JP2018087765A - Degradation diagnostic device for tile and degradation diagnostic method for tile - Google Patents

Degradation diagnostic device for tile and degradation diagnostic method for tile Download PDF

Info

Publication number
JP2018087765A
JP2018087765A JP2016231496A JP2016231496A JP2018087765A JP 2018087765 A JP2018087765 A JP 2018087765A JP 2016231496 A JP2016231496 A JP 2016231496A JP 2016231496 A JP2016231496 A JP 2016231496A JP 2018087765 A JP2018087765 A JP 2018087765A
Authority
JP
Japan
Prior art keywords
tile
hitting
floating
sound
tiles
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2016231496A
Other languages
Japanese (ja)
Other versions
JP6796827B2 (en
Inventor
名知 博司
Hiroshi Nachi
博司 名知
貴惠 船越
Kie Funakoshi
貴惠 船越
周男 ▲高▼橋
周男 ▲高▼橋
Kaneo Takahashi
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shimizu Construction Co Ltd
Shimizu Corp
Original Assignee
Shimizu Construction Co Ltd
Shimizu Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shimizu Construction Co Ltd, Shimizu Corp filed Critical Shimizu Construction Co Ltd
Priority to JP2016231496A priority Critical patent/JP6796827B2/en
Publication of JP2018087765A publication Critical patent/JP2018087765A/en
Application granted granted Critical
Publication of JP6796827B2 publication Critical patent/JP6796827B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

PROBLEM TO BE SOLVED: To provide a degradation diagnostic device for a tile and a degradation diagnostic method for the tile which enhance reliability of degradation diagnosis.SOLUTION: A degradation diagnostic device 100 for tiles diagnoses presence or absence of degradation of a plurality of tiles vertically and horizontally arranged and fixed onto a body surface through an inspection by rattling sound generated by hitting surfaces of the tiles. The degradation diagnostic device includes: floating determination means 14 for determining floating of the tiles indicating degradation of the tiles based on hitting sound; and control means 16 for controlling a hitting inspection for the tiles within the predetermined range. In a first hitting inspection for the predetermined range of the tiles, when the tiles determined to be in a floating state are found, the control means 16 controls the predetermined range of the tiles to be subjected to second time hitting inspection. The floating determination means 14 performs final floating determination of the tiles based on the hitting sound generated by first and second time hitting inspections.SELECTED DRAWING: Figure 1

Description

本発明は、タイルの劣化診断装置およびタイルの劣化診断方法に関するものである。   The present invention relates to a tile deterioration diagnosis apparatus and a tile deterioration diagnosis method.

従来、建物の外壁や床に貼設されたタイルでは、経年劣化等によって浮き、剥離、割れのような異常が生じることがある。特に外壁等のタイルでは浮き、剥離、割れによってタイル陶片が剥落すると大きな事故につながるおそれがあることから、これを未然に防止するための取り組みとして、タイルの劣化状況を診断(検査、調査)することが行なわれてきた。   Conventionally, in tiles pasted on the outer wall or floor of a building, abnormalities such as floating, peeling, and cracking may occur due to deterioration over time. In particular, tile tiles such as outer walls may cause a major accident if the tile ceramic pieces fall off due to floating, peeling, or cracking. As an effort to prevent this from happening, diagnose the deterioration of the tile (inspection and investigation). Has been done.

タイルの劣化診断方法としては、外観目視法、打音検査法、反発法、赤外線診断法等がある。このうち、打音検査法は、熟練した検査員がテストハンマーでタイル面を叩き、劣化部と健全部の微妙な音の違いを聞き分けることにより、外観では判別しにくいタイルの浮きや剥離の有無を比較的容易に判別できるため多用されている。   As a method for diagnosing the deterioration of tiles, there are a visual appearance method, a hammering inspection method, a rebound method, an infrared diagnostic method, and the like. Of these, in the sound inspection method, a skilled inspector hits the tile surface with a test hammer and distinguishes the subtle difference in sound between the deteriorated part and the sound part. Is often used because it can be distinguished relatively easily.

一方、打音検査法と同様、劣化部と健全部の微妙な音の違いによって劣化部分を特定するものとして、擦過法を用いた劣化診断方法が知られている(例えば、特許文献1を参照)。擦過法は、例えば、直径20mm程度の金属球を検査対象のタイル面に押し付け、タイル面を金属球で擦るように移動させ、その時に発生する音(擦過音)からタイルの浮きや剥離等の劣化部分の有無を判別し、劣化部分の位置を特定するものである。   On the other hand, a deterioration diagnosis method using a fretting method is known as a method for identifying a deteriorated part by a subtle difference in sound between a deteriorated part and a sound part, as in the sound hitting inspection method (see, for example, Patent Document 1). ). The rubbing method is, for example, pressing a metal ball having a diameter of about 20 mm against the tile surface to be inspected, moving the tile surface so as to be rubbed with the metal ball, and lifting or peeling the tile from the sound (friction sound) generated at that time. The presence or absence of a deteriorated portion is determined, and the position of the deteriorated portion is specified.

また、この擦過法は、金属球を検査対象面のタイル面に押し付けた状態を維持しつつ移動することによる擦過音を捉える手法であるため、打音検査法と比較し、ロボット等で自動化を図りやすい。すなわち、ロボット等を操作し、マイクロフォンで録音された擦過音を検査員がコンピュータ等で分析することで診断を行うことができるため、検査員の経験や資質といった個人差の影響が少なく、高精度で診断を行うことが可能になる。   In addition, this rubbing method is a method of capturing the rubbing sound caused by moving the metal ball while pressing the metal ball against the tile surface of the inspection target surface. Easy to plan. In other words, since the inspector can operate the robot, etc., and the inspector analyzes the fuzzing sound recorded by the microphone with a computer, etc., the diagnosis is less affected by individual differences such as the inspector's experience and qualities, and high accuracy Diagnosis can be performed with this.

この擦過法を用いたタイルの劣化診断装置として、本願出願人は、特許文献2に示すような装置を既に提案している。この装置は、擦過部材をタイル面に押し付けつつ移動させて発生する擦過音を擦過音記録手段で捉えてタイルの劣化の有無を診断する装置であって、擦過音記録手段で捉えた擦過音に基づいて、タイルの劣化を表す異常音を抽出する異常音抽出手段と、異常音抽出手段で抽出した異常音のうち、予め設定した所定の閾値以上の周波数成分の異常音を陶片浮きと判定し、所定の閾値未満の周波数成分の異常音を下地浮きと判定する浮きの種別判定手段を備えるものである。この装置によれば、擦過音に基づいてタイルの浮きの種別を容易に識別することができる。   As an apparatus for diagnosing tile deterioration using this rubbing method, the applicant of the present application has already proposed an apparatus as shown in Patent Document 2. This device is a device for diagnosing the presence or absence of deterioration of a tile by detecting the rubbing sound generated by moving the rubbing member against the tile surface with the rubbing sound recording means. Based on the abnormal sound extracting means for extracting the abnormal sound representing the deterioration of the tile and the abnormal sound extracted by the abnormal sound extracting means, the abnormal sound having a frequency component equal to or higher than a predetermined threshold value is determined to be floating And a float type determining means for determining that an abnormal sound having a frequency component less than a predetermined threshold is a base float. According to this apparatus, it is possible to easily identify the type of tile floating based on the rubbing sound.

