FI117507B - Menetelmä ligniinin poistamiseksi vedestä - Google Patents

Menetelmä ligniinin poistamiseksi vedestä Download PDF

Info

Publication number
FI117507B
FI117507B FI20040967A FI20040967A FI117507B FI 117507 B FI117507 B FI 117507B FI 20040967 A FI20040967 A FI 20040967A FI 20040967 A FI20040967 A FI 20040967A FI 117507 B FI117507 B FI 117507B
Authority
FI
Finland
Prior art keywords
calcium
compound
process according
added
aluminum
Prior art date
Application number
FI20040967A
Other languages
English (en)
Swedish (sv)
Other versions
FI20040967A (fi
FI20040967A0 (fi
Inventor
Paeivi Rousu
Heikki Palonen
Arja Paloniemi
Reetta Taittonen
Original Assignee
Kemira Oyj
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kemira Oyj filed Critical Kemira Oyj
Publication of FI20040967A0 publication Critical patent/FI20040967A0/fi
Priority to FI20040967A priority Critical patent/FI117507B/fi
Priority to RU2007103838/05A priority patent/RU2408543C2/ru
Priority to AT05763636T priority patent/ATE398701T1/de
Priority to US11/571,846 priority patent/US7794604B2/en
Priority to BRPI0513065A priority patent/BRPI0513065B1/pt
Priority to CN200580030193.4A priority patent/CN101023215B/zh
Priority to EP05763636A priority patent/EP1774088B1/en
Priority to PCT/FI2005/000324 priority patent/WO2006005797A1/en
Priority to DE602005007610T priority patent/DE602005007610D1/de
Priority to CA2573035A priority patent/CA2573035C/en
Publication of FI20040967A publication Critical patent/FI20040967A/fi
Application granted granted Critical
Publication of FI117507B publication Critical patent/FI117507B/fi

Description

1 1 7507
Menetelmä ligniinin poistamiseksi vedestä
Keksintö koskee menetelmä ligniinin poistamiseksi vesipitoisesta liuoksesta kal-siumyhdisteen avulla.
5 Sellumassan valkaisusekvenssissä on usein yksi tai useampia peroksidivaiheita. Valkaisuolosuhteet ovat pH:ltaan alkaalisia ja suhteellisen kuumia (> 60 °C).
Näissä olosuhteissa massan sisältämä ligniini osittain liukenee ja osittain muuttuu kuidun pinnassa vähemmän värilliseksi. Valkaisun jälkeen massa pestään ja suo-dosvesi ajetaan yleensä jätevesilaitokselle. Veteen liukeneva ligniini värjää veden 10 kellanruskeaksi. Ligniinin katsotaan olevan vaikeasti biohajoavan, jolloin sen vaikutus on suuri puhdistetun jäteveden ominaisuuksissa. Tämän vuoksi olisi edullista jos se voitaisiin poistaa vedestä ennen jäteveden biologista käsittelyä.
Kalsiumin ligniiniä saostava vaikutus on tunnettu asia. Siitä löytyy useita kirjallisuusviitteitä aivan viime vuosiltakin. Kuitenkin sen saostava vaikutus on sangen 15 rajoitettu. Ks. alla oleva taulukko 2.
Keksinnön tavoitteena on siis löytää entistä tehokkaampi menetelmä ligniinin j .. poistamiseksi vesipitoisesta liuoksesta kuten selluloosamassan valkaisun jäteve- • · : destä. Tähän tavoitteeseen on nyt päästy lisäämällä vesipitoiseen liuokseen kal-
siumyhdisteen lisäksi myös alumiiniyhdistettä. H
···''' . '~A
* · · • · · m .**·. 20 Kuten mainittiin, keksintö liittyy läheisesti ligniinin poistamiseen selluloosamassan valkaisuvedestä. Yleensä tämä valkaisuvesi on emäksinen, jolloin sen pH on suu- ruusluokkaa 10. Tällöin on keksinnön kannalta edullista, jos vesipitoisen liuoksen *** pH säädetään arvoon 4,5 - 7, edullisesti pH-arvoon 5 - 6. Tämä voi esim. tapah- . tua lisäämällä epäorgaanista happoa kuten rikkihappoa. Mikäli käytettävä alumiini- • · · •»j 25 yhdiste on vedessä happamasti reagoiva, pH saattaa muutenkin asettua toivotulle tasolle.
