CN1298981A - Polyester film coiled material plastic flooring and production method thereof - Google Patents
Polyester film coiled material plastic flooring and production method thereof Download PDFInfo
- Publication number
- CN1298981A CN1298981A CN 00123325 CN00123325A CN1298981A CN 1298981 A CN1298981 A CN 1298981A CN 00123325 CN00123325 CN 00123325 CN 00123325 A CN00123325 A CN 00123325A CN 1298981 A CN1298981 A CN 1298981A
- Authority
- CN
- China
- Prior art keywords
- polyester film
- floor leather
- production method
- coiled
- pattern
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The production method of floor leather is characterized by that it uses polyester film as surface layer, and uses no base material, and uses a printing machine to print pattern on the back surface of polyester film, then uses a coating machine to coat polyvinyl chloride foamed resin on the polyester film printed with pattern, then the polyester film is fed into drying oven, and foamed and plasticized at 150-200 deg.C for 2-5 min, and finally the polyester film floor leather is made up through the processes of cooling, cutting edge and rolling. Its advantages are simple process, less equipment, saving energy and low cost. High definition, wear resistance, heat resistance, tear resistance, high strength and good insulating property.
Description
The invention belongs to a kind of is the plastic floor leather and the production technology thereof of superficial layer with the polyester film.
In order to adapt to worker, agricultural production high speed development, the needs of the market boom, the improving constantly of living standards of the people, house decorative material and automobile decoration material have become the focus that people pay close attention to.At present, coiled material floor leather product is because of characteristics such as laying conveniently, pattern is attractive in appearance, easy to clean, price are suitable, and is very popular, is widely used in all trades and professions.But the production technology more complicated of original production plastic floor leather product, investment is big and the cost height, yield poorly, and consumes a large amount of manpower and materials etc.Must be in its production process through base material for setting off (as domestic general nonwoven fabric, cotton, glass felt, release liners, paper etc.).In order to make product surface smooth, need at first on base material, to be coated with the priming coat thickener during production, through press polish after the preplasticizing, coat the foaming thickener afterwards again, after the preplasticizing in the surface of semi-finished printing various patterns, be coated with the upper layer thickener then, carry out high temperature foaming and plasticizing fully,, form product through press polish, cooling, side cut, rolling, the anti-wear performance of its product is poor, cold tolerance is poor, tear resistance is relatively poor, insulating properties are low, and production unit also needs large number quipments, fund input.
Purpose of the present invention exactly in order to address the above problem, provides a kind of wear-resisting, tear-resistant performance height, and the coiled polyester film as floor leather of good insulation preformance.
Another object of the present invention provides that a kind of technology is simple, production cost is low, quality is good, output is high and the production method of easy-operating coiled polyester film as floor leather.
Purpose of the present invention realizes by following technical proposals, that is:
Coiled polyester film as floor leather comprises polyester film superficial layer and foaming layer, and foaming layer is directly to be coated on the polyester film that is printed on pattern, the formation that combines after foaming, polyester film be superficial layer also be substrate layer.
The production method of coiled polyester film as floor leather product comprises:
1, adopt polyester film to do superficial layer.This polyester film had both been done superficial layer and had also been replaced substrate layer.
2, by the back face printing pattern of printing machine at polyester film;
3, be coated with the foam polyvinyl chloride resin by coating machine on the polyester film of pattern being printed on, then, enter baking oven and in the 150-200 Celsius temperature, foam and plastified 2-5 minute, after cooling, side cut, rolling, promptly become the coiled polyester film as floor leather final products.
Also can adopt polyester film through printing machine behind polyester film back face printing pattern, will be printed on the polyester film of pattern and sheet material that industrial chemicals is made is combined into plastic floor leather through compounding machine.
The advantage of coiled polyester film as floor leather production method of the present invention:
1, compare with original production process, technology is simple, easy to operate, equipment is few, small investment, the saving energy.
2, polyester film had both been done superficial layer and had also been done substrate layer simultaneously in process of production, and the real many usefulness of a film that belong to the original production process ratio, had both been saved raw material and also reduced cost.
3, compare with original production process, the new technology of this invention is not only saved several procedures in process of production, simultaneously also save substrate layer and polyvinyl chloride priming coat, thereby made production process saving great deal of raw materials, human and material resources, equipment, fund reduce cost.
4, compare with the product that former explained hereafter goes out, coiled polyester film as floor leather, surface smoothness is good, attractive in appearance, the clear patterns degree is good, heat resistance is good, tear(ing) strength is good, intensity is high, good insulation preformance, and cold tolerance is good.
5, with original production process than the one-level rate that has improved product.
(1) base material of former employing is a nonwoven fabric, and the nonwoven surface injustice has wandering fibre or micelle, even priming operation thickener in process of production also can't make final product surface smooth fully, can't print complete pattern, therefore causes the one-level rate of product lower.
(2) present, adopt other base material (as glass felt, paper, release liners etc.) too, except that the air spots of product, in process of production owing to reasons such as the pulling force of base material and tearing strengths, phenomenon of rupture is often arranged, make that production can't steady and continuous production.Not only reduce one-level rate, output, waste great deal of raw materials simultaneously.
This product can be widely used in floor file face (plastic floor leather) and decorate leather etc.
Embodiment:
The production method of coiled polyester film as floor leather: be with polyester film web uncoiler uncoiling, when needing joint, behind the make-up machine joint, enter cloth storage device, enter printing machine again and carry out the back face printing pattern, polyester film coated machine in printing back is coated with the foam polyvinyl chloride thickener being printed on the polyester film of pattern, again through 150-200 degree centigrade baking oven foaming plasticizing 2-5 minute, cool off back, side cut, rolling, form coiled polyester film as floor leather.
Claims (3)
1, coiled polyester film as floor leather comprises superficial layer and foaming layer, it is characterized in that superficial layer is the polyester rete.
2, the production method of coiled polyester film as floor leather, it is characterized in that comprising the employing polyester film, through printing machine behind polyester film back face printing pattern, with coating machine application of polyvinyl resin thereon, foaming is 2-5 minute under the 150-200 Celsius temperature, then through cooling off, be distributed into coiled polyester film as floor leather.
3, the production method of coiled polyester film as floor leather according to claim 2 is characterized in that adopting polyester film, behind polyester film back face printing pattern, will be printed on the polyester film of pattern and sheet material that industrial chemicals make be combined into plastic floor leather through compounding machine through printing machine.