材4が貼着されている。そして前記キャ
ップ部材2は、前記シャッター3の移動方向(図2、図
4の矢印A方向)の直角方向に対して両側に、シャッタ
ー3の移動方向をガイドするガイド部2cを有し、前記
可撓性フィルム5を貼着したシール部材4は前記開口1
aと前記ガイド部2cとにわたって設けられている。
As shown in FIGS. 1 to 4, the developer supply container C in this embodiment has an opening 1a for supplying a developer to a developing hopper 7 provided in the copying machine main body P. 6, a shutter 3 for closing the opening 1a, a closed position for closing the opening 1a, and an open position for retracting from the closed position and opening the opening 1a. And a cap member 2 for supporting the shutter 3, and a sealing member 4 to which a flexible film 5 is adhered is adhered to a surface 3a of the shutter 3 on the opening 1a side. . The cap member 2 has guide portions 2c for guiding the moving direction of the shutter 3 on both sides with respect to a direction perpendicular to the moving direction of the shutter 3 (the direction of arrow A in FIGS. 2 and 4). The sealing member 4 to which the flexible film 5 is attached is
a and the guide portion 2c.

【0048】ここで、可撓性フィルム5を貼着したシー
ル部材4は柔らかい弾性体で、キャップ部材2とシャッ
ター3との間のシール性を維持して、落下等の衝撃にて
容器本体1内部に収納されている現像剤6がキャップ部
材2とシャッター3との間から漏れ出るのを防止するこ
とを要求される。また、可撓性フィルム5は、キャップ
部材2の現像剤補給用の開口2aを持つフランジのフラ
ンジ面2bと低摩擦抵抗で摺動し、シャッター開閉に要
する力、即ちシャッター開閉強度を小さくすることが要
求される。
Here, the sealing member 4 to which the flexible film 5 is adhered is a soft elastic body, and maintains the sealing property between the cap member 2 and the shutter 3 so that the container main body 1 is impacted by dropping or the like. It is required to prevent the developer 6 stored inside from leaking from between the cap member 2 and the shutter 3. Further, the flexible film 5 slides with low frictional resistance on the flange surface 2b of the flange having the developer supply opening 2a of the cap member 2 to reduce the force required for opening and closing the shutter, that is, the shutter opening and closing strength. Is required.

【0049】そこで具体的には、可撓性フィルム5の材
質として、ポリエステル、OPP、ポリアミド、ポリエ
チレン、フッ素樹脂の単層、またはこれらの複合層を基
材とし、表面にシリコンオイル、シリコンワックス、シ
リコン系塗料等をコーティングしたものを用いる。可撓
性フィルムの基材の厚さは4μm〜100μmであるこ
とが好ましい。さらに、より好ましくは基材の厚さが1
0μm〜50μmのものを用いる。これは、基材が厚す
ぎるとシール部材4の弾性が有効に生かされず、落下時
にトナー漏れが発生するためである。逆に基材が薄すぎ
るとフイルムをシール部材4に貼着する際にフィルムが
ねじれるしわがよる等組立性が悪化するためである。シ
リコンオイルのコーティング層の厚さは0.05μm〜
2μmであることが好ましい。さらに、より好ましくは
シリコンオイルのコーティング層の厚さが0.1μm〜
0.5μmであるものを用いる。これはコーティング層
が厚すぎると容器本体1の内部の現像剤6への悪影響が
懸念され、薄すぎるとシャッター開閉強度低下の効果が
ないためである。
Therefore, specifically, as a material of the flexible film 5, a single layer of polyester, OPP, polyamide, polyethylene, or fluororesin or a composite layer thereof is used as a base material, and silicon oil, silicon wax, One coated with a silicone paint or the like is used. The thickness of the flexible film substrate is preferably 4 μm to 100 μm. More preferably, the thickness of the substrate is 1
One having a thickness of 0 μm to 50 μm is used. This is because if the base material is too thick, the elasticity of the seal member 4 cannot be effectively utilized, and toner leakage occurs when the base material falls. On the other hand, if the base material is too thin, the film is twisted when the film is adhered to the sealing member 4, and the assembling property is deteriorated. Silicon oil coating layer thickness is 0.05μm ~
It is preferably 2 μm. More preferably, the thickness of the silicone oil coating layer is 0.1 μm or more.
One having a thickness of 0.5 μm is used. This is because if the coating layer is too thick, the developer 6 inside the container main body 1 may be adversely affected, and if the coating layer is too thin, there is no effect of lowering the shutter opening / closing strength.

【0050】シール部材4の材質として、シリコン、ウ
レタン、発泡ポリエチレン等のゴムやスポンジ、望まし
くは硬度20〜70°、圧縮永久歪み4%以下、セルサ
イズ60〜300μm、比重が0.2〜0.5である低
発泡ポリウレタンを10〜30%圧縮して用いる。
Rubber or sponge such as silicone, urethane or foamed polyethylene, desirably a hardness of 20 to 70 °, a compression set of 4% or less, a cell size of 60 to 300 μm, and a specific gravity of 0.2 to 0 The low-foamed polyurethane of 0.5 is used after being compressed by 10 to 30%.

【0051】シャッター3とシール部材4、可撓性フィ
ルム5とシール部材4、それぞれの接着は、シャッター
開閉時に剥れたり、ずれたりしない程度の接着強度が必
要で、シャッター3とシール部材4は、出来れば二色成
型により一体成型することが望ましい。
The adhesive between the shutter 3 and the sealing member 4 and the adhesive between the flexible film 5 and the sealing member 4 need to have such an adhesive strength that they do not peel or shift when the shutter is opened and closed. If possible, it is desirable to integrally mold by two-color molding.

【0052】シャッター3は、落下等の衝撃において、
折れたり、捩れたりせず、さらに、可撓性フィルム5を
貼着したシール部材4を均一に圧縮出来るだけの剛性を
持つことが要求される。またキャップ部材2との摺動摩
擦抵抗が小さいことも必要である。具体的には材質とし
て、ポリスチレン、ポリプロピレン、ABS等のプラス
チック樹脂、前記プラスチック樹脂にガラス繊維を混合
した混合材料、さらにはステンレス等の金属が挙げられ
る。
The shutter 3 can be used to
It is required that the seal member 4 not be bent or twisted and have sufficient rigidity to uniformly compress the seal member 4 to which the flexible film 5 is adhered. It is also necessary that the sliding friction resistance with the cap member 2 is small. Specific examples of the material include a plastic resin such as polystyrene, polypropylene, and ABS; a mixed material obtained by mixing glass fibers with the plastic resin; and a metal such as stainless steel.

