CN109722177A - Shield lower identification of fingerprint tempered glass film layered structure - Google Patents

Shield lower identification of fingerprint tempered glass film layered structure Download PDF

Info

Publication number
CN109722177A
CN109722177A CN201910095294.3A CN201910095294A CN109722177A CN 109722177 A CN109722177 A CN 109722177A CN 201910095294 A CN201910095294 A CN 201910095294A CN 109722177 A CN109722177 A CN 109722177A
Authority
CN
China
Prior art keywords
glue
layer
line
fingerprint
identification
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201910095294.3A
Other languages
Chinese (zh)
Inventor
严伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dongguan Xinya Photoelectric Technology Co Ltd
Original Assignee
Dongguan Xinya Photoelectric Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dongguan Xinya Photoelectric Technology Co Ltd filed Critical Dongguan Xinya Photoelectric Technology Co Ltd
Priority to CN201910095294.3A priority Critical patent/CN109722177A/en
Publication of CN109722177A publication Critical patent/CN109722177A/en
Pending legal-status Critical Current

Abstract

The invention discloses shield lower identification of fingerprint tempered glass film layered structure, including AF layers, AG or AR layers, filling glue-line or glue layer, toughened glass layer, silk-screen layer, the first glue-line, first base material layer, high resiliency glue-line, the second substrate layer, the second glue-line, release film and identification of fingerprint regional opening.The present invention is poured into using high transparent resin or organosilicon, filling, supplement, the mode of splicing is in conjunction with identification of fingerprint regional opening, reach opposed flattened integrated tempered glass film, it can make photoresist type using filling glue-line or glue layer simultaneously, ultrasonic type and acoustic wave type pass through, across to reach identification of fingerprint effect, meet the protection glass of hand-set lid curved surface or plane simultaneously, identification of fingerprint regional opening is circle, ellipse, triangle, square, quadrangle, polygon etc., it is combined into tempered glass film surface using single-layer or multi-layer coating structure, to reach anti-fingerprint (AF) and anti-dazzle (AG) or antireflection (AR).

