JP2014105280A - 反応性シクロオレフィンポリマーとその製造方法 - Google Patents
反応性シクロオレフィンポリマーとその製造方法 Download PDFInfo
- Publication number
- JP2014105280A JP2014105280A JP2012258914A JP2012258914A JP2014105280A JP 2014105280 A JP2014105280 A JP 2014105280A JP 2012258914 A JP2012258914 A JP 2012258914A JP 2012258914 A JP2012258914 A JP 2012258914A JP 2014105280 A JP2014105280 A JP 2014105280A
- Authority
- JP
- Japan
- Prior art keywords
- cycloolefin polymer
- reactive
- polymer
- molecular weight
- producing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
【解決手段】ノルボルネン誘導体をモノマーとして用いて開環メタセシス重合を行った後、水素化することにより製造されたシクロオレフィンポリマーを溶融させ、330〜380℃で熱分解することにより製造され、数平均分子量(Mn)が10,000〜50,000、分子量分布の分散度(Mw/Mn)が2.0〜10.0であり、分子鎖にビニリデン基を有する、反応性シクロオレフィンポリマー。
【選択図】図1
Description
一般式(2):
一般式(3):
一般式(4):
熱分解装置としてガラス製小型熱分解装置を使用した。シクロオレフィンポリマー(上記ポリマー2)5gを反応器に仕込み、系内を窒素置換後、2mmHgに減圧して、反応器を200℃に加熱して溶融した。その後、370℃に設定されたメタルバスに反応器を沈め、熱分解を行った。熱分解中は、系内を2mmHg程度の減圧状態に保ち、溶融ポリマーを導入されたキャピラリーから排出される窒素ガスのバブリングによって攪拌した。1時間経過後、反応器をメタルバスからあげ、室温まで冷却した後、反応系を常圧にし、反応器内の残渣を熱キシレンにて溶解した後、メタノールに滴下して再沈殿精製して、反応性シクロオレフィンポリマーを得た。
Claims (3)
- 下記一般式(1)
で表されるシクロオレフィンポリマーを溶融させ、330〜380℃で熱分解することにより製造され、数平均分子量(Mn)が10,000〜50,000、分子量分布の分散度(Mw/Mn)が2.0〜10.0であり、分子鎖にビニリデン基を有することを特徴とする、反応性シクロオレフィンポリマー。 - 前記シクロオレフィンポリマーは、
R1及びR2が互いに架橋することによりシクロペンタンを形成していることを特徴とする、請求項1に記載の反応性シクロオレフィンポリマー。 - 数平均分子量(Mn)が10,000〜50,000、分子量分布の分散度(Mw/Mn)が2.0〜10.0であり、分子鎖にビニリデン基を有する反応性シクロオレフィンポリマーの製造方法であって、
下記一般式(1)
で表されるシクロオレフィンポリマーを溶融させ、330〜380℃で熱分解することを特徴とする、反応性シクロオレフィンポリマーの製造方法。