【0053】図1、図3、図4に示す通り、キャップ部
材2は容器本体1に取り付けられており、容器本体1か
ら複写機本体Pに設けられた現像ホッパー7に現像剤6
を補給するための開口2aとシャッター3の開閉移動を
ガイドするコの字状のシャッターガイド部2cを有す
る。そして、容器本体1との結合部において、密封性を
保つ構造を持つことが必要である。このキャップ部材2
の材質としては、シャッター材と同様の材質が考えられ
る。
As shown in FIGS. 1, 3, and 4, the cap member 2 is attached to the container main body 1, and the developer 6 is transferred from the container main body 1 to the developing hopper 7 provided in the copying machine main body P.
Opening 2a for replenishing the shutter, and a U-shaped shutter guide portion 2c for guiding the opening and closing movement of the shutter 3. Then, it is necessary to have a structure for maintaining the hermeticity at the joint with the container body 1. This cap member 2
May be the same as the shutter material.

【0054】例えば、図1〜図4に示すように、キャッ
プ部材2(ガイド部2cが一体成形された場合)容器本
体1、キャップ部材2の材質にポリプロピレン、シャッ
ター3の材質にガラス繊維入りポリプロピレン、可撓性
フィルム5にはシリコンオイルをコーティングしたOP
Pフィルム(商品名:カルランテープ、日東電工社)、
シール部材4には厚さ2.4mmの発泡ポリウレタン
(商品名:ポロン、イノアック社)を用いて、可撓性フ
ィルム5を貼着したシール部材4を前述した通りシャッ
ター3に貼着し、約20%圧縮した状態でキャップ部材
2に組み込んで実験を行った。この構成によれば図5に
示すようなキャップ部材2にシール部材4を貼着した場
合と比較して、現像剤補給口径を約10mm程度増加さ
せることが出来た。その結果現像剤6の排出時間が約1
5秒となり、従来の約半分の時間で複写機本体Pに現像
剤6の補給を完了することが可能になった。また本実施
例の現像剤補給容器Cを組み立てるに当たって、容器本
体1に現像剤6を充填するについてもタクトアップが可
能になった。
[0054] For example, as shown in FIGS. 1 to 4, cap
OP member 2 (in the case where guide portion 2c is integrally formed) OP in which the material of container body 1 and cap member 2 is polypropylene, the material of shutter 3 is polypropylene containing glass fiber, and the flexible film 5 is silicon oil.
P film (product name: Karlan tape, Nitto Denko Corporation),
As the seal member 4, a 2.4-mm-thick foamed polyurethane (trade name: PORON, INOAC CORPORATION) was used, and the seal member 4 to which the flexible film 5 was attached was attached to the shutter 3 as described above. An experiment was conducted by incorporating the cap member 2 in a compressed state of 20%. According to this configuration, the developer supply aperture can be increased by about 10 mm as compared with the case where the seal member 4 is attached to the cap member 2 as shown in FIG. As a result, the discharge time of the developer 6 is about 1
This is 5 seconds, which makes it possible to complete the replenishment of the developer 6 to the copying machine main body P in about half the conventional time. Further, in assembling the developer supply container C of the present embodiment, it is possible to increase the tact time when the container 6 is filled with the developer 6.

【0055】本実施例の100個の現像剤補給容器Cを
作り、開封テストを行った結果、シャッター3を開くの
に要する力、即ち、開封強度は3〜4kgf程度であ
り、容器本体1内の現像剤6はほとんど残らず現像ホッ
パー7に供給することが出来た。
As a result of making 100 developer supply containers C of this embodiment and performing an opening test, the force required to open the shutter 3, that is, the opening strength is about 3 to 4 kgf. Almost no developer 6 could be supplied to the developing hopper 7.

【0056】さらに、環境物流テストとして、振動テス
ト、減圧テスト、落下テスト、高温高湿テストについ
て、各条件ごとに現像剤補給容器Cを10個ずつ用いて
行ったが、いずれのテストにおいても現像剤6の漏れ等
の異常はみられず、画出しテストを行ったが、画質は良
好であり、問題は発生しなかった。
Further, as the environmental logistics test, a vibration test, a pressure reduction test, a drop test, and a high temperature and high humidity test were performed using ten developer supply containers C for each condition. An abnormality such as leakage of the agent 6 was not observed, and an image output test was performed. However, the image quality was good and no problem occurred.

【0057】さらに、本実施例の可撓性フィルム5の基
材のみをシリコンオイルをコーティングしたPETフイ
ルムに変更した構成の現像剤補給容器Cで開封テスト、
環境物流テストを行った結果、可撓性フィルム5にシリ
コンオイルをコーティングしたOPPフィルムを用いた
現像剤補給容器Cと同様問題は発生しなかった。画出し
テストについても問題は発生しなかった。
Further, an opening test was performed using a developer supply container C having a configuration in which only the base material of the flexible film 5 of this embodiment was changed to a PET film coated with silicone oil.
As a result of conducting an environmental distribution test, no problem occurred as in the case of the developer supply container C using the OPP film in which the flexible film 5 was coated with silicone oil. No problems occurred in the image test.

【0058】本実施例の現像剤補給容器Cを用いて、複
写機本体Pに設けられた現像ホッパー7に現像剤6を補
給する状態を図4に示す。図4に示すように、操作者が
シャッター3の把手3cを掴んで、矢印A方向へシャッ
ター3を開くと容器本体1内部の現像剤6が開放された
開口1aを通じて落下して現像ホッパー7に補給され
る。容器本体1に現像剤6が残った状態でここで、現像
ホッパー7が満杯になった場合等に操作者がシャッター
3の把手3cを掴んで、シャッター3を図4において矢
印Aと反対方向に押して閉鎖位置まで移動させて、開口
1aを閉じることがある。このように補給を途中で止め
ても、開口1aはシャッター3に貼着された可撓性フィ
ルム5を貼着したシール部材4とキャップ部材2との間
でシールされており、現像剤6が漏れて飛散することは
ない。このように現像ホッパー7へ現像剤6を補給後、
シャッター3を閉じて現像剤補給容器Cを現像ホッパー
7から外す際、特に現像剤6の飛散等はみられなかっ
た。
FIG. 4 shows a state in which the developer 6 is supplied to the developing hopper 7 provided in the copying machine main body P by using the developer supply container C of this embodiment. As shown in FIG. 4, when the operator grasps the handle 3c of the shutter 3 and opens the shutter 3 in the direction of arrow A, the developer 6 inside the container body 1 falls through the opened opening 1a and enters the developing hopper 7. Replenished. In a state where the developer 6 remains in the container main body 1, the operator grasps the handle 3 c of the shutter 3 when the developing hopper 7 is full or the like, and moves the shutter 3 in the direction opposite to the arrow A in FIG. The opening 1a may be closed by pushing to move to the closed position. Even if replenishment is stopped in the middle, the opening 1a is sealed between the cap member 2 and the sealing member 4 to which the flexible film 5 attached to the shutter 3 is attached. It does not leak and scatter. After supplying the developer 6 to the developing hopper 7 in this manner,
When the shutter 3 was closed to remove the developer supply container C from the developing hopper 7, no scattering of the developer 6 was observed.

