CN1272074C - 超细活化复合吸附型室内空气净化剂 - Google Patents
超细活化复合吸附型室内空气净化剂 Download PDFInfo
- Publication number
- CN1272074C CN1272074C CN 200310112788 CN200310112788A CN1272074C CN 1272074 C CN1272074 C CN 1272074C CN 200310112788 CN200310112788 CN 200310112788 CN 200310112788 A CN200310112788 A CN 200310112788A CN 1272074 C CN1272074 C CN 1272074C
- Authority
- CN
- China
- Prior art keywords
- indoor air
- air purification
- purification agent
- zeolite
- type
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明公开了超细活化复合吸附型室内空气净化剂,将经过活化处理和超细加工后的凹凸棒石粘土或海泡石粘土和沸石按配比混匀,进行聚合造粒并烘干,再与颗粒状活性炭按比例混合,即得到本发明所指的“超细活化复合吸附型室内空气净化剂”。这些物质都具有大的比表面积和丰富且复杂的分子孔道。由于它们的分子孔道分别与苯、甲苯、二甲苯、甲醛、氨气以及放射性氡等污染物分子的大小相匹配,这些有害气体分子在运动过程中作为吸附质被吸附,特别是当净化剂被安装在风机一端而强迫室内气体从净化剂中通过时,有害气体则被快速过滤和吸附在吸附剂分子孔道中,从而达到净化空气的目的。
Description
技术领域
本发明涉及一种室内空气净化剂,尤其是一种针对现代建筑物以及室内装饰装修引起的空气污染而进行复合吸附净化的空气净化剂,同时适用于车、船等交通工具内的空气净化,属于环境保护技术领域,具体涉及超细活化复合吸附型室内空气净化剂。
背景技术
现代城镇居民约80%的时间在室内和交通工具内度过,各种新型建筑材料、建筑添加剂以及装饰修造成了室内空气的普遍被污染。新出厂或新修饰、油漆后的车、船等交通工具内也有较高浓度的有机污染物。
现有的空气净化装置主要起到过滤颗粒悬浮物和灭菌的作用,对有机污染物以及氨气、放射性氡等的净化效果不够理想。
发明内容
本发明的目的在于:在充分了解室内空气中最具危害性的主要污染物分子特征的基础上,提出一种超细活化复合吸附型室内空气净化剂,该净化剂以分子筛的物理吸附方式,对室内空气中的苯、甲苯、二甲苯、甲醛、氨气以及放射性氡等常见的主要污染气体进行吸附净化,具有安全无副作用和吸附量大,使用寿命长的特点。
本发明的技术解决方案是:该净化剂主要组成物质为经过酸或碱活化、烘干处理和超细粉碎加工的海泡石族粘土矿物、沸石以及活性炭。这些物质都具有大的比表面积和丰富且复杂的分子孔道。由于它们的分子孔道分别与苯、甲苯、二甲苯、甲醛、氨气以及放射性氡等污染物分子的大小相匹配,这些有害气体分子由于范德华力的作用在运动过程中作为吸附质被吸附在净化剂的分子孔道中,特别是当净化剂被安装在风机一端而强迫室内气体从净化剂中通过时,室内空气中的有害气体则被快速过滤和吸附在与其分子大小相匹配的吸附剂分子孔道中,从而达到净化空气的目的。
为了便于空气流通和对污染物的吸剂,将经过活化处理和超细加工后的凹凸棒石粘土或海泡石粘土和沸石按配比混匀,进行聚合造粒并烘干,再与颗粒状活性炭按比例混合,即得到本发明所指的“超细活化复合吸附型室内空气净化剂”。
首先分别将前三种矿物材料在1%-10%浓度盐酸或者硫酸溶液中进行浸泡,之后用纯水或清水漂洗,脱水后再在200-400℃的温度下烘干,然后分别将它们在超细粉碎设备中粉碎到800至2000目的细度。将经过上述处理后的活性超细凹凸棒石粘土或者海泡石粘土与活性超细沸石按1∶10至10∶1的比例混匀,加水聚合造粒,制成各种有利于空气流通和物质交换的颗粒,再经烘干后与颗粒状活性炭按1∶2至20∶1的比例混合,即得到本发明所指的“超细活化吸附型室内空气净化剂”。
将“超细活化复合吸附型室内空气净化剂”与风扇或各种空气净化器进行组合,则形成动态的吸附净化。
本发明还可以有很多其他实施方式。例如,粘土矿物凹凸棒石和海泡石可以完全互相代替,也可以部分用膨润土代替;沸石可以选用丝光沸石、斜发沸石等各种天然沸石或人造沸石以及它们的混合物;几种主要成分的配比可以根据污染物结构的不同而有较大范围的调整,甚至可以不采用其中的某种材料,其中凹凸棒石粘土或者海泡石粘土即海泡石族粘土矿物与沸石的配比为1∶10至10∶1,无机矿物材料与活性炭的配比为1∶2至20∶1;活性炭可以是颗粒状或粉末状产品;对上述无机矿物材料可以进行20%以下浓度的盐酸、硫酸或者NaOH溶液浸泡,纯水或清水漂洗,脱水后再在200℃-400℃的温度下烘干等不同程度的活化处理,也可以粉碎到80目-2000目各种不同的粒度;对活性炭也可以进行20%以下浓度的盐酸、硫酸或者NaOH溶液浸泡活化处理;上述组分经加水聚合造粒,可以制成各种有利于空气流通和物质交换的颗粒状,也可以直接用粉末状活性炭与上述超细无机矿物混合、造粒、烘干。
