JP2009018848A - Shrink label - Google Patents

Shrink label Download PDF

Info

Publication number
JP2009018848A
JP2009018848A JP2007184110A JP2007184110A JP2009018848A JP 2009018848 A JP2009018848 A JP 2009018848A JP 2007184110 A JP2007184110 A JP 2007184110A JP 2007184110 A JP2007184110 A JP 2007184110A JP 2009018848 A JP2009018848 A JP 2009018848A
Authority
JP
Japan
Prior art keywords
shrink film
shrink
perforation
label
weak seal
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2007184110A
Other languages
Japanese (ja)
Inventor
Hiroyuki Otsuka
浩之 大塚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toppan Inc
Original Assignee
Toppan Printing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toppan Printing Co Ltd filed Critical Toppan Printing Co Ltd
Priority to JP2007184110A priority Critical patent/JP2009018848A/en
Publication of JP2009018848A publication Critical patent/JP2009018848A/en
Pending legal-status Critical Current

Abstract

<P>PROBLEM TO BE SOLVED: To provide a shrink label capable of being easily peeled from a vessel without time and labor. <P>SOLUTION: The tubular label has a bonded part (12) formed by bonding inner surfaces of both ends (17 and 18) of the shrink film (11) on each other with the front ends (17a and 18a) of both ends (17 and 18) offset from each other, and further has a weak seal part (16) formed by aligning the inner surface of the end (17), the front end (17a) of which extends from the plastered part (12) beyond the front end (18a) of the other end (18), as well as the plastered part (12) along the outer surface of the shrink film (11) and plastering the same on the outer surface of the shrink film (11) for sealing via a peeling agent (15) wherein a perforation (13) is formed on the shrink film (11) which extends from the plastered part (12) in a direction opposite to the weak seal part (16) and is located in an inside of the tube. <P>COPYRIGHT: (C)2009,JPO&INPIT

Description

本発明はシュリンクラベルに関する。   The present invention relates to a shrink label.

一般にシュリンクラベルとは、加熱によって熱収縮する合成樹脂性フィルム(シュリンクフィルム)に商品表示を予め印刷しておき、そのフィルムを筒状に貼り合わせたものを容器に被せた後に、加熱した空気などで加熱することで、容器の形状に沿って装着するラベルである。   In general, a shrink label is a product that is pre-printed on a synthetic resin film (shrink film) that heat-shrinks by heating, and a container that is laminated with the film is covered with a container, and then heated, etc. It is a label that is attached along the shape of the container by heating with.

従来、シュリンクラベルを容器から剥離し易くするものとして、貼り合わせ部の両側にそれぞれ1本ずつミシン目が入っており、シュリンクラベルの天地どちらかからその2本のミシン目を破り、容器から剥離するものがある。   Conventionally, there is one perforation on each side of the bonded part to make it easier to peel the shrink label from the container, and the two perforations are broken from either side of the shrink label and peeled from the container There is something to do.

しかしながら、シュリンクラベルと容器とは密着しており、そのわずかな隙間に指を入れてミシン目を破ることが難しい。   However, the shrink label and the container are in close contact with each other, and it is difficult to break a perforation by putting a finger into the slight gap.

そこで剥離性を向上させるために、シュリンクラベルの天地何れかの端部に、ミシン目を切り裂く起点となる箇所をつまみ易くするつまみタブを設けたり(例えば特許文献1参照)、2本のミシン目の間にミシン目を破断するきっかけとなる切込みを入れたものがある(例えば特許文献2参照)。   Therefore, in order to improve the peelability, a knob tab that makes it easy to pinch the starting point for tearing the perforation is provided at either end of the shrink label (see, for example, Patent Document 1). Is provided with a notch that causes the perforation to break (see, for example, Patent Document 2).

しかしながら、つまみタブを設けても、切込みを入れても、同様に、摘みにくく、爪に引っ掛ける程度で剥離性は良くない。
特開2006−347598号公報 特開2007−15732号公報
However, even if a knob tab is provided or a cut is made, similarly, it is difficult to pick and the peelability is not good enough to be caught on a nail.
JP 2006-347598 A JP 2007-15732 A

本発明は斯かる背景技術に鑑みてなされたもので、容器から手間がかからず容易に剥離できるシュリンクラベルを提供することを課題とする。   The present invention has been made in view of such background art, and an object of the present invention is to provide a shrink label that can be easily peeled off from a container without trouble.