一方、本願出願人は、この擦過音(機械打音法)によるタイルの浮きの自動判定システムを搭載した外壁診断システムを既に開発している。この外壁診断システムは、図6に示すように、建物本体2からケーブル3等で吊下げられた懸垂式の外壁移動装置1からなる。この外壁移動装置1は、昇降動作で外壁タイル面4を移動し、一回の動作で幅1.8m程度の範囲の診断が可能である。外壁移動装置1は、外壁タイル面4を平行往復でスライドしながら診断用ハンマーで擦過して、擦過音、映像、写真を操作用パソコンに転送し、診断状況を画面表示するとともに、記録を保存する。   On the other hand, the applicant of the present application has already developed an outer wall diagnostic system equipped with an automatic tile floating determination system based on this rubbing sound (mechanical sounding method). As shown in FIG. 6, the outer wall diagnosis system includes a suspended outer wall moving device 1 suspended from a building body 2 by a cable 3 or the like. This outer wall moving device 1 can move the outer wall tile surface 4 by a lifting operation and can perform diagnosis in a range of about 1.8 m in width by one operation. The outer wall moving device 1 slides the outer wall tile surface 4 in a parallel reciprocating motion and rubs it with a diagnostic hammer, transfers the rubbing sound, video, and photo to the operation PC, displays the diagnosis status on the screen, and saves the record. To do.

特開2015−28467号公報Japanese Patent Laid-Open No. 2015-28467 特願2015−181205号Japanese Patent Application No. 2015-181205

ところで、機械打音法の場合、打音ピッチに限界があるため、打音データは1枚のタイルに対して1〜2点しか得られない。特に、図7(1)、(2)に示される50角や50二丁のような幅100mm以下の小型タイルの場合には、タイル1枚に対して打音1点で浮きを判定することになる。同じ箇所を何回も叩くことが可能な熟練技術者による診断方法と比較すると、信頼性が劣ると言わざるを得ない。このため、劣化診断の信頼性を向上させることのできる技術が求められていた。   By the way, in the case of the mechanical sounding method, since the sounding pitch is limited, only 1 or 2 points of sounding data can be obtained for one tile. In particular, in the case of small tiles with a width of 100 mm or less, such as the 50 corners and 50 two-chome shown in FIGS. 7 (1) and (2), the floating is determined with one hitting sound per tile. become. It must be said that the reliability is inferior when compared with a diagnosis method by a skilled engineer who can strike the same part many times. For this reason, the technique which can improve the reliability of a deterioration diagnosis was calculated | required.

本発明は、上記に鑑みてなされたものであって、劣化診断の信頼性を向上させたタイルの劣化診断装置およびタイルの劣化診断方法を提供することを目的とする。   The present invention has been made in view of the above, and an object of the present invention is to provide a tile deterioration diagnosis apparatus and a tile deterioration diagnosis method in which reliability of deterioration diagnosis is improved.

上記した課題を解決し、目的を達成するために、本発明に係るタイルの劣化診断装置は、縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断装置であって、打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定手段と、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御手段とを備え、所定の範囲のタイルに対する1回目の打音検査において、タイルの浮きと判定されたタイルが有った場合には、制御手段は、その所定の範囲のタイルに対して2回目の打音検査を行うように制御し、浮き判定手段は、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定することを特徴とする。   In order to solve the above-described problems and achieve the object, the tile deterioration diagnosis apparatus according to the present invention is arranged in a plurality of vertical and horizontal directions, and the presence or absence of deterioration of the tiles fixed to the surface of the housing is checked against the tile surface. A tile deterioration diagnosis apparatus for diagnosing through a hitting test using generated hitting sound, a float determination means for determining a tile lift indicating tile deterioration based on a hitting sound, and a predetermined tile among a plurality of tiles arranged Control means for controlling the sound inspection for the tiles in the range, and in the first sound inspection for the tiles in the predetermined range, if there is a tile that is determined to be a floating tile, the control means includes: Control is performed so that the second hammering test is performed on the tiles in the predetermined range, and the float determination means determines whether the tile floats based on the hammering sounds generated in the first and second hammering tests. To judge And butterflies.

また、本発明に係る他のタイルの劣化診断装置は、縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断装置であって、打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定手段と、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御手段とを備え、制御手段は、所定の範囲のタイルに対して2回の打音検査を行うように制御し、浮き判定手段は、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定することを特徴とする。   In addition, another tile deterioration diagnosis apparatus according to the present invention diagnoses the presence or absence of deterioration of tiles arranged in a plurality of rows and columns and fixed to the surface of the casing through a sound-inspection test using a sound generated by hitting the surface of the tile. A tile deterioration diagnosis apparatus for controlling a floating determination unit that determines a floating of a tile that represents deterioration of a tile based on a hitting sound, and a hammering test for a tile in a predetermined range among a plurality of tiles arranged. Control means, and the control means performs control so that the sound hitting test is performed twice for tiles in a predetermined range, and the float determination means is a sound hitting sound generated in the first and second sound hitting inspections. Based on the above, it is characterized in that the main determination is made on the floating of the tile.

また、本発明に係る他のタイルの劣化診断装置は、上述した発明において、浮き判定手段は、1回目の打音検査において浮きと判定されたタイルが、2回目の打音検査においても浮きと判定された場合に、タイルの浮きとして本判定することを特徴とする。   Further, in the tile deterioration diagnosis apparatus according to the present invention, in the above-described invention, the float determination means determines that a tile that has been determined to float in the first hammering test is floated in the second hammering test. If it is determined, the determination is made as a floating tile.

また、本発明に係るタイルの劣化診断方法は、縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断方法であって、打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定ステップと、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御ステップとを備え、所定の範囲のタイルに対する1回目の打音検査において、タイルの浮きと判定されたタイルが有った場合には、制御ステップは、その所定の範囲のタイルに対して2回目の打音検査を行うように制御し、浮き判定ステップは、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定することを特徴とする。   In addition, the tile deterioration diagnosis method according to the present invention is a tile that diagnoses the presence / absence of deterioration of tiles arranged in a vertical and horizontal direction and fixed on the surface of a cabinet through a sound-inspection test using a sound generated by hitting the surface of the tile. A method for diagnosing deterioration of a tile, wherein a float determination step for determining the float of the tile representing the deterioration of the tile based on the hitting sound, and a control step for controlling the hitting test for a tile in a predetermined range among a plurality of tiles arranged And when there is a tile that is determined to be a floating tile in the first sound-inspection test for tiles in the predetermined range, the control step performs the second step on the tiles in the predetermined range. Control is performed so as to perform a hammering test, and the floating determination step is characterized in that the floating of the tile is finally determined based on the hammering sound generated in the first and second hammering tests.

また、本発明に係る他のタイルの劣化診断方法は、縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断方法であって、打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定ステップと、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御ステップとを備え、制御ステップは、所定の範囲のタイルに対して2回の打音検査を行うように制御し、浮き判定ステップは、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定することを特徴とする。   In addition, another tile deterioration diagnosis method according to the present invention diagnoses the presence or absence of deterioration of tiles arranged in a plurality of lengths and widths and fixed to the surface of a cabinet through a hitting test using a hitting sound generated by hitting the surface of the tile. A method for diagnosing tile deterioration, which controls a float determination step for determining a float of a tile that represents the deterioration of the tile based on the hitting sound, and a hammering test for a tile in a predetermined range among a plurality of tiles arranged A control step, wherein the control step performs control so that the tapping inspection is performed twice for tiles in a predetermined range, and the float determination step is performed by the first and second percussion inspections. Based on the above, it is characterized in that the main determination is made on the floating of the tile.

