Prior art keywords
concavo
mineral
attapulgite
ore deposit
convex excellent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 03158243
Other languages
English (en)
Other versions
CN1552529A (zh
Inventor
许盛英
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 03158243 priority Critical patent/CN1224463C/zh
Publication of CN1552529A publication Critical patent/CN1552529A/zh
Application granted granted Critical
Publication of CN1224463C publication Critical patent/CN1224463C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Landscapes

  • Manufacture And Refinement Of Metals (AREA)

Abstract

一种凹凸棒湿法选矿工艺,其特征在于这种工艺是为了解决目前凹凸棒的生产中,原矿利用率较低的一种新工艺。该工艺是将含有泥土等杂质的凹凸棒矿混合物,经粉碎后输入水解池中,浸泡24小时后,用高压气泵进行冲翻,并通过用不锈钢钢丝制成的圆桶筛筛去1毫米以上的杂质,送入有坡度的沉淀池中,继续用高压气泵进行冲翻,12小时后,由于凹凸棒矿的比重较轻,它在整个沉淀物中的最上层,用泥浆泵吸取这部分凹凸棒矿送入平底沉淀池中,15小时后放出多余的水,经过2-3天的自然干燥,取出这部分凹凸棒矿即为半成品矿,以此达到精选凹凸棒矿的目的。本发明能有效的提高凹凸棒矿的利用率和矿的凹凸棒含量,由于凹凸棒矿在水中崩解率较高,湿法选矿所得到的凹凸棒矿,经干燥后,物理加工性能特好,可以深加工为高档产品。

Description

凹凸棒湿法选矿工艺
技术领域:
本发明涉及一种湿法选矿工艺,具体涉及一种凹凸棒湿法选矿工艺。
背景技术:
凹凸棒矿的矿藏量在我国并不多,主要分布在江苏省的盱眙县、六合县,安徽省的明光市。由于早期对凹凸棒矿的性能和价值认识不足,开采比较混乱,造成泥土等杂质掺入凹凸棒矿中,大大降低了凹凸棒矿的总体含量,有的凹凸棒矿已失去了开采价值。面对这种状况,有关部门已开始采取了一些解决措施,以控制胡乱开采的局面。但如何充分利用大量的人为造成的废矿,以及低品位的矿源再开发,就成为一个大难题。有关单位已投入了大量的资金和人力,收效并不明显。
中国专利公开号CN 14541181A,公开日是2003年11月05日,名称为“精制的绿坡缕石粘土”,公开了“用于生产绿坡缕石粘土(漂白土)的方法,它能显著除去其他种类的粘土和矿物质,从而产生提高的性能。使用了一种独特的分散剂,它能将单一绿坡缕石颗粒完全分散在水中,这样可将颗粒保持在悬浮液中,并且所述分散剂不能完全分散其他粘土和矿物种,这样可以很容易地通过各种方法将其分离开来。”
上述发明专利文件的说明书和权利要求书中,还重点描述:“一种处理天然存在的粘土矿石以将坡缕石粘土与其他的物质分离开来的方法,包括以下步骤:碾压粘土矿石,在水中加入分子量为4,000-5,000的聚丙烯酸钠,用聚丙烯酸钠水溶液制备粘土矿石的浆液以将绿坡缕石粘土分散在水中,将分散的绿坡缕石粘土与未分散的物质分离,和干燥分散的绿坡缕石粘土。”
在权利要求11中描述:“权利要求1的方法,其中干燥的坡缕石粘土包含吸附在其上的聚丙烯酸钠。”
“绿坡缕石粘土”在我国又称为“凹凸棒矿”,是同一类粘土矿。绿坡缕石粘土,可以广泛应用于食品、油脂和医药等加工行业,而“精制的绿坡缕石粘土”中含有“聚丙烯酸钠”等分散剂,不能广泛应用于食品、油脂和医药等加工行业,否则,将会直接影响到其产品的质量和其它指标。因此,“精制的绿坡缕石粘土”,应用范围较窄。
发明内容:
本发明的目的是克服现有技术中不足之处,提供一种不需要添加任何分散剂,利用凹凸棒矿的物理性能,用湿法选矿的工艺,有效的提高凹凸棒矿的利用率和矿的凹凸棒含量。
本发明的工艺是将含有泥土等杂质的凹凸棒矿混合物,经粉碎并输入水解池中,浸泡24小时后,用高压气泵进行冲翻,并通过用不锈钢钢丝制成的园桶筛筛去1毫米以上的杂质,送入有坡度的沉淀池中,继续用高压气泵进行冲翻,12小时后,由于凹凸棒矿的比重较轻,它在整个沉淀物中的最上层,用泥浆泵吸取这部分凹凸棒矿送入平底沉淀池中,15小时后放出多余的水,经过2-3天的自然干燥,取出这部分凹凸棒矿即为成品矿,以此达到精选凹凸棒矿的目的。
本发明不需要添加任何分散剂,用湿法选矿工艺,就可以精选凹凸棒矿,并能提高凹凸棒矿的利用率和矿的凹凸棒含量;由于凹凸棒中不含聚丙烯酸钠等分散剂,没有改变凹凸棒的各种指标,物理和化学性能都比较好,用途广泛,可以深加工为高档产品,具有较好的经济和社会效益。
具体实施方式:
本发明解决其技术问题所采用的实施技术方式是:
1、初选凹凸棒矿:在矿区选择一个平坦的晒场,将需要处理的凹凸棒矿运至该晒场,均匀铺开,厚度在8厘米以内。晾晒1--3天后,凹凸棒矿开始有裂纹,并稍有自然散开现象,此时可以进行翻晒,并挑去一些能人工检出的泥土杂质,以此减少下一工序的工作量。
2、粉碎和水解:经过初步筛选晒干的凹凸棒矿运至生产厂区内,进行粉碎,细度控制在3毫米以内,并输入水解池中(水解池的大小可根据生产单位的条件确定),水解池中的水一定要高于凹凸棒矿,浸泡24小时后,用高压气泵进行冲翻,与此同时,将水解后的凹凸棒矿泥浆,用不锈钢钢丝制成的圆桶筛,筛去1毫米以上的杂质,送入有坡度的沉淀池中。
3、沉淀:筛选后的凹凸棒矿泥浆,进入有坡度的沉淀池后,继续用高压气泵进行冲翻,12小时后,由于凹凸棒矿的比重较轻,它分布在整个沉淀物中的最上层,用泥浆泵吸取这部分凹凸棒矿泥浆,送入平底沉淀池中,平底沉淀池的大小可根据生产单位的条件确定,15小时后放出多余的水,经过2-3天的自然干燥,取出这部分凹凸棒矿即为成品矿。