• * • *
On myös havaittu, että kalsium- ja alumiiniyhdisteiden lisäysjärjestys on tärkeä • * ’·;·* poistettaessa ligniiniä keksinnön mukaisesti. Edullisen suoritusmuodon mukaan :T: vesipitoiseen liuokseen lisätään ensin kalsiumyhdiste, säädetään liuos sen jälkeen 30 tarvittaessa ko. pH arvoon, ja lisätään alumiiniyhdiste. On myös edullista, mikäli menetelmässä alkaaliseen ligniinipitoiseen veteen lisätään kalsiumyhdiste, annetaan reagoida tietyn ajan, sen jälkeen säädetään pH neutraaliksi tai lievästi happamaksi ja lopuksi lisätään alumiiniyhdiste. Näin muodostuu runsas sakka ja ligniinin 2 117507 kellertävä väri poistuu lähes kokonaan. Sakan laskeutumista voi edistää flokkulan-tin lisäyksellä.
Ligniinin pitoisuutta kuvaava suure on UV absorbanssi aallonpituudella 280 nm. Parhaimmillaan absorbanssi aleni keksinnössä tasolta 3,7 tasolle 1,8.
5 Vesipitoiseen liuokseen lisätään edullisesti 10 - 10 000 mg/l, vielä edullisemmin 50 - 1000 mg/l kalsiumia vastaava määrä kalsiumyhdistettä. Vesipitoiseen liuokseen lisätään edullisesti 100 - 10 000 mg/l, vielä edullisemmin 300 - 1000 mg/l alumiiniyhdistettä.
Keksinnössä käytettävä kalsiumyhdiste on edullisesti valittu kalsiumoksidista, 10 kalsiumhydroksidista ja epäorgaanisista kalsiumsuoloista. Edullisemmin kalsium-yhdiste on kalsiumkloridi tai kalsiumsulfaatti, edullisimmin kalsiumkloridi.
Alumiiniyhdiste on edullisesti polymeerinen alumiinihydroksidi tai polymeerinen alumiinihydroksidisuola. Polymeerinen rakenne muodostuu kun yhdiste sisältää hydroksyyliryhmiä, jotka muodostavat oksosiltoja. Vielä edullisemmin alumiiniyh-15 diste on polymeerinen alumiinihydroksidisulfaatti, polymeerinen alumiinihydroksi-dikloridi tai polymeerinen alumiinihydroksidiformiaatti. Kaikkein edullisimmin alumiiniyhdiste on alumiinihydroksidikloridia, jonka OH/AI-suhde on 1:10 - 9:10.
• · • · ** y Seuraavassa keksintöä valaistaan suoritus- ja vertailuesimerkkien avulla, joiden • · * *·:·* tarkoituksena on vain valaista keksintöä.
• · ·
* · I
• · * ·***: 20 Esimerkit * * · * · ·
Tausta ··· • · • · • ♦ ·
Olkimassan valkaisun jätevedet sisältävät liuennutta ligniiniä. Sen oletetaan ··· olevan vaikeasti poistettavissa biologisin puhdistusmenetelmin. Tässä työssä sei- • · · · .*··. vitettiin ligniinin seostamista eri kemikaaleilla; monivalenttisilla kationeilla ja orgaa- y}' 25 nisillä polymeereillä.
• · ♦ «· • ···.·
Yhteenveto • · · • · · v : Työssä selvitettiin Ca-, Fe- ja Al-suolojen vaikutusta näyteveden sameuteen, COD.hen, TOC:iin ja ligniinin pitoisuutta kuvaavaan UV absorbanssiin aallonpituudella 280 nm.
117507 3 "
Selkeästi tehokkaimmaksi yhdistelmäksi osoittautui kalsiumin ja polymeerisen alumiinisuolan (Kempac 18) yhteiskäyttö. Alla olevassa taulukossa on kalsium lisätty CaCb vesiliuoksena.