また、本発明に係る他のタイルの劣化診断方法は、上述した発明において、浮き判定ステップは、1回目の打音検査において浮きと判定されたタイルが、2回目の打音検査においても浮きと判定された場合に、タイルの浮きとして本判定することを特徴とする。   Further, in the tile deterioration diagnosis method according to the present invention, in the above-described invention, the floating determination step is performed such that a tile determined to be floating in the first hammering test is floated in the second hammering test. If it is determined, the determination is made as a floating tile.

本発明に係るタイルの劣化診断装置によれば、縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断装置であって、打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定手段と、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御手段とを備え、所定の範囲のタイルに対する1回目の打音検査において、タイルの浮きと判定されたタイルが有った場合には、制御手段は、その所定の範囲のタイルに対して2回目の打音検査を行うように制御し、浮き判定手段は、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定するので、浮きが疑われるタイルに対して2回目の打音検査を行うことによって浮き判定の精度を高めることができる。これにより、劣化診断の信頼性を向上させることができるという効果を奏する。   According to the tile deterioration diagnosis apparatus according to the present invention, a plurality of tiles that are vertically and horizontally arranged and diagnose the presence / absence of deterioration of the tiles fixed to the surface of the housing through a sound-inspection test using a sound generated by hitting the surface of the tile. And a control unit for controlling a hammering test for tiles in a predetermined range among a plurality of tiles arranged in the tile. When there is a tile that is determined to be a floating tile in the first sound-inspection test for the tile in the predetermined range, the control means performs the second time on the tile in the predetermined range. Control is performed so as to perform the hammering inspection, and the floating determination means makes a final determination of the floating of the tile based on the hammering sound generated in the first and second hammering inspections. Second strike It is possible to improve the accuracy of the float determined by performing a test. Thereby, there exists an effect that the reliability of deterioration diagnosis can be improved.

また、本発明に係る他のタイルの劣化診断装置によれば、縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断装置であって、打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定手段と、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御手段とを備え、制御手段は、所定の範囲のタイルに対して2回の打音検査を行うように制御し、浮き判定手段は、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定するので、2回の打音検査を行うことによって浮き判定の精度を高めることができる。これにより、劣化診断の信頼性を向上させることができるという効果を奏する。   In addition, according to another tile deterioration diagnosis apparatus according to the present invention, a plurality of vertical and horizontal tiles, and whether or not the tiles fixed on the surface of the casing are deteriorated are checked for hitting sound by hitting sound generated by hitting the tile surface. A tile deterioration diagnosis apparatus for diagnosing through a float determination means for determining a tile lift indicating deterioration of a tile based on a hitting sound, and a hammering test for a tile in a predetermined range among a plurality of tiles arranged. A control means for controlling the control means so as to perform the second hammering test for a predetermined range of tiles, and the floating determination means is generated in the first and second hammering tests. Since the tile lifting is determined based on the hitting sound, the accuracy of the lifting determination can be increased by performing the hitting test twice. Thereby, there exists an effect that the reliability of deterioration diagnosis can be improved.

また、本発明に係る他のタイルの劣化診断装置によれば、浮き判定手段は、1回目の打音検査において浮きと判定されたタイルが、2回目の打音検査においても浮きと判定された場合に、タイルの浮きとして本判定するので、浮き判定の精度を高めることができるという効果を奏する。   Further, according to another tile deterioration diagnosis apparatus according to the present invention, the floating determination means determines that a tile determined to be floating in the first hammering test is floating in the second hammering test. In this case, since the main determination is made as the floating of the tile, there is an effect that the accuracy of the floating determination can be improved.

また、本発明に係るタイルの劣化診断方法によれば、縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断方法であって、打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定ステップと、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御ステップとを備え、所定の範囲のタイルに対する1回目の打音検査において、タイルの浮きと判定されたタイルが有った場合には、制御ステップは、その所定の範囲のタイルに対して2回目の打音検査を行うように制御し、浮き判定ステップは、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定するので、浮きが疑われるタイルに対して2回目の打音検査を行うことによって浮き判定の精度を高めることができる。これにより、劣化診断の信頼性を向上させることができるという効果を奏する。   Further, according to the tile deterioration diagnosis method according to the present invention, the presence or absence of deterioration of the tiles arranged in the vertical and horizontal directions and fixed to the surface of the casing is diagnosed through a sound-inspection test using a sound generated by hitting the surface of the tile. A method for diagnosing tile deterioration, which controls a float determination step for determining a float of a tile that represents the deterioration of the tile based on the hitting sound, and a hammering test for a tile in a predetermined range among a plurality of tiles arranged And when there is a tile determined to be a floating tile in the first sound-inspection test for the tile in the predetermined range, the control step is performed for the tile in the predetermined range. Control is performed to perform the second hammering test, and the float determination step makes a final determination of tile lifting based on the hammering sounds generated in the first and second hammering tests. It is possible to improve the accuracy of the float determined by carrying out a second tapping sound check on Le. Thereby, there exists an effect that the reliability of deterioration diagnosis can be improved.

また、本発明に係る他のタイルの劣化診断方法によれば、縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断方法であって、打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定ステップと、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御ステップとを備え、制御ステップは、所定の範囲のタイルに対して2回の打音検査を行うように制御し、浮き判定ステップは、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定するので、2回の打音検査を行うことによって浮き判定の精度を高めることができる。これにより、劣化診断の信頼性を向上させることができるという効果を奏する。   Further, according to another tile deterioration diagnosis method according to the present invention, a plurality of vertical and horizontal tiles that are fixed to the surface of the casing are checked for the presence or absence of deterioration of the tiles by hitting sound generated by hitting the tile surface. A tile deterioration diagnosis method for diagnosing through a float determination step for determining a tile lift that represents deterioration of a tile based on the hitting sound, and a hammering test for tiles in a predetermined range among a plurality of tiles arranged. A control step for controlling, and the control step is controlled so as to perform the second hammering test for a predetermined range of tiles, and the floating determination step occurs in the first and second hammering tests. Since the tile lifting is determined based on the hitting sound, the accuracy of the lifting determination can be increased by performing the hitting test twice. Thereby, there exists an effect that the reliability of deterioration diagnosis can be improved.

また、本発明に係る他のタイルの劣化診断方法によれば、浮き判定ステップは、1回目の打音検査において浮きと判定されたタイルが、2回目の打音検査においても浮きと判定された場合に、タイルの浮きとして本判定するので、浮き判定の精度を高めることができるという効果を奏する。   Further, according to another tile deterioration diagnosis method according to the present invention, in the floating determination step, the tile determined to be floating in the first hammering test is determined to be floating in the second hammering test. In this case, since the main determination is made as the floating of the tile, there is an effect that the accuracy of the floating determination can be improved.

図1は、本発明に係るタイルの劣化診断装置の実施の形態を示す概略構成図である。FIG. 1 is a schematic configuration diagram showing an embodiment of a tile deterioration diagnosis apparatus according to the present invention. 図2は、従来のタイルの浮きの判定の結果に基づいた機械打音方法の説明図である。FIG. 2 is an explanatory diagram of a conventional mechanical sounding method based on the result of determination of tile lifting. 図3は、本発明のタイルの浮きの判定の結果に基づいた機械打音方法の説明図である。FIG. 3 is an explanatory diagram of the mechanical sounding method based on the result of the determination of the floating of the tile according to the present invention. 図4は、往復2回によるタイルの浮きの判定原理を示す説明図である。FIG. 4 is an explanatory diagram illustrating the principle of determination of tile floating by two reciprocations. 図5は、タイルの浮きの判定原理を示す図であり、(1)は2回法、(2)は1回法である。FIGS. 5A and 5B are diagrams showing the determination principle of tile floating, where (1) is a two-time method and (2) is a one-time method. 図6は、従来の外壁診断システムの一例を示す概略斜視図である。FIG. 6 is a schematic perspective view showing an example of a conventional outer wall diagnostic system. 図7は、従来のタイルと診断箇所の一例を示す図であり、(1)は50角、(2)は50二丁、(3)は二丁掛けの場合である。FIG. 7 is a diagram showing an example of a conventional tile and a diagnostic part, where (1) is 50 corners, (2) is 50 doubles, and (3) is double hooks.