Claims (2)

1、一种凹凸棒湿法选矿工艺,其特征在于,不需要添加任何分散剂,利用凹凸棒矿的物理性能,将需要处理的凹凸棒矿,经过自然晾晒、粉碎、水解、浸泡、冲翻、筛分、沉淀、转池、沉淀、放水和自然干燥的新工艺,精选凹凸棒矿。
2、根据权利要求1所述的凹凸棒湿法选矿工艺,其特征在于,将含有泥土等杂质的凹凸棒矿混合物,经粉碎后输入水解池中,浸泡24~36小时,用高压气泵进行冲翻,并通过用不锈钢钢丝制成的园桶筛筛去1毫米以上的杂质,送入有坡度的沉淀池中,继续用高压气泵进行冲翻,12小时后,由于凹凸棒矿的比重较轻,它在整个沉淀物中的最上层,用泥浆泵吸取这部分凹凸棒矿送入平底沉淀池中,15小时后放出多余的水,经过2-3天的自然干燥,取出这部分凹凸棒矿即为成品矿,以此达到精选凹凸棒矿的目的。
CN 03158243 2003-09-18 2003-09-18 凹凸棒湿法选矿工艺 Expired - Fee Related CN1224463C (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 03158243 CN1224463C (zh) 2003-09-18 2003-09-18 凹凸棒湿法选矿工艺

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 03158243 CN1224463C (zh) 2003-09-18 2003-09-18 凹凸棒湿法选矿工艺

Publications (2)

Publication Number Publication Date
CN1552529A CN1552529A (zh) 2004-12-08
CN1224463C true CN1224463C (zh) 2005-10-26

Family

ID=34324111

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 03158243 Expired - Fee Related CN1224463C (zh) 2003-09-18 2003-09-18 凹凸棒湿法选矿工艺

Country Status (1)