【0059】本実施例における現像剤補給容器Cの組立
方法は次の通りである。まず、複写機本体Pに設けられ
た現像ホッパー7に現像剤6を供給するための開口1a
を有して、現像剤6を収納可能な容器本体1を準備し、
また、前記開口1aを閉鎖するためのシャッター3を準
備し、前記開口1aを閉鎖する閉鎖位置と、該閉鎖位置
から退避して前記開口1aを開放する開放位置とを取り
得るよう前記シャッター3を支持するキャップ部材2を
準備し、前記シャッター3の前記開口1a側の面3aに
弾性シール部材4を取り付け、さらに弾性シール部材4
の前記開口1a側にシリコンオイル層が来るように該シ
リコンオイルで片面がコーティングされた可撓性フィル
ム5を設置するものである。そしてシャッター3に可撓
性フィルム5を貼着したシール部材4を取り付けるに当
たっては可撓性フィルム5、シール部材4両者ともシャ
ッター3の移動方向をガイドするキャップ部材2と前記
開口1aとに渡るように貼着する。
The method of assembling the developer supply container C in this embodiment is as follows. First, an opening 1a for supplying the developer 6 to a developing hopper 7 provided in the main body P of the copying machine.
And preparing a container body 1 capable of storing the developer 6,
Further, a shutter 3 for closing the opening 1a is prepared, and the shutter 3 is set so as to take a closed position for closing the opening 1a and an open position for retreating from the closed position and opening the opening 1a. A cap member 2 to be supported is prepared, and an elastic seal member 4 is attached to a surface 3a of the shutter 3 on the opening 1a side.
The flexible film 5 coated on one side with the silicone oil is placed so that the silicone oil layer comes to the opening 1a side. In attaching the seal member 4 with the flexible film 5 stuck to the shutter 3, both the flexible film 5 and the seal member 4 pass over the cap member 2 for guiding the moving direction of the shutter 3 and the opening 1a. Stick it on

【0060】「実施例2」本実施例では、シール部材4
をシャッター3に取り付けるにあたって、シール部材4
の材料としてウレタンゴムを用い、2色成型によりシー
ル部材4をシャッター3と一体成型した。さらに、シー
ル部材4の前記開口1a側にシリコンオイル層が来るよ
うに該シリコンオイルで片面がコーティングされた可撓
性フィルム5を貼着した。それ以外の点については実施
例1と同じである。
Embodiment 2 In this embodiment, the sealing member 4
When attaching to the shutter 3, the sealing member 4
The sealing member 4 was integrally formed with the shutter 3 by two-color molding using urethane rubber as a material for the above. Further, a flexible film 5 coated on one side with the silicone oil was attached so that the silicone oil layer came to the opening 1a side of the sealing member 4. The other points are the same as in the first embodiment.

【0061】本実施例では、シール部材を貼着する必要
がないので、工程削減によるコストダウンを図ることが
出来る。
In this embodiment, since it is not necessary to attach a seal member, the cost can be reduced by reducing the number of steps.

【0062】本実施例でも開封テスト、環境物流テスト
を行ったが、問題は発生しなかった。
In this example, an opening test and an environmental distribution test were performed, but no problem occurred.

【0063】「実施例3」前述実施例によれば、スライ
ドシャッター方式の現像剤補給容器Cにおいて、シャッ
ター3とキャップ部材2との間に配置される可撓性フィ
ルム5を貼着したシール部材4をシャッター3の現像剤
補給用の開口1aに対する面に可撓性フィルム5を該開
口1aに面する側にして貼着する(図1〜図4)。この
ように可撓性フィルム5を貼着したシール部材4をシャ
ッター3に貼着し、キャップ部材2のシャッターガイド
部2c内に可撓性フィルム5を貼着したシール部材4を
配置することにより、シール性の安定化が図れ、キャッ
プ部材2におけるシール部材4の貼着スペースが不要に
なる。そのため、キャップ部材2のシャッターガイド部
2cを容器本体1の開口1aのすぐ脇に位置させること
が可能となり、さらなるシール性の向上が図れる。さら
に、可撓性フィルム5を貼着してシール部材4をシャッ
ター3に貼着して組み立てることで、可撓性フィルム5
を貼着したシール部材4が、開口1aの周縁部に沿って
食い込み変形することで、さらなるシール性の向上が図
れる。
[Embodiment 3] According to the above-described embodiment, in the developer supply container C of the slide shutter type, the sealing member on which the flexible film 5 disposed between the shutter 3 and the cap member 2 is adhered. The flexible film 5 is attached to the surface of the shutter 3 facing the opening 1a for supplying developer, with the flexible film 5 facing the opening 1a (FIGS. 1 to 4). By attaching the sealing member 4 to which the flexible film 5 has been attached in this way to the shutter 3, and disposing the sealing member 4 to which the flexible film 5 has been attached in the shutter guide portion 2 c of the cap member 2. In addition, the sealing property can be stabilized, and the space for attaching the sealing member 4 in the cap member 2 becomes unnecessary. Therefore, the shutter guide portion 2c of the cap member 2 can be located immediately beside the opening 1a of the container body 1, and the sealing property can be further improved. Furthermore, the flexible film 5 is adhered, the seal member 4 is adhered to the shutter 3 and the flexible film 5 is assembled.
The sealing member 4 to which is adhered is deformed by biting along the periphery of the opening 1a, so that the sealing property can be further improved.

【0064】シール部材4は、柔らかい弾性体で、キャ
ップ部材2とシャッター3の間のシール性を保ち、落下
衝撃等にて容器本体1内部の現像剤6の漏れを防止する
ことが要求される。そこで具体的には、シール部材4の
材質として、シリコン、ウレタン等のゴムやスポンジ、
望ましくは、硬度20〜70°、圧縮永久歪み4%以
下、セルサイズ60〜300μm、比重0.2〜0.5
である低発泡ポリウレタンを5〜50%圧縮し望ましく
は20〜40%圧縮して用いる。
The seal member 4 is required to be a soft elastic body, to maintain the sealing property between the cap member 2 and the shutter 3, and to prevent the developer 6 inside the container body 1 from leaking due to a drop impact or the like. . Therefore, specifically, rubber or sponge such as silicon, urethane, etc.
Desirably, hardness is 20 to 70 °, compression set is 4% or less, cell size is 60 to 300 μm, specific gravity is 0.2 to 0.5.
Is used after being compressed by 5 to 50%, preferably by 20 to 40%.