本発明に係るタイルの劣化診断装置およびタイルの劣化診断方法は、熟練診断者のやり方を真似た機械打音法によりタイルの浮きを判定するものである。以下に、本発明の実施の形態について、図6に示すような外壁診断システムの外壁移動装置に適用する場合を例にとり、図面に基づいて詳細に説明する。なお、この実施の形態によりこの発明が限定されるものではない。   The tile deterioration diagnosis apparatus and the tile deterioration diagnosis method according to the present invention determine whether a tile is lifted by a mechanical sounding method imitating a method of an expert diagnostician. Hereinafter, embodiments of the present invention will be described in detail with reference to the drawings, taking as an example a case where the present invention is applied to an outer wall moving apparatus of an outer wall diagnosis system as shown in FIG. Note that the present invention is not limited to the embodiments.

(タイルの劣化診断装置)
まず、本発明に係るタイルの劣化診断装置の実施の形態について説明する。
(Tile degradation diagnosis device)
First, an embodiment of a tile deterioration diagnosis apparatus according to the present invention will be described.

図1に示すように、本発明に係るタイルの劣化診断装置100は、診断用ハンマー10(叩き手段)と、打音記録手段12と、浮き判定手段14と、制御手段16とを備えている。このタイルの劣化診断装置100は、建物の外壁面において縦横に複数並べて固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するものである。   As shown in FIG. 1, a tile deterioration diagnosis apparatus 100 according to the present invention includes a diagnostic hammer 10 (striking means), a sound recording means 12, a float determination means 14, and a control means 16. . The tile deterioration diagnosis apparatus 100 diagnoses the presence or absence of deterioration of a plurality of tiles fixed side by side in the vertical and horizontal directions on the outer wall surface of a building through a hammering test using a hammering sound generated by hitting the surface of the tile.

このタイルの劣化診断装置100は、図6に示すような外壁診断システムの外壁移動装置1に搭載される。図6に示すように、外壁診断システムは、建物本体2からケーブル3等で吊下げられた懸垂式の外壁移動装置1からなる。なお、上述したように、外壁移動装置1は、昇降動作で外壁タイル面4を移動し、一回の動作で所定範囲(例えば幅1.8m程度)の範囲の診断が可能である。外壁移動装置1は、外壁タイル面4を平行往復でスライドしながら上記の診断用ハンマー10で擦過して、擦過音(打音)、映像、写真を操作用パソコンに転送し、診断状況を画面表示するとともに、記録を保存する。   The tile deterioration diagnosis apparatus 100 is mounted on the outer wall moving apparatus 1 of the outer wall diagnosis system as shown in FIG. As shown in FIG. 6, the outer wall diagnosis system includes a suspended outer wall moving device 1 suspended from a building body 2 by a cable 3 or the like. Note that, as described above, the outer wall moving device 1 can move the outer wall tile surface 4 by the lifting and lowering operation, and can diagnose a predetermined range (for example, a width of about 1.8 m) by one operation. The outer wall moving device 1 is rubbed with the diagnostic hammer 10 while sliding the outer wall tile surface 4 in parallel reciprocation, and transfers the rubbing sound (sounding sound), video, and photo to the operation PC, and displays the diagnosis status on the screen. Display and save records.

診断用ハンマー10は、外壁タイル面4を擦過することによって各タイルの表面を叩くためのものである。診断用ハンマー10でタイルを叩くことによって打音を発生させて打音検査を行う。診断用ハンマー10は、タイル面に当接する金属球を備えた従来の擦過棒などにより構成することができる。診断用ハンマー10には、必要に応じてモーター等からなる移動進退機構などを設けることができる。   The diagnostic hammer 10 is for hitting the surface of each tile by rubbing the outer wall tile surface 4. A hammering sound is generated by hitting a tile with the diagnostic hammer 10 to perform a hammering test. The diagnostic hammer 10 can be configured by a conventional rubbing rod having a metal ball that abuts against the tile surface. The diagnostic hammer 10 can be provided with a moving forward / backward mechanism composed of a motor or the like as required.

打音記録手段12は、診断用ハンマー10に内蔵またはその近傍に設けられ、図示しないエンコーダによって検出される位置データに対応した位置で発生する打音を捉えて記録するものである。診断用ハンマー10がタイルの並びに沿って所定方向(例えば横方向)に移動することで、打音が発生し、エンコーダによる診断用ハンマー10の位置データとともにこの位置データに対応した位置で発生した打音データが打音記録手段12に記録される。なお、後述するように、記録された打音データをフィルター処理することでタイルの浮きなどの劣化の有無が判定されることとなる。   The sound recording unit 12 is provided in or near the diagnostic hammer 10 and captures and records a sound generated at a position corresponding to position data detected by an encoder (not shown). When the diagnostic hammer 10 moves in a predetermined direction (for example, in the horizontal direction) along the tiles, a hitting sound is generated, and the hit data generated at the position corresponding to the position data together with the position data of the diagnostic hammer 10 by the encoder. Sound data is recorded in the sound recording means 12. Note that, as will be described later, the presence or absence of deterioration such as tile floating is determined by filtering the recorded hitting sound data.

浮き判定手段14は、打音記録手段12に記録された打音データに基づいて、タイルの劣化を表すタイルの浮きを判定するものであり、コンピューターなどを用いて構成される。なお、打音記録手段12に記録された打音データには、一般に、打音の他に、風音、モーターや振動等の機械音、自動車等の外部環境音も含まれている。そこで、この浮き判定手段14は、例えば風音、機械音、外部環境音などのノイズ音を減衰処理するとともに、タイルの打音を強調させる処理を行い、予め設定した所定の条件(例えば周波数特性の条件)を満たす音信号のものをタイルの浮きとして判定する。   The float determination means 14 is for determining tile lift indicating the deterioration of the tile based on the hitting sound data recorded in the hitting sound recording means 12, and is configured using a computer or the like. Note that the hitting data recorded in the hitting sound recording means 12 generally includes wind sounds, mechanical sounds such as motors and vibrations, and external environmental sounds such as automobiles in addition to the hitting sounds. Therefore, the floating determination means 14 performs a process of attenuating noise sounds such as wind sounds, mechanical sounds, and external environmental sounds, and performing a process of emphasizing the hitting sound of tiles, for example, to set predetermined conditions (for example, frequency characteristics). The sound signal satisfying the condition (1) is determined as a floating tile.

ここで、タイルの浮きには、陶片浮きと下地浮きがある。陶片浮きとは、モルタル等のタイルの下地からタイル陶片が浮いたり剥離した状態をいい、下地浮きとは、モルタル等のタイルの下地自体が外壁等から浮いたり剥離した状態をいう。本実施の形態では、陶片浮きと下地浮きのいずれかの音信号に該当した場合をタイルの浮きとして判定する。   Here, there are ceramic float and base float in the floating of the tile. The ceramic float is a state in which the tile ceramic pieces are floated or peeled off from the ground of the tile such as mortar, and the ground floating is a state in which the ground of the tile itself such as mortar is floated or peeled off from the outer wall or the like. In the present embodiment, the case where the sound signal corresponds to any one of the ceramic float and base float is determined as the tile lift.

