CN203680776U - 一种唇口加厚型口型板 - Google Patents
一种唇口加厚型口型板 Download PDFInfo
- Publication number
- CN203680776U CN203680776U CN201420036249.3U CN201420036249U CN203680776U CN 203680776 U CN203680776 U CN 203680776U CN 201420036249 U CN201420036249 U CN 201420036249U CN 203680776 U CN203680776 U CN 203680776U
- Authority
- CN
- China
- Prior art keywords
- mouth
- shaped plate
- die panel
- lip
- treads
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种唇口加厚型口型板,具体涉及一种用于轮胎行业防止挤出胎面脱层的唇口加厚型口型板。要解决的技术问题是目前轮胎挤出胎面易脱层,在使用过程中易发生肩空的现象,员工的劳动强度大,本实用新型包括口型板I,口型板I上设有唇口I,在口型板I的一侧设置口型板II,口型板II的上设有唇口II,唇口I和唇口II相互对接连通。采用这样的结构后的本实用新型可以有效解决挤出胎面脱层问题,胎面合格率明显提升,胎面重量波动减小,员工劳动强度降低,消除了因挤出胎面脱层带来轮胎在使用过程中发生肩空现象的隐患。
Description
技术领域
本实用新型涉及一种口型板,具体涉及一种用于轮胎行业防止挤出胎面脱层的唇口加厚型口型板。
背景技术
轮胎行业内经常发生一种产品质量缺陷就是挤出胎面脱层,并带来轮胎在使用过程中发生肩空的现象。目前全钢载重子午线轮胎胎面主要有两种类型:单胶型胎面和复合型胎面,其中复合型胎面又分为两种类型:翼胶型胎面和通底层型胎面;在生产复合型胎面时,胎冠胶与基部胶容易出现脱层,造成胎面返回量大,胎面重量波动大,并且会导致轮胎在使用过程中发生肩空现象。复合型胎面中通底层胎面脱层最严重,脱层比例达到90%以上,其次是翼胶型胎面,其脱层比例达到60%以上。在目前行业内轮胎生产工艺中,如图1和图2所示,口型板1上设置唇口2的厚度为15mm~23mm之间不等,胶料在口型板型腔中停留时间短,胎冠胶与基部胶粘合面间的接触时间短,胎面在出型时膨胀量大,这样形成了胎面易脱层,为了降低胎面脱层率,需要员工在胎面肩部手动不停的扎眼,员工的劳动强度大。
发明内容
本实用新型要解决的技术问题是轮胎挤出胎面易脱层,在使用过程中易发生肩空的现象,员工的劳动强度大,提供一种避免胎面脱层,员工的劳动强度低的唇口加厚型口型板。
为实现上述目的,本实用新型采用下述技术方案:一种唇口加厚型口型板,包括口型板I,口型板I上设有唇口I,在口型板I的一侧设置口型板II,口型板II的上设有唇口II,唇口I和唇口II相互对接连通。
所述的口型板I的厚度为15~23mm。
所述的口型板II的厚度是口型板I的厚度的0.8-1.2倍。
所述的口型板II的厚度是口型板I的厚度的1倍。
本实用新型加工方法简单、实用、便捷,应用前景好。使用此新型的唇口加厚型样板,可以有效解决挤出胎面脱层问题,胎面合格率明显提升,胎面重量波动减小,员工劳动强度降低,消除了因挤出胎面脱层带来轮胎在使用过程中发生肩空现象的隐患。
附图说明
图1是现有技术结构示意图。
图2是图1的A-A剖视结构示意图。
图3是本实用新型结构示意图。
图4是图3的A-A向剖视图。
具体实施方式
如图3至图4所示,本实用新型包括口型板I1,口型板I1上设有唇口I2,在口型板I1的一侧设置口型板II3,口型板II3的上设有唇口II4,唇口I2和唇口II4相互对接连通。唇口I2和唇口II4的内腔形成口型板型腔,口型板II3设置在口型板I1的出口面,增加口型板型腔的有效厚度。
所述的口型板I1的厚度为15~23mm。口型板I1的厚度可以是15 mm、17 mm、19 mm、20 mm、22 mm、23 mm。
所述的口型板II3的厚度是口型板I1的厚度的0.8-1.2倍。所述的口型板II3的厚度是口型板I1的厚度的1倍。也可以是0.8倍、0.9倍、1.0倍、1.1倍、1.2倍。
在生产胎面时,沿胎面厚度方向上会出现膨胀现象,胎面离开口型板型腔的一瞬间,胎面的膨胀度要比胎面在口型板型腔内的膨胀度要大很多,只有延长胎面在口型板型腔内的停留时间,才能最大幅度的降低整个胎面的膨胀度、延长粘合面分子间相互渗透的时间、改善粘合面分子间的相互渗透效果,达到彻底解决复合型胎面脱层的目的。延长胎面在口型板型腔内停留时间的方法是:在口型板出口面增加口型板型腔的有效厚度,即给在口型板I1上增加一个口型板II3,扩大口型板型腔的有效厚度。当口型板型腔的有效厚度过少时,胎冠胶与基部胶在口型板型腔中的接触时间少,不能有效地降低整个胎面的膨胀量,粘合面分子间相互渗透的时间不足、粘合面分子间相互渗透的效果不好,不能彻底的解决复合型胎面脱层。当口型板型腔的有效厚度过大时,出现挤出机挤出压力过大,造成胎面基部胶边部破边的现象。只有当口型板II3的厚度是口型板I1的厚度的0.8-1.2倍时,尤其是口型板II3的厚度是口型板I1的厚度的1倍时,整个胎面的膨胀度达到最小,粘合面分子间相互渗透的时间也充足、粘合面分子间相互渗透的效果达到最好,彻底解决复合型胎面脱层。
Claims (4)
1.一种唇口加厚型口型板,包括口型板I(1),口型板I(1)上设有唇口I(2),其特征在于:在口型板I(1)的一侧设置口型板II(3),口型板II(3)的上设有唇口II(4),唇口I(2)和唇口II(4)相互对接连通。
2.根据权利要求1所述的唇口加厚型口型板,其特征在于:所述的口型板I(1)的厚度为15~23mm。
3.根据权利要求2所述的唇口加厚型口型板,其特征在于:所述的口型板II(3)的厚度是口型板I(1)的厚度的0.8-1.2倍。
4.根据权利要求3所述的唇口加厚型口型板,其特征在于:所述的口型板II(3)的厚度是口型板I(1)的厚度的1倍。