CN201549571U - 锌离子电池 - Google Patents
锌离子电池 Download PDFInfo
- Publication number
- CN201549571U CN201549571U CN200920101192XU CN200920101192U CN201549571U CN 201549571 U CN201549571 U CN 201549571U CN 200920101192X U CN200920101192X U CN 200920101192XU CN 200920101192 U CN200920101192 U CN 200920101192U CN 201549571 U CN201549571 U CN 201549571U
- Authority
- CN
- China
- Prior art keywords
- negative electrode
- zinc
- electrode plate
- positive electrode
- layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
锌离子电池涉及一种电源,具体涉及一种利用锌空气反应发电的装置。它包括壳体(1)、正、负电极柱(2)、(3)及正、负极板(4)、(5),壳体(1)内充有电解液,所述正极板(4)由活化膜层(6)和防水粉层(7)构成,防水粉层(7)内埋设有与正电极柱(2)电连接的导电网(8),正极板(4)嵌在壳体(1)壁上,负极板(5)由锌粉压片层(9)内埋设与负电极柱(3)电连接的导电网(8)构成,负极板(5)置于壳体(1)内。它具有工作电流大、结构及制造工艺简单、可重复充电及方便更换锌负极的优点。
Description
技术领域
本实用新型涉及一种电源,具体涉及一种利用锌空气反应发电的装置。
背景技术
无汞、无锡、无镉、无铅电池和高碱性锌电池是我国电池行业的发展方向。
在我们日常生活中普遍采用的锌锰电池是一种碱性电池,它使用了天然等杂质含量较高的材料,为防止锌在电解液中的腐蚀,必须在电池隔离层中加入缓蚀剂,最常用的缓蚀剂是氯化汞,通常加在糊式电池的浆糊中或纸板电池的浆层纸中,这也使汞成为电池中污染环境的主要有害元素。
锌空气电池是一种碱性电池,它由空气电极、壳体、碱液、金属锌负极组成。它的特点来源于空气电极。空气电极去极剂(活性物质)是空气中的氧,因此只要空气能够源源不断地输送给电池,空气电极就能连续不断工作,可谓取之不尽用之不竭,因此正极容量无限。正极本身不带有活性物质,体积可以做到无限小,重量比一般电池正极都要轻。比能量在200-270wh/kg是锌锰干电池的4-5倍。这款电池也有它的缺点:一是正极孔率不是很大,工作电流不够大,二是不能充电,成本较高。
实用新型内容
本实用新型所要解决的技术问题是:提供一种可复充的大工作电流的锌离子电池。
本实用新型的技术解决方案是:它包括壳体、正、负电极柱及正、负极板,壳体内充有电解液,所述正极板由活化膜层和防水粉层构成,防水粉层内埋设有与正电极柱电连接的导电网,正极板嵌在壳体壁上,负极板由锌粉压片层内埋设与负电极柱电连接的导电网构成,负极板置于壳体内。
本实用新型的技术效果是:它具有工作电流大、结构及制造工艺简单、可重复充电及方便更换锌负极的优点。
附图说明
图1为本实用新型实施方式1的正剖结构示意图;
图2为本实用新型实施方式1的侧剖结构示意图;
图3为图2中I处的放大图;
图4为本实用新型实施方式2的正剖结构示意图。
具体实施方式
实施方式一:
如图1、2和3所示,本实施方式的锌离子电池包括壳体1、正、负电极柱2、3及正、负极板4、5,壳体1内充有电解液,所述正极板4由活化膜层6和防水粉层7构成,防水粉层7内埋设有与正电极柱2电连接的导电网8,正极板4嵌在壳体1壁上,其内、外面分别与壳体1内腔和外部接触,负极板5由锌粉压片层9内埋设与负电极柱3电连接的导电网8构成,负极板5置于壳体1内。壳体1由上盖10和下壳11组成,负电极柱3设于上盖10上,正电极柱2和正极板4设于下壳11上,上盖10与下壳11通过胶粘或螺栓连接,可通过胶条密封。正极板4可使空气中的氧气直接通过并参与反应。电解液采用KOH(氢氧化钾)。
所述负极板5于锌粉压片层9外包裹有棉纸层14。
负极板5的锌用完后即可打开密封的上盖10,取出废锌料,再加入新的负极,再发电。
实施方式二:
如图4所示,它与实施方式一不同的是,所述壳体1上设有充电极柱12,充电极柱12通过导线连接有充电极13,充电极13置于壳体1内。充电极柱12设于上盖10上。上盖10上设有透气孔15,透气孔15上设有只允许空气透过不允许液体流出的透气片16。
本实用新型的电池装置锌料可以不取出,作为一次电池使用;也可以在锌负极用完后打开密封电池盖,更换废锌料,进行机械充电;还可以放入不锈钢充电极直接充电,能复充30次左右,其使用寿命大大延长,成本大幅降低。
Claims (3)
1.锌离子电池,包括壳体(1)、正、负电极柱(2)、(3)及正、负极板(4)、(5),壳体(1)内充有电解液,其特征在于,所述正极板(4)由活化膜层(6)和防水粉层(7)构成,防水粉层(7)内埋设有与正电极柱(2)电连接的导电网(8),正极板(4)嵌在壳体(1)壁上,负极板(5)由锌粉压片层(9)内埋设与负电极柱(3)电连接的导电网(8)构成,负极板(5)置于壳体(1)内。
2.如权利要求1所述的锌离子电池,其特征在于,所述壳体(1)上设有充电极柱(12),充电极柱(12)通过导线连接有充电极(13),充电极(13)置于壳体(1)内。
3.如权利要求1所述的锌离子电池,其特征在于,所述负极板(5)于锌粉压片层(9)外包裹有棉纸层(14)。