制御手段16は、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御するためのものである。この制御手段16は、所定の範囲のタイルに対する1回目の打音検査において、浮き判定手段14によりタイルの浮きと判定されたタイルが有った場合には、その所定の範囲のタイルに対して2回目の打音検査を行うように制御する。この場合、浮き判定手段14は、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定する。本判定の方法としては、後述する図5(1)の2回法でもよいし、図5(2)の1回法でもよい。信頼性の高い2回法を採用する場合には、1回目の打音検査において浮きと判定されたタイルが、2回目の打音検査においても浮きと判定された場合に、タイルの浮きとして本判定することとなる。このように、浮きが疑われるタイルに対して2回目の打音検査を行うことによって浮き判定の精度を高めることができる。これにより、劣化診断の信頼性を向上させることができる。なお、上記の判定結果は、ディスプレイなどの可視化手段に表示してもよい。このようにすればタイルの浮きを容易に把握することが可能となる。   The control means 16 is for controlling the sound hit inspection for tiles in a predetermined range among the tiles arranged in a plurality. When there is a tile that is determined to be floating by the floating determination unit 14 in the first sound-inspection test for the tile in the predetermined range, the control unit 16 applies the tile to the tile in the predetermined range. Control is performed to perform the second hammering test. In this case, the floating determination means 14 makes a main determination on the tile floating based on the hitting sound generated in the first and second hitting inspections. The determination method may be the two-time method shown in FIG. 5 (1) or the one-time method shown in FIG. 5 (2). When the highly reliable two-time method is adopted, if a tile that is determined to be floating in the first hammering test is determined to be floating in the second hammering test, the tile is lifted as a tile. It will be judged. As described above, the accuracy of the floating determination can be improved by performing the second hitting test on the tile suspected of floating. Thereby, the reliability of deterioration diagnosis can be improved. In addition, you may display said determination result on visualization means, such as a display. In this way, it is possible to easily grasp the floating of the tile.

次に、上記構成の動作および作用について、50角のタイルが縦横に複数個ずつ並べられた外壁タイル面4の劣化診断を行う場合を例にとり説明する。   Next, the operation and action of the above configuration will be described by taking as an example the case of performing deterioration diagnosis of the outer wall tile surface 4 in which a plurality of 50-corner tiles are arranged vertically and horizontally.

タイルの劣化診断装置100を搭載した外壁移動装置1を図6に示すようにケーブル3等で支持し、診断対象面の外壁タイル面4に沿うように配置する。そして、診断用ハンマー10を横方向に往復移動させつつ、その並びの各タイルの表面を叩いて打音検査を行うように制御するものとする。さらに、横方向の往復移動によって上下に隣り合う2段の打音検査が済んだら、診断用ハンマー10を上段または下段にスライド移動させた後、同様の手順で打音検査を行うように制御するものとする。また、発生する打音を打音記録手段12で捉え、捉えた打音に基づいて、各タイルの浮きを浮き判定手段14で判定するものとする。   The outer wall moving device 1 on which the tile degradation diagnosis device 100 is mounted is supported by a cable 3 or the like as shown in FIG. 6 and arranged along the outer wall tile surface 4 of the diagnosis target surface. Then, the diagnostic hammer 10 is controlled to reciprocate in the horizontal direction so as to hit the surface of each tile in the array and perform a hammering test. Further, after the two-stage hitting test adjacent to the upper and lower sides is completed by the reciprocating movement in the horizontal direction, the diagnostic hammer 10 is slid to the upper stage or the lower stage, and then controlled so as to perform the hammering test in the same procedure. Shall. Further, it is assumed that the generated hitting sound is captured by the hitting sound recording unit 12 and the floating determination unit 14 determines the floating of each tile based on the captured hitting sound.

図2は従来のタイルの浮きの判定方法を、図3は本実施の形態のタイルの浮きの判定方法を示している。図中の複数配列した□はタイルを示し、タイルの中に表示された●印(黒丸印)は浮きと判定されなかった場合を、◎印(二重丸印)は浮きと判定された場合を示している。   FIG. 2 shows a conventional tile floating determination method, and FIG. 3 shows a tile floating determination method according to this embodiment. Multiple squares in the figure indicate tiles. The ● mark (black circle) displayed in the tile is not determined to be floating, and the ◎ mark (double circle) is determined to be floating. Is shown.

図2に示すように、従来の打音手順では、タイル一段ごとに、診断用ハンマー10が横方向に平行往復で上段または下段にスライドしながら打音検査するため、タイル1枚に対して常に打音1点での診断になる。なお、図2において往路は、上段のタイルを左から右に移動する方向、復路は、下段のタイルを右から左に移動する方向となる。   As shown in FIG. 2, in the conventional sounding procedure, the diagnostic hammer 10 performs a sounding test while sliding to the upper or lower stage in parallel reciprocation in the horizontal direction for each tile. Diagnosis is made with a single hit sound. In FIG. 2, the forward path is a direction in which the upper tile is moved from left to right, and the backward path is a direction in which the lower tile is moved from right to left.

これに対し、本実施の形態の打音手順では、図3(1)に示すように、往路でタイルの浮きの判定がなかった場合には、上記の従来と同じ打音手順をとる。一方、図3(2)に示すように、往路(1回目の打音検査)でいずれかのタイルに浮きの判定があった場合には、復路は浮きの判定があった同じ段を繰り返し打音検査する(2回目の打音検査)。図3(2)の例では、上段を往復して打音検査する。   On the other hand, in the sounding procedure of the present embodiment, as shown in FIG. 3 (1), the same sounding procedure as the above-described conventional method is used when there is no determination of the floating of the tile in the forward path. On the other hand, as shown in FIG. 3 (2), when there is a floating determination on any tile in the forward path (first hit sound inspection), the same path where the floating determination was made is repeated on the return path. Sound inspection (second percussion inspection). In the example of FIG. 3 (2), the sound is inspected by reciprocating the upper stage.

そして、図4に示すように、繰り返しの打音検査の結果、浮き判定手段14は、2回ともタイルの浮きと判定された場合をタイルの浮きとして本判定する。   Then, as shown in FIG. 4, as a result of the repeated hammering test, the floating determination unit 14 makes a main determination as a tile floating when it is determined that the tile has been lifted twice.

このように、本実施の形態によれば、タイル1枚に対して打音1回の結果に対して、浮きと判定された段のみを打音2回とすることで、従来の診断方法の2倍の信頼性が得られる。また、タイルの浮きがないと判定された箇所は、従来どおりタイル1枚に対して打音1回で判定されることになるため、診断時間の増加を必要最小限に抑えることが可能である。   As described above, according to the present embodiment, with respect to the result of one hitting sound per tile, only the step determined to be lifted is set to two hitting sounds, so that the conventional diagnostic method can be used. Double reliability is obtained. In addition, since it is determined with one hitting sound for one tile as in the conventional case that the tile is determined not to float, it is possible to suppress an increase in diagnosis time to the minimum necessary. .

