CN201172299Y - Equipment for making modified asphalt waterproof coil material by non-tyre thermal construction - Google Patents

Equipment for making modified asphalt waterproof coil material by non-tyre thermal construction Download PDF

Info

Publication number
CN201172299Y
CN201172299Y CNU2008200305508U CN200820030550U CN201172299Y CN 201172299 Y CN201172299 Y CN 201172299Y CN U2008200305508 U CNU2008200305508 U CN U2008200305508U CN 200820030550 U CN200820030550 U CN 200820030550U CN 201172299 Y CN201172299 Y CN 201172299Y
Authority
CN
China
Prior art keywords
coiled material
modified asphalt
steel band
transmission steel
asphalt waterproof
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CNU2008200305508U
Other languages
Chinese (zh)
Inventor
巢文革
马东远
曹良
马永祥
闵建彬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SZFSS
Original Assignee
SZFSS
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SZFSS filed Critical SZFSS
Priority to CNU2008200305508U priority Critical patent/CN201172299Y/en
Application granted granted Critical
Publication of CN201172299Y publication Critical patent/CN201172299Y/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

A device which is used to produce non-reinforced heat construction modified asphalt waterproofing coiled materials relates to a manufacturing device of non-reinforced modified asphalt waterproofing coiled materials, which comprises a framework, a driving wheel, a driven wheel, a transport steel tape, a scraping-coating groove, a film sticking device and a film uncoiling device, and further comprises a water spraying device, a transport tape, a constant tension springing device and a recoiling machine, wherein the transport steel tape is tensioned between the driving wheel and the driven wheel, the scraping-coating groove and the film sticking device are arranged above the transport steel tape, the film uncoiling device is arranged at the front of the transport steel tape, and the constant tension springing device comprises a frame, front and rear conveying rollers, an upright post, a receiving plate which rotates up and down around the upright post, and cylinders which are arranged on the frame and at one end of the receiving plate. After employing the technical scheme, the device efficiently resolves deformation and wrinkle problems of polyolefine films, and the tension problem caused by power traction. The production can be conducted continuously, thereby realizing product industrialization production.

