CN202280962U - 煤化工黑水闪蒸罐阀门管口耐磨管 - Google Patents

煤化工黑水闪蒸罐阀门管口耐磨管 Download PDF

Info

Publication number
CN202280962U
CN202280962U CN2011203178686U CN201120317868U CN202280962U CN 202280962 U CN202280962 U CN 202280962U CN 2011203178686 U CN2011203178686 U CN 2011203178686U CN 201120317868 U CN201120317868 U CN 201120317868U CN 202280962 U CN202280962 U CN 202280962U
Authority
CN
China
Prior art keywords
pipe
wear
chemical industry
layer
black water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2011203178686U
Other languages
English (en)
Inventor
马东海
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2011203178686U priority Critical patent/CN202280962U/zh
Application granted granted Critical
Publication of CN202280962U publication Critical patent/CN202280962U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种煤化工黑水闪蒸罐阀门管口耐磨管,包括硬质合金外层,所述硬质合金外层的内壁上设有抗气蚀层。所述硬质合金外层和抗气蚀层的厚度均为10mm。本实用新型的煤化工黑水闪蒸罐阀门管口耐磨管采用双层结构,外层为硬质合金层,内层为抗气蚀层,能够很好的解决管道磨损、腐蚀、气蚀三种问题,并且价格低,结构简单,使用寿命长。

Description

煤化工黑水闪蒸罐阀门管口耐磨管
技术领域
本实用新型涉及一种煤化工黑水闪蒸罐阀门管口耐磨管。
背景技术
目前在煤化工黑水闪蒸罐阀门管口上经常要使用输送管道,在输送管道中运送的介质主要是黑水,由于黑水中含有固体颗粒,粒径小于等于63微米,颗粒主要包含煤尘、渣粒,PH为6呈弱酸性;煤尘的硬度2.5-3.5,渣粒硬度为6.0;而黑水压力为阀前压力4.0MPa(g),阀后常压,温度为闪蒸前215℃,闪蒸后95℃,磨蚀处介质流速大于600m/s,磨蚀处管径及减压阀后高速水流冲刷磨损输送管道,输送管道损耗很快,其损耗因素主要为:磨损、腐蚀、气蚀。现有的输送管道采用不锈钢或硬质合金,不锈钢材料耐磨损性能差,10mm厚的不锈钢10天时间便磨穿,造成生产停工,硬质合金硬度高,但抗气蚀能力弱,且造价成本高,20mm厚的硬质合金使用寿命也仅有60天,给企业生产带来极大的不便。
实用新型内容
为解决上述技术问题,本实用新型提供一种结构简单、使用寿命长的煤化工黑水闪蒸罐阀门管口耐磨管。
本实用新型的煤化工黑水闪蒸罐阀门管口耐磨管,包括硬质合金外层,所述硬质合金外层的内壁上设有抗气蚀层。
本实用新型的煤化工黑水闪蒸罐阀门管口耐磨管,所述硬质合金外层和抗气蚀层的厚度均为10mm。
与现有技术相比本实用新型的有益效果为:本实用新型的煤化工黑水闪蒸罐阀门管口耐磨管采用双层结构,外层为硬质合金层,内层为抗气蚀层,能够很好的解决管道磨损、腐蚀、气蚀三种问题,并且价格低,结构简单,使用寿命长。
附图说明
图1是本实用新型实施例所述的煤化工黑水闪蒸罐阀门管口耐磨管的结构示意图。
图中:
1、硬质合金外层;2、抗气蚀层。
具体实施方式
下面结合附图和实施例,对本实用新型的具体实施方式作进一步详细描述。以下实施例用于说明本实用新型,但不用来限制本实用新型的范围。
如图1所示,一种煤化工黑水闪蒸罐阀门管口耐磨管,包括硬质合金外层1,所述硬质合金外层1的内壁上设有抗气蚀层2。
本实用新型的煤化工黑水闪蒸罐阀门管口耐磨管,所述硬质合金外层1和抗气蚀层2的厚度均为10mm。
本实用新型的煤化工黑水闪蒸罐阀门管口耐磨管采用双层结构,外层为硬质合金层,内层为抗气蚀层,能够很好的解决管道磨损、腐蚀、气蚀三种问题,并且价格低,结构简单,使用寿命长。
以上所述仅是本实用新型的优选实施方式,应当指出,对于本技术领域的普通技术人员来说,在不脱离本实用新型技术原理的前提下,还可以做出若干改进和变型,这些改进和变型也应视为本实用新型的保护范围。

Claims (2)

1.一种煤化工黑水闪蒸罐阀门管口耐磨管,包括硬质合金外层(1),其特征在于:所述硬质合金外层(1)的内壁上设有抗气蚀层(2)。
2.根据权利要求1所述的煤化工黑水闪蒸罐阀门管口耐磨管,其特征在于:所述硬质合金外层(1)和抗气蚀层(2)的厚度均为10mm。
CN2011203178686U 2011-08-29 2011-08-29 煤化工黑水闪蒸罐阀门管口耐磨管 Expired - Fee Related CN202280962U (zh)