なお、上記の実施の形態において、タイルの劣化診断装置100は、上記の構成に加えて、浮き判定手段14の処理結果などを可視化するディスプレイやプリンターなどの可視化手段を備えてもよい。この場合、可視化手段は、診断対象のタイルの並びと、タイルの浮きと判定された箇所をグラフィック処理、マッピング処理して可視化してもよい。例えば、浮き判定手段14による判定結果を、図3のように可視化してもよい。可視化された情報を見ることで、ユーザーはタイルの浮きと判定された箇所の位置を容易に把握することができ、将来のタイルの補修計画の立案に役立てることが可能となる。   In the above-described embodiment, the tile deterioration diagnosis apparatus 100 may include a visualization unit such as a display or a printer that visualizes the processing result of the floating determination unit 14 in addition to the above configuration. In this case, the visualization means may visualize the arrangement of tiles to be diagnosed and the portion determined to be a floating tile by graphic processing and mapping processing. For example, the determination result by the floating determination unit 14 may be visualized as shown in FIG. By viewing the visualized information, the user can easily grasp the position of the part determined to be the floating of the tile, which can be used for the planning of a future tile repair plan.

また、上記の実施の形態においては、1回目の打音検査でタイルの浮きと判定されたタイルが有ったときに、制御手段16が2回目の打音検査を行うように制御する場合を例にとり説明したが、本発明はこれに限るものではない。例えば、制御手段16は単に、所定の範囲のタイルに対して2回の打音検査を行うように制御してもよい。つまり同じ箇所を2回づつ打音検査してもよい。この場合、1回目の打音検査で浮きと判定されたタイルが無い場合でも2回目の打音検査を行うことになる。このため、その分だけ上記の実施の形態よりも打音検査数は増える。しかし、この方法でも、2回の打音検査を行えるので浮き判定の精度を高めることができ、劣化診断の信頼性を向上させることができる。   Further, in the above-described embodiment, when there is a tile that is determined to be a floating tile in the first hammering test, the control unit 16 performs control to perform the second hammering test. Although described by way of example, the present invention is not limited to this. For example, the control means 16 may simply perform control so as to perform two hitting tests on a predetermined range of tiles. That is, the same portion may be hit twice. In this case, the second hammering test is performed even when there is no tile determined to be floating in the first hammering test. For this reason, the number of sound hit inspections is increased as compared with the above-described embodiment. However, even with this method, since the hammering test can be performed twice, the accuracy of the floating determination can be increased, and the reliability of the deterioration diagnosis can be improved.

この同じ箇所を2回づつ打音検査する方法としては、例えば以下の(1)〜(4)の方法がある。   As a method for inspecting the same portion twice, for example, there are the following methods (1) to (4).

(1)上下から打音検査を行う方法
この方法は、横方向に往復移動する診断用ハンマー10を、建物の下階から上階に向けて移動させつつ打音検査を行った後、同じ箇所を上階から下階に向けて移動させつつ打音検査を行うものである。この方法によれば、全てのタイルで2回の打音検査が可能になる反面、打音検査に要する時間が2倍に増えることとなる。
(1) Method of performing hammering test from above and below This method is the same place after performing hammering test while moving the diagnostic hammer 10 reciprocating in the horizontal direction from the lower floor to the upper floor of the building. The sound is inspected while moving from the upper floor to the lower floor. According to this method, it is possible to perform the sounding inspection twice for all tiles, but the time required for the sounding inspection is doubled.

(2)吊り位置を半分ずらして打音検査を行う方法
この方法は、外壁移動装置1の吊り位置を横方向に半分だけずらして打音検査を行うことで、打音検査を行う範囲を横方向の半分だけ重複させる方法である。この方法によれば、全てのタイルで2回の打音検査が可能になる反面、打音検査に要する時間が2倍に増え、外壁移動装置1の盛替え回数も2倍に増えることとなる。
(2) Method of performing a hammering test by shifting the suspension position by half This method shifts the suspension position of the outer wall moving device 1 by a half in the horizontal direction to perform a hammering test, thereby laterally changing the range of the hammering test. This is a method of overlapping only half of the direction. According to this method, the tapping inspection can be performed twice for all the tiles, but the time required for the percussion inspection is doubled and the number of times the outer wall moving device 1 is replaced is doubled. .

(3)2玉式打音ハンマーを用いて打音検査を行う方法
この方法は、診断用ハンマー10である打音ハンマーを1玉から2玉に変更して打音検査を行う方法である。2本の打音ハンマーを横方向に並べてセットした場合には、横方向の一回の移動によって同じ並びのタイルを2回打音することになる。2本の打音ハンマーを縦方向に並べてセットした場合には、縦方向のタイルの並びに沿って打音ハンマーを縦方向に動かして1行2回打音で検査する方法(繰り返して打音検査する方法ではない)と、横方向のタイルの並びに沿って打音ハンマーを横方向に動かして上下2段のタイルの並びについて2行1回打音で検査する方法が選択可能である。いずれの方法でも、打音検査に要する時間は通常方法(上記の実施の形態)の場合と同じ1行1回打音となる。
(3) Method of performing a hammering test using a two-ball hammering hammer This method is a method of performing a hammering test by changing the hammering hammer that is the diagnostic hammer 10 from one ball to two balls. When two hammers are set side by side, the tiles in the same row are hit twice by one movement in the horizontal direction. When two hammers are set side by side in the vertical direction, the hammer is moved in the vertical direction along the vertical tiles and inspected with two taps per line. It is possible to select a method of inspecting the arrangement of the upper and lower two-tiered tiles with two hits once per row by moving the hitting hammer in the horizontal direction along the tiles in the horizontal direction. In any of the methods, the time required for the sound hit inspection is the same as that for the normal method (the above-described embodiment) once per line.

(4)1駆動2回路で打音検査を行う方法
この方法は、診断用ハンマー10である2つの打音ハンマーを、隣り合う上下のタイルの並びに沿う周回路に沿って移動させるものである。打音ハンマーは、例えば周回路の左右端の上段と下段とに設置するものとし、周回路の1回の駆動で、横方向を上下段で同時に打音検査する。この方法は、打音検査に要する時間は通常方法(上記の実施の形態)の場合と同じ1行1回打音となる。
(4) Method of performing hammering test with one drive and two circuits In this method, two hammering hammers that are diagnostic hammers 10 are moved along a peripheral circuit along the adjacent upper and lower tiles. The hammering hammer is installed, for example, at the upper and lower stages of the left and right ends of the circumferential circuit, and the hammering test is performed simultaneously on the upper and lower stages in the lateral direction by one driving of the circumferential circuit. In this method, the time required for the sound hit inspection is the same as that for the normal method (the above embodiment), once per line.

上記の同じ箇所を2回づつ打音検査する場合において、浮き判定手段14でタイルの浮きを判定する方法としては、2回法と1回法を選択可能である。2回法は、図5(1)に示すように、1回目と2回目の打音検査の少なくとも一方でタイルの浮きと判定されたものを、タイルの浮きとして本判定する方法である。1回法は、図5(2)に示すように、1回目と2回目の打音検査の両方でタイルの浮きと判定されたものを、タイルの浮きとして本判定する方法である。2回法の方が信頼性の高い判定方法である。信頼性を向上するためには、浮き判定手段14による判定方法として2回法を採用することが望ましい。   In the case where the sound hitting inspection is performed twice for the same portion, the method for determining tile lifting by the lifting determination means 14 can be selected from the two-time method and the one-time method. As shown in FIG. 5 (1), the two-time method is a method in which a tile that has been determined to be a floating tile is determined as a floating tile at least one of the first and second percussion inspections. As shown in FIG. 5 (2), the one-time method is a method in which a tile that has been determined to be a floating tile in both the first and second percussion inspections is determined as a floating tile. The two-time method is a more reliable determination method. In order to improve the reliability, it is desirable to adopt the twice method as the determination method by the floating determination means 14.