Description

A kind of equipment of making no tire heat construction modified asphalt waterproof coiled material
Technical field
The utility model relates to waterproof roll, specially refers to the making apparatus of no tire heat construction modified asphalt waterproof coiled material product.
Background technology
Before the utility model proposes, no tire modified asphalt waterproof coiled material mainly is meant no-wadding adhesive modified asphalt waterproof coiled material (promptly not having the cold construction modified asphalt waterproof coiled material of tire), often adopt the blade coating moulding process during manufacturing, the bottom surface barrier paper on the winding up roller is introduced the surface of transmission steel band with the device of opening a book, and utilize moving of transmission steel band to drive bottom surface barrier paper reach, by scrape hopper the even blade coating of modified pitch of heating to bottom surface barrier paper upper surface, again surface coating is covered the upper surface of modified pitch after tentatively cooling off.Bottom surface barrier paper and surface coating all have very high hot strength, so these two kinds of materials become the carrier of production process medium power tractions such as the moulding coiled material cools off, draws, batches jointly, needn't too much consider the strain problem of coiled material, directly batch to get final product.And when not having the tire heat construction modified asphalt waterproof coiled material and adopting polyolefin film as bottom surface material and surface coating (the also available fine sand of surfacing cover layer), situation is just made a world of difference.Polyolefin film materials itself does not have great hot strength, can not become the carrier of power traction; The modified pitch blade coating of heating can make the wrinkling distortion of film to polyolefin film, cause this kind coiled material to produce continuously, also just can't implement suitability for industrialized production.
The utility model content
The technical problems to be solved in the utility model is to overcome deficiency of the prior art, proposes a kind of equipment of making no tire heat construction polyolefin film waterproof roll.Thereby polyolefin film distortion and caused strain problem when producing gauffer problem and power traction when effectively solving the blade coating modified pitch.
The utility model is to realize by following technical measures.A kind of equipment of making no tire heat construction modified asphalt waterproof coiled material, comprise frame, be arranged at driving wheel and driven pulley on the described frame, be stretched in the transmission steel band between described driving wheel and the driven pulley, be arranged at described transmission steel band the top scrape painted groove, film sticking apparatus, be arranged at the film winding device in the place ahead of described transmission steel band, it is characterized in that: also comprise the water spray facility that is arranged at described transmission steel band inboard, be connected the transport tape at the rear of described transmission steel band, coiling machine after being arranged at the permanent tension force spring facility of described transport tape back and being arranged at described permanent tension force spring facility; The bearing plate that described permanent tension force spring facility comprises framework, the front and back conveying roller above described framework, be arranged on column in the described framework, rotate up and down around the block bearing on the described column, be arranged at the cylinder between described framework and described bearing plate one end.
The described painted groove of scraping comprises that at least former and later two scrape painted groove.
Described water spray facility comprises cooling water pipeline, has the pallet of discharge opening and is no less than one water-cooling-sprayer.
Sander is set described after scraping painted groove, to replace film sticking apparatus.(being used to produce the no tire heat construction polyolefin film waterproof roll that the surfacing cover layer is a fine sand)
Be stretched in that transmission steel band between described driving wheel and the driven pulley is subjected to being arranged at described driving wheel on the described frame and the driving of driven pulley is constantly turned round.Be subjected to affecting of described transmission steel band, the film winding device that is arranged at the place ahead of described transmission steel band described polyolefin film winding up roller is opened and transmission steel band transmission steel band that described polyolefin film is drawn the above as the bottom surface film.Described polyolefin film drives reach by described transmission steel strip surface, by the described painted groove of scraping, the upper surface of already heated described modified pitch at least twice blade coating to described polyolefin film bottom surface.Simultaneously, by comprising cooling water pipeline, have the pallet of discharge opening and being no less than the described water spray facility of one water-cooling-sprayer, water is sprayed on the inner surface of described transmission steel band, the temperature of described modified pitch is cooled down rapidly, after treating that temperature descends, the polyolefin film paving that described film sticking apparatus will be attracted by another decoiling equipment on described modified pitch face, thereby form described water-proof coiled material without tire heat construction product.
Described sand under the described polyolefin film of the upper surface of described water-proof coiled material without tire heat construction product can be spread by described sander replaces, and forms sand of a facial mask, the water-proof coiled material without tire heat construction product of the described modified pitch of sandwich.
Described water-proof coiled material without tire heat construction product continues to be cooled on described transmission steel band, and is introduced into described transport tape.Described transport tape is introduced described permanent tension force spring facility with described water-proof coiled material without tire heat construction product, and then described water-proof coiled material product is transferred on the described coiling machine clot rolls off the production line.In described permanent tension force spring facility, under the normal condition in described framework, one end (perk end) of the described bearing plate that rotates up and down around the described block bearing on the described column is subjected to being arranged at the pulling of the described cylinder between described framework and described bearing plate one end (perk end), the other end of described bearing plate (piling up end) perk.After described transport tape was introduced the conveying roller of described permanent tension force spring facility with described water-proof coiled material without tire heat construction product, described water-proof coiled material without tire heat construction product constantly fell, and was deposited on the other end (piling up end) of the bearing plate of described perk.Coiled material product on the plate is swept away by the conveying roller that is positioned at described framework top by described coiling machine again.When described coiled material product continued to send here on the accumulation end that is deposited in described bearing plate, described bearing plate was subjected to the gravity effect of described coiled material product, piled up end and constantly sank.Sink to meaning that more at most the described coiled material product of sending here is many more, described coiling machine has little time described coiled material product rolled away and rolls off the production line, and the leading portion production process should underspeed or improve the speed of described coiling machine.Otherwise, when the described coiled material product on sending and be deposited in described bearing plate here constantly reduces, be subjected to the pulling of described cylinder, the perk end of described bearing plate constantly sinks, the other end is piled up end and is then lifted on constantly, shows that the leading portion production process should improve speed or reduce the speed of described coiling machine.The amount of the described coiled material product on described bearing plate remains in certain scope like this, and the described coiled material product that stores on the plate is in relaxed state, and the constant tension that produces when batching and very little guarantees that described coiled material product is not broken.
