CN1640352A - 一种保温容器连通管连接缝隙的填充办法 - Google Patents

一种保温容器连通管连接缝隙的填充办法 Download PDF

Info

Publication number
CN1640352A
CN1640352A CN 200410015122 CN200410015122A CN1640352A CN 1640352 A CN1640352 A CN 1640352A CN 200410015122 CN200410015122 CN 200410015122 CN 200410015122 A CN200410015122 A CN 200410015122A CN 1640352 A CN1640352 A CN 1640352A
Authority
CN
China
Prior art keywords
stainless steel
communicating pipe
insulating container
slit
container
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200410015122
Other languages
English (en)
Inventor
陈安涛
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 200410015122 priority Critical patent/CN1640352A/zh
Publication of CN1640352A publication Critical patent/CN1640352A/zh
Pending legal-status Critical Current

Abstract

一种不锈钢保温容器连通管连接缝隙的填充的方法,它将设置在不锈钢保温容器侧部或底部的不锈钢连通管与内胆壁连接处的连接缝隙用钎焊的方法在内胆壁内侧进行填充,使得不锈钢保温容器在电解抛光时,电解液不能渗入缝隙中,避免了残留在缝隙中的电解液对不锈钢保温容器污染,提高了产品的品质,消除了对人体健康的隐患。

Description

一种保温容器连通管连接缝隙的填充办法
本发明涉及一种不锈钢保温容器连通管连接缝隙的填充办法,尤其是在双层不锈钢真空保温壶或瓶的侧部或底部设置连通管时,连通管与内胆壁连接后在内胆腔内产生的连通管与内胆壁的连接缝隙的填充方法。
背景技术:
在带连通管的双层不锈钢真空保温容器实际生产中,经常会发生这样的情况,产品在仓库里存放一定的时间或将产品交给客户后一段时间,会发现生在内胆腔的连通管与内胆壁的连接出现锈迹或斑痕,严重影响了产品的品质。出现这种情况的原因是由于连通管与内胆壁连接后,内胆壁内侧与连通管连接处还存在缝隙,而内胆腔是采用电解抛光的,在电解抛光的过程中,电解液就会渗入缝隙里,电解抛光后用清水清洗内腔。由于缝隙较窄,无法彻底清洗到渗入缝隙里的电解液,因此内腔清洗后部分电解液仍然残留在缝隙里,当清洗后的双层不锈钢真空保温容器存放一定时间后,残留在缝隙里的电解液就会慢慢流出来,使缝隙的附近产生锈迹或斑痕。双层不锈钢真空保温容器一般是用来装饮用水或咖啡的,电解液是对人体有害的物质,会对人体的健康造成影响,因此必须在技术上彻底解决这个问题。
发明内容:
为了解决电解液渗入连通管与内胆壁连接的缝隙里而对双层不锈钢真空保温容器产生污染,影响产品品质,影响人体健康,本发明提供了一种填充缝隙的方法,在内胆壁的表面堵住了缝隙,使电解液不能渗入缝隙,提高了产品的品质,消除了对人体健康的隐患。
本发明解决其技术问题所采用的技术方案是电解抛光工艺之前,用钎焊的方法将不锈钢连通管与双层不锈钢真空保温容器内胆壁连接后在内胆腔一侧产生的连接缝隙堵住,使其在电解抛光的过程中,电解液不能渗入缝隙中,即在连通管与内胆壁的连接加工艺中增加一道钎焊的工序。原来连接内胆壁与不锈钢连通管的加工工艺如下:
内胆打孔→***不锈钢连通管→在内胆外侧处氩弧焊或电阻焊连接。
本发明采用后连接内胆壁与不锈钢连通管的加工工艺如下:
内胆打孔→***不锈钢连通管→内胆外侧处氩弧焊或电阻焊连接→内胆内侧处钎焊填充缝隙,
本发明的有益效果是填住了双层不锈钢保温容器与不锈钢连通管连接后在内胆内腔壁上出现的缝隙,使得其在电解抛光过程中,电解液不能渗入缝隙中,避免了电解液对容器产生的污染,提高了产品的品质,消除了对人体健康的隐患。
附图说明:
下面结合附图和实施例对本发明进一步的说明:
图1是双层不锈钢真空保温容器的主剖面构造图
图2是本发明第一个实施例的放大图;
图3是本发明第一实施例不锈钢连通管的主剖面构造图;
图4是图3的A1-A1的剖视图;
图5是图3的右视图;
图6是本发明第二个实施例的放大图;
图7是本发明第二个实施例不锈钢连通管的主剖面构造图;
图8是图7的A2-A2的部视图;
图9是图7的右视图;
图中,1内胆、2外壳、3真空层、4抽真空铜管、5外底盖、6不锈钢连通管、7不锈钢连通管和与内胆壁焊缝、8不锈钢连通管与外壳壁焊缝、9缝隙、10钎焊填充缝。
在图1中,内胆(1)与外壳(2)在口部氩弧焊连接,带抽真空铜管(4)的排气底盖与外壳(2)在底部氩弧焊连接,不锈钢连通管(6)一头与内胆(1)的壁的外侧用氩弧焊或电阻焊连接,内侧用钎焊填充缝隙;另一头与外壳(2)的壁用的外侧氩弧焊或电阻焊连接,通过抽真空铜管(4)将外壳(2)与内胆(1)之间空间抽成真空状态形成真空层(3),外底盖(5)安装在外壳(2)的底部将抽真空铜管(4)隐蔽其中。
在图2中,不锈钢连通管(6)的形状如图3、图4、图5所示,不锈钢连通管(6)与内胆(1)在外侧氩弧焊连接形成不锈钢连通管与内胆壁焊缝(7),与外壳(2)在外侧氩弧焊连接形成了不锈钢连通管与外壳壁焊缝(8),内胆(1)与不锈钢连通管(6)连接的缝隙(9),用钎焊的方法在内胆腔内侧填充缝隙(9)形成的钎焊填充缝(10)。
在图(6)中不锈钢连通管(6)的形状如图(7)、图(8)、图(9)所示,其它的说明与图(2)中的说明相同。

Claims (1)

1、一种不锈钢保温容器连通管连接缝隙的填充方法,其特征是:将不锈钢连通管与保温容器内胆壁连接处的内腔一侧的缝隙用钎焊的方法填充。
CN 200410015122 2004-01-14 2004-01-14 一种保温容器连通管连接缝隙的填充办法 Pending CN1640352A (zh)