(タイルの劣化診断方法)
次に、本発明に係るタイルの劣化診断方法の実施の形態について説明する。
(Tile degradation diagnosis method)
Next, an embodiment of the tile deterioration diagnosis method according to the present invention will be described.

本実施の形態に係るタイルの劣化診断方法は、縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断する方法である。   The tile deterioration diagnosis method according to the present embodiment is a method of diagnosing the presence or absence of deterioration of tiles arranged in rows and columns and fixed to the surface of a frame through a sound-inspection test using a sound generated by hitting the surface of the tile. It is.

この方法は、打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定ステップと、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御ステップとを備えている。浮き判定ステップは上記の浮き判定手段14による処理に相当し、制御ステップは上記の制御手段16による処理に相当する。   This method includes a float determination step for determining the float of the tile representing the deterioration of the tile based on the hitting sound, and a control step for controlling the hitting test for the tiles in a predetermined range among the plurality of tiles arranged. Yes. The float determination step corresponds to the process by the float determination unit 14, and the control step corresponds to the process by the control unit 16.

診断用ハンマー10による打音検査の結果、図3(2)に示すように、往路(1回目)の打音検査において、浮きと判定されたタイルが有った場合には、制御ステップは、その並びのタイルに対して復路(2回目)の打音検査を行うように制御する。一方、浮き判定ステップは、往路と復路の打音検査で発生した打音に基づいて、タイルの浮きを本判定する。例えば図4に示すように、往路と復路の両方で浮きと判定とされたタイルを、タイルの浮きが有るものとして本判定する。   As a result of the hammering test by the diagnostic hammer 10, as shown in FIG. 3 (2), when there is a tile that is determined to float in the hammering test of the forward path (first time), the control step is: Control is performed so that the tap sound inspection is performed on the return tile (second time) for the tiles arranged in the row. On the other hand, in the floating determination step, the tile floating is finally determined based on the hitting sound generated in the hitting inspection in the forward path and the return path. For example, as shown in FIG. 4, a tile that is determined to float in both the forward path and the return path is determined as having a tile lift.

このように、本実施の形態によれば、浮きが疑われるタイルに対して2回目の打音検査を行うことによって浮き判定の精度を高めることができる。これにより、劣化診断の信頼性を向上させることができる。   As described above, according to the present embodiment, it is possible to improve the accuracy of the floating determination by performing the second hammering test on the tile that is suspected of floating. Thereby, the reliability of deterioration diagnosis can be improved.

以上説明したように、本発明に係るタイルの劣化診断装置によれば、縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断装置であって、打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定手段と、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御手段とを備え、所定の範囲のタイルに対する1回目の打音検査において、タイルの浮きと判定されたタイルが有った場合には、制御手段は、その所定の範囲のタイルに対して2回目の打音検査を行うように制御し、浮き判定手段は、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定するので、浮きが疑われるタイルに対して2回目の打音検査を行うことによって浮き判定の精度を高めることができる。これにより、劣化診断の信頼性を向上させることができる。   As described above, according to the tile deterioration diagnosis apparatus according to the present invention, a plurality of tiles arranged vertically and horizontally, and the presence or absence of deterioration of the tiles fixed to the surface of the casing are determined by the hitting sound generated by hitting the tile surface. A tile deterioration diagnosis apparatus for diagnosing through sound inspection, the float determination means for determining the float of the tile representing the deterioration of the tile based on the hitting sound, and the hitting sound for a tile in a predetermined range among the plurality of tiles arranged Control means for controlling the inspection, and when there is a tile determined to be a floating tile in the first sound-inspection test for the tile in the predetermined range, the control means includes the tile in the predetermined range. The float determination means performs the main determination of the tile lift based on the hitting sounds generated in the first and second hitting inspections. Suspect Thailand It is possible to improve the accuracy of the float determined by carrying out a second tapping sound check on. Thereby, the reliability of deterioration diagnosis can be improved.

また、本発明に係る他のタイルの劣化診断装置によれば、縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断装置であって、打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定手段と、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御手段とを備え、制御手段は、所定の範囲のタイルに対して2回の打音検査を行うように制御し、浮き判定手段は、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定するので、2回の打音検査を行うことによって浮き判定の精度を高めることができる。これにより、劣化診断の信頼性を向上させることができる。   In addition, according to another tile deterioration diagnosis apparatus according to the present invention, a plurality of vertical and horizontal tiles, and whether or not the tiles fixed on the surface of the casing are deteriorated are checked for hitting sound by hitting sound generated by hitting the tile surface. A tile deterioration diagnosis apparatus for diagnosing through a float determination means for determining a tile lift indicating deterioration of a tile based on a hitting sound, and a hammering test for a tile in a predetermined range among a plurality of tiles arranged. A control means for controlling the control means so as to perform the second hammering test for a predetermined range of tiles, and the floating determination means is generated in the first and second hammering tests. Since the tile lifting is determined based on the hitting sound, the accuracy of the lifting determination can be increased by performing the hitting test twice. Thereby, the reliability of deterioration diagnosis can be improved.

また、本発明に係る他のタイルの劣化診断装置によれば、浮き判定手段は、1回目の打音検査において浮きと判定されたタイルが、2回目の打音検査においても浮きと判定された場合に、タイルの浮きとして本判定するので、浮き判定の精度を高めることができる。   Further, according to another tile deterioration diagnosis apparatus according to the present invention, the floating determination means determines that a tile determined to be floating in the first hammering test is floating in the second hammering test. In this case, since the main determination is made as a tile floating, the accuracy of the floating determination can be improved.

また、本発明に係るタイルの劣化診断方法によれば、縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断方法であって、打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定ステップと、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御ステップとを備え、所定の範囲のタイルに対する1回目の打音検査において、タイルの浮きと判定されたタイルが有った場合には、制御ステップは、その所定の範囲のタイルに対して2回目の打音検査を行うように制御し、浮き判定ステップは、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定するので、浮きが疑われるタイルに対して2回目の打音検査を行うことによって浮き判定の精度を高めることができる。これにより、劣化診断の信頼性を向上させることができる。   Further, according to the tile deterioration diagnosis method according to the present invention, the presence or absence of deterioration of the tiles arranged in the vertical and horizontal directions and fixed to the surface of the casing is diagnosed through a sound-inspection test using a sound generated by hitting the surface of the tile. A method for diagnosing tile deterioration, which controls a float determination step for determining a float of a tile that represents the deterioration of the tile based on the hitting sound, and a hammering test for a tile in a predetermined range among a plurality of tiles arranged And when there is a tile determined to be a floating tile in the first sound-inspection test for the tile in the predetermined range, the control step is performed for the tile in the predetermined range. Control is performed to perform the second hammering test, and the float determination step makes a final determination of tile lifting based on the hammering sounds generated in the first and second hammering tests. It is possible to improve the accuracy of the float determined by carrying out a second tapping sound check on Le. Thereby, the reliability of deterioration diagnosis can be improved.