【0065】シール部材4の圧縮は、最近の現像剤補給
容器の容量増加傾向に対応して、高いシール性を維持す
るために、圧縮率及び圧縮応力を増加させることが望ま
しい。すなわち、圧縮率が小さいとシール部材4の圧縮
応力も小さくなり、十分なシール性が得られず、落下衝
撃等にて現像剤6の漏れが発生してしまう。特に、大容
量の現像剤補給容器等の現像剤補給口の口径が大きい場
合には、落下衝撃等にてシャッター3の部材が撓みやす
いため、シール部材4の圧縮率の設定値が小さいと、瞬
間的にシール性がなくなってしまう可能性がある。とこ
ろが逆に、圧縮率が大きくなりすぎるとシール部材4の
圧縮圧力も大きくなって、シール性は向上するが、同時
にシャッター3の開閉強度も大きくなってしまう。
In the compression of the seal member 4, it is desirable to increase the compression ratio and the compressive stress in order to maintain a high sealing property in response to the recent tendency of increasing the capacity of the developer supply container. That is, if the compression ratio is small, the compression stress of the seal member 4 also becomes small, so that sufficient sealing properties cannot be obtained, and the developer 6 leaks due to a drop impact or the like. In particular, when the diameter of the developer supply port such as a large-capacity developer supply container is large, the member of the shutter 3 is easily bent by a drop impact or the like. There is a possibility that the sealing property may be lost instantaneously. Conversely, if the compression ratio is too high, the compression pressure of the seal member 4 is also increased, and the sealing performance is improved, but at the same time, the opening and closing strength of the shutter 3 is also increased.

【0066】そこで、高いシール性と低いシャッター開
閉強度を同時に実現するために、シール部材4の表面に
可撓性フィルム5を配置する。シール部材4に容器本体
1のシール機能を持たせ、可撓性フィルム5に低いシャ
ッター開閉強度機能を持たせることによって機能分離を
行う。可撓性フィルム5によって、キャップ部材2の現
像剤補給用の開口2aを持つフランジ面2bと低抵抗で
摺動し、シャッター開閉強度を小さくすることができ
る。
Therefore, a flexible film 5 is disposed on the surface of the sealing member 4 in order to simultaneously achieve high sealing performance and low shutter opening / closing strength. Function separation is performed by providing the sealing member 4 with the sealing function of the container body 1 and giving the flexible film 5 a low shutter opening / closing strength function. The flexible film 5 slides with low resistance on the flange surface 2b of the cap member 2 having the opening 2a for supplying the developer, and the shutter opening / closing strength can be reduced.

【0067】具体的に、可撓性フィルム5は、基材の厚
さが4μm〜100μm、さらにより好ましくは基材の
厚さが10μm〜50μmのものを用いる。シリコンオ
イルのコーティング層の厚さは0.05μm〜2μmで
あるものを用い、さらに、より好ましくはシリコンオイ
ルのコーティング層の厚さが0.1μm〜0.5μmで
あるものを用いる。基材の厚さが厚すぎると、シール部
材4が開口2aの周縁部に沿って食い込み変形せず、十
分なシール性の効果が得られない。また、シリコンオイ
ルのコーティング層の厚さは、厚すぎると容器本体1内
部のトナーへ悪影響を及ぼし、逆に薄すぎるとシャッタ
ー開閉強度低下の十分な効果が得られない。
Specifically, the flexible film 5 has a substrate thickness of 4 μm to 100 μm, and more preferably a substrate thickness of 10 μm to 50 μm. The thickness of the silicone oil coating layer is 0.05 μm to 2 μm, and more preferably the thickness of the silicone oil coating layer is 0.1 μm to 0.5 μm. If the thickness of the base material is too large, the sealing member 4 does not bite and deform along the peripheral edge of the opening 2a, and a sufficient sealing effect cannot be obtained. If the thickness of the silicone oil coating layer is too large, the toner inside the container body 1 is adversely affected.

【0068】つまり、シール部材4の圧縮率及び圧縮圧
力、また、可撓性フィルム5の厚さ及びコーティング層
の厚さは、いずれも適正な範囲に制御することが望まし
い。シール部材4の圧縮率は0.1kg/cm2 〜2.
0kg/cm2 でシール性及びシャッター開閉強度を満
足するがより好ましくは0.6〜1.5kg/cm2
値がよい。
That is, it is desirable that the compression ratio and the compression pressure of the seal member 4 and the thickness of the flexible film 5 and the thickness of the coating layer are all controlled within appropriate ranges. The compression ratio of the seal member 4 is 0.1 kg / cm 2 to 2.
0 kg / cm 2 satisfies the sealing property and shutter opening / closing strength, but more preferably 0.6 to 1.5 kg / cm 2 .

【0069】キャップ部材2は、容器本体1から現像ホ
ッパー7に現像剤6を補給するための開口2aとシャッ
ター3をガイドするコの字状のシャッターガイド部2c
を持ち、容器本体1との結合部において、密封性を保つ
構造を持つことが必要である。キャップ部材2の材質と
してはポリスチレン、ポリプロピレン、ABS等のプラ
スチック樹脂、及びその樹脂のガラス繊維強化材料、ま
たは、ステンレス等の金属が挙げられる。
The cap member 2 has an opening 2 a for supplying the developer 6 from the container body 1 to the developing hopper 7 and a U-shaped shutter guide portion 2 c for guiding the shutter 3.
It is necessary to have a structure for maintaining the hermeticity at the joint with the container body 1. Examples of the material of the cap member 2 include a plastic resin such as polystyrene, polypropylene, and ABS, a glass fiber reinforced material of the resin, and a metal such as stainless steel.

【0070】シャッター3は、落下衝撃において、折れ
たり、捩れたりせず、さらに可撓性フィルム5を貼着し
たシール部材4を均一に圧縮できるだけの剛性を持つこ
とが要求される。前記の通り、現像剤補給容器の容量増
加にともない、現像剤補給口の口径が大きくなり、さら
にシール部材4の圧縮率及び圧縮応力が大きくなると、
シール部材4を支持しているシャッター3が変形して、
現像剤6の漏れが発生しやすくなる。シャッター3の部
材は板状であり、キャップ部材2よりも変形しやすく、
また、開閉時にシャッター3の撓みによるシャッター開
閉強度の上昇、現像剤6の漏れ等のトラブルを防止する
ためにも、シャッター3の部材の剛性を確保することが
望ましい。
The shutter 3 is required not to be broken or twisted by a drop impact and to have a rigidity capable of uniformly compressing the seal member 4 to which the flexible film 5 is adhered. As described above, with the increase in the capacity of the developer supply container, the diameter of the developer supply port increases, and when the compression ratio and the compression stress of the seal member 4 increase,
The shutter 3 supporting the sealing member 4 is deformed,
Leakage of the developer 6 is likely to occur. The member of the shutter 3 is plate-shaped, and is more easily deformed than the cap member 2,
It is also desirable to ensure the rigidity of the members of the shutter 3 in order to prevent problems such as an increase in shutter opening / closing strength due to the bending of the shutter 3 during opening and closing and leakage of the developer 6.