The utility model has not only proposed a kind of new water-proof coiled material product after adopting abovementioned technology in the waterproof roll field---no tire heat construction modified asphalt waterproof coiled material product, and proposed to make the technical equipment of this product.Be provided with described water spray facility and described permanent tension force spring facility, polyolefin film distortion and caused strain problem when producing gauffer problem and power traction when effectively solving the blade coating modified pitch.Production is carried out continuously, and product appearance also obtains changing looking.Help not having the exploitation of tire modified asphalt waterproof coiled material product center kind, help the raising of building waterproofing technique level and equipment.
Description of drawings
Fig. 1 is the utility model embodiment schematic diagram.
Fig. 2 is the schematic diagram of permanent tension force spring facility.
Fig. 3 is the schematic diagram of water spray facility.
1 is the transmission steel band among the figure, and 2 is driving wheel, and 3 is driven pulley, and 4 is the film winding device, and 5 for scraping painted groove, and 6 is film sticking apparatus, and 7 is sander, and 8 is transport tape, and 9 is permanent tension force spring facility, and 10 is coiling machine.
9-1 is a column, and 9-2 is a block bearing, and 9-3 is a bearing plate, and 9-4 is a framework, and 9-5 is a cylinder, and 9-6 is a conveying roller.
11-1 is a cooling water pipeline, and 11-2 is a pallet, and 11-3 is a discharge opening, and 11-4 is a water-cooling-sprayer.
101 is water-proof coiled material without tire heat construction (product), and 102 is density polyethylene film with high (PE film), and 103 is modified pitch, and 104 is sand.
The specific embodiment
The utility model is described in further detail below in conjunction with drawings and Examples.
Embodiment: as Fig. 1~shown in Figure 3.Make the equipment of no tire heat construction modified asphalt waterproof coiled material, comprise the frame (not shown), be arranged at driving wheel 2 and driven pulley 3 on the frame, be stretched in the transmission steel band 1 between driving wheel 2 and the driven pulley 3, former and later two of top that are arranged at transmission steel band 1 are scraped painted groove 5, film sticking apparatus 6, be arranged at the film winding device 4 in the place ahead of transmission steel band 1, also comprise the water spray facility 11 that is arranged at transmission steel band 1 inboard, be connected the transport tape 8 at the rear of transmission steel band 1, coiling machine 10 after being arranged at the permanent tension force spring facility 9 of transport tape 8 back and being arranged at permanent tension force spring facility 9, permanent tension force spring facility 9 comprises framework 9-4, be positioned at the front and back conveying roller 9-6 of framework 9-4 top, be arranged on the column 9-1 in the framework 9-4, the bearing plate 9-3 that rotates up and down around the block bearing 9-2 on the column 9-1, be arranged at the cylinder 9-5 between framework 9-4 and bearing plate 9-3 one end; Sander 7 is set, to replace film sticking apparatus after scraping painted groove 5; Water spray facility 11 comprises cooling water pipeline 11-1, has the pallet 11-2 of discharge opening 11-3 and is no less than one water-cooling-sprayer 11-4.
Be stretched in that transmission steel band 1 between driving wheel 2 and the driven pulley 3 is subjected to being arranged at driving wheel 2 on the frame (figure is by expression) and the driving of driven pulley 3 is constantly turned round.Be subjected to transmitting affecting of steel band 1, the film winding device 4 in the place ahead that is arranged at transmission steel band 1 is opened density polyethylene film with high (PE film) 102 windings up roller and density polyethylene film with high (PE film) 102 is drawn the transmission steel band and transmits steel band 1 as the bottom surface film.Density polyethylene film with high (PE film) 102 drives reach by transmission steel band 1 surface, and by scraping painted groove 5, modified pitch 103 twice blade coating that are 160 ℃ to temperature are to the upper surface of density polyethylene film with high (PE film) 102.Simultaneously, by comprising cooling water pipeline 11-1, have the pallet 11-2 of discharge opening and being no less than the water spray facility 11 of one water-cooling-sprayer 11-3, water is sprayed on the inner surface of transmission steel band 1, the temperature of modified pitch 103 is cooled down rapidly, when treating that temperature is reduced to 90 ℃, density polyethylene film with high (PE film) 102 pavings that film sticking apparatus 6 will be attracted by another decoiling equipment (not shown) on the modified pitch face, thereby form described no tire heat construction modified asphalt waterproof coiled material product 101.
Sand 104 under the density polyethylene film with high (PE film) 102 of the upper surface of no tire heat construction modified asphalt waterproof coiled material 101 products can be spread by sander 7 replaces, form sand of a facial mask, the no tire heat construction modified asphalt waterproof coiled material product 101 of the described modified pitch of sandwich.
No tire heat construction modified asphalt waterproof coiled material product 101 continues to be cooled on transmission steel band 1, and is introduced into transport tape 8.Transport tape 8 will not have tire heat construction modified asphalt waterproof coiled material product 101 and will introduce permanent tension force spring facility 9, and then water-proof coiled material product 101 is transferred on the coiling machine 10 clot will roll off the production line.In permanent tension force spring facility 9, under the normal condition in framework 9-4, the A end (perk end) of the bearing plate 9-3 that rotates up and down around the block bearing 9-2 on the column 9-1 is subjected to being arranged at the pulling of the cylinder 9-5 between framework 9-4 and the bearing plate A end (perk end), B end (pile up and hold) perk of bearing plate 9-3.After transport tape 8 was introduced the place ahead conveying roller 9-6 of permanent tension force spring facility 9 with water-proof coiled material without tire heat construction product 101, water-proof coiled material without tire heat construction product 101 constantly fell, and was deposited on the B end (accumulation end) of the bearing plate 9-3 of perk.Coiled material product 101 on the plate is swept away by the rear conveying roller 9-6 that is positioned at framework 9-4 top by coiling machine 10 again.Be deposited on the bearing plate 9-3 when coiled material product 101 continues to send here, bearing plate 9-3 is subjected to the gravity effect of coiled material product 101, and B end (piling up end) constantly sinks.Sink to meaning that more at most the coiled material product of sending here 101 is many more, coiling machine 10 has little time coiled material product 101 rolled away and rolls off the production line, and the leading portion production process should underspeed or improve the speed of coiling machine 10.Otherwise, when the coiled material product 101 on sending and be deposited in bearing plate 9-3 here constantly reduces, be subjected to the pulling of cylinder 9-5, the A end (perk end) of the bearing plate 9-3 of perk constantly sinks, lift on B end (piling up end) is then continuous, show that the leading portion production process should improve the speed of speed or reduction coiling machine 10.The amount of the coiled material product 101 on bearing plate 9-3 remains in certain scope like this, and the coiled material product 101 that stores on the plate is in relaxed state, and the constant tension that produces when batching and very little guarantees that coiled material product 101 is not broken.
Above-described only is preferred implementation of the present utility model.Should be pointed out that for the person of ordinary skill of the art under the prerequisite that does not break away from the utility model principle, can also make some modification and improvement, these also should be considered as belonging to protection domain of the present utility model.