依照本发明所生产的“超细活化复合吸附型室内空气净化剂”,经过江苏省环境监测中心分别进行静态和动态净化效果监测,结果表明都具有良好的净化效果。其中与风扇进行组合的动态净化器在1M3试验仓内的动态净化监测结果是:在甲醛、氨气、苯和甲苯污染浓度分别为国家室内空气质量卫生标准GB18883-2002标准值9倍、5倍、458倍和162倍的情况下,4小时动态吸附净化结果全部达到上述国标的卫生标准,吸附净化率分别为89.9%、80.0%、99.8%和100%。
具体实施方式
本发明的超细活化吸附型室内空气净化剂主要以凹凸棒石粘土或海泡石粘土、沸石和活性炭为原料。
首先分别将前三种矿物材料在1%-10%浓度盐酸或者硫酸溶液中进行浸泡,之后用纯水或清水漂洗,脱水后再在200-400℃的温度下烘干,然后分别将它们在超细粉碎设备中粉碎到800至2000目的细度。将经过上述处理后的活性超细凹凸棒石粘土或者海泡石与活性超细沸石按1∶10至10∶1的比例混匀,加水聚合造粒,制成各种有利于空气流通和物质交换的颗粒,再经烘干后与颗粒状活性炭按1∶2至20∶1的比例混合,即得到本发明所指的“超细活化吸附型室内空气净化剂”。
监测结果证明,本发明对现代城镇室内空气中的主要有害气体污染物具有十分有效的吸附净化作用,而且生产原料来源丰富,成本较低。
实例1:首先分别将凹凸棒石粘土、海泡石粘土、沸石三种无机矿物材料在1%浓度盐酸溶液中进行浸泡,之后用纯水或清水漂洗,脱水后再在200℃的温度下烘干,然后分别将它们在超细粉碎设备中粉碎到800目的细度。将经过上述处理后的活性超细凹凸棒石粘土或者海泡石与活性超细沸石按1∶10的比例混匀,加水聚合造粒,制成各种有利于空气流通和物质交换的颗粒,再经烘干后与颗粒状活性炭按1∶2的比例混合,即得到本发明所指的“超细活化吸附型室内空气净化剂”。
实例2:首先分别将凹凸棒粘土、海泡石粘土、沸石三种矿物材料在10%浓度硫酸溶液中进行浸泡,之后用纯水或清水漂洗,脱水后再在400℃的温度下烘干,然后分别将它们在超细粉碎设备中粉碎到2000目的细度。将经过上述处理后的活性超细凹凸棒石粘土或者海泡石与活性超细沸石按10∶1的比例混匀,加水聚合造粒,制成各种有利于空气流通和物质交换的颗粒,再经烘干后与颗粒状活性炭按20∶1的比例混合,即得到本发明所指的“超细活化吸附型室内空气净化剂”。
实例3:首先分别将凹凸棒粘土、海泡石粘土、沸石三种矿物材料在5%浓度盐酸溶液中进行浸泡,之后用纯水或清水漂洗,脱水后再在300℃的温度下烘干,然后分别将它们在超细粉碎设备中粉碎到1500目的细度。将经过上述处理后的活性超细凹凸棒石粘土或者海泡石与活性超细沸石按1∶1的比例混匀,加水聚合造粒,制成各种有利于空气流通和物质交换的颗粒,再经烘干后与颗粒状活性炭按10∶1的比例混合,即得到本发明所指的“超细活化吸附型室内空气净化剂”。
Claims (10)
1、一种超细活化复合吸附型室内空气净化剂,其特征在于:该净化剂主要成份包括:经过活化处理和超细粉碎加工的海泡石族粘土矿物、沸石以及活性炭,海泡石族粘土矿物和沸石按配比混匀后与活性炭按比例混合即得该净化剂。
2、根据权利要求1所述超细活化复合吸附型室内空气净化剂,其特征在于:海泡石族粘土矿物有凹凸棒石粘土和海泡石粘土,或膨润土代替。
3、根据权利要求1所述超细活化复合吸附型室内空气净化剂,其特征在于:沸石为各种天然沸石或人造沸石以及它们的混合物。
4、根据权利要求3所述超细活化复合吸附型室内空气净化剂,其特征在于:沸石为丝光沸石或斜发沸石。
5、根据权利要求1所述超细活化复合吸附型室内空气净化剂,其特征在于:活性炭是颗粒状或粉末状产品。
6、根据权利要求1所述超细活化复合吸附型室内空气净化剂,其特征在于:净化剂中几种主要成分的配比根据污染物结构的不同而有较大范围的调整,其中凹凸棒石粘土或者海泡石粘土与沸石的配比为1∶10至10∶1,无机矿物材料与活性炭的配比为1∶2至20∶1。
7、根据权利要求1所述超细活化复合吸附型室内空气净化剂,其特征在于:对海泡石族粘土矿物、沸石进行不同程度的活化处理,在1%-20%浓度盐酸、硫酸或者NaOH溶液中进行浸泡活化,之后用纯水或清水漂洗,脱水后再在200℃-400℃的温度下烘干,经过活化处理的无机矿物材料粉碎到80至2000目。
8、根据权利要求1所述超细活化复合吸附型室内空气净化剂,其特征在于:对活性炭用20%以下浓度的盐酸、硫酸或NaOH溶液浸泡活化处理。
9、根据权利要求1所述超细活化复合吸附型室内空气净化剂,其特征在于:经过活化处理和超细粉碎的无机矿物材料经加水聚合造粒并烘干,制成各种有利于空气流通和物质交换的颗粒状,然后与颗粒状活性炭按比例混合。
10、根据权利要求1所述超细活化复合吸附型室内空气净化剂,其特征在于:直接用粉末状活性炭按比例与超细无机矿物混合、造粒、烘干。