Ca Kempac18 pH Sameus UV abs COD TOC __mg/l mg/l ___NTU 280 nm mg/l mg/l 0 - - 10,2 66 3,673 2326 803 1 1000 1000 5,3 5 1,861 1276 375 2 100 1000 5,8 3 2,316 1374 393 5 ________
CaCI2:n voi korvata vaikeampi liukoisilla kalsiumoksidilla tai kipsillä. Saostustulos heikkenee lievästi.
Orgaanisten flokkulanttien käyttö ei tehostanut saostusta, flokinmuodostusta eikä 10 sedimentoitumista.
Tulokset Näyte oli merkitty: WS:n raaka- ja pesuvesien seos 21.4.2004. Siitä määritettiin seuraavat ominaisuudet: • · • * * «· : ·*· Taulukko 1. Alkuperäinen vesi * » · ·.· ! Sentrifugoimaton Sentrifugoitu • · * pH 1Ö2 1Ö2
Sameus NTU 66,4 ··“ COD mg/l 2170 2326 TOC mg/l 797,3 802,9 *** Kat.tarve mekv/I 2,259 2,342 UV-abs 280 nm 3,673 . SS mg/l 52 15 ________ __ • · * * t • · II* ..· Taulukoissa 2-5 on esitetty koetuloksia pieninä kokonaisuuksina. Näissä kokeissa • · kalsium on lisätty CaC^ina (taulukossa ilmoitettu annos määrä on Ca:na). Tulok-*...* sista ilmenee selvästi kalsiumin ja polymeerisen alumiinisuolan yhteiskäytön edulli- 20 suus. Oleellista on myös pH:n säädön tarve.
• · · • · *···* Huomionarvoista on todeta, ettei pelkkä pH:n lasku 3:een alenna UV absorbanssia lainkaan.
4 117507
Saostumista ja flokinmuodostumista yritettiin tehostaa polymeereillä (Fennopolit A321, K1384, K3450 ja K506). Näiden vaikutus jäi hyvin minimaaliseksi ja usein polymeerin lisäys jopa heikensi flokinmuodostusta. Tämä ei kuitenkaan merkitse ettei polymeeri toimisi käytännön olosuhteissa.
5 Taulukossa 6 on ns. konfirmaatiokoe 1 litran näytteille. Nämä näytteet toimitettiin Ouluun. Saostuman selkeytymistä seurattiin silmämääräisesti. Suurempi Ca-an-nos paransi selvästi sedimentoitumista ja tiivisti sakkaa.
Taulukossa 7 on vertailtu eri kalsium-suolojen vaikutusta saostumiseen. Annoksen pieneneminen alle 1 g/L vaikuttaa välittömästi UV-absorbanssiin. Kalsiumoksidi ja 10 kipsi olivat lähes samanveroisia, kipsi, ehkä lievästi tehokkaampi. Kempacin määrään pienentäminen puoleen vei välittömästi tehon näiltä molemmilta Ca-suoloilta.
Suoritus
Testaus tehtiin 50 - 100 mL:n näytteillä. Kalsium-suola lisättiin ensin, sekoitettiin -2 min tai V2 tuntia niissä tapauksissa joissa suola oli kiinteänä. Tämän jälkeen 15 säädettiin pH 7, lisättiin toinen koagulantti. Sekoitettiin vielä pari minuuttia. Lopuksi vesi sentrifugoitiin ja kirkasteesta määritettiin ko. ominaisuudet.
Taulukko 2.
Koe nro Koagulantti pH " Sameus UV-abs COD TOC HUOM mg/l NTU 280 nm mgfl mg/l • ·· .
10,2 66 3,673 2326 803 1 Ca 10 10,1 52 2 Ca 100 10,0 32 3 Ca 1000 9,7 13 3,645 1564 555 4 Ca 5000 9,4 3
Ca 5000 9,3 2 lisätty kiinteänä ··· 5 Fennoferri 100 10,1 53 ""m 6 Fennoferri 500 9,8 63 4,000 2202 801 7 Fennoferri 1000 8,8 77 ./ 8 Kempac18 100 10,1 56 : 9 Kempad 8 500 9,7 64 3,831 2260 803 10 Kempad 8 1000 8,3 83 "* 11 Aluna 10 10,2 54 12 Aluna 100 10,1 59 13 Aluna 500 9,2 59 14 Aluna 1000 7,0 74 3,588 2232 788 5 117507
Taulukko 3.
