CN202573201U - 一种透明聚偏氟乙烯/聚甲基丙烯酸甲酯共挤片材 - Google Patents
一种透明聚偏氟乙烯/聚甲基丙烯酸甲酯共挤片材 Download PDFInfo
- Publication number
- CN202573201U CN202573201U CN 201220250523 CN201220250523U CN202573201U CN 202573201 U CN202573201 U CN 202573201U CN 201220250523 CN201220250523 CN 201220250523 CN 201220250523 U CN201220250523 U CN 201220250523U CN 202573201 U CN202573201 U CN 202573201U
- Authority
- CN
- China
- Prior art keywords
- pmma
- pvdf
- polymethyl methacrylate
- transparent
- sheet
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种建筑场馆中应用的透明片材,特别是一种透明聚偏氟乙烯(PVDF)/聚甲基丙烯酸甲酯(PMMA)共挤片材,主要是为了解决传统PMMA片材材料耐候性不足,容易出现开裂等问题。技术方案是由两台挤出机在一定温度下分别加热熔化PVDF和PMMA原料,然后经过共挤和冷却定型,获得PVDF/PMMA共挤片材,由于PVDF层的耐候性和耐腐蚀性等均优于PMMA层,所以能够提高片材的使用寿命和降低后期维护成本。
Description
技术领域
本实用新型涉及一种建筑场馆中应用的透明片材,特别是一种透明聚偏氟乙烯(PVDF)/聚甲基丙烯酸甲酯(PMMA)共挤片材。
背景技术
PMMA片材因为具有良好的透明性,所以被广泛用于制作透明塑料窗,替代普通玻璃,应用于大型体育场馆、车站顶棚等建筑。但是,PMMA的耐候性不能满足建筑行业的需要。另外随着环境的恶化,酸雨等污染不断加剧,PMMA的抗酸雨腐蚀等性能也不够理想,在长期使用过程中,会出现片材开裂、腐蚀变形、透明性下降等问题。
发明内容
本实用新型的目的是提供一种透明聚偏氟乙烯/聚甲基丙烯酸甲酯共挤片材,与传统的PMMA片材材料相比,其耐候性和抗腐蚀性显著提高。本实用新型的加工成型工艺简单,一次共挤出成型,生产效率高。
附图说明
图1为本实用新型一种透明PVDF/PMMA共挤片材的局部剖视示意图。
图中:1-PMMA层 2-PVDF层
具体实施方式
下面结合附图和具体实施方式对本实用新型作进一步的说明。
本实用新型涉及的一种透明聚偏氟乙烯/聚甲基丙烯酸甲酯共挤片材,由两台挤出机在一定温度下分别加热熔化PVDF和PMMA原料,然后经过共挤口模,将已经熔化的PMMA层1和PVDF层2一起挤出,再通过冷却辊对片材进行冷却定型,挤出机加热温度为200-240℃,冷却辊温度为20-30℃。整个生产过程严格控制温度,以确保PMMA层1和PVDF层2紧密结合。
Claims (3)
1.一种透明聚偏氟乙烯/聚甲基丙烯酸甲酯共挤片材,其特征在于,所述片材包括聚偏氟乙烯层和聚甲基丙烯酸甲酯层。
2.如权利要求1所述的一种透明聚偏氟乙烯/聚甲基丙烯酸甲酯共挤片材,其特征在于,所述聚偏氟乙烯层厚度为0.01mm到0.05mm。
3.如权利要求1所述的一种透明聚偏氟乙烯/聚甲基丙烯酸甲酯共挤片材,其特征在于,所述聚甲基丙烯酸甲酯层厚度为0.5mm到1.0mm。