CN209176277U - A kind of anti-aging composite water-proof coiled material - Google Patents

A kind of anti-aging composite water-proof coiled material Download PDF

Info

Publication number
CN209176277U
CN209176277U CN201821633974.3U CN201821633974U CN209176277U CN 209176277 U CN209176277 U CN 209176277U CN 201821633974 U CN201821633974 U CN 201821633974U CN 209176277 U CN209176277 U CN 209176277U
Authority
CN
China
Prior art keywords
layer
fixedly installed
coiled material
waterproof
composite water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201821633974.3U
Other languages
Chinese (zh)
Inventor
王中刚
李红
曹廷山
崇卫红
唐军
袁学勤
孙晖
黄卫红
崔慧
王中强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu Sen Yuan Waterproof Material Ltd By Share Ltd
Original Assignee
Jiangsu Sen Yuan Waterproof Material Ltd By Share Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangsu Sen Yuan Waterproof Material Ltd By Share Ltd filed Critical Jiangsu Sen Yuan Waterproof Material Ltd By Share Ltd
Priority to CN201821633974.3U priority Critical patent/CN209176277U/en
Application granted granted Critical
Publication of CN209176277U publication Critical patent/CN209176277U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model relates to technical field of buildings, and disclose a kind of anti-aging composite water-proof coiled material, including material body, the inside of the material body is fixedly installed with wearing layer, the inside of the wearing layer is fixedly installed with abrasive rubber, and the bottom of the wearing layer is fixedly installed with waterproof layer, and the bottom of the waterproof layer is fixedly installed with elastic layer, the inside of the elastic layer is fixedly mounted elastic piece, and the bottom of the elastic layer is fixedly installed with erosion resistant coating.Wearing layer has been fixedly mounted to the inside of coiled material by setting and abrasive rubber is mounted with to wearing layer inside, achieve the effect that be hardly damaged inside coiled material in transport and installation, elastic layer has been fixedly mounted to coiled material inside by setting, reach coiled material and possesses elasticity and non-damageable effect when installing and using, erosion resistant coating has been fixedly mounted to coiled material inside by setting, the not perishable and aging after coiled material is installed is achieved the effect that, has been convenient for people to use.