Koe nro Koagulantti 1MH2S04 pH Sameus UV-abs COD TOC
__I mg/l μΐ /50 ml NTU 280 nm mg/l mg/l 15 - - 675 3 146 3,854 2240 699 16 Ca 1000 225 6,8 1 3,591 1660 537 17 Fennoferri 500 150 7,0 63 3,700 2354 754 18 Kempac18 500 125 6,9 60 3,529 2406 747 19 Aluna 500 100 6,9 67 3,822 2378 897
Taulukko 4.
Koe nro Koagulantti Koagulantti pH Sameus UV-abs COD TOC
__| mg/l__mg/l___NTU 280 nm mg/l mg/l 20 Ca 1000 Kempac18 100 6,4 18 3,523 1590 530,2 21 Ca 1000 Kempac18 500 5,4 3 1,795 1286 405,9 22 Ca 1000 Kempac18 1000 5,3 2 1,605 1264 396,5 23 Ca 1000 Fennoferri 500 6,1 39 3,528 1492 473,3 24 Ca 1000 PEO 5 7,0 5 3,492 25 Ca 1000 PEO 10 7,0 5 3,531 30 Ca 100 Kempad 8 1000 5,8 1 1.919 31 Ca 500 Kempad 8 1000 5,7 3 2,169 34 FF240 400 7,2 335 3,800 35 FF240 800 7,4 7 3,370 36 ORC2003 400 6,8 124 4,000 ' f. 37 ORC2003 800 6,4 155 3,790 • · · • __ • · · • · :T: Taulukko 5.
··· _ _ _ ____
Koe nro Koagulantti Koagulantti pH Sameus UV-abs ··· mg/l mg/l NTU 280 nm • · · 26 Ca 100 Kempad 8 1000 8,4 63 3,596 27 Ca 500 Kempad 8 1000 7,8 18 3,654 28 Ca 1000 Kempad 8 1000 8,4 6 3,480 ·:* 29 Ca 1000 Kempad 8 5000 9,3 5 3,586 ['·'·' 32 FF240 400 272 3>772 33 FF240 800 373 4,000 e» ___ • 5 pH.ta ei säädetty e··'1.
• · • · ···;'.
• · e ♦ ♦ e • » · ··· • e ♦ · • e e 6 117507
Taulukko 6.
Ca ~~ Kempac18 pH Sameus UV-abs COD TOC __tng/l mg/l NTU 280 nm mg/l mg/l 0 - - 10,2 66 3,673 2326 803 1 1000 1000 5,3 5 1,861 1276 375 2 100 1000 5,8 3 2,316 1374 393
Nopea sekoitus 400 rpm 10 sek, jonka aikana lisättiin Ca, hidas sekoitus 5 min. pH säädettiin magneettisekoittajalla
Nopea sekoitus 400 rpm 10 sek, jonka aikana lisättiin Kempac, hidas sekoitus 5 min.
Annettiin laskeutua yön yli
Kokeessa 1 sakan osuus n. 100 ml/500 ml
Kokeessa 2 sakan osuus n. 200 ml/500 ml
Kokeessa 2 sakka laskeutui hitaammin ja se oli kevyempää, osa oli pinnassa._
Taulukko 7. Kalsiumin eri lisäysmuodot
Koe nro Koagulanttl Koagulantti 1M H^SO,, pH Sameus UV-abs COD TOC
mg/l mg/l μΙ/IOOmi NTU 280 nm mg/l mg/l 0 ... . - 10,2 66 3,673 2326 803 1 CaO Ca 1000 Kempac18 1000 560 5,9 1 1,978 1372 391 2 CaSOd Ca 1000 Kempac18 1000 400 5,8 1 1,928 1356 391 , 3 Ca(OH)2 Ca_ 1000 Kempac18 1000 600 5,9 2 2,167 1406 410_ ’ 5 CacT Ca 100 Kempac18 " 1000 6j“| 33 Γ 3,016 1552 472 ;·. 4 CaO | Ca I 500 |Kempac18| 1000 500 6,8 7 2,469 1478 446 • 7 CaS04 Ca 100 Kempac18 1000 £“j 10 2,274 1434 426 : 6 CaSOi Ca 500 Kenpac18 1000 6.3 7 2,387 1420 432 8 CaO Ca 1000 Kempac18 500 6^5 43 3,595 ·,' * 9 CaO Ca 1000 Kempac18 100___6,9 64 3,622___ ,**·, 10 CaS04 Ca 1000 Kempac18 500 6,3 " 24 3,606 *···* 11 CaS04 Ca 1000 Kempac18 100 6,7 22 3,688 ··· • _ _ _
·«·· ^^ -linn I
»·· • · 5 . . ‘ ··* ♦ «·· • * · • · » · *·· k • » • · » · · « «·· « · * · * · · ··· •k·.
