CN1632028A - 一种用于纺织行业的粘合剂及其制备方法 - Google Patents
一种用于纺织行业的粘合剂及其制备方法 Download PDFInfo
- Publication number
- CN1632028A CN1632028A CN 200410067873 CN200410067873A CN1632028A CN 1632028 A CN1632028 A CN 1632028A CN 200410067873 CN200410067873 CN 200410067873 CN 200410067873 A CN200410067873 A CN 200410067873A CN 1632028 A CN1632028 A CN 1632028A
- Authority
- CN
- China
- Prior art keywords
- textile industry
- tackiness agent
- agent
- initiator
- water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种用于纺织行业的粘合剂,由醋酸乙烯酯、丙烯酸丁酯、丙烯酸、聚乙烯醇、乳化剂、引发剂、水以及碳酸氢钠配置而成。该粘合剂的生产成本低廉,具有较好的增塑响应特性和稳定性,粘度也较高。
Description
技术领域
本发明属于化工领域,尤其涉及一种用于纺织行业的粘合剂。
背景技术
随着社会的高速发展,人类的生活要求越来越舒适,为了便于生产和降低产品的成本,我们使用各种各样的粘合剂用于纺织工业各种物品相互粘接,以达到良好的使用效果。目前市场上使用的适用于纺织行业的粘合剂的生产成本都比较高,增塑响应特性比较差,性能很不稳定,粘度也比较低。
发明内容
本发明的目的是解决上述问题,提供了一种生产成本低的用于纺织行业的粘合剂。
本发明的技术方案是:一种用于纺织行业的粘合剂,其特征在于包括下列重量比的组分:
醋酸乙烯酯 20%-30%
丙烯酸丁酯 2%-3%
丙烯酸 1%-2%
聚乙烯醇 2%-3%
乳化剂 0.5%-1%
引发剂 0.1%-3%
水 60%-73%
碳酸氢钠 0.2%-0.4%
还包括适量消泡剂;
所述的引发剂是过硫酸铵;
所述的乳化剂是OP乳化剂;
本发明粘合剂的最佳组分包括:
醋酸乙烯酯 23%
丙烯酸丁酯 2.5%
丙烯酸 1%
聚乙烯醇 2.5%
乳化剂 0.5%
引发剂 0.2%
水 70%
碳酸氢钠 0.3%
消泡剂 适量
一种用于纺织行业的粘合剂的制备方法,包括以下步骤:
(1)配置混合单体:将醋酸乙烯酯、丙烯酸丁酯、丙烯酸混合;
(2)将聚乙烯醇和水在85℃-95℃下混合溶解;
(3)取上述聚乙烯醇水溶液在60℃-75℃下加乳化剂、碳酸氢钠搅拌均匀溶解,出现泡沫后可以加入消泡剂,然后加入步骤(1)中的部分混合单体和引发剂,反应后再滴加剩余的混合单体,滴加完成后再升温至85℃~90℃,反应0.5小时,冷却后即得。
按本发明的技术方案设计的一种用于纺织行业的粘合剂,比常规常规产品允许添加更多的水,降低了生产成本,还具有较好的增塑响应特性和稳定性,粘度也较高。
具体实施方式
下面通过具体实施例对本发明做进一步的说明。
实施例1:本实施例粘合剂采用如下配方:
醋酸乙烯酯 120kg 丙烯酸丁酯 12kg
丙烯酸 6kg 聚乙烯醇 12kg
OP-10 3kg 过硫酸铵 1kg
水 350kg 碳酸氢钠 1.5kg
消泡剂N,N,N-三(聚氧丙烯聚氧乙烯)胺 适量
制备方法:按下述步骤:
(1)配置混合单体:将醋酸乙烯酯、丙烯酸丁酯、丙烯酸混合;
(2)将聚乙烯醇和水在90℃下混合溶解;
(3)取上述聚乙烯醇水溶液在75℃下加乳化剂OP-10、碳酸氢钠搅拌均匀溶解,出现泡沫后可以加入消泡剂N,N,N-三(聚氧丙烯聚氧乙烯)胺,然后加入步骤(1)中的部分混合单体和引发剂过硫酸铵,反应后再滴加剩余的混合单体,滴加完成后再升温至85℃~90℃,反应0.5小时,冷却后即得。
Claims (6)
1、一种用于纺织行业的粘合剂,其特征在于包括下列重量比的组分:
醋酸乙烯酯 20%-30%
丙烯酸丁酯 2%-3%
丙烯酸 1%-2%
聚乙烯醇 2%-3%
乳化剂 0.5%-1%
引发剂 0.1%-3%
水 60%-73%
碳酸氢钠 0.2%-0.4%
2、根据权利要求1所述的一种用于纺织行业的粘合剂,其特征在于还包括适量消泡剂。
3、根据权利要求1所述的一种用于纺织行业的粘合剂,其特征在于所述的引发剂是过硫酸铵。
4、根据权利要求1所述的一种用于纺织行业的粘合剂,其特征在于所述的乳化剂是OP乳化剂。
5、根据权利要求1所述的一种用于纺织行业的粘合剂,其特征在于由下述组分构成:醋酸乙烯酯 23%
丙烯酸丁酯 2.5%
丙烯酸 1%
聚乙烯醇 2.5%
乳化剂 0.5%
引发剂 0.2%
水 70%
碳酸氢钠 0.3%
消泡剂 适量
6、根据权利要求1所述的一种用于纺织行业的粘合剂的制备方法,包括以下步骤:
(1)配置混合单体:将醋酸乙烯酯、丙烯酸丁酯、丙烯酸混合;
(2)将聚乙烯醇和水在85℃-95℃下混合溶解;
(3)取上述聚乙烯醇水溶液在60℃-75℃下加乳化剂、碳酸氢钠搅拌均匀溶解,出现泡沫后可以加入消泡剂,然后加入步骤(1)中的部分混合单体和引发剂,反应后再滴加剩余的混合单体,滴加完成后再升温至85℃~90℃,反应0.5小时,冷却后即得。