【0071】すなわち、シャッター3の曲げ弾性率が小
さいと、シャッター3が変形して前記問題点が発生して
まうが、逆に曲げ弾性率を大きくしすぎると脆くなり、
物流時の衝撃等によりクラックが発生したり、割れてし
まう可能性がある。また、曲げ弾性率が極端に高い材料
は種類が少なく、コストも高くなる傾向がある。
That is, if the bending elastic modulus of the shutter 3 is small, the shutter 3 is deformed and the above problem occurs, but if the bending elastic modulus is too large, it becomes brittle.
Cracks may occur or break due to impact during distribution. Further, there are few kinds of materials having extremely high flexural modulus, and the cost tends to be high.

【0072】本実施例によれば、シャッター3の曲げ弾
性率についても、適正な範囲の構成を用いることが望ま
しく、具体的には20000kg/cm2 〜10000
0kg/cm2 内で選択できるが50000〜8000
0kg/cm2 のものを用いることが望ましい。(JI
S−K7203参考) なお、シャッター3の材料としては、前記内容を前提と
した上で、キャップ部材2と同種の材料から選定するこ
とが望ましい。
According to the present embodiment, it is desirable that the shutter 3 has a flexural modulus in a proper range, specifically, 20,000 kg / cm 2 to 10,000.
It can be selected within 0kg / cm 2 50000~8000
It is desirable to use one of 0 kg / cm 2 . (JI
The material of the shutter 3 is desirably selected from the same type of material as the cap member 2 on the premise of the above contents.

【0073】さらに、前記手法により高いシール性を維
持したまま、シャッター3の開閉強度を低下させて操作
性を向上させるために、シャッター3の部材のシール部
材4貼着面と反対側の面3dに低摩擦抵抗材料を配置さ
せることが望ましい。特に、大容量の現像剤補給容器等
の現像剤補給口の口径が大きい場合には、シャッター
3、キャップ部材2共に大きく、シャッター3の開閉時
の摺動面積も大きくなることから、シャッター開閉強度
低下の有効な手段である。
Further, in order to reduce the opening / closing strength of the shutter 3 and improve the operability while maintaining the high sealing performance by the above-mentioned method, the surface 3d of the member of the shutter 3 on the side opposite to the surface on which the sealing member 4 is adhered. It is desirable to dispose a low friction resistance material on the surface. In particular, when the diameter of the developer supply port of a large-capacity developer supply container or the like is large, both the shutter 3 and the cap member 2 are large, and the sliding area when opening and closing the shutter 3 is large. It is an effective means of lowering.

【0074】シャッター面3dに配置する低抵抗材料と
しては、シリコンオイル及びシリコン樹脂、フッ素樹
脂、パラフィン系ワックス類、超高分子ポリエチレン等
を選択できる。
As the low-resistance material disposed on the shutter surface 3d, silicone oil and silicone resin, fluororesin, paraffin waxes, ultra-high-molecular polyethylene and the like can be selected.

【0075】シャッター面3dに低摩擦抵抗材料として
シリコンオイルを塗布する場合、粘度と塗布量を制御す
る必要がある。粘度は低すぎると前記シール部材4とキ
ャップ部材2との摺動面において、シャッター開閉時に
シャッター3が脈動して操作性が悪化してしまう。逆に
粘度が高すぎると、シャッター3への塗布がしづらくな
る。したがって、100〜10000cSt粘度のもの
を用いることが可能であるが本実施例によれば粘度は1
000〜5000cStのものを用いることがより好ま
しい。
When applying silicone oil as a low friction resistance material to the shutter surface 3d, it is necessary to control the viscosity and the amount of application. If the viscosity is too low, the shutter 3 pulsates on the sliding surface between the seal member 4 and the cap member 2 when the shutter is opened and closed, resulting in poor operability. Conversely, if the viscosity is too high, it becomes difficult to apply the composition to the shutter 3. Therefore, it is possible to use one having a viscosity of 100 to 10000 cSt, but according to the present embodiment, the viscosity is 1
It is more preferable to use one of 000 to 5,000 cSt.

【0076】また、シリコンオイルのシャッター面3d
への塗布量についても、少なすぎると十分なオイル膜が
形成されず、シャッター開閉強度の上昇を引き起こして
しまう。逆に、多すぎると塗布面のベタつきやゴミ、現
像剤6の付着が生じてしまう。したがって、本実施例に
よれば塗布量は、0.01mg〜0.5mgがシャッタ
ー開閉強度が小さく、塗布面のベタつきやゴミ、現像剤
の付着が生じないが、0.05〜0.1mg/cm2
あることがより望ましい。
The shutter surface 3d of silicone oil
If the amount of coating is too small, a sufficient oil film will not be formed, causing an increase in shutter opening / closing strength. Conversely, if the amount is too large, the applied surface becomes sticky, dusty, and the developer 6 adheres. Therefore, according to the present embodiment, the application amount is 0.01 mg to 0.5 mg, the shutter opening / closing strength is small, and there is no sticking of the application surface, no dust, and no adhesion of the developer. cm 2 is more desirable.

【0077】本実施例では、容器本体1に現像剤6を
1.5kg充填し、キャップ部材2に設けた現像剤補給
用の開口2aを直径62mmに限定した。このためシャ
ッター3の材質には、ガラス繊維強化ポリプロピレンを
用いた。この材料の曲げ弾性率は約52000kg/c
2 である。
In this embodiment, the container body 1 is filled with 1.5 kg of the developer 6, and the opening 2a for supplying the developer provided in the cap member 2 is limited to a diameter of 62 mm. For this reason, glass fiber reinforced polypropylene was used as the material of the shutter 3. The flexural modulus of this material is about 52000 kg / c
m 2 .

【0078】可撓性フィルム5に、シリコンオイルを塗
布したフィルムを貼着したシール部材4は実施例1と同
じ材質を用い、シャッター3に貼着した。これを約23
%圧縮した状態でキャップ部材2に組み込んだ。この
時、シール部材4の圧縮応力は約0.7kg/cm2
あった。
The sealing member 4 in which a film coated with silicone oil was adhered to the flexible film 5 was adhered to the shutter 3 using the same material as in Example 1. About 23
It was incorporated into the cap member 2 in a state of being compressed by%. At this time, the compressive stress of the seal member 4 was about 0.7 kg / cm 2 .