本発明において上記課題を解決するために、まず請求項1の発明では、シュリンクフィルムの両端部の先端を互いにずらして両端部の内面同士を貼り合わせて貼り合わせ部を形成し、さらに、前記貼り合わせ部から先端が他の端部の先端よりも長く出ている端部の内面を、前記貼り合わせ部とともに、前記シュリンクフィルムの外面に沿わせて、前記シュリンクフィルムの外面に剥離剤を介してシールして弱シール部を形成した筒状のラベルであって、
前記貼り合わせ部から前記弱シール部とは反対方向に出ていて、前記筒の内側方向にある前記シュリンクフィルムに、ミシン目が形成されていることを特徴とするシュリンクラベルとしたものである。
In order to solve the above-mentioned problems in the present invention, first, in the invention of claim 1, the ends of both ends of the shrink film are shifted from each other, the inner surfaces of both ends are bonded together to form a bonded portion, and the bonding is further performed. The inner surface of the end portion whose tip extends from the mating portion is longer than the tip of the other end portion, along with the bonding portion, along the outer surface of the shrink film, and via the release agent on the outer surface of the shrink film A cylindrical label that is sealed to form a weak seal portion,
The shrink label is characterized in that a perforation is formed in the shrink film that protrudes in the opposite direction from the weak seal portion from the bonded portion and is in the inner direction of the cylinder.

また請求項2の発明では、前記貼り合わせ部から前記弱シール部とは反対方向に出ていて、前記筒の外側方向にある前記シュリンクフィルムに、ミシン目が形成されていることを特徴とする請求項1記載のシュリンクラベルとしたものである。   The invention according to claim 2 is characterized in that a perforation is formed in the shrink film that protrudes in the direction opposite to the weak seal portion from the bonded portion and is in the outer direction of the tube. The shrink label according to claim 1 is provided.

請求項1の発明は、弱シール部を指で剥離して、貼り合わせ部を指で摘んで、ミシン目を破ることにより、容器から手間がかからず容易に剥離できるという効果がある。   According to the first aspect of the present invention, the weak seal portion is peeled off with a finger, the bonded portion is picked up with a finger, and the perforation is broken, so that there is an effect that it can be easily peeled off from the container without taking time and effort.

請求項2の発明は、筒の内側方向だけでなく外側方向にもミシン目があるので、請求項1の発明よりも容器から手間がかからず容易に剥離できるという効果がある。   According to the second aspect of the present invention, since there are perforations not only in the inner direction of the cylinder but also in the outer direction, there is an effect that it can be easily peeled off from the container with less effort than the first aspect of the present invention.

以上、本発明は、容器から手間がかからず容易に剥離できるシュリンクラベルを提供できるという効果がある。   As described above, the present invention has an effect that it is possible to provide a shrink label that can be easily peeled off from a container without trouble.

以下に、本発明の最良の一実施形態を図面に基いて説明する。   Hereinafter, the best embodiment of the present invention will be described with reference to the drawings.

図1は、本発明のシュリンクラベルを装着した容器の側面を示す。また図2は、本発明のシュリンクラベルの断面を一部分拡大したものである。   FIG. 1 shows the side of a container equipped with the shrink label of the present invention. FIG. 2 is a partially enlarged cross-sectional view of the shrink label of the present invention.

本発明のシュリンクラベルは、図2に示すように、方形の形状をしているシュリンクフィルム(11)の両端部(17,18)の先端(17a,18a)を、互いにずらして両端部(17,18)の内面同士を貼り合わせて貼り合わせ部(12)を形成し、さらに、貼り合わせ部(12)から先端(17a)が他の端部(18)の先端(18a)よりも長く出ている端部(17)の内面を、貼り合わせ部(12)とともに、シュリンクフィルム(11)の外面に沿わせて、シュリンクフィルム(11)の外面に剥離剤(15)を介してシールして弱シール部(16)を形成した筒状のラベルである。   As shown in FIG. 2, the shrink label of the present invention has both ends (17 a, 18 a) of the both ends (17 a, 18 a) of the shrink film (11) having a square shape shifted from each other. , 18) are bonded together to form a bonded portion (12), and the tip (17a) from the bonded portion (12) is longer than the tip (18a) of the other end (18). The inner surface of the end portion (17) is sealed along the outer surface of the shrink film (11) together with the bonding portion (12), and the outer surface of the shrink film (11) is sealed via a release agent (15). It is the cylindrical label which formed the weak seal part (16).

そして本発明のシュリンクラベルは、図2に示すように、貼り合わせ部(12)から弱シール部(16)とは反対方向に出ていて、筒の内側方向にあるシュリンクフィルム(11)に、連続的または断続的なミシン目(13)があり、このミシン目(13)は、図1に示すように、貼り合わせ部(12)に沿って縦方向に形成されている。   And, as shown in FIG. 2, the shrink label of the present invention protrudes from the bonded portion (12) in the opposite direction to the weak seal portion (16), and on the shrink film (11) in the inner direction of the tube, There is a continuous or intermittent perforation (13), and the perforation (13) is formed in the longitudinal direction along the bonding portion (12) as shown in FIG.

さらに本発明のシュリンクラベルは、図2に示すように、貼り合わせ部(12)から弱シール部(16)とは反対方向に出ていて、筒の外側方向にあるシュリンクフィルム(11)に、連続的または断続的なミシン目(14)があり、このミシン目(14)は、図1に示すように、貼り合わせ部(12)に沿って縦方向に形成されていても良い。   Furthermore, as shown in FIG. 2, the shrink label of the present invention protrudes from the bonded portion (12) in the opposite direction to the weak seal portion (16), and on the shrink film (11) in the outer direction of the tube, There is a continuous or intermittent perforation (14), and the perforation (14) may be formed in the longitudinal direction along the bonding portion (12) as shown in FIG.