Claims (4)

1. equipment of making no tire heat construction modified asphalt waterproof coiled material, comprise frame, be arranged at described driving wheel (2) and driven pulley (3) on the described frame, be stretched in the described transmission steel band (1) between described driving wheel (2) and the driven pulley (3), be arranged at the described painted groove (5) of scraping of the top of described transmission steel band (1), described film sticking apparatus (6), be arranged at the described film winding device (4) in the place ahead of described transmission steel band (1), it is characterized in that: also comprise being arranged at the inboard described water spray facility (11) of described transmission steel band (1), be connected the described transport tape (8) at the rear of described transmission steel band (1), described coiling machine (10) after being arranged at the described permanent tension force spring facility (9) of described transport tape (8) back and being arranged at described permanent tension force spring facility (9); The described bearing plate (9-3) that described permanent tension force spring facility (9) comprises described framework (9-4), be positioned at the described front and back conveying rollers (9-6) of described framework (9-4) top, be arranged on the described column (9-1) of described framework (9-4), rotate up and down around the described block bearing (9-2) on the described column (9-1), be arranged at the described cylinder (9-5) between a described framework (9-4) and described bearing plate (9-3) end.
2. a kind of equipment of making no tire heat construction modified asphalt waterproof coiled material according to claim 1 is characterized in that: the described painted groove (5) of scraping comprises that at least former and later two scrape painted groove.
3. a kind of equipment of making no tire heat construction modified asphalt waterproof coiled material according to claim 1 is characterized in that: described water spray facility (11) comprises cooling water pipeline (11-1), has the pallet (11-2) of discharge opening (11-3) and is no less than one water-cooling-sprayer (11-4).
4. a kind of equipment of making no tire heat construction modified asphalt waterproof coiled material according to claim 1 is characterized in that: at the described painted groove (5) of scraping sander (7) is set afterwards.
CNU2008200305508U 2008-01-04 2008-01-04 Equipment for making modified asphalt waterproof coil material by non-tyre thermal construction Expired - Lifetime CN201172299Y (en)