【0079】さらに、本実施例ではシャッター3のシー
ル部材貼着面3aと反対側の面3dにシリコンオイルを
塗布した。このシリコンオイルの粘度は3000cSt
であり、塗布量は約0.1mg/cm2 に設定した。
Further, in this embodiment, silicone oil is applied to the surface 3d of the shutter 3 opposite to the surface 3a to which the seal member is attached. The viscosity of this silicone oil is 3000 cSt
And the coating amount was set to about 0.1 mg / cm 2 .

【0080】前記現像剤補給容器Cの構成において、実
際に100個の容器を作り、現像剤補給テストを行った
結果、シャッター開封強度は約2〜4kgf程度であ
り、容器本体1内の現像剤6はほとんど残らず本体現像
ホッパー7に補給することができた。通常、図4に示す
ように、容器本体1を上にしキャップ部材2を下にして
現像ホッパー7に現像剤補給容器Cを装着し操作者はシ
ャッター3の開閉を行うにあたって、シャッター3の把
手3cを掴んで開閉を行う。そのため図2に示す状態で
いうと上側に下向きに力がかかりやすく、シャッター3
の上面、つまりシール部材貼着面3a及びその反対側の
面3dと、キャップ部材2との摺動抵抗が大きくなる傾
向があるが、本実施例によれば、シリコンオイルコーテ
ィングフィルムとシリコンオイル塗布との相乗効果によ
り、シャッター開閉強度の上昇を防止することができ
た。
In the configuration of the developer supply container C, 100 containers were actually made and a developer supply test was performed. As a result, the shutter opening strength was about 2 to 4 kgf. 6 could be replenished to the developing hopper 7 with almost no residue. Normally, as shown in FIG. 4, the developer supply container C is mounted on the developing hopper 7 with the container main body 1 facing upward and the cap member 2 facing downward. To open and close. For this reason, in the state shown in FIG.
Although the sliding resistance between the upper surface of the cap member 2, that is, the sealing member attaching surface 3a and the surface 3d on the opposite side and the cap member 2 tends to increase, according to this embodiment, the silicone oil coating film and the silicone oil coating With the synergistic effect of the above, it was possible to prevent an increase in shutter opening / closing strength.

【0081】さらに、本実施例についても、実施例1と
同様、環境物流テスト、画出しテスト等を行ったが、特
に異常は発生しなかった。
Further, in this embodiment, as in the case of the first embodiment, an environmental distribution test, an image-drawing test, and the like were performed, but no particular abnormality occurred.

【0082】上記において、シャッター3の可撓性フィ
ルム5の配置されたシール部材4の取り付け面の反対側
の面にシリコンコーティングフィルムを貼着することに
より、一層良好な結果を得ることができる。
In the above, even better results can be obtained by sticking a silicon coating film on the surface of the shutter 3 opposite to the mounting surface of the seal member 4 on which the flexible film 5 is disposed.

【0083】前述実施例によれば、シール部材4をシャ
ッター3の部材に取り付け、シャッターガイド部2cと
シャッター3との間隙を一様に塞ぐようにしたので、ト
ナー補給口を最大限にとることができ、補給性能及び充
填性能を同時に向上させることが出来る。また、シャッ
ター3、キャップ部材2のコンパクト化を図ることがで
きるため、最終的に現像剤補給容器Cのコンパクト化も
図ることができる。さらに、シャッターカイド部2cの
中にシール部材4を配置するため、シール性を安定して
維持することができる。また、シール部材4の形状が単
純になるため、シール部材4の貼り付け、組み立て性が
向上する。
According to the above-described embodiment, the seal member 4 is attached to the shutter 3 to uniformly close the gap between the shutter guide 2c and the shutter 3, so that the toner supply port is maximized. And the replenishment performance and the filling performance can be simultaneously improved. Further, since the shutter 3 and the cap member 2 can be downsized, the developer supply container C can be finally downsized. Further, since the seal member 4 is disposed in the shutter guide portion 2c, the sealing performance can be stably maintained. Further, since the shape of the seal member 4 is simplified, the sticking of the seal member 4 and the ease of assembly are improved.

【0084】又、本発明にかかわるシール部材の硬度は
日本工業規格(K6401)ウレタンフォーム硬さ試験
によるスプリング式A硬度である。
The hardness of the seal member according to the present invention is a spring type A hardness according to a Japanese Industrial Standard (K6401) urethane foam hardness test.

【0085】[0085]

【発明の効果】本出願に係る第1の発明によれば、シャ
ッターの現像剤が収納される側の表面であって、開口部
に対応する領域とガイド部に対応する領域にまたがって
設けられ、シャッターとガイド部との間で圧縮される弾
性シール部材を有することにより、開口部に対応する領
域とガイド部に対応する領域との境界でのシャッターと
容器の密封性を保つことができる。さらに、本発明によ
れば弾性シール部材表面に設けられたガイド部と摺動す
る可撓性フィルムを備え、この可撓性フィルムはその表
面にシリコン系材料のコーティング層を備えることによ
りガイド部と可撓性フィルムのコーティング層との摺動
性を向上させて、シャッターを開閉する力を低減するこ
とができる。
According to a first aspect of the present application, according to the present invention, Sha
On the side where the developer of the
Over the area corresponding to the
A bullet that is provided and compressed between the shutter and the guide
By having a conductive seal member, the area corresponding to the opening
Shutter at the boundary between the area and the area corresponding to the guide
The hermeticity of the container can be maintained. Further, according to the present invention,
Slides with the guide provided on the surface of the elastic seal member.
Flexible film, and the flexible film has a surface
By providing a silicon-based coating layer on the surface
Between the guide part and the coating layer of the flexible film
To reduce the force to open and close the shutter.
Can be.

【0086】本出願に係る第2の発明によれば第1の発
明において、前記ガイド部は、前記シャッター、前記弾
性シール部材及び前記可撓性フィルムを挟む、一体成形
された凹部を備えることにより、制限された範囲の中
で、現像剤補給口を最大限に大きくすることができるた
め、補給性能と同時に現像剤を容器内へ充填する際の充
填機能の向上が図れる。
According to a second aspect of the present invention, in the first aspect, the guide portion is formed integrally with the shutter, the elastic seal member, and the flexible film.
By providing the recessed portion, the developer replenishing port can be maximized within a limited range, so that the replenishing performance and the filling function when the developer is filled into the container can be improved at the same time. I can do it.

【0087】本出願に係る第3の発明によれば、第1又
は第2の発明において、前記弾性シール部材は発泡体で
あることにより、可撓性フィルムに対する加圧力を小さ
くしても密封性の均一化を計ることができシャッターを
開閉する力を低減できる。
According to the third aspect of the present application , the first or the second aspect
In the second invention, the elastic sealing member is a foam.
In some cases, the pressing force on the flexible film can be reduced.
Even if it does, the uniformity of sealing can be measured and the shutter
The opening and closing force can be reduced.