Description

A kind of anti-aging composite water-proof coiled material
Technical field
The utility model relates to technical field of buildings, specially a kind of anti-aging composite water-proof coiled material.
Background technique
Coiled material refers to continuous coiled steel, is divided into coiled sheet and coiling, is a kind of rollable flexible building materials production at web-like Product are connected as ne-leakage between engineering foundation and building, are the first barriers of entire engineering waterproofing, are risen to entire engineering Vital effect.
Pitch class or high score subclass waterproof material are immersed on carcass, the waterproof material product being fabricated to, with coiled material shape Formula provides, referred to as waterproof roll, different according to main composition material, is divided into asphalt water-proof coiled material, high-polymer modified pitch waterproof Coiled material and synthetic polymeric waterproofing material.
Waterproof roll is a kind of rollable sheet waterproof material, be important species in construction engineering waterproof material it One, waterproof roll requires have good water resistance, to the stability of temperature change, certain mechanical strength, extensibility and anti-disconnected Fragility, but current waterproof roll effect in terms of anti-aging and anticorrosion is poor, when use have the defects that it is certain, therefore And propose that a kind of anti-aging composite water-proof coiled material is mentioned above to solve the problems, such as.
Utility model content
(1) the technical issues of solving
In view of the deficiencies of the prior art, the utility model provides a kind of anti-aging composite water-proof coiled material, have waterproof, The advantages that anti-aging and anticorrosion, solves the problems, such as that coiled material is non-watertight, easy to aging and perishable.
(2) technical solution
To realize above-mentioned waterproof, anti-aging and etch-proof purpose, the utility model is provided the following technical solutions: Yi Zhongkang Aging composite water-proof coiled material, including material body, the inside of the material body are fixedly installed with wearing layer, and the inside of the wearing layer is solid Dingan County is equipped with abrasive rubber, and the bottom of the wearing layer is fixedly installed with waterproof layer, and the bottom of the waterproof layer is fixedly installed with Elastic layer, the inside of the elastic layer are fixedly mounted elastic piece, and the bottom of the elastic layer is fixedly installed with erosion resistant coating, described The bottom of erosion resistant coating is fixedly installed with thermal insulation layer, and the bottom of the thermal insulation layer is fixedly installed with ductile layers, the ductile layers it is interior Flexible item is fixedly mounted in portion, and the bottom of the ductile layers is fixedly installed with damp-proof layer, and the bottom of the damp-proof layer is fixedly mounted There is conflict layer, there are two microsprings group, the opposite sides of two microsprings groups for the inside fixed installation of the material body It is fixedly installed with barrier rubber, two opposite sides of the barrier rubber are fixedly installed with seal rubber.
Preferably, the bottom for contradicting layer is fixedly installed with adhesive layer, and the bottom of the adhesive layer is coated with adhesive glue, And the bottom of adhesive glue is bonded with spacer.
Preferably, the inside of the waterproof layer is fixedly installed with waterproof membrane, and waterproof membrane is evenly distributed in waterproof layer It is internal.
Preferably, the inside of the erosion resistant coating is fixedly installed with phenolic resin piece and epoxy sheet, and erosion resistant coating is interior Portion is coated with anticorrosive paint.
Preferably, the inside of the thermal insulation layer is fixedly installed with glass fiber sheets, and the thickness of glass fiber sheets is not more than 0. 3 centimeters.
Preferably, the two sides of the microsprings group are fixedly installed with limited block, the limited block and the fixed company of material body It connects.
(3) beneficial effect
Compared with prior art, the utility model provides a kind of anti-aging composite water-proof coiled material, has following beneficial Effect:
1, by setting wearing layer has been fixedly mounted to the inside of coiled material and to resistance in the anti-aging composite water-proof coiled material Abrasive rubber is mounted with inside mill layer, has achieved the effect that be hardly damaged inside coiled material in transport and installation, passes through setting pair Waterproof layer has been fixedly mounted and waterproof membrane is mounted with to waterproof layer inside inside coiled material, water can be prevented by having reached entire coiled material The effect entered is flowed, elastic layer has been fixedly mounted to coiled material inside by setting, has reached coiled material and has possessed bullet when installing and using Property and non-damageable effect, by setting erosion resistant coating has been fixedly mounted to coiled material inside, reached coiled material installation after be not easy The effect of corrosion and aging, is convenient for people to use.
2, the anti-aging composite water-proof coiled material has been fixedly mounted thermal insulation layer to coiled material inside by setting, has reached volume By setting ductile layers have been fixedly mounted to coiled material inside and to toughness in the effect for possessing good heat-insulating capability after material installation Layer is internal to be mounted with toughness item, has reached the coiled material when installing and using and has possessed the non-damageable effect of toughness, by being arranged to volume Damp-proof layer has been fixedly mounted inside material, has achieved the effect that coiled material is not susceptible to moisture or corrosion aging when in use, by being arranged to volume Microsprings group has been fixedly mounted inside material, has achieved the effect that coiled material possesses more high tenacity.
Detailed description of the invention
FIG. 1 is a schematic structural view of the utility model;
Fig. 2 is the utility model Fig. 1 side structure schematic view;
Fig. 3 is the structural schematic diagram of A in the utility model Fig. 1.
