CN201104313Y - 耐高温薄型涤纶玻璃丝烧结漆包铜扁线 - Google Patents
耐高温薄型涤纶玻璃丝烧结漆包铜扁线 Download PDFInfo
- Publication number
- CN201104313Y CN201104313Y CNU2008200568734U CN200820056873U CN201104313Y CN 201104313 Y CN201104313 Y CN 201104313Y CN U2008200568734 U CNU2008200568734 U CN U2008200568734U CN 200820056873 U CN200820056873 U CN 200820056873U CN 201104313 Y CN201104313 Y CN 201104313Y
- Authority
- CN
- China
- Prior art keywords
- wire
- flat wire
- copper strap
- conductor
- enameled
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种耐高温薄型涤纶玻璃丝烧结漆包铜扁线,以填补我国水轮发电机用的耐高温薄型涤纶玻璃丝烧结漆包铜扁线的空白,它包括导体,所述导体包覆有扁线状漆包线,在所述扁线状漆包线上绕包有涤纶丝、玻璃丝和混合纤维组合成的绝缘层,所述绝缘层经烘焙、烧结在所述扁线状漆包线上;通过对漆包铜扁线的铜导体使用轧-拉法进行拉制,使导体的尺寸达到高精度,然后制成200级耐热聚酯亚胺/聚酰胺酰亚胺复合型漆包铜扁线,再绕包上涤纶丝、玻璃丝和混合纤维经烘焙、烧结,使涤纶丝熔化,将涤纶丝、玻璃丝与漆包铜扁线熔为一体,实现本实用新型的目的。
Description
技术领域
本实用新型涉及一种漆包铜扁线,特别涉及一种用于水轮发电机的耐高温薄型涤纶玻璃丝烧结漆包铜扁线。
背景技术
由于我国近来大力发展电力工业,特别是水电发展的突飞猛进,水轮发电机用的耐高温薄型涤纶玻璃丝烧结漆包铜扁线在国内尚属空白,这种电磁线需要有高要求的耐温等级,薄的绝缘厚度,高的耐电压要求和很强的机械特性,它是在预先制造好的漆包铜扁线上绕包一层,按一定比例混合的涤纶玻璃丝,然后经烧结使涤纶丝熔化,使涤沦玻璃丝与漆包线熔为一体而获得优良的电气与机械特性。
目前,国外也只有极少数几家电磁线公司能生产,我厂成功的研制成功并已用于我国多处重点工程中。
实用新型内容
本实用新型所要解决的技术问题在于提供一种耐高温薄型涤纶玻璃丝烧结漆包铜扁线,以填补我国水轮发电机用的耐高温薄型涤纶玻璃丝烧结漆包铜扁线的空白。
本实用新型所要解决的技术问题可以通过以下技术方案来实现:
一种耐高温薄型涤纶玻璃丝烧结漆包铜扁线,它包括导体,其特征在于,所述导体包覆有扁线状漆包线,在所述扁线状漆包线上绕包有涤纶丝、玻璃丝和混合纤维组合成的绝缘层,所述绝缘层经烘焙、烧结在所述扁线状漆包线上。
所述导体为铜导体。
所述绝缘层由涤纶丝、玻璃丝和混合纤维烧结而成。
所述扁线状漆包线为200级耐热聚酯亚胺/聚酰胺酰亚胺复合型漆包铜扁线。
本实用新型的耐高温薄型涤纶玻璃丝烧结漆包铜扁线,通过对漆包铜扁线的铜导体使用轧-拉法进行拉制,使导体的尺寸达到高精度,然后制成200级耐热聚酯亚胺/聚酰胺酰亚胺复合型漆包铜扁线,再绕包上涤纶丝、玻璃丝和混合纤维经烘焙、烧结,使涤纶丝熔化,将涤纶丝、玻璃丝与漆包铜扁线熔为一体,实现本实用新型的目的。