【0088】本出願に係る第4の発明によれば、第1又
は第2もしくは第3の発明において、可撓性フィルムの
基材の厚さは4μm〜100μmであることにより、シ
ール部材の弾性力が失われることが小さく、シール部材
への貼着等を含めた加工が可能である。
According to the fourth aspect of the present application , the first or the second aspect
Is the flexible film of the second or third invention.
When the thickness of the substrate is 4 μm to 100 μm,
The loss of elastic force of the sealing member is small,
It is possible to perform processing including sticking to the surface.

【0089】本出願に係る第5の発明によれば、第1か
ら第4の何れか1つの発明において、可撓性フィルムの
コーティング層の厚さは0.05μm〜2μmであるこ
とにより、安定したコーティング層が得られると共に摺
動によるコーティング層の剥離のおそれが小さい。
[0089] According to the fifth aspect of the present application, or the first
In any one of the fourth to fourth inventions, the flexible film
The thickness of the coating layer should be 0.05 μm to 2 μm.
As a result, a stable coating layer can be obtained and
The risk of peeling of the coating layer due to movement is small.

【0090】本出願に係る第6の発明によれば、第1か
ら第5の何れか1つの発明において、弾性シール部材は
前記シャッターと2色成型したものであることにより、
シール部材がシャッターに強固に固定される。
According to the sixth invention of the present application , the first invention
In any one of the fifth to fifth inventions, the elastic seal member is
By being molded with the shutter and two colors,
The seal member is firmly fixed to the shutter.

【0091】本出願に係る第7の発明によれば、第1か
ら第6の何れか1つの発明において、シール部材は硬度
20〜70°、圧縮永久歪み4%以下、セルサイズ60
〜300μm、比重が0.2〜0.5である低発泡ポリ
ウレタンであって、該シール部材を5〜50%圧縮して
用いることによりシール性能及びシャッター開閉力の点
で好ましい結果が得られる。
According to the seventh invention of the present application , the first invention
In any one of the sixth to sixth aspects of the present invention, the seal member has hardness.
20-70 °, compression set 4% or less, cell size 60
Low foamed poly having a specific gravity of 0.2 to 0.5
Urethane, the seal member is compressed by 5 to 50%
Seal performance and shutter opening / closing force
And a preferable result is obtained.

【0092】本出願に係る第8の発明によれば、第7の
発明において、シール部材の圧縮応力が0.1kg/c
2 〜2.0kg/cm 2 であることにより、シール
性能を良好とし、シャッター開閉力を軽くすることを両
立できる。
According to the eighth invention of the present application , the seventh invention
In the invention, the compressive stress of the seal member is 0.1 kg / c.
m 2 to 2.0 kg / cm 2 , seal
To improve performance and reduce the shutter opening / closing force
Can stand.

【0093】本出願に係る第9の発明によれば第1から
第8の何れか1つの発明において、シャッターの部材の
曲げ弾性率が20000kg/cm 2 〜100000
kg/cm 2 であることにより、シャッターが変形せ
ず物流時に衝撃によりクラックが入ったり割れたりしな
い。
According to the ninth invention of the present application, the first
In any one of the eighth inventions, the shutter member
Flexural modulus 20000kg / cm 2 ~100000
kg / cm 2 causes the shutter to deform.
Cracks and breaks due to impact during distribution
No.

【0094】本出願に係る第10の発明によれば、第1
から第9の何れか1つの発明において、シャッターの前
記弾性部材が設けられた面とは反対側の面に、低摩擦抵
抗材料が塗布されることにより、シャッター開閉力を更
に一層小さくする効果がある。
According to the tenth invention of the present application , the first invention
To the ninth aspect, before the shutter.
A low friction resistance is provided on the surface opposite to the surface on which the elastic member is provided.
The application of a resistance material improves the shutter opening and closing force.
Has the effect of making it even smaller.

【0095】本出願に係る第11の発明によれば、第1
0の発明において、前記低摩擦抵抗材料はシリコンオイ
ルであることにより、好適な結果を得る。
According to the eleventh invention of the present application , the first invention
0 invention, the low friction resistance material is silicon oil
, A good result is obtained.

【0096】本出願に係る第12の発明によれば、第1
1の発明において、前記シリコンオイルの粘度が100
cSt〜10000cStであるものでもって施工容易
で好適な結果を得る。
According to the twelfth invention of the present application , the first invention
In one aspect, the silicone oil has a viscosity of 100
Easy construction with cSt to 10000 cSt
With good results.

【0097】本出願に係る第13の発明によれば、第1
1又は第12の発明において、シリコンオイルの塗布量
が0.01mg/cm 2 〜0.5mg/cm 2 である
ことにより、シャッターとシャッター支持手段間の摺動
面にオイル膜が一様に出来、且つオイル塗布面へのベタ
つきや、ゴミ或は現像剤のベタつきが生じない。
According to the thirteenth invention of the present application , the first invention
In the first or twelfth aspect, the amount of silicone oil applied
It is but 0.01mg / cm 2 ~0.5mg / cm 2
The sliding between the shutter and the shutter support means
Oil film can be formed uniformly on the surface and solid on oil applied surface
No sticking or sticking of dust or developer occurs.

【0098】[0098]

【0099】[0099]

【0100】[0100]

【0101】[0101]

【0102】[0102]

【0103】[0103]

【0104】[0104]

【0105】[0105]

【0106】[0106]

【0107】[0107]

【0108】[0108]

【0109】[0109]

【0110】[0110]

【0111】[0111]

【0112】[0112]

【0113】[0113]

【0114】[0114]

【0115】[0115]

【0116】[0116]

【0117】[0117]

【図面の簡単な説明】[Brief description of the drawings]

【図1】本発明の実施例を適用した現像剤補給容器の側
断面図である。
FIG. 1 is a side sectional view of a developer supply container to which an embodiment of the present invention is applied.

【図2】図1に示した現像剤補給容器の外観斜視図であ
る。
FIG. 2 is an external perspective view of the developer supply container shown in FIG.

【図3】図1に示した現像剤補給容器の拡大断面図であ
る。
FIG. 3 is an enlarged sectional view of the developer supply container shown in FIG.

【図4】図1に示した現像剤補給容器による画像形成装
置本体に対する現像剤の補給状態を示す側断面図であ
る。
FIG. 4 is a side sectional view showing a state in which the developer is supplied to the image forming apparatus main body by the developer supply container shown in FIG. 1;

【図5】比較例として示す現像剤補給容器の側断面図で
ある。
FIG. 5 is a side sectional view of a developer supply container shown as a comparative example.

