CN2591286Y - Corrosion resisting fan - Google Patents

Corrosion resisting fan Download PDF

Info

Publication number
CN2591286Y
CN2591286Y CN 02292866 CN02292866U CN2591286Y CN 2591286 Y CN2591286 Y CN 2591286Y CN 02292866 CN02292866 CN 02292866 CN 02292866 U CN02292866 U CN 02292866U CN 2591286 Y CN2591286 Y CN 2591286Y
Authority
CN
China
Prior art keywords
resistance
coating layer
corrosion
utility
thickness
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 02292866
Other languages
Chinese (zh)
Inventor
李晓东
李京
陆卫忠
史杰智
高英
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Institute of Metal Research of CAS
Original Assignee
Institute of Metal Research of CAS
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Institute of Metal Research of CAS filed Critical Institute of Metal Research of CAS
Priority to CN 02292866 priority Critical patent/CN2591286Y/en
Application granted granted Critical
Publication of CN2591286Y publication Critical patent/CN2591286Y/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The utility model aims to provide a corrosion resisting blower. The utility model is characterized in that one or more parts of the outside surface the inner wall of a pipeline of a blower (1), the outer wall of the pipeline, an impeller and a blade are provided with a fusing combining epoxy powdery coating layer (2), and the thickness of the fusing combining epoxy powdery coating layer (2) is between 0.3 mm and 1.2 mm. In addition, the epoxy powdery coating layer (2) has the characteristics of stable chemical property, oil resistance, acid resistance, alkali resistance, resistance of sea water corrosion, strong adhesive force, high resistance to impact, etc.

Description

A kind of corrosion resistant fan
Technical field:
The utility model relates to blower fan, especially a kind of corrosion resistant fan.
Background technique:
Blower fan is the device that often adopts in the exhaust and the engineering of supplying gas, and row, when sending the gas of corrosive materials such as containing oil, acid, alkali, salt, the pipeline and the blade of blower fan is had certain corrosive action.Adopt thick-walled structure and stainless steel material for corrosion protection, this makes cost too high.
Summary of the invention:
The purpose of this utility model is to provide a kind of corrosion resistant blower fan, it is characterized in that one of inner-walls of duct, pipeline outer wall, the impeller of blower fan (1), appearance of blade are located or many places are provided with smelting combined epoxy powder coating layer (2), thickness is 0.3~1.2mm.
The optimum thickness of the utility model floating coat (2) is 0.5~0.8mm.
Anticorrosive paint layer used in the utility model is the commercially available prod, and as the SEBF anticorrosive paint of Metal Corrosion and Protection Inst., Chinese Academy of Sciences's development and exploitation, it has following characteristics:
1 stable chemical performance, oil resistant, acidproof, alkaline-resisting, seawater corrosion resistance.
2 strong adhesions, excellent in cushion effect.
3 abrasion resistance properties good (in corrosive environment) are five times of cast iron.
4 serviceability temperatures are extensive, are-40~150 ℃ in the air, are 0~100 ℃ in the solution, in the seawater 〉=and 100 ℃ (because experimental condition is only done seawater>110 ℃ experiment).
5 anticorrosive coat thickness ranges are at 30~3000 μ m, can carry out car, mill, machining such as plane, mill.
6 anticorrosive coat even compacts, smooth smooth, resistance is little, the efficiency of transmission height.
7 anticorrosive coats are nontoxic, tasteless, pollution-free.
8 long service life (according to the foreign data introduction, similar anticorrosive coat, safe operation is more than 30 years), price performance is much better than other process for protecting.
A layer thickness is anti-corrosion uniformly, wearing layer owing to employing high-performance adhere, thermosetting epoxy powder form at the metal surface of Fan pipeline, impeller, blade melting and solidification for the utility model, makes pipeline, impeller, blade have stronger wear-corrosion resistance.Overcome the shortcoming of blower fan corrosion resistance difference under the occasion of discharging, carrying the gas that contains Korrosionsmedium in the past, enlarged the scope of its application.Such blower fan corrosion-resistant coating has high mechanical strength and impact resistance, good anti-corrosion, wear-resisting property, and prevent electrochemical corrosion.The utility model can be widely used in oil, chemical industry, electric power, shipbuilding, cement, food sanitation and pharmaceutical industries.
Description of drawings:
Fig. 1 blower fan schematic representation.
Fig. 2 A district enlarged diagram.
Embodiment:
Below by embodiment in detail the utility model is described in detail.
Embodiment 1
The inner-walls of duct of blower fan (1) (as shown in Figure 1) scribbles SEBF coating (2), thickness 0.6mm.
Embodiment 2
The impeller of blower fan (1) and blade surface scribble SEBF coating (2), thickness 0.8mm.
Embodiment 3
The inner and outer walls of pipeline of blower fan and impeller, blade surface scribble SEBF coating (2), thickness 0.8mm.

Claims (2)

1. corrosion resistant fan, it is characterized in that: one of appearance of the inner-walls of duct of blower fan (1), pipeline outer wall, impeller, blade is located or many places are provided with smelting combined epoxy powder coating layer (2), and thickness is 0.3~1.2mm.
2. according to the described corrosion resistant fan of claim 1, it is characterized in that: coating (2) thickness is 0.5~0.8mm.
CN 02292866 2002-12-27 2002-12-27 Corrosion resisting fan Expired - Fee Related CN2591286Y (en)