CN201825848U - 高硼硅厚板平拉玻璃供料道结构 - Google Patents

高硼硅厚板平拉玻璃供料道结构 Download PDF

Info

Publication number
CN201825848U
CN201825848U CN201020555467XU CN201020555467U CN201825848U CN 201825848 U CN201825848 U CN 201825848U CN 201020555467X U CN201020555467X U CN 201020555467XU CN 201020555467 U CN201020555467 U CN 201020555467U CN 201825848 U CN201825848 U CN 201825848U
Authority
CN
China
Prior art keywords
glass
high borosilicate
forehearth
thick
plate horizontally
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201020555467XU
Other languages
English (en)
Inventor
朱彦武
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
QINHUANGDAO CITY HENGYAN GLASS CO Ltd
Original Assignee
QINHUANGDAO CITY HENGYAN GLASS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by QINHUANGDAO CITY HENGYAN GLASS CO Ltd filed Critical QINHUANGDAO CITY HENGYAN GLASS CO Ltd
Priority to CN201020555467XU priority Critical patent/CN201825848U/zh
Application granted granted Critical
Publication of CN201825848U publication Critical patent/CN201825848U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

一种高硼硅厚板平拉玻璃供料道结构,它包括有前部设置放料孔的玻璃液料道,该玻璃液料道装配有加热硅碳棒和热电偶,在玻璃液料道的前端连接有玻璃成型工作室,该玻璃成型工作室装配有成型室加热硅碳棒和成型室热电偶,在玻璃液料道与玻璃成型工作室之间设置有玻璃液闸板,在玻璃成型工作室的前端安装有玻璃成型闸板。本实用新型能够满足高硼硅厚板平拉玻璃生产的要求,确保高硼硅厚板平拉玻璃的拉引质量。

Description

高硼硅厚板平拉玻璃供料道结构
技术领域
本实用新型涉及玻璃生产设备,具体涉及一种高硼硅厚板平拉玻璃供料道结构。
背景技术
在玻璃生产中,供料道的作用是将玻璃液进行必要的温度调节和均化,以保证玻璃板拉引的质量。对于高硼硅厚板平拉玻璃,玻璃熔液温度相对较高,且厚板成型时玻璃液在成型槽口外属于低温成型,要求提供更为合理而稳定的成型温度,现行的平拉玻璃供料道结构,难以满足高硼硅厚板平拉玻璃的生产要求。
发明内容
本实用新型的目的在于针对上述问题,提供一种能够满足高硼硅厚板平拉玻璃生产要求,确保玻璃板拉引质量的高硼硅厚板平拉玻璃供料道结构。
实现上述目的的技术方案是:一种高硼硅厚板平拉玻璃供料道结构,它包括有前部设置放料孔的玻璃液料道,该玻璃液料道装配有加热硅碳棒和热电偶,在所述玻璃液料道的前端连接有一玻璃成型工作室,该玻璃成型工作室装配有成型室加热硅碳棒和成型室热电偶,在所述玻璃液料道与玻璃成型工作室之间设置有玻璃液闸板,在所述玻璃成型工作室的前端安装有玻璃成型闸板。
本实用新型在常规玻璃液料道的前端设置一个更加便于实现温度调整和稳定控制的玻璃成型工作室,从而能够确保高硼硅厚板平拉玻璃的拉引质量。
附图说明
附图是本高硼硅厚板平拉玻璃供料道结构示意图。
具体实施方式
结合附图对本实用新型的具体实施方式进行说明。
如附图,本高硼硅厚板平拉玻璃供料道结构包括有在前部设置放料孔1的玻璃液料道2,该玻璃液料道装配有加热硅碳棒3和热电偶4,在玻璃液料道2的前端连接有一呈方形的玻璃成型工作室5,该玻璃成型工作室装配有成型室加热硅碳棒6和成型室热电偶7,在玻璃液料道2与玻璃成型工作室之间设置有玻璃液闸板8,在玻璃成型工作室5的前端安装有玻璃成型闸板9。
本实用新型与玻璃液相接触部分采用锆刚玉材料成型,其它部分采用粘土保温材料成型。

Claims (1)

1.一种高硼硅厚板平拉玻璃供料道结构,包括有在前部设置放料孔(1)的玻璃液料道(2),该玻璃液料道(2)装配有加热硅碳棒(3)和热电偶(4),其特征是:在玻璃液料道(2)的前端连接有一玻璃成型工作室(5),该玻璃成型工作室(5)装配有成型室加热硅碳棒(6)和成型室热电偶(7),在玻璃液料道(2)与玻璃成型工作室(5)之间设置有玻璃液闸板(8),在玻璃成型工作室(5)的前端安装有玻璃成型闸板(9)。
CN201020555467XU 2010-09-30 2010-09-30 高硼硅厚板平拉玻璃供料道结构 Expired - Fee Related CN201825848U (zh)