附图说明
图1为本实用新型的结构示意图。
具体实施方式
为了使本实用新型实现的技术手段、创作特征、达成目的与功效易于明白了解,下面结合具体图示,进一步阐述本实用新型。
一种耐高温薄型涤纶玻璃丝烧结漆包铜扁线,它包括导体1,所述导体1包覆有扁线状漆包线3,在所述扁线状漆包线3上绕包有涤纶丝、玻璃丝和混合纤维组合成的绝缘层2,所述绝缘层2经烘焙、烧结在所述扁线状漆包线3上。所述绝缘层2由涤纶丝、玻璃丝和混合纤维烧结而成。
在本实用新型中,所述导体1通过轧-拉法进行加工;导体1先经过精轧轧制到一定尺寸,然后经过模具的拉伸,一次成型;由于导体1进入成型模具前先经过轧机的轧制已经基本成型,在进入模具进行拉制时,对成型模具的抗拉力就很小,大大降低了对于模具的磨损,解决了模具磨损带来的导体1尺寸精度波动的问题;同时,在进入模具前的导体1尺寸可以通过调节轧机轧辊任意调节,这样能保证在进入模具后导体1尺寸的精度,保持导体1尺寸的波动控制在0.01mm的范围内,实现在导体的尺寸高精度。
漆包铜扁线的生产:
由于漆包铜扁线在绕包涤纶玻璃丝后还要经过350℃约5分钟左右的高温烘烤,但不能影响它的技术指示,如击穿电压不能降低弯曲后漆膜不能开裂,拉伸后漆膜不能脱离等,因此它要有很高的热性能;在本实用新型中,所述漆包铜扁线为200级耐热聚酯亚胺/聚酰胺酰亚胺复合型漆包铜扁线,它的主要热性能软件击穿指标在380℃以上,它的主要固化度指标玻璃化转化温度Tg在200℃以上,所述漆包铜扁线的两层漆膜厚度的最佳比例为4∶6。
涤沦丝和玻璃丝的选择:
涤纶丝在整个烧结过程中先熔化后冷却起到粘结玻璃丝与漆包铜扁线的作用,故要求涤沦丝在保证电磁线的耐温等级下,熔点越低越好,而且要求熔化后具有良好的流平性,冷却后使漆包扁线、玻璃丝和涤纶丝熔为一体;而涤纶丝的这些性质取决于涤纶丝的聚合度的大小,在本实用新型中,所述涤纶丝的聚合度为50~80,在绕包中所述玻璃丝和涤纶丝之间的最佳比例为35~45%,使涤纶丝、玻璃丝烧结后能使电磁线具有优良的电性能,又有良好的机械性能。
绕包和烧结过程:
涤纶玻璃丝漆包铜扁线绕包和烧结过程是电磁线生产的最后工序,也是最关键的工序;为使涤纶玻璃丝漆包铜扁线烧结后具有较强的抗拉强度和耐弯曲性能,本实用新型中,在绕包时采用偏心双丝团绕包头,使绕包角度为35°,大的绕包节距为7mm,而且具有优良的恒张力作用。
绕包后的烘焙阶段,既要使涤纶丝熔化、流平,又不能烘坏涤纶玻璃丝漆包铜扁线,本实用新型中,烘焙温度为300~400℃,烘焙时间为15~25分钟。
以上显示和描述了本实用新型的基本原理和主要特征及其优点。本行业的技术人员应该了解,本实用新型不受上述实施例的限制,上述实施例和说明书中描述的只是说明本实用新型的原理,在不脱离本实用新型精神和范围的前提下,本实用新型还会有各种变化和改进,这些变化和改进都落入要求保护的本实用新型范围内。本实用新型要求保护范围由所附的权利要求书及其等效物界定。
Claims (3)
1、一种耐高温薄型涤纶玻璃丝烧结漆包铜扁线,它包括导体,其特征在于,所述导体包覆有扁线状漆包线,在所述扁线状漆包线上绕包有涤纶丝、玻璃丝和混合纤维组合成的绝缘层。
2、根据权利要求1所述的耐高温薄型涤纶玻璃丝烧结漆包铜扁线,其特征在于:所述扁线状漆包线为200级耐热聚酯亚胺复合型漆包铜扁线。
3、根据权利要求1所述的耐高温薄型涤纶玻璃丝烧结漆包铜扁线,其特征在于:所述扁线状漆包线为200级聚酰胺酰亚胺复合型漆包铜扁线。