シュリンクフィルム(11)は、加熱によって熱収縮する合成樹脂フィルムであれば良く、例えば、ポリテレフタル酸エチレン(PET)フィルム、ポリスチレン(PS)フィルム、或いは、ポリ塩化ビニル(PVC)フィルムなどが挙げられる。   The shrink film (11) may be a synthetic resin film that is thermally contracted by heating, and examples thereof include a polyethylene terephthalate (PET) film, a polystyrene (PS) film, and a polyvinyl chloride (PVC) film. .

本発明のシュリンクフィルムは、容器に被せた後に、加熱した空気などで加熱することで、図1に示すように、容器の形状に沿って装着される。   The shrink film of the present invention is attached along the shape of the container as shown in FIG. 1 by being heated with heated air after being put on the container.

以下に、容器に装着された本発明のシュリンクフィルムを、その容器から剥離する方法を説明する。   Below, the method to peel the shrink film of this invention with which the container was mounted | worn from the container is demonstrated.

まず、図2に示すように、弱シール部(16)は、端部(17)の内面を、シュリンクフィルム(11)の外面に剥離剤(15)を介してシールして形成したものなので、指で手間がかからず容易に剥離することができる。そこで、弱シール部(16)を剥離すると、図3に示すように、貼り合わせ部(12)付近がシュリンクフィルム(11)の外面方向に突出するので、貼り合わせ部(12)付近を指で手間がかからず容易に摘むことが可能になる。そして、貼り合わせ部(12)付近を指で摘むことにより、貼り合わせ部(12)に沿って縦方向にミシン目(13,14)を破って、本発明のシュリンクラベルを容器から手間がかからず容易に剥離することができる。   First, as shown in FIG. 2, the weak seal portion (16) is formed by sealing the inner surface of the end portion (17) to the outer surface of the shrink film (11) via a release agent (15). It can be easily peeled off with little fingers. Therefore, when the weak seal portion (16) is peeled off, the vicinity of the bonding portion (12) protrudes toward the outer surface of the shrink film (11) as shown in FIG. It can be easily picked up without trouble. Then, by picking the vicinity of the bonding portion (12) with a finger, the perforations (13, 14) are broken in the vertical direction along the bonding portion (12), and the shrink label of the present invention is troublesome from the container. It can be easily peeled off.

本発明のシュリンクラベルを装着した容器の側面を示す図。The figure which shows the side surface of the container equipped with the shrink label of this invention. 本発明のシュリンクラベルの断面を一部分拡大した図。The figure which expanded a section of the shrink label of the present invention partially. 本発明のシュリンクラベルを容器から剥離する方法を説明する拡大断面図。The expanded sectional view explaining the method of peeling the shrink label of this invention from a container.

符号の説明Explanation of symbols

11…シュリンクフィルム
12…貼り合わせ部
13…ミシン目
14…ミシン目
15…剥離剤
16…弱シール部
17…端部
17a…先端
18…端部
18a…先端
DESCRIPTION OF SYMBOLS 11 ... Shrink film 12 ... Bonding part 13 ... Perforation 14 ... Perforation 15 ... Release agent 16 ... Weak seal part 17 ... End 17a ... Tip 18 ... End 18a ... Tip

Claims (2)

シュリンクフィルムの両端部の先端を互いにずらして両端部の内面同士を貼り合わせて貼り合わせ部を形成し、さらに、前記貼り合わせ部から先端が他の端部の先端よりも長く出ている端部の内面を、前記貼り合わせ部とともに、前記シュリンクフィルムの外面に沿わせて、前記シュリンクフィルムの外面に剥離剤を介してシールして弱シール部を形成した筒状のラベルであって、
前記貼り合せ部から前記弱シール部とは反対方向に出ていて、前記筒の内側方向にある前記シュリンクフィルムに、ミシン目が形成されていることを特徴とするシュリンクラベル。
The ends of the shrink film are shifted from each other, the inner surfaces of both ends are bonded together to form a bonded portion, and the end of the bonded portion is longer than the other ends. A cylindrical label that forms a weak seal portion by sealing the inner surface of the shrink film along with the bonded portion along the outer surface of the shrink film with a release agent on the outer surface of the shrink film,
A shrink label, wherein a perforation is formed on the shrink film that protrudes from the bonding portion in a direction opposite to the weak seal portion and is in an inner direction of the tube.
前記貼り合せ部から前記弱シール部とは反対方向に出ていて、前記筒の外側方向にある前記シュリンクフィルムに、ミシン目が形成されていることを特徴とする請求項1記載のシュリンクラベル。   The shrink label according to claim 1, wherein a perforation is formed in the shrink film that protrudes in a direction opposite to the weak seal portion from the bonding portion and is in an outer direction of the cylinder.
JP2007184110A 2007-07-13 2007-07-13 Shrink label Pending JP2009018848A (en)