【符号の説明】[Explanation of symbols]

1 容器本体 2 キャップ部材 3 シャッター 4 シール部材 5 可撓性フィルム 6 現像剤 7 現像ホッパー 2c シャッターガイド部 DESCRIPTION OF SYMBOLS 1 Container main body 2 Cap member 3 Shutter 4 Seal member 5 Flexible film 6 Developer 7 Development hopper 2c Shutter guide part

───────────────────────────────────────────────────── フロントページの続き (56)参考文献 特開 平3−293382(JP,A) 特開 昭59−201838(JP,A) 実開 昭61−19258(JP,U) 実開 平2−140074(JP,U) ──────────────────────────────────────────────────続 き Continuation of the front page (56) References JP-A-3-293382 (JP, A) JP-A-59-201838 (JP, A) JP-A-61-19258 (JP, U) JP-A-2-293 140074 (JP, U)

Claims (13)

(57)【特許請求の範囲】(57) [Claims] 【請求項1】 画像形成装置の本体に現像剤を補給する
現像剤補給容器であって、現像剤を補給する開口部を備
え、現像剤を収納する容器本体と、前記開口部を閉鎖す
るシャッターと、前記シャッターを、前記開口部を閉鎖
する閉鎖位置と、前記開口部を開放する開放位置と、に
移動可能にガイドするガイド部であって、前記シャッタ
ーの移動方向と直角方向において前記シャッターの端部
に設けられ、前記移動方向に沿って延びて設けられたガ
イド部と、を有する現像剤補給容器において、 前記シャッターの現像剤が収納される側の表面であっ
て、前記開口部に対応する領域と前記ガイド部に対応す
る領域にまたがって設けられ、前記シャッターと前記ガ
イド部との間で圧縮される弾性シール部材と、前記弾性
シール部材表面に設けられ前記ガイド部と摺動する可撓
性フィルムと、を有し、この可撓性フィルムはその表面
にシリコン系材料のコーティング層を備えることを特徴
とする現像剤補給容器。
1. A developer replenishing container for replenishing developer to a main body of an image forming apparatus, comprising: an opening for replenishing developer, a container main body for storing developer, and a shutter for closing the opening. And a guide portion movably guiding the shutter to a closed position for closing the opening portion, and an open position for opening the opening portion, wherein the guide portion of the shutter in a direction perpendicular to the moving direction of the shutter. A guide portion provided at an end portion and extending along the moving direction, wherein a surface of the shutter on the side where the developer is stored, corresponding to the opening portion An elastic seal member provided over an area corresponding to the guide portion and an area corresponding to the guide portion, and an elastic seal member compressed between the shutter and the guide portion; It has a flexible film guide portion and the sliding, and this flexible film developer supply container, characterized in that it comprises a coating layer of silicon material on the surface thereof.
【請求項2】 前記ガイド部は、前記シャッター、前記
弾性シール部材及び前記可撓性フィルムを挟む、一体成
形された凹部を備えることを特徴とする請求項1の現像
剤補給容器。
2. The integrated guide, wherein the guide section sandwiches the shutter, the elastic seal member and the flexible film.
The developer supply container according to claim 1, further comprising a shaped concave portion.
【請求項3】 前記弾性シール部材は発泡体であること
を特徴とする請求項1又は2の現像剤補給容器。
3. The developer supply container according to claim 1, wherein said elastic seal member is a foam.
【請求項4】 前記可撓性フィルムの基材の厚さは4μ
m〜100μmであることを特徴とする請求項1乃至3
のいずれかの現像剤補給容器。
4. The thickness of the flexible film substrate is 4 μm.
4. The structure according to claim 1, wherein the thickness is in the range of m to 100 μm.
Any one of the developer supply containers.
【請求項5】 前記コーティング層の厚さは0.05μ
m〜2μmであることを特徴とする請求項1乃至4のい
ずれかの現像剤補給容器。
5. The coating layer has a thickness of 0.05 μm.
The developer supply container according to any one of claims 1 to 4, wherein the thickness of the developer supply container is from m to 2 m.
【請求項6】 前記弾性シール部材は前記シャッターと
2色成型したものであることを特徴とする請求項1乃至
5のいずれかの現像剤補給容器。
6. The developer supply container according to claim 1, wherein said elastic seal member is formed by two-color molding with said shutter.
【請求項7】 前記シール部材は硬度20〜70°、圧
縮永久歪み4%以下、セルサイズ60〜300μm、比
重が0.2〜0.5の発泡ポリウレタンであって、前記
シール部材を5〜50%圧縮して用いることを特徴とす
る請求項1乃至6のいずれかの現像剤補給容器。
7. The sealing member is a polyurethane foam having a hardness of 20 to 70 °, a compression set of 4% or less, a cell size of 60 to 300 μm, and a specific gravity of 0.2 to 0.5. 7. The developer supply container according to claim 1, wherein the developer supply container is used after being compressed by 50%.
【請求項8】 前記シール部材の圧縮応力が0.1kg
/cm2〜2.0kg/cm2であることを特徴とする請
求項7の現像剤補給容器。
8. The compressive stress of the seal member is 0.1 kg.
8. The developer supply container according to claim 7, wherein the amount of the developer supply container is from 2.0 kg / cm 2 to 2.0 kg / cm 2 .
【請求項9】 前記シャッターの曲げ弾性率が2000
0kg/cm2〜100000kg/cm2であることを
特徴とする請求項1乃至8のいずれかの現像剤補給容
器。
9. The bending elastic modulus of the shutter is 2000.
One of the developer supply container according to claim 1 to 8, characterized in that a 0kg / cm 2 ~100000kg / cm 2 .
【請求項10】 前記シャッターの前記弾性シール部材
が設けられた面とは反対側の面に、低摩擦抵抗材料が塗
布されていることを特徴とする請求項1乃至9のいずれ
かの現像剤補給容器。
10. The developer according to claim 1, wherein a low frictional resistance material is applied to a surface of the shutter opposite to a surface on which the elastic seal member is provided. Supply container.
【請求項11】 前記低摩擦抵抗材料はシリコンオイル
であることを特徴とする請求項10の現像剤補給容器。
11. The developer supply container according to claim 10, wherein said low friction resistance material is silicone oil.
【請求項12】 前記シリコンオイルの粘度は100c
St〜10000cStであることを特徴とする請求項
11の現像剤補給容器。
12. The silicone oil has a viscosity of 100 c.
The developer supply container according to claim 11, wherein St is 10000 cSt.
【請求項13】 前記シリコンオイルの塗布量は0.0
1mg/cm2〜0.5mg/cm2であることを特徴と
する請求項11又は12の現像剤補給容器。
13. The coating amount of the silicone oil is 0.0
Developer supply container according to claim 11 or 12, characterized in that a 1mg / cm 2 ~0.5mg / cm 2 .
JP6278466A 1994-10-18 1994-10-18 Developer supply container Expired - Fee Related JP3054323B2 (en)