CN202584851U - 一种自粘漆包线 - Google Patents
一种自粘漆包线 Download PDFInfo
- Publication number
- CN202584851U CN202584851U CN 201220262732 CN201220262732U CN202584851U CN 202584851 U CN202584851 U CN 202584851U CN 201220262732 CN201220262732 CN 201220262732 CN 201220262732 U CN201220262732 U CN 201220262732U CN 202584851 U CN202584851 U CN 202584851U
- Authority
- CN
- China
- Prior art keywords
- self
- enamelled coating
- enameled wire
- adhesion
- polyurethane
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种自粘漆包线,包括金属线芯、以及位于该金属线芯外的绝缘漆层,所述绝缘漆层外涂覆有自粘漆层。本实用新型的有益效果在于:由于在绝缘漆层外设置有自粘漆层,从而使得本实用新型具有良好的粘结性能,无需浸漆粘合,简化工艺,降低成本。
Description
(一)技术领域
本实用新型涉及一种自粘漆包线。
(二)背景技术
目前,在漆包线的生产领域中,由纯铜材料作为漆包线的导体芯,然后在导体芯的外面涂覆一层漆膜作为绝缘层。这种漆包线,没有粘合层,因而不具有自粘性能,线圈成型不好,易松散,整体机械强度低。因此,这种漆包线在制作成绕组或者线圈成型后,还需要经过浸漆粘合、烧烤等工序,制作工艺比较复杂,成本高。
(三)发明内容
为了克服现有技术中存在上述的不足,本实用新型提供一种结构简单、成本低、并带有自粘漆层的自粘漆包线。
本实用新型解决其技术问题的技术方案是:一种自粘漆包线,包括金属线芯、以及位于该金属线芯外的绝缘漆层,所述绝缘漆层外涂覆有自粘漆层。
进一步,所述自粘漆层为热熔型的自粘漆层,通过通电加热,能够使漆包线成型;或者,所述自粘漆层为酒精型的自粘漆层,通过溶剂溶液的浸泡,能够使漆包线成型。
进一步,所述绝缘漆层为聚氨酯漆层,聚氨酯漆层使得本实用新型具有直焊性,当需要焊接时,无需刮去聚氨酯漆层,可直接将本实用新型安置于所要焊接部位进行焊接。聚氨酯漆层还具有耐高频的特性,在高频环境下,聚氨酯漆层的介质损耗很低。另外,聚氨酯涂层里还可以混入各种染料,可以使得漆包线呈现各种各样的颜色,使得本实用新型在工作时便于辨别不同线的功能和用途。
进一步,所述聚氨酯漆层具有八层,使得聚氨酯漆层的厚度适中,可防漏电,绝缘效果更好。
本实用新型的有益效果在于:由于在绝缘漆层外设置有自粘漆层,从而使得本实用新型具有良好的粘结性能,无需浸漆粘合,简化工艺,降低成本。
(四)附图说明
图1是本实用新型的截面示意图。
(五)具体实施方式
下面结合附图和具体实施方式对本实用新型作进一步详细说明。
参照图1,一种自粘漆包线,包括金属线芯1、以及位于该金属线芯1外的绝缘漆层2,所述绝缘漆层2外涂覆有自粘漆层3。
所述自粘漆层3为热熔型的自粘漆层,通过通电加热,能够使漆包线成型;或者,所述自粘漆层3为酒精型的自粘漆层,通过溶剂溶液的浸泡,能够使漆包线成型。
本实用新型由于在绝缘漆层2外设置有自粘漆层3,从而使得本实用新型具有良好的粘结性能,无需浸漆粘合,简化工艺,降低成本。
所述绝缘漆层2为聚氨酯漆层,聚氨酯漆层使得本实用新型具有直焊性,当需要焊接时,无需刮去聚氨酯漆层,可直接将本实用新型安置于所要焊接部位进行焊接。聚氨酯漆层还具有耐高频的特性,在高频环境下,聚氨酯漆层的介质损耗很低。另外,聚氨酯涂层里还可以混入各种染料,可以使得漆包线呈现各种各样的颜色,使得本实用新型在工作时便于辨别不同线的功能和用途。
所述聚氨酯漆层具有八层,使得聚氨酯漆层的厚度适中,可防漏电,绝缘效果更好。
Claims (5)
1.一种自粘漆包线,包括金属线芯、以及位于该金属线芯外的绝缘漆层,其特征在于:所述绝缘漆层外涂覆有自粘漆层。
2.按照权利要求1所述的自粘漆包线,其特征在于:所述自粘漆层为热熔型的自粘漆层。
3.按照权利要求1所述的自粘漆包线,其特征在于:所述自粘漆层为酒精型的自粘漆层。
4.按照权利要求1~3中任一项所述的自粘漆包线,其特征在于:所述绝缘漆层为聚氨酯漆层。
5.按照权利要求4所述的自粘漆包线,其特征在于:所述聚氨酯漆层具有八层。