In figure: 1 material body, 2 wearing layers, 3 waterproof layers, 4 elastic layers, 5 erosion resistant coatings, 6 thermal insulation layers, 7 ductile layers, 8 toughness items, 9 Damp-proof layer, 10 contradict layer, 11 abrasive rubbers, 12 elastic force blocks, 13 microsprings groups, 14 barrier rubber, 15 seal rubbers.
Specific embodiment
The following will be combined with the drawings in the embodiments of the present invention, carries out the technical scheme in the embodiment of the utility model Clearly and completely describe, it is clear that the described embodiments are only a part of the embodiments of the utility model, rather than whole Embodiment.Based on the embodiments of the present invention, those of ordinary skill in the art are without making creative work Every other embodiment obtained, fall within the protection scope of the utility model.
Referring to Fig. 1, a kind of anti-aging composite water-proof coiled material, including material body 1, the inside of material body 1 are fixedly installed with resistance to Layer 2 is ground, the inside of wearing layer 2 is fixedly installed with abrasive rubber 11, and the bottom of wearing layer 2 is fixedly installed with waterproof layer 3, waterproof layer 3 inside is fixedly installed with waterproof membrane, and waterproof membrane is evenly distributed in the inside of waterproof layer 3, the fixed peace in the bottom of waterproof layer 3 Equipped with elastic layer 4, the inside of elastic layer 4 is fixedly mounted elastic piece 12, and the bottom of elastic layer 4 is fixedly installed with erosion resistant coating 5, prevents The inside of rotten layer 5 is fixedly installed with phenolic resin piece and epoxy sheet, and the inside of erosion resistant coating 5 is coated with anticorrosive paint, prevents The bottom of rotten layer 5 is fixedly installed with thermal insulation layer 6, and the inside of thermal insulation layer 6 is fixedly installed with glass fiber sheets, and glass fiber sheets Thickness is not more than 0. 3 centimeters, and the bottom of thermal insulation layer 6 is fixedly installed with ductile layers 7, and the inside of ductile layers 7 is fixedly installed with tough Property item 8, the bottom of ductile layers 7 is fixedly installed with damp-proof layer 9, and the bottom of damp-proof layer 9, which is fixedly installed with, contradicts layer 10, contradicts layer 10 Bottom be fixedly installed with adhesive layer, the bottom of adhesive layer is coated with adhesive glue, and the bottom of adhesive glue is bonded with spacer, material The inside of body 1 is fixedly mounted there are two microsprings group 13, and the two sides of microsprings group 13 are fixedly installed with limited block, limits Block is fixedly connected with material body 1, and the opposite side of two microsprings groups 13 is fixedly installed with barrier rubber 14, two barrier rubbers The opposite side of glue 14 is fixedly installed with seal rubber 15.
When in use, wearing layer 2 can make coiled material possess better wearability, the waterproof inside coiled material in transport and installation Layer 3 can make coiled material possess good waterproof effect when in use, and the elastic layer 4 inside coiled material can make coiled material not rapid wear when in use Bad, the thermal insulation layer 6 inside coiled material can make coiled material possess good heat insulation, and the ductile layers 8 in coiled material can make to roll up when in use Material possesses good toughness, is hardly damaged coiled material, and the damp-proof layer 9 inside coiled material can be such that coiled material is not susceptible to moisture or corrosion when in use And aging, there is good toughness, waterproofness and anti-corrosion moisture resistance when being entirely provided at use.
In conclusion the anti-aging composite water-proof coiled material, has been fixedly mounted wearing layer 2 to the inside of coiled material by setting And to abrasive rubber 11 is mounted with inside wearing layer 2, achieved the effect that be hardly damaged inside coiled material in transport and installation, Waterproof layer 3 has been fixedly mounted to coiled material inside by setting and to waterproof membrane is mounted with inside waterproof layer 3, has reached entire volume The effect that material can prevent water flow from entering has been fixedly mounted elastic layer 4 to coiled material inside by setting, has reached coiled material and installed Possess elasticity and non-damageable effect when use, erosion resistant coating 5 has been fixedly mounted to coiled material inside by setting, has reached and has rolled up Not perishable and aging effect, is convenient for people to use after material installation.
Also, by setting thermal insulation layer 6 has been fixedly mounted to coiled material inside, reached coiled material installation after possess it is good every Ductile layers 7 have been fixedly mounted to coiled material inside by setting and to being mounted with toughness item inside ductile layers 7 in the effect of thermal energy power 8, reach the coiled material when installing and using and possessed the non-damageable effect of toughness, coiled material inside has been fixedly mounted by setting anti- Damp layer 9, has achieved the effect that coiled material is not susceptible to moisture or corrosion aging when in use, coiled material inside has been fixedly mounted by setting micro- Type groups of springs 13 has achieved the effect that coiled material possesses more high tenacity.
It should be noted that the terms "include", "comprise" or its any other variant are intended to the packet of nonexcludability Contain, so that the process, method, article or equipment for including a series of elements not only includes those elements, but also including Other elements that are not explicitly listed, or further include for elements inherent to such a process, method, article, or device. In the absence of more restrictions, the element limited by sentence "including a ...", it is not excluded that including the element Process, method, article or equipment in there is also other identical elements.
While there has been shown and described that the embodiments of the present invention, for the ordinary skill in the art, It is understood that these embodiments can be carried out with a variety of variations in the case where not departing from the principles of the present invention and spirit, repaired Change, replacement and variant, the scope of the utility model is defined by the appended claims and the equivalents thereof.

