CN210334397U - PCD welding tool with ceramic coating - Google Patents

PCD welding tool with ceramic coating Download PDF

Info

Publication number
CN210334397U
CN210334397U CN201920542182.3U CN201920542182U CN210334397U CN 210334397 U CN210334397 U CN 210334397U CN 201920542182 U CN201920542182 U CN 201920542182U CN 210334397 U CN210334397 U CN 210334397U
Authority
CN
China
Prior art keywords
groove
welding
pcd
accommodating
matching
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201920542182.3U
Other languages
Chinese (zh)
Inventor
刘文玉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Changzhou Hengchao Tool Making Co ltd
Original Assignee
Changzhou Hengchao Tool Making Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Changzhou Hengchao Tool Making Co ltd filed Critical Changzhou Hengchao Tool Making Co ltd
Priority to CN201920542182.3U priority Critical patent/CN210334397U/en
Application granted granted Critical
Publication of CN210334397U publication Critical patent/CN210334397U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model belongs to the technical field of cutting tools, in particular to a PCD welding tool with a ceramic coating, the front end of the tool body is provided with a welding groove for welding a PCD blade, the surface of the PCD blade and the front end of the tool body correspond to the joint of the PCD blade, the surface of the welding groove is provided with the ceramic coating, the position in the welding groove near the outer side is provided with an arc-shaped sunken accommodating and stopping groove, a plurality of matching grooves which are evenly distributed are arranged in the welding groove at the inner side of the accommodating and stopping groove, the depth of the accommodating and stopping groove is greater than the depth of the matching groove, the bottom end surface of the PCD blade is provided with a matching bulge corresponding to the matching groove, the position corresponding to the accommodating and stopping groove is provided with an accommodating and stopping bulge, the height of the bulge is less than the depth of the accommodating and stopping groove, the groove surface of the welding groove corresponding to the outer part of the accommodating and stopping groove is an inclined plane from the outside to the inside, the, the conditions of insufficient soldering, solder beading and the like are avoided, and the using effect of the cutter is improved.

