CN201773083U - 金属熔体电阻率快速检测装置 - Google Patents
金属熔体电阻率快速检测装置 Download PDFInfo
- Publication number
- CN201773083U CN201773083U CN2010200447169U CN201020044716U CN201773083U CN 201773083 U CN201773083 U CN 201773083U CN 2010200447169 U CN2010200447169 U CN 2010200447169U CN 201020044716 U CN201020044716 U CN 201020044716U CN 201773083 U CN201773083 U CN 201773083U
- Authority
- CN
- China
- Prior art keywords
- probe
- resistivity
- connects
- detection device
- vacuum pump
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
金属熔体电阻率快速检测装置。液态金属的物理性能研究一直是科学研究的热门课题,各国科学家为此做了大量的研究工作,近年来在我国也取得了一些可喜的研究成果。金属熔体电阻率快速检测装置,其组成包括:探头(1),所述的探头连接的计算机电路,同时连接升降机构(7)和真空泵(8),所述的探头的帽内有填充的耐高温材料和封口的耐高温密封胶,所述的探头包括穿过其中的电热偶(13)、两个直筒形的双石英管电导池(14)和所述的石英管连接的电极(15)。本实用新型用于铸造和冶金领域。
Description
技术领域:
本发明涉及冶金和铸造领域,具体涉及一种金属熔体电阻率快速检测装置及检测方法。
背景技术:
液态金属的物理性能研究一直是科学研究的热门课题,各国科学家为此做了大量的研究工作,近年来在我国也取得了一些可喜的研究成果。电阻率是液态金属非常重要的物理参数之一,除了由于金属液固相变时电阻率会发生突变外,还发现在远高于液相线的高温区段,液态金属的结构改变也会由电阻率的变化灵敏地反映出来。因此,通过电阻率-温度曲线的研究,可以获得固态和液态金属的组织结构随温度演化的许多有用信息。不论是固态金属还是液态金属其电阻率通常较小,为了精确地测量其电阻值。在金属熔体电阻率测试中,通常是将四根电极埋在带有毛细管的电导池中,电导池可以是单根的浸入管,也可以是双“U”管。当坩埚中金属熔体达到预定温度时,将带有电极的电导池浸入熔体使金属熔体充填电导池,形成测试的通电回路。由于熔体电阻与试样形状关系密切,因此对电导池有很高要求,而异型电导池很难保证精确的尺寸精度。而异型电导池要保证精确的尺寸精度很难。
发明内容:
本发明的目的是提供一种具有较高实用价值的以电导池形状简单、负压抽吸取样、接触电极测量为主要特征的金属熔体电导率检测装置。
上述发明的目的通过以下的技术方案实现:
金属熔体电阻率快速检测装置,其组成包括:探头,所述的探头连接的计算机电路同时连接升降机构和负压抽吸取样真空泵,所述的探头帽内有填充的耐 高温材料和封口的耐高温密封胶,所述的探头包括穿过其中的电热偶、两个直筒形的双石英管电导池和所述的石英管连接的电极。
所述的金属熔体电阻率快速检测装置,所述的真空泵通过缓冲罐连接探头,所述的探头有探头帽,所述的计算机电路包括电源和滤波电路,所述的滤波电路连接数据放大器,所述的数据放大器连接信号采集板卡,所述的信号采集板卡连接计算机。
有益效果:
1.本发明的探头加工制作简单,采用双石英管电导池,两个直筒形的石英管可以使电导池的长度、内径等参数都很精确、快速地测量,这对于获得准确的测量结果至关重要,是提高合金熔体电阻率测量值精度最根本、最有效的措施。
2.本发明的负压抽吸取样方法不仅能够保证合金熔体快速充填电导池,提高测试速度,而且能保证合金熔体在完全充满电导池的同时又不易滞留气泡,同时具有操作简单,易于实现自动化在线测量的特点。
附图说明:
图1是本发明的***结构图。
图2是图1的探头结构图。
图3是图1的***电路框图。
图4是图1的***电路图。
本发明的具体实施方式:
实施例1:
金属熔体电阻率快速检测装置,其组成包括:探头1,所述的探头1连接的计算机电路同时连接升降机构7和真空泵8,所述的探头内填充的耐高温材 料11和封口的耐高温密封胶12,所述的探头1包括穿过其中的电热偶13、两个直筒形的双石英管电导池14和所述的石英管连接的电极15。
所述的真空泵通过缓冲罐9连接探头1,所述的探头有探头帽10,计算机电路包括所述的探头1同时连接电源2和滤波电路3,所述的滤波电路3连接数据放大器4,所述的数据放大器4连接信号采集板卡5,所述的信号采集板卡5连接计算机6,所述的真空泵8通过缓冲罐9连接探头1。
Claims (2)
1.一种金属熔体电阻率快速检测装置,其组成包括:探头,其特征是:所述的探头连接的计算机电路同时连接升降机构和负压抽吸取样真空泵,所述的探头帽内有填充的耐高温材料和封口的耐高温密封胶,所述的探头包括穿过其中的电热偶、两个直筒形的双石英管电导池和所述的石英管连接的电极。
2.根据权利要求1所述的金属熔体电阻率快速检测装置,其特征是:所述的真空泵通过缓冲罐连接探头,所述的探头有探头帽,所述的计算机电路包括电源和滤波电路,所述的滤波电路连接数据放大器,所述的数据放大器连接信号采集板卡,所述的信号采集板卡连接计算机。