Claims (6)

1. a kind of anti-aging composite water-proof coiled material, including material body (1), it is characterised in that: the fixed peace in the inside of the material body (1) Equipped with wearing layer (2), the inside of the wearing layer (2) is fixedly installed with abrasive rubber (11), and the bottom of the wearing layer (2) is solid Dingan County is equipped with waterproof layer (3), and the bottom of the waterproof layer (3) is fixedly installed with elastic layer (4), the inside of the elastic layer (4) It is fixedly mounted elastic piece (12), the bottom of the elastic layer (4) is fixedly installed with erosion resistant coating (5), the bottom of the erosion resistant coating (5) Portion is fixedly installed with thermal insulation layer (6), and the bottom of the thermal insulation layer (6) is fixedly installed with ductile layers (7), the ductile layers (7) Flexible item (8) are fixedly mounted in inside, and the bottom of the ductile layers (7) is fixedly installed with damp-proof layer (9), the damp-proof layer (9) Bottom be fixedly installed with and contradict layer (10), the inside of the material body (1) is fixedly mounted there are two microsprings group (13), two The opposite side of the microsprings group (13) is fixedly installed with barrier rubber (14), and two barrier rubber (14) are opposite Side be fixedly installed with seal rubber (15).
2. a kind of anti-aging composite water-proof coiled material according to claim 1, it is characterised in that: conflict layer (10) Bottom is fixedly installed with adhesive layer, and the bottom of the adhesive layer is coated with adhesive glue, and the bottom of adhesive glue is bonded with spacer.
3. a kind of anti-aging composite water-proof coiled material according to claim 1, it is characterised in that: the waterproof layer (3) Inside is fixedly installed with waterproof membrane, and waterproof membrane is evenly distributed in the inside of waterproof layer (3).
4. a kind of anti-aging composite water-proof coiled material according to claim 1, it is characterised in that: the erosion resistant coating (5) Inside is fixedly installed with phenolic resin piece and epoxy sheet, and the inside of erosion resistant coating (5) is coated with anticorrosive paint.
5. a kind of anti-aging composite water-proof coiled material according to claim 1, it is characterised in that: the thermal insulation layer (6) Inside is fixedly installed with glass fiber sheets, and the thickness of glass fiber sheets is not more than 0. 3 centimeters.
6. a kind of anti-aging composite water-proof coiled material according to claim 1, it is characterised in that: the microsprings group (13) two sides are fixedly installed with limited block, and the limited block is fixedly connected with material body.
CN201821633974.3U 2018-10-09 2018-10-09 A kind of anti-aging composite water-proof coiled material Expired - Fee Related CN209176277U (en)