CN1423003A - Soybean fiber velvet and production method thereof - Google Patents

Soybean fiber velvet and production method thereof Download PDF

Info

Publication number
CN1423003A
CN1423003A CN 01137359 CN01137359A CN1423003A CN 1423003 A CN1423003 A CN 1423003A CN 01137359 CN01137359 CN 01137359 CN 01137359 A CN01137359 A CN 01137359A CN 1423003 A CN1423003 A CN 1423003A
Authority
CN
China
Prior art keywords
soybean fiber
production method
water
agent
fiber velvet
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 01137359
Other languages
Chinese (zh)
Inventor
华凤言
蔡可夫
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
DONGTAI COTTON IND KNITTING Co Ltd JIANGSU
Original Assignee
DONGTAI COTTON IND KNITTING Co Ltd JIANGSU
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by DONGTAI COTTON IND KNITTING Co Ltd JIANGSU filed Critical DONGTAI COTTON IND KNITTING Co Ltd JIANGSU
Priority to CN 01137359 priority Critical patent/CN1423003A/en
Publication of CN1423003A publication Critical patent/CN1423003A/en
Pending legal-status Critical Current

Abstract

The invention discloses a method of using soybean fiber to produce color velours, the process is: soybean fiber gauze, spinning, baking, rough, cuttihng steaming, dyeing, soap, washing, coloring and softening, dehydrating, fine cutting, fixing, curling. The velours is smooth, colorful, unfading, the producing of velours has new material source.

Description

Soybean fiber velvet and production method
The invention belongs to a kind of production method of velvet, particularly a kind ofly produce velvet method with the fibre and soya yarn.
Existing VELVET has and adopts cotton yarn to make, and also has the real silk of employing and other chemical fibre woven, and its production method is earlier raw material to be carried out the damp-warm syndrome balance, again through whole yarn, weave, operations such as shorn velvet, dyeing, typing finish.
The purpose of this invention is to provide a kind of new VELVET kind is that VELVET is sought a kind of new material source.
The present invention realizes with following technical scheme: it is that raw material is knitted choosing that the alleged soybean fiber velvet of the present invention is meant with the fibre and soya yarn, and its technological process of production is: fibre and soya cotton yarn → knitting → cure → preliminary shearing → boiling-off → dye → soap → fixation softness → dehydration → fine pruning → typing → clot.
Wherein knittingly under workshop temperature 19-25 ℃, the situation of humidity 50-60 ℃ degree, weave with speed of a motor vehicle 15-25 rev/min with the cylinder loom.
Cure with the cylinder machine and under 80 ℃ of temperature, cured 20 seconds.
Boiling process is with hydrogen peroxide (H 2O 2), NaOH (NaCl), bleeding agent, stabilizing agent adds the poach refining for batching, the consumption of various batchings is (accounting for the water percetage by weight):
Hydrogen peroxide 4-7%
NaOH 2-5%
Bleeding agent 0.3-0.6%
The concrete scouring process of stabilizing agent 2-4% is to add bleeding agent, stabilizing agent when heating water to 30 ℃, adds hydrogen peroxide, NaOH when continuing to heat to 65 ℃ then, keeps temperature 30-50 second when being warming up to 80-98 ℃ again after cloth is added.
The raw materials used prescription that dyes is (accounting for the water percetage by weight):
Silk levelling agent 0.4-0.6%
Dyestuff 2-8%
Salt (NaCl) 2-5% concrete grammar is that water, cloth and various raw material are put into dyeing machine, is stirred to while heating when being warming up to 80-90 ℃ and is incubated 20-40 minute.
The addition of soap washing cleanser is the 0.4-0.6% of water weight.
It is raw material that the fixation softening step adopts formaldehydeless fixation, softener, and wherein the addition of formaldehyde-free color fixing agent is the heavy 0.5-1% of water, and the addition of softener is the 3-4% of water weight; Fixation, soft time respectively are 20 seconds.
Other operation all routinely prior art carry out.
Soybean fiber velvet with technique scheme is produced belongs to the environmental protection lining, and has easy dyeing, and is bright in luster, the COLOR FASTNESS height, and matte is smooth, do not fall advantages such as hair, for velvet production provides new raw material sources.
Embodiment one:
Raw material: fibre and soya yarn
Technological parameter:
19 ℃ of knitting workshop temperature, humidity 50 degree, cylinder loom, 25 rev/mins of the speed of a motor vehicle.
Cure: temperature was cured in the cylinder machine 20 seconds for 80 ℃.
Boiling-off:
Materials: hydrogen peroxide 4% NaOH 2%
Bleeding agent 0.3% stabilizing agent 2%
80 ℃ of 50 seconds times of temperature
Dyeing:
Materials: silk levelling agent: 0.4% Saphire Brown fuel 8%
Salt: 2%
Temperature: 80 ℃ of temperature retention times: 40 minutes
Soap: cleanser consumption 0.4%
The fixation softness:
20 seconds 0.5% time of formaldehyde-free color fixing agent
20 seconds 3% time of softener
The VELVET matte of producing with described process is smooth, does not fall hair, the color Saphire Brown, and COLOR FASTNESS reaches national standard.
Embodiment two:
Raw material: fibre and soya yarn
Technological parameter:
25 ℃ of knitting workshop temperature, humidity 60 degree, cylinder loom, 15 rev/mins of the speed of a motor vehicle.
Cure: temperature was cured in the cylinder machine 20 seconds for 80 ℃.
Boiling-off:
Materials: hydrogen peroxide 7% NaOH 5%
Bleeding agent 0.6% stabilizing agent 4%
98 ℃ of 30 seconds times of temperature
Dyeing:
Materials: silk levelling agent: 0.6% Gardenia Yellow 8%
Salt: 5%
Temperature: 80 ℃ of temperature retention times: 40 minutes
Soap: cleanser consumption 0.6%
The fixation softness:
20 seconds 1% time of formaldehyde-free color fixing agent
The VELVET matte that 20 seconds 4% time of softener produces with described process is smooth, does not fall hair, the color yellow, and COLOR FASTNESS reaches national standard.