• · · »»· • · • · «t«

Claims (12)

117507
1. Menetelmä ligniinin poistamiseksi vesipitoisesta liuoksesta lisäämällä siihen kalsiumyhdistettä ja alumiiniyhdistettä, tunnettu siitä, että kalsiumyhdiste ja vesipitoinen liuos yhdistetään liuokseksi, jonka pH on 4,5 - 7, ja lisätään sitten alumiini- 5 yhdiste tähän liuokseen ligniinin saostamiseksi.
2. Patenttivaatimuksen 1 mukainen menetelmä, tunnettu siitä, että vesipitoinen liuos on sellumassan valkaisun emäksinen jätevesi.
3. Patenttivaatimuksen 1 tai 2 mukainen menetelmä, tunnettu siitä, että liuoksen pH säädetään arvoon 5-6.
4. Jonkin edellisen patenttivaatimuksen mukainen menetelmä, tunnettu siitä, ' että vesipitoiseen liuokseen lisätään 10 - 10 000 mg/l kalsiumia vastaava määrä kalsiumyhdistettä. I
5. Patenttivaatimuksen 4 mukainen menetelmä, tunnettu siitä, että vesipitoiseen liuokseen lisätään 50 - 1000 mg/l kalsiumia vastaava määrä kalsiumyhdistettä.
6. Jonkin edellisen patenttivaatimuksen mukainen menetelmä, tunnettu siitä, että vesipitoiseen liuokseen lisätään 100-10 000 mg/l alumiiniyhdistettä.
·*·.. 7. Patenttivaatimuksen 6 mukainen menetelmä, tunnettu siitä, että vesipitoi- « . seen liuokseen lisätään 300 - 1000 mg/l alumiiniyhdistettä.
• · * ··· • · · *·' * 8. Jonkin edellisen patenttivaatimuksen mukainen menetelmä, tunnettu siitä, ··· 20 että kalsiumyhdiste on valittu kalsiumoksidista, kalsiumhydroksidista ja epäorgaa-nisistä kalsiumsuoloista. • * * • · • ·
9. Patenttivaatimuksen 7 mukainen menetelmä, tunnettu sitä, että kalsiumyh- . . diste on kalsiumkloridi tai kalsiumsulfaatti, edullisesti kalsiumkloridi. * · · • · * • ♦ · ·
10. Jonkin edellisen patenttivaatimuksen mukainen menetelmä, tunnettu siitä, .·!·. 25 että alumiiniyhdiste on polymeerinen alumiinihydroksidi tai polymeerinen alumiini- ti· l.·m hydroksidisuola.
• · ♦ .’*** 11. Patenttivaatimuksen 10 mukainen menetelmä, tunnettu siitä, että alumiiniyh- • · · diste on polymeerinen alumiinihydroksidisulfaatti, polymeerinen alumiinihydroksi-dikloridi tai polymeerinen alumiinihydroksidiformiaatti. 117507
12. Patenttivaatimuksen 11 mukainen menetelmä, tunnettu siitä, että alumiiniyh-diste on alumiinihydroksidikloridia, jonka OH/AI-suhde on 1:10 - 9:10. 5
FI20040967A 2004-07-09 2004-07-09 Menetelmä ligniinin poistamiseksi vedestä FI117507B (fi)