Country Link
CN (1) CN1224463C (zh)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101279064B (zh) * 2008-05-28 2010-08-25 陈士芳 凹凸棒醇基灭虱制剂
CN101284104B (zh) * 2008-05-28 2010-08-25 陈士芳 凹凸棒灭虱粉剂
CN101279065B (zh) * 2008-05-28 2010-08-25 陈士芳 凹凸棒水基灭虱制剂

Families Citing this family (12)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101284125B (zh) * 2008-05-28 2010-09-29 陈士芳 凹凸棒水基冻疮制剂
CN101585694B (zh) * 2009-03-27 2011-10-26 解云 凹凸棒膏状内墙腻子的生产方法
CN101585684B (zh) * 2009-03-27 2011-08-24 解云 凹凸棒内墙腻子粉
CN101875541B (zh) * 2010-03-26 2011-12-07 许盛英 凹凸棒油泥及其生产方法
CN101875554B (zh) * 2010-03-26 2011-12-07 许盛英 彩色凹凸棒油泥及其生产方法
CN101875836B (zh) * 2010-03-26 2011-12-07 许盛英 凹凸棒防水油泥及其生产方法
CN101973059B (zh) * 2010-07-30 2011-08-24 许庆华 白色凹凸棒软陶泥的生产方法
CN101973063B (zh) * 2010-07-30 2011-07-20 许庆华 棕色凹凸棒软陶泥的生产方法
CN101973733B (zh) * 2010-07-30 2011-08-24 许庆华 紫色凹凸棒软陶泥的生产方法
CN101973734B (zh) * 2010-07-30 2012-05-23 许庆华 橙色凹凸棒软陶泥的生产方法
CN101973062B (zh) * 2010-07-30 2011-07-20 许庆华 黑色凹凸棒软陶泥的生产方法
CN101973732B (zh) * 2010-07-30 2011-07-20 许庆华 金色凹凸棒软陶泥的生产方法

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101279064B (zh) * 2008-05-28 2010-08-25 陈士芳 凹凸棒醇基灭虱制剂
CN101284104B (zh) * 2008-05-28 2010-08-25 陈士芳 凹凸棒灭虱粉剂
CN101279065B (zh) * 2008-05-28 2010-08-25 陈士芳 凹凸棒水基灭虱制剂

Also Published As

Publication number Publication date
CN1552529A (zh) 2004-12-08

Similar Documents

Publication Publication Date Title
CN1224463C (zh) 凹凸棒湿法选矿工艺
CN101254959B (zh) 膨润土污水处理方法
CN101062502A (zh) 弱磁性铁矿石的选矿新工艺
CN101126125A (zh) 一种铝土矿选矿尾矿综合利用方法
CN101219828B (zh) 蓝藻水华生物絮凝剂及制备
CN103785198A (zh) 一种高效深锥污泥浓缩装置
CN105327773B (zh) 回收霞石矿尾矿中霞石矿的方法
CN103553274A (zh) 一种中纤板生产废水的处理工艺
CN1775812A (zh) 玉米淀粉污水零排放生产工艺
CN208327584U (zh) 一种处理油田污水的高效过滤器
CN112456672A (zh) 一种矿井水处理方法及***
Zhang et al. Factors affecting microalgae harvesting efficiencies using electrocoagulation-flotation for lipid extraction
CN101607225A (zh) 一种极细粒煤的选别工艺
CN103964653A (zh) 一种造纸厂废水回收处理工艺
CN202860678U (zh) 一种高效脱泥组合设备
CN1884092A (zh) 一种脱除硫酸锌溶液中钙离子的方法
CN102107953A (zh) 处理糖蜜酒精废液的方法
CN111035991A (zh) 一种铁尾矿干排脱水***及工艺
CN102863130A (zh) 活性污泥的处理方法
CN211799351U (zh) 一种铁尾矿干排脱水***
CN205035216U (zh) 造纸厂白水多级处理回用***
CN108543623A (zh) 一种海泡石的提纯工艺
CN107936844B (zh) 一种水性涂料
CN113562884A (zh) 一种矿山排土场淋溶水处理方法
CN105621837A (zh) 用水葫芦处理剩余污泥中重金属的***及方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
C19 Lapse of patent right due to non-payment of the annual fee
CF01 Termination of patent right due to non-payment of annual fee