Claims (10)

1, a kind of soybean fiber velvet and production method, it is characterized in that with the fibre and soya yarn be raw material, its technological process of production is: fibre and soya cotton yarn → knitting → cure → preliminary shearing → boiling-off → dye → soap → fixation softness → dehydration → fine pruning → typing → clot.
2, soybean fiber velvet according to claim 1 and production method is characterized in that knitting employing cylinder loom weaves with speed of a motor vehicle 15-25 rev/min under workshop temperature 19-25 ℃, the situation of humidity 50-60 ℃ degree.
3, soybean fiber velvet according to claim 1 and production method is characterized in that curing with the cylinder machine and cured 20 seconds under 80 ℃ of temperature.
4, soybean fiber velvet according to claim 1 and production method is characterized in that boiling-off is with hydrogen peroxide (H 2O 2), NaOH (NaCl), bleeding agent, stabilizing agent adds the poach refining for batching, the consumption of various batchings is (accounting for the water percetage by weight):
Hydrogen peroxide 4-7%
NaOH 2-5%
Bleeding agent 0.3-0.6%
Stabilizing agent 2-4%
5, according to claim 1 or 4 described soybean fiber velvet and production methods, it is characterized in that scouring process is to add bleeding agent, stabilizing agent when heating water to 30 ℃, add hydrogen peroxide, NaOH when continuing to heat then, keep temperature 30-50 second when being warming up to 80-98 ℃ again after cloth is added to 65 ℃.
6, soybean fiber velvet according to claim 1 and production method, the raw materials used prescription that it is characterized in that dyeing are (accounting for the water percetage by weight):
Silk levelling agent 0.4-0.6%
Dyestuff 2-8%
Salt (NaCl) 2-5%
7, according to the production method of claim 1 or 4 described soybean fiber velvets, it is characterized in that water, cloth and various raw material are put into dyeing machine, be stirred to while heating when being warming up to 80-90 ℃ and be incubated 20-40 minute.
8, the production method of soybean fiber velvet according to claim 1, the addition that it is characterized in that the soap washing cleanser are the heavy 0.4-0.6% of water.
9, the production method of soybean fiber velvet according to claim 1, it is characterized in that it is raw material that the fixation softening step adopts formaldehyde-free color fixing agent, softener, the addition of formaldehyde-free color fixing agent is the heavy 0.5-1% of water, and the addition of softener is the 3-4% of water weight.
10,, it is characterized in that fixation time, soft time respectively are 20 seconds according to the production method of claim 1 or 9 described soybean fiber velvets.
CN 01137359 2001-12-06 2001-12-06 Soybean fiber velvet and production method thereof Pending CN1423003A (en)