CN201895180U - 节能环保型电焊条 - Google Patents
节能环保型电焊条 Download PDFInfo
- Publication number
- CN201895180U CN201895180U CN2010206338324U CN201020633832U CN201895180U CN 201895180 U CN201895180 U CN 201895180U CN 2010206338324 U CN2010206338324 U CN 2010206338324U CN 201020633832 U CN201020633832 U CN 201020633832U CN 201895180 U CN201895180 U CN 201895180U
- Authority
- CN
- China
- Prior art keywords
- electrode
- steel core
- coating
- periphery
- welding
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种节能环保型电焊条,它包括有钢芯、药皮,药皮设在钢芯的***,所述药皮的***还设有金属粉胶合层,焊条的夹持端的截面为多边形结构,其特征在于:所述夹持端的钢芯的端面上设有螺孔,另一端设有与螺孔相配合的连接螺杆,所述连接螺杆是由钢芯以及钢芯***的药皮构成。由于焊条的夹持端为方形结构,大大增强了电焊钳对焊条夹持的牢固性;由于增设了金属粉胶合层,焊接时,不用更换焊条,便可对铜、锌等材料进行焊接,简化操作,提高了工作效率和扩大了应用范围;本实用新型的最大特点是焊条的夹持部分,没有被扔掉,而是连接在新装上的节能环保型电焊条的连接螺杆上,从而使焊接材料得到了充分的利用,避免了浪费。
Description
技术领域
本实用新型涉及一种节能环保的电焊条。
背景技术
传统的节能环保型电焊条的夹持端都是圆柱形结构,在使用过程中,电焊机的电焊钳对焊条的夹持不够牢固,焊接时,如果焊条发生了偏移,就需要停止工作,对焊条重新进行夹持,故会影响其工作效率。
另外传统的焊条是由钢芯和药皮构成,这种结构的焊条,如果需要焊接铜、锌等材料时,需要更换焊条,故操作费时费力。
目前所使用的节能环保型电焊条,最大的缺点,节能环保型电焊条的夹持部分没有得到利用,而是当作废弃物给扔掉了,大大浪费了焊接材料,不能满足节能环保的要求。
发明内容
为了克服上述之不足,本实用新型的目的在于提供一种便于夹持、应用范围广的节能环保型电焊条。
为解决上述技术问题,本实用新型所采用的技术方案是:
节能环保型电焊条,包括有钢芯、药皮,药皮设在钢芯的***,所述药皮的***还设有金属粉胶合层,焊条的夹持端的截面为多边形结构,其特征在于:所述夹持端的钢芯的端面上设有螺孔,另一端设有与螺孔相配合的连接螺杆,所述连接螺杆是由钢芯以及钢芯***的药皮构成。
所述焊条的夹持端的截面为四边形结构。
本实用新型的有益效果在于:由于焊条的夹持端为方形结构,大大增强了电焊钳对焊条夹持的牢固性;由于增设了金属粉胶合层,焊接时,不用更换焊条,便可对铜、锌等材料进行焊接,简化操作,提高了工作效率和扩大了应用范围;本实用新型的最大特点是焊条的夹持部分,没有被扔掉,而是连接在新装上的节能环保型电焊条的连接螺杆上,从而使焊接材料得到了充分的利用,避免了浪费。
附图说明
下面结合附图和具体实施方式对本实用新型作进一步详细说明:
图1为本实用新型的结构示意图。
图中:1、钢芯;2、药皮;3、金属粉胶合层;4、夹持端;5、螺孔;6、连接螺杆。
具体实施方式
如图1所示,节能环保型电焊条,包括有钢芯1、药皮2,药皮2设在钢芯1的***,所述药皮2的***还设有金属粉胶合层3,焊条的夹持端的截面为多边形结构,其特征在于:所述夹持端的钢芯1的端面上设有螺孔5,另一端设有与螺孔5相配合的连接螺杆6,所述连接螺杆6是由钢芯以及钢芯***的药皮构成。所述焊条的夹持端4的截面为四边形结构。
金属粉胶合层3是由铜粉、锌粉和钢粉等按一定比例配制而成,焊接时可根据需要调整电流,对铜、锌等材料进行焊接,也就是说在焊接的过程中,对局部的铜材质等部件焊接时,就很方便,不用更换焊条,简化操作,提高了焊接的效率。
使用的过程中,当焊条用完后,所剩下的夹持部分,没有被扔掉,而是连接在新装上的节能环保型电焊条的连接螺杆上,从而使焊接材料得到了充分的利用,避免了浪费。
Claims (2)
1.一种节能环保型电焊条,包括有钢芯(1)、药皮(2),药皮(2)设在钢芯(1)的***,所述药皮(2)的***还设有金属粉胶合层(3),焊条的夹持端的截面为多边形结构,其特征在于:所述夹持端的钢芯(1)的端面上设有螺孔(5),另一端设有与螺孔(5)相配合的连接螺杆(6),所述连接螺杆(6)是由钢芯以及钢芯***的药皮构成。
2.根据权利要求1所述的节能环保型电焊条,其特征在于:所述焊条的夹持端(4)的截面为四边形结构。