また、本発明に係る他のタイルの劣化診断方法によれば、縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断方法であって、打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定ステップと、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御ステップとを備え、制御ステップは、所定の範囲のタイルに対して2回の打音検査を行うように制御し、浮き判定ステップは、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定するので、2回の打音検査を行うことによって浮き判定の精度を高めることができる。これにより、劣化診断の信頼性を向上させることができる。   Further, according to another tile deterioration diagnosis method according to the present invention, a plurality of vertical and horizontal tiles that are fixed to the surface of the casing are checked for the presence or absence of deterioration of the tiles by hitting sound generated by hitting the tile surface. A tile deterioration diagnosis method for diagnosing through a float determination step for determining a tile lift that represents deterioration of a tile based on the hitting sound, and a hammering test for tiles in a predetermined range among a plurality of tiles arranged. A control step for controlling, and the control step is controlled so as to perform the second hammering test for a predetermined range of tiles, and the floating determination step occurs in the first and second hammering tests. Since the tile lifting is determined based on the hitting sound, the accuracy of the lifting determination can be increased by performing the hitting test twice. Thereby, the reliability of deterioration diagnosis can be improved.

また、本発明に係る他のタイルの劣化診断方法によれば、浮き判定ステップは、1回目の打音検査において浮きと判定されたタイルが、2回目の打音検査においても浮きと判定された場合に、タイルの浮きとして本判定するので、浮き判定の精度を高めることができる。   Further, according to another tile deterioration diagnosis method according to the present invention, in the floating determination step, the tile determined to be floating in the first hammering test is determined to be floating in the second hammering test. In this case, since the main determination is made as a tile floating, the accuracy of the floating determination can be improved.

以上のように、本発明に係るタイルの劣化診断装置およびタイルの劣化診断方法は、建物の外壁や床に貼設されたタイルの経年劣化等による浮きなどの異常の有無を診断するのに有用であり、特に、タイルの浮きを精度よく判定するのに適している。   As described above, the tile deterioration diagnosis apparatus and tile deterioration diagnosis method according to the present invention are useful for diagnosing the presence or absence of abnormalities such as floating due to aged deterioration of tiles affixed to the outer wall or floor of a building. In particular, it is suitable for accurately determining the floating of a tile.

10 診断用ハンマー(叩き手段)
12 打音記録手段
14 浮き判定手段
16 制御手段
100 タイルの劣化診断装置
10 Hammer for diagnosis (beating means)
12 Tapping sound recording means 14 Floating judgment means 16 Control means 100 Tile degradation diagnosis device

Claims (6)

縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断装置であって、
打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定手段と、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御手段とを備え、
所定の範囲のタイルに対する1回目の打音検査において、タイルの浮きと判定されたタイルが有った場合には、制御手段は、その所定の範囲のタイルに対して2回目の打音検査を行うように制御し、浮き判定手段は、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定することを特徴とするタイルの劣化診断装置。
A tile degradation diagnosis device for diagnosing the presence or absence of degradation of tiles arranged in rows and columns and fixed on the surface of a cabinet through a hammering test using a hammering sound generated by hitting the surface of the tile,
A float determining means for determining the floating of the tile representing the deterioration of the tile based on the hitting sound, and a control means for controlling the hitting test for a predetermined range of tiles among the plurality of tiles arranged,
When there is a tile that is determined to be a floating tile in the first sound hit inspection for a tile in a predetermined range, the control unit performs a second sound check for the tile in the predetermined range. A tile deterioration diagnosis device characterized in that the floating determination means performs the main determination on the floating of the tile based on the hitting sound generated in the first and second hitting tests.
縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断装置であって、
打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定手段と、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御手段とを備え、
制御手段は、所定の範囲のタイルに対して2回の打音検査を行うように制御し、浮き判定手段は、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定することを特徴とするタイルの劣化診断装置。
A tile degradation diagnosis device for diagnosing the presence or absence of degradation of tiles arranged in rows and columns and fixed on the surface of a cabinet through a hammering test using a hammering sound generated by hitting the surface of the tile,
A float determining means for determining the floating of the tile representing the deterioration of the tile based on the hitting sound, and a control means for controlling the hitting test for a predetermined range of tiles among the plurality of tiles arranged,
The control means performs control so that the sound hitting inspection is performed twice for tiles in a predetermined range, and the float determination means determines the tile sound based on the sound hitting sounds generated in the first and second sound hitting inspections. A tile deterioration diagnosis apparatus, characterized in that a float is fully determined.
浮き判定手段は、1回目の打音検査において浮きと判定されたタイルが、2回目の打音検査においても浮きと判定された場合に、タイルの浮きとして本判定することを特徴とする請求項1または2に記載のタイルの劣化診断装置。   The floating determination means, when a tile determined to be floating in the first hammering test is determined to be floating in the second hammering test, makes a main determination as a tile floating. The tile deterioration diagnosis apparatus according to 1 or 2. 縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断方法であって、
打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定ステップと、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御ステップとを備え、
所定の範囲のタイルに対する1回目の打音検査において、タイルの浮きと判定されたタイルが有った場合には、制御ステップは、その所定の範囲のタイルに対して2回目の打音検査を行うように制御し、浮き判定ステップは、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定することを特徴とするタイルの劣化診断方法。
A tile deterioration diagnosis method for diagnosing the presence / absence of deterioration of tiles arranged vertically and horizontally and fixed to the surface of a cabinet through a hammering test using a hammering sound generated by hitting the surface of the tile,
A float determination step for determining the float of the tile representing the deterioration of the tile based on the hitting sound, and a control step for controlling a hitting test for a tile in a predetermined range among the tiles arranged in a plurality,
When there is a tile that is determined to be a floating tile in the first sound-inspection test for a tile in a predetermined range, the control step performs a second sound-inspection test for the tile in the predetermined range. A tile deterioration diagnosis method characterized in that the floating determination step performs the main determination of the floating of the tile based on the hitting sound generated in the first and second hitting tests.
縦横に複数並べられ、躯体表面に固定されたタイルの劣化の有無を、タイルの表面を叩いて発生する打音による打音検査を通じて診断するタイルの劣化診断方法であって、
打音に基づいてタイルの劣化を表すタイルの浮きを判定する浮き判定ステップと、複数並べられたタイルのうち所定の範囲のタイルに対する打音検査を制御する制御ステップとを備え、
制御ステップは、所定の範囲のタイルに対して2回の打音検査を行うように制御し、浮き判定ステップは、1回目と2回目の打音検査で発生した打音に基づいて、タイルの浮きを本判定することを特徴とするタイルの劣化診断方法。
A tile deterioration diagnosis method for diagnosing the presence / absence of deterioration of tiles arranged vertically and horizontally and fixed to the surface of a cabinet through a hammering test using a hammering sound generated by hitting the surface of the tile,
A float determination step for determining the float of the tile representing the deterioration of the tile based on the hitting sound, and a control step for controlling a hitting test for a tile in a predetermined range among the tiles arranged in a plurality,
The control step performs control so that the hammering inspection is performed twice for the tiles in a predetermined range, and the floating determination step is performed based on the hammering sounds generated in the first and second hammering tests. A method for diagnosing tile deterioration, characterized by determining whether or not a float is present.
浮き判定ステップは、1回目の打音検査において浮きと判定されたタイルが、2回目の打音検査においても浮きと判定された場合に、タイルの浮きとして本判定することを特徴とする請求項4または5に記載のタイルの劣化診断方法。   The floating determination step is characterized in that when the tile determined to be floating in the first hammering test is determined to be floating in the second hammering test, the main determination is made as a tile floating. 6. The tile deterioration diagnosis method according to 4 or 5.
JP2016231496A 2016-11-29 2016-11-29 Tile deterioration diagnosis device and tile deterioration diagnosis method Active JP6796827B2 (en)