CN202702735U - Composite film for scratch-retardant and explosion-proof glass - Google Patents
Composite film for scratch-retardant and explosion-proof glass Download PDFInfo
- Publication number
- CN202702735U CN202702735U CN 201220330727 CN201220330727U CN202702735U CN 202702735 U CN202702735 U CN 202702735U CN 201220330727 CN201220330727 CN 201220330727 CN 201220330727 U CN201220330727 U CN 201220330727U CN 202702735 U CN202702735 U CN 202702735U
- Authority
- CN
- China
- Prior art keywords
- layer
- base material
- polyethylene base
- film
- material film
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
The utility model discloses a composite film for a scratch-retardant and explosion-proof glass; and the composite film comprises a first polyethylene base material film and a second polyethylene base material film, wherein the upper surface of the first polyethylene base material film is plated with a metal layer; the lower surface of the second polyethylene base material film is coated with an antistatic agent coating; a plastic isolating layer is fixed on the other surface of the metal layer of the first polyethylene base material film; the antistatic agent coating is bonded with the plastic isolating layer by an adhesive layer; the upper surface of the second polyethylene base material film is coated with a scratch-retardant and wear resistant layer; the lower surface of the first polyethylene base material film is provided with a pressure-sensitive adhesive layer; the other surface of the pressure-sensitive adhesive layer is laminated with a parting material layer; the other surface of the pressure-sensitive adhesive layer is laminated with the parting material layer; and the parting material layer is a parting paper layer or a parting film layer. The composite film for the scratch-retardant and explosion-proof glass, disclosed by the utility model, is beneficial for reflecting and blocking solar rays and infrared rays of visible lights and has an obvious heat insulation effect; an electroplating metal layer can be preferably protected, metal oxidation is prevented and the service life of a product is prolonged; therefore, the composite film for the scratch-retardant and explosion-proof glass, disclosed by the utility model, can be suitable for places with higher requirements.
Description
Technical field
The utility model relates to a kind of diaphragm, relates in particular to a kind of scratch resistant implosion guard composite film-stuck.
Background technology
The products such as glass, sheet metal, plastic plate and electronic product are in carrying and use procedure, and its table and be subject to easily contact staining or polishing scratch and scratch usually adopts diaphragm to cover its surface and makes it to avoid damage and pollute.Diaphragm generally is made of substrate layer and the adhesive layer that is coated on this substrate layer; the prior art diaphragm; often adopt the common polythene base film as substrate layer; because polyethylene base material film is high molecular polymer; its dielectric constant is little, belongs to non-conductor, and insulating properties are higher; therefore, the generation of static is unescapable.When traditional diaphragm is applied to electron trade, adsorb easily dust and impurity, even generation static causes heavy losses.And those skilled in the art fail to give enough attention on antioxygenic property, therefore, how to prevent burning, have improved the life-span that produces, to be applicable to requiring higher place also to become the direction that those of ordinary skills make great efforts.
Summary of the invention
The utility model provides a kind of scratch resistant implosion guard composite film-stuck; this scratch resistant implosion guard both had been conducive to reflect and intercept the infrared ray of sunray and visible light with composite film-stuck; effect of heat insulation is remarkable; can better protect electroplated metal layer again; prevent burning; improved the life-span of product, thereby applicable to requiring higher place.
For achieving the above object, the technical solution adopted in the utility model is: a kind of scratch resistant implosion guard composite film-stuck, comprise the first polyethylene base material film of the metal-coated layer of upper surface and the second polyethylene base material film that lower surface is coated with the antistatic additive coating, one plastic partition absciss layer is fixed in another surface of metal level of described the first polyethylene base material film, described antistatic additive coating and plastic partition absciss layer are bonding by an adhesive-layer, and described the second polyethylene base material film upper surface is coated with an anti-scratch wearing layer; Described the first polyethylene base material film lower surface has a pressure-sensitive adhesive layer, and another surface label of this pressure-sensitive adhesive layer is covered with the separated type material layer.
Further improved technical scheme is as follows in the technique scheme:
In the such scheme, described separated type material layer is off-style paper layer or release film layer.
Because technique scheme is used, the utility model compared with prior art has following advantages:
Scratch resistant implosion guard composite film-stuck in the utility model; metal level upper surface at the first polyethylene base material film has a plastic partition absciss layer; the infrared ray that both had been conducive to electroplated metal layer reflection and obstruct sunray and visible light; effect of heat insulation is remarkable; can better protect electroplated metal layer again; prevent burning, improved the life-span of product, thereby applicable to requiring higher place.
Description of drawings
Accompanying drawing 1 is the scratch resistant implosion guard of the utility model composite film-stuck structural representation.
In the above accompanying drawing: 1, metal level; 2, the first polyethylene base material film; 3, the second polyethylene base material film; 4, adhesive-layer; 5, antistatic additive coating; 6, pressure-sensitive adhesive layer; 7, separated type material layer; 8, anti-scratching wearproof layer; 9, plastic partition absciss layer.
The specific embodiment
Below in conjunction with drawings and Examples the utility model is further described:
Embodiment: a kind of scratch resistant implosion guard composite film-stuck, comprise the first polyethylene base material film 2 of the metal-coated layer 1 of upper surface and the second polyethylene base material film 3 that lower surface is coated with antistatic additive coating 5, one plastic partition absciss layer 9 is fixed in metal level 1 another surface of described the first polyethylene base material film 2, bonding by an adhesive-layer 4 between described antistatic additive coating 5 and the plastic partition absciss layer 9, described the second polyethylene base material film 3 upper surfaces are coated with an anti-scratch wearing layer 8; Described the first polyethylene base material film 2 lower surfaces have a pressure-sensitive adhesive layer 6, and these pressure-sensitive adhesive layer 6 another surface labels are covered with separated type material layer 7.
Above-mentioned separated type material layer 7 is off-style paper layer or release film layer.
When adopting above-mentioned scratch resistant implosion guard to use composite film-stuck; metal level upper surface at the first polyethylene base material film has a plastic partition absciss layer; the infrared ray that both had been conducive to electroplated metal layer reflection and obstruct sunray and visible light; effect of heat insulation is remarkable; can better protect electroplated metal layer again; prevent burning, improved the life-span of product, thereby applicable to requiring higher place.
Above-described embodiment only is explanation technical conceive of the present utility model and characteristics, and its purpose is to allow the personage who is familiar with technique can understand content of the present utility model and according to this enforcement, can not limit protection domain of the present utility model with this.All equivalences of doing according to the utility model Spirit Essence change or modify, and all should be encompassed within the protection domain of the present utility model.
Claims (2)
1. scratch resistant implosion guard composite film-stuck, it is characterized in that: comprise the first polyethylene base material film (2) of the metal-coated layer of upper surface (1) and the second polyethylene base material film (3) that lower surface is coated with antistatic additive coating (5), one plastic partition absciss layer (9) is fixed in described first another surface of polyethylene base material film (2) metal level (1), bonding by an adhesive-layer (4) between described antistatic additive coating (5) and the plastic partition absciss layer (9), described the second polyethylene base material film (3) upper surface is coated with an anti-scratch wearing layer (8); Described the first polyethylene base material film (2) lower surface has a pressure-sensitive adhesive layer (6), and another surface label of this pressure-sensitive adhesive layer (6) is covered with separated type material layer (7).
2. scratch resistant implosion guard composite film-stuck according to claim 1, it is characterized in that: described separated type material layer (7) is off-style paper layer or release film layer.