Description

PCD welding tool with ceramic coating
Technical Field
The utility model belongs to the technical field of cutting tool, concretely relates to PCD welding cutter with ceramic coating.
Background
The PCD cutter is a polycrystalline diamond cutter, and the diamond cutter has the characteristics of high hardness, high compressive strength, good heat conductivity, good wear resistance and the like, and can obtain high processing precision and processing efficiency in high-speed cutting. In order to save cost, the PCD cutter is a split structure, and the PCD cutter is formed by welding a PCD blade on a conductor. And welding flux is arranged between the PCD blade and the cutter body, and the PCD blade and the cutter body are bonded together through the welding flux by heating.
In the current welding structure, only the cutter groove matched with the blade structure is arranged at the corresponding position on the cutter body, in the welding process, the welding flux is easy to control badly, the welding seam is not tightly controlled, the welding seam is extremely easy to be too large, even the welding seam is subjected to false welding and sheet falling, the welding strength is poor, the welding flux overflows too much to form accumulated tumors in some cases, the appearance is extremely poor, high points behind cutting edges are easy to generate, and the cutter is made to lose efficacy. This problem is exacerbated with the increasing number of forming tools available today.
SUMMERY OF THE UTILITY MODEL
The utility model aims to solve the technical problem that to above-mentioned defect, provide the PCD welding cutter that has ceramic coating, cutter intensity is good, and welding quality is good, avoids appearing the condition such as rosin joint, solder accretion, improves the result of use of cutter.
The utility model provides a technical scheme that its technical problem adopted as follows:
the PCD welding cutter with the ceramic coating comprises a cutter body and a PCD blade, wherein the front end of the cutter body is provided with a welding groove for welding the PCD blade, the surface of the PCD blade and the surface of the front end of the cutter body, which corresponds to the joint of the PCD blade, except the surface of the welding groove, are provided with the ceramic coating,
an arc-shaped sunken accommodating groove is arranged in the welding groove close to the outer side, a plurality of matching grooves which are uniformly distributed are arranged in the welding groove at the inner side of the accommodating groove, the depth of the accommodating groove is greater than that of the matching grooves,
the bottom end surface of the PCD blade is provided with a matching bulge corresponding to the matching groove and a containing stop bulge corresponding to the containing stop groove, the height of the containing stop bulge is less than the depth of the containing stop groove,
the groove surface of the welding groove corresponding to the outside of the containing groove is an inclined surface from outside to inside, and an inclined surface connecting part matched with the inclined surface structure is arranged at the position corresponding to the PCD blade.
Furthermore, the structure of the matching protrusion is matched with the structure of the matching groove, and the matching grooves are in smooth transition.
Furthermore, a communicated pore channel is arranged between the matching grooves, and one end part of the pore channel is communicated with the containing stopping groove.
Furthermore, a convex block which protrudes upwards is arranged in the accommodating groove.
Furthermore, the included angle between the inclined plane and the horizontal plane is 3-5 degrees.
The utility model has the advantages that: by adopting the scheme, the arrangement of the accommodating groove and the matching groove can improve the welding connection strength of the blade and the cutter body, can avoid the formation of accretions at welding seams by redundant welding fluxes, improves the quality of the welding seams, improves the using effect of the cutter, reduces the welding difficulty, facilitates the welding operation, and promotes the improvement of the production efficiency of the cutter.
Drawings
The foregoing and other objects, features, and advantages of the invention will be apparent from the following detailed description taken in conjunction with the accompanying drawings.
Fig. 1 is a schematic cross-sectional structure diagram of the cutter body and the PCD blade at the separation state in the embodiment of the present invention.
Fig. 2 is a schematic cross-sectional structure diagram of the cutter body and the PCD blade after being welded according to an embodiment of the present invention.
Wherein: the tool comprises a tool body 1, a welding groove 11, a containing groove 12, a matching groove 13, a pore passage 14, an inclined plane 15, a PCD blade 2, a matching bulge 21, a containing bulge 22 and an inclined plane connecting part 23.
Detailed Description
The present invention will be further explained with reference to the accompanying drawings.
Referring to fig. 1 and 2, a PCD welding tool with a ceramic coating, a tool body 1, a PCD blade 2, a welding groove 11 for welding the PCD blade 2 is arranged at the front end of the tool body 1, a ceramic coating is arranged on the surface of the welding groove at the position where the surface of the PCD blade 2 and the front end of the tool body 1 correspond to the PCD blade 2, the ceramic coating is arranged at the front end of the tool body 1 and the surface of the PCD blade 2, the hardness, the wear resistance and the lubrication effect of a cutting part are improved, the arrangement structure not only has a reinforcing effect, but also reduces the cost, it is not necessary to arrange a coating on the whole tool, a welding flux is arranged in the welding groove 11 for welding, specifically, an arc-shaped concave accommodating groove 12 is arranged at the position close to the outer side of the welding groove 11, a plurality of uniformly-distributed matching grooves 13 are arranged in the groove of the accommodating groove 11 at the inner side of the accommodating groove 12, the depth of the accommodating groove 12 is greater than the depth of the matching groove 13, the matching groove 13 is smooth transition between the matching grooves, and the groove 13, the groove is arranged, and the groove is arranged, the groove bottom of the groove 13 is provided with the groove, the groove 21, the groove is provided with the groove, the groove is provided with a groove, the groove is provided with the groove, the groove is provided with the groove.
Furthermore, an upward convex bump 121 can be disposed in the accommodating groove 12 to reduce the volume of the accommodating groove, so that the accommodating groove is fully filled with the redundant solder, thereby avoiding the occurrence of insufficient soldering and ensuring effective soldering connection.
The above is only the preferred embodiment of the present invention, not to the limitation of the present invention in any form, all the techniques of the present invention are substantially any simple modification and equivalent changes to the above embodiments, all falling within the protection scope of the present invention.

Claims (5)

1. The PCD welding cutter with the ceramic coating comprises a cutter body and a PCD blade, and is characterized in that the front end of the cutter body is provided with a welding groove for welding the PCD blade, the surface of the PCD blade and the front end of the cutter body corresponding to the joint of the PCD blade and the surface of the welding groove are provided with the ceramic coating,
an arc-shaped sunken accommodating groove is arranged in the welding groove close to the outer side, a plurality of matching grooves which are uniformly distributed are arranged in the welding groove at the inner side of the accommodating groove, the depth of the accommodating groove is greater than that of the matching grooves,
the bottom end surface of the PCD blade is provided with a matching bulge corresponding to the matching groove and a containing stop bulge corresponding to the containing stop groove, the height of the containing stop bulge is less than the depth of the containing stop groove,
the groove surface of the welding groove corresponding to the outside of the containing groove is an inclined surface from outside to inside, and an inclined surface connecting part matched with the inclined surface structure is arranged at the position corresponding to the PCD blade.
2. The ceramic coated PCD welding tool of claim 1, wherein the mating projection is configured to conform to a mating groove configuration, the mating grooves having smooth transitions therebetween.
3. The ceramic coated PCD welding tool of claim 1, wherein the mating grooves define therebetween a communicating bore, an end of the bore leading to the pocket groove.
4. A PCD welding cutter with a ceramic coating according to claim 1, characterised in that the receiving and stopping groove is provided with an upwardly protruding projection.
5. The ceramic coated PCD welding tool of claim 1, wherein the angle of the chamfer is between 3 ° and 5 ° from the horizontal.
CN201920542182.3U 2019-04-19 2019-04-19 PCD welding tool with ceramic coating Expired - Fee Related CN210334397U (en)