Description

Shield lower identification of fingerprint tempered glass film layered structure
Technical field
The present invention relates to tempered glass technical field of membrane, specially shield lower identification of fingerprint tempered glass film layered structure.
Background technique
Tempered glass belongs to safety glass, and glass has fairly good antiwear characteristic, and very rigid, Vickers hardness Reaching 622 to 701, tempered glass is a kind of prestressed glass in fact, for the intensity for improving glass, usually used chemistry or object The method of reason forms compression in glass surface, and glass bears to offset skin stress first when external force, to improve carrying energy Power, reinforcing glass itself anti-wind pressure, cold and heat, impact etc., and tempered glass protective film is then higher for mobile phone screen The protection of security level, but fingerprint (photoresist type, ultrasonic type and acoustic wave type) can not there is shielding down for existing tempered glass film It passes through, penetrate the drawbacks of glass, so that the use scope of tempered glass film is limited, for this purpose, it is proposed that shielding lower fingerprint Recognize tempered glass film layered structure.
Summary of the invention
The purpose of the present invention is to provide lower identification of fingerprint tempered glass film layered structure is shielded, to solve above-mentioned background technique The problem of middle proposition.
To achieve the above object, the invention provides the following technical scheme: shielding lower identification of fingerprint tempered glass film layered structure, It include: AF layers, AG or AR layers, filling glue-line or glue layer, toughened glass layer, silk-screen layer, the first glue-line, first base material layer, height Elastic glue-line, the second substrate layer, the second glue-line, release film and identification of fingerprint regional opening, AF layers of the bottom are connected with AG Or AR layers, and AG or AR layers of bottom is connected with toughened glass layer, the right end of the toughened glass layer inner surface offers fingerprint Regional opening is recognized, and the inner surface of identification of fingerprint regional opening is provided with filling glue-line or glue layer, the toughened glass layer Bottom be connected with silk-screen layer, and the bottom of silk-screen layer is connected with first base material layer, the first base material layer by the first glue-line Bottom the second substrate layer is connected with by high resiliency glue-line, and the bottom of the second substrate layer be connected with by the second glue-line it is release Film.
The present invention is exactly to cancel AG and AR layers there are also second of technical solution, identification of fingerprint tempered glass film under such screen Cost is just greatly saved, structure is as shown in Figure 2.
Above two scheme all the second glue-line all be using high resiliency glue-line (using silica gel, rubber, silicon rubber, PU glue, Acryl glue, OCA, UV glue, thermosol or pressure-sensitive thermosol, thickness 0.001~1mm 10g ~ 20000g viscosity), also referred to as full glue Second glue-line can also be become common glue-line (using silica gel, rubber, silicon rubber, PU glue, pressure by formula tempered glass film, this product Gram force glue, OCA, UV glue, thermosol or pressure-sensitive thermosol, thickness 0.001~1mm 10g ~ 10000g viscosity) it is also referred to as side glue formula steel Change glass-film.
In addition the silk-screen layer 5 of the technical program can be located at 7 lower position of first base material layer, form Fig. 3 structure.
Preferably, hand painting, spraying, plating or Vacuum Deposition are used for described AF layers, and AF layers are AF anti-fingerprint liquid or the anti-finger of AF Line ingot, with a thickness of 0.0001~1mm.
Preferably, hand painting, spraying, plating or Vacuum Deposition are used for the AG or AR layers, and AG or AR layers is AG(anti-glare) Organosilicon or resin or AR(antireflection) organosilicon or resin, AG or AR layers are with a thickness of 0.0001~1mm.This AG or AR layers It is that can cancel this layer.
Preferably, the filling glue-line or glue layer are high transparent resin (heat curing type, vulcanization type, AB agent mixing type, UV Type).
Preferably, the toughened glass layer is sodium calcium, middle aluminium or high aluminosilicate glass, with a thickness of 0.001~1mm.
Preferably, the silk-screen layer is silk-screen, bat printing, transfer, printing, spraying, UV develops or offset printing, with a thickness of 0.0001~1mm.
Preferably, first glue-line, the second glue-line and high resiliency glue-line are silica gel, rubber, silicon rubber, PU glue, pressure Gram force glue, OCA, UV glue, thermosol or pressure-sensitive thermosol, the thickness of the first glue-line, the second glue-line and high resiliency glue-line are 0.001~1mm, and the viscosity of the first glue-line and high resiliency glue-line is 10g~10000g, the viscosity of the second glue-line be 0g~ 1000g。
Preferably, the first base material layer and the second substrate layer be transparent, optical grade, anti-blue light PET, Pi, PU, TPU, PE, PC, PMMA or PP film, and the thickness of first base material layer and the second substrate layer is 0.001~1mm.
Preferably, the release film is fluorine element release film, non-silicon release film or silicon release film, with a thickness of 0.001~ 1mm。
Preferably, the shape of the identification of fingerprint regional opening be circle, ellipse, triangle, square, quadrangle, Polygon etc..
Compared with prior art, beneficial effects of the present invention are as follows:
The present invention offers identification of fingerprint regional opening in the right end of toughened glass layer inner surface, and in identification of fingerprint regional opening Inner surface be provided with filling glue-line or glue layer, the side pour into, fill using high transparent resin or organosilicon, supplementing, splicing Formula reaches opposed flattened integrated tempered glass film in conjunction with identification of fingerprint regional opening, while utilizing filling glue-line or glue Layer can be such that photoresist type, ultrasonic type and acoustic wave type passes through, across to reach identification of fingerprint effect, while meet hand-set lid The protection glass of curved surface or plane, identification of fingerprint regional opening is circle, ellipse, triangle, square, quadrangle, polygon Shape etc. is combined into tempered glass film surface using single-layer or multi-layer coating structure, to reach anti-fingerprint (AF) and anti-dazzle (AG) or antireflection (AR).
Detailed description of the invention
Fig. 1 is schematic structural view of the invention.
Fig. 2 is to cancel AG layers and AR schematic diagram of a layer structure.
Fig. 3 is that silk-screen layer is located at schematic diagram below first base material layer.
In figure: 1 AF layers, 2 AG or AR layers, 3 filling glue-lines or glue layer, 4 toughened glass layers, 5 silk-screen layers, 6 first glue Layer, 7 first base material layers, 8 high resiliency glue-lines, 9 second substrate layers, 10 second glue-lines, 11 release films, 12 identification of fingerprint regions are opened Hole.
Specific embodiment
Following will be combined with the drawings in the embodiments of the present invention, and technical solution in the embodiment of the present invention carries out clear, complete Site preparation description, it is clear that described embodiments are only a part of the embodiments of the present invention, instead of all the embodiments.It is based on Embodiment in the present invention, it is obtained by those of ordinary skill in the art without making creative efforts every other Embodiment shall fall within the protection scope of the present invention.
AF layer 1, AG or AR layer 2 of the invention, filling glue-line or glue layer 3, toughened glass layer 4, silk-screen layer 5, the first glue Layer 6, first base material layer 7, high resiliency glue-line 8, the second substrate layer 9, the second glue-line 10, release film 11 and identification of fingerprint regional opening 12 components are universal standard part or component as known to those skilled in the art, and structure and principle are all this technology personnel It is learnt by technical manual or is known by routine experiment method.
Embodiment one:
Referring to Fig. 1, shielding lower identification of fingerprint tempered glass film layered structure, including AF layer 1, AG or AR layer 2, filling glue-line or benefit Glue-line 3, toughened glass layer 4, silk-screen layer 5, the first glue-line 6, first base material layer 7, high resiliency glue-line 8, the second substrate layer 9, second Glue-line 10, release film 11 and identification of fingerprint regional opening 12, AF layer 1 are applied using hand, and AF layer 1 is AF anti-fingerprint liquid, thickness For 0.0001~1mm, the bottom of AF layer 1 is connected with AG or AR layer 2, and AG or AR layer 2 can be cancelled, and forms whooe-rubber type or side glue formula Tempering film another kind structure, AG or AR layer 2 are applied using hand, and AG or AR layer 2 is AG(anti-glare) organosilicon, AG or AR layer 2 are thick Degree is 0.0001~1mm, and the bottom of AG or AR layer 2 is connected with toughened glass layer 4, and toughened glass layer 4 is soda-lime glass, thick Degree is 0.001~1mm, and the right end of 4 inner surface of toughened glass layer offers identification of fingerprint regional opening 12, and identification of fingerprint region is opened The shape in hole 12 is circle, and the inner surface of identification of fingerprint regional opening 12 is provided with filling glue-line or glue layer 3, thoroughly using height The mode that ming tree rouge or organosilicon are poured into, filled, supplementing, splicing is combined with identification of fingerprint regional opening 12, reaches opposed flattened The tempered glass film of one, while photoresist type, ultrasonic type and acoustic wave type can be made smoothly to lead to using filling glue-line or glue layer 3 It crosses, across to reach identification of fingerprint effect, while meeting the protection glass of hand-set lid curved surface or plane, identification of fingerprint region is opened Hole 12 is circle, ellipse, triangle, square, quadrangle, polygon etc., is combined using single-layer or multi-layer coating structure At tempered glass film surface, to reach anti-fingerprint (AF) and anti-dazzle (AG) or antireflection (AR), fills glue-line or glue layer 3 is Heat curing type high transparent resin, the bottom of toughened glass layer 4 are connected with silk-screen layer 5, silk-screen layer 5 can also as under first base material 7, Silk-screen layer 5 is silk-screen, and with a thickness of 0.0001~1mm, and the bottom of silk-screen layer 5 is connected with first base material by the first glue-line 6 The bottom of layer 7, first base material layer 7 is connected with the second substrate layer 9, first base material layer 7 and the second substrate layer by high resiliency glue-line 8 9 be transparent membrane, and the thickness of first base material layer 7 and the second substrate layer 9 is 0.001~1mm, and the second substrate layer 9 Bottom is connected with release film 11 by the second glue-line 10, and the first glue-line 6, the second glue-line 10 and high resiliency glue-line 8 are silica gel, the The thickness of one glue-line 6, the second glue-line 10 and high resiliency glue-line 8 is 0.001~1mm, and the first glue-line 6 and high resiliency glue-line 8 Viscosity be 10g~10000g, the viscosity of the second glue-line 10 is 0g~1000g, and release film 11 is fluorine element release film, thickness For 0.001~1mm.
Embodiment two:
Referring to Fig. 1, shielding lower identification of fingerprint tempered glass film layered structure, including AF layer 1, AG or AR layer 2, filling glue-line or benefit Glue-line 3, toughened glass layer 4, silk-screen layer 5, the first glue-line 6, first base material layer 7, high resiliency glue-line 8, the second substrate layer 9, second Glue-line 10, release film 11 and identification of fingerprint regional opening 12, AF layer 1 is using spraying, and AF layer 1 is AF anti-fingerprint liquid, thickness For 0.0001~1mm, the bottom of AF layer 1 is connected with AG or AR layer 2, and AG or AR layer 2 can be cancelled, and forms whooe-rubber type or side glue formula Tempering film another kind structure, AG or AR layer 2 are using spraying, and AG or AR layer 2 is AG(anti-glare) resin, 2 thickness of AG or AR layer It is connected with toughened glass layer 4 for the bottom of 0.0001~1mm, and AG or AR layer 2, toughened glass layer 4 is middle lead glass, thickness For 0.001~1mm, the right end of 4 inner surface of toughened glass layer offers identification of fingerprint regional opening 12, identification of fingerprint regional opening 12 shape is ellipse, and the inner surface of identification of fingerprint regional opening 12 is provided with filling glue-line or glue layer 3, thoroughly using height The mode that ming tree rouge or organosilicon are poured into, filled, supplementing, splicing is combined with identification of fingerprint regional opening 12, reaches opposed flattened The tempered glass film of one, while photoresist type, ultrasonic type and acoustic wave type can be made smoothly to lead to using filling glue-line or glue layer 3 It crosses, across to reach identification of fingerprint effect, while meeting the protection glass of hand-set lid curved surface or plane, identification of fingerprint region is opened Hole 12 is circle, ellipse, triangle, square, quadrangle, polygon etc., is combined using single-layer or multi-layer coating structure At tempered glass film surface, to reach anti-fingerprint (AF) and anti-dazzle (AG) or antireflection (AR), fills glue-line or glue layer 3 is Vulcanization type high transparent resin, the bottom of toughened glass layer 4 are connected with silk-screen layer 5, silk-screen layer 5 can also as under first base material 7, Silk-screen layer 5 is bat printing, and with a thickness of 0.0001~1mm, and the bottom of silk-screen layer 5 is connected with first base material by the first glue-line 6 The bottom of layer 7, first base material layer 7 is connected with the second substrate layer 9, first base material layer 7 and the second substrate layer by high resiliency glue-line 8 9 be optical grade film, and the thickness of first base material layer 7 and the second substrate layer 9 is 0.001~1mm, and the second substrate layer 9 Bottom release film 11 is connected with by the second glue-line 10, the first glue-line 6, the second glue-line 10 and high resiliency glue-line 8 are rubber, The thickness of first glue-line 6, the second glue-line 10 and high resiliency glue-line 8 is 0.001~1mm, and the first glue-line 6 and high resiliency glue-line 8 viscosity is 10g~10000g, and the viscosity of the second glue-line 10 is 0g~1000g, and release film 11 is non-silicon release film, thick Degree is 0.001~1mm.
Embodiment three:
Referring to Fig. 1, shielding lower identification of fingerprint tempered glass film layered structure, including AF layer 1, AG or AR layer 2, filling glue-line or benefit Glue-line 3, toughened glass layer 4, silk-screen layer 5, the first glue-line 6, first base material layer 7, high resiliency glue-line 8, the second substrate layer 9, second Glue-line 10, release film 11 and identification of fingerprint regional opening 12, AF layer 1 is using plating, and AF layer 1 is AF anti-fingerprint ingot, thickness For 0.0001~1mm, the bottom of AF layer 1 is connected with AG or AR layer 2, and AG or AR layer 2 can be cancelled, and forms whooe-rubber type or side glue formula Tempering film another kind structure, AG or AR layer 2 are using plating, and AG or AR layer 2 is AR(antireflection) organosilicon, AG or AR layer 2 are thick Degree is 0.0001~1mm, and the bottom of AG or AR layer 2 is connected with toughened glass layer 4, and toughened glass layer 4 is high aluminosilicate glass, With a thickness of 0.001~1mm, the right end of 4 inner surface of toughened glass layer offers identification of fingerprint regional opening 12, identification of fingerprint region The shape of aperture 12 is square, and the inner surface of identification of fingerprint regional opening 12 is provided with filling glue-line or glue layer 3, is utilized The mode that high transparent resin or organosilicon are poured into, filled, supplementing, splicing is combined with identification of fingerprint regional opening 12, reaches opposite Smooth integrated tempered glass film, while photoresist type, ultrasonic type and acoustic wave type can be made smooth using filling glue-line or glue layer 3 By, across to reach identification of fingerprint effect, while meeting the protection glass of hand-set lid curved surface or plane, identification of fingerprint region Aperture 12 is circle, ellipse, triangle, square, quadrangle, polygon etc., utilizes single-layer or multi-layer coating structure group Tempered glass film surface is synthesized, to reach anti-fingerprint (AF) and anti-dazzle (AG) or antireflection (AR), fills glue-line or glue layer 3 For AB agent mixing type high transparent resin, the bottom of toughened glass layer 4 is connected with silk-screen layer 5, and silk-screen layer 5 can also be as the first base Under material 7, silk-screen layer 5 is spraying, and with a thickness of 0.0001~1mm, and the bottom of silk-screen layer 5 is connected with the by the first glue-line 6 The bottom of one substrate layer 7, first base material layer 7 is connected with the second substrate layer 9, first base material layer 7 and second by high resiliency glue-line 8 Substrate layer 9 is PU film, and the thickness of first base material layer 7 and the second substrate layer 9 is 0.001~1mm, and the second substrate layer 9 bottom is connected with release film 11 by the second glue-line 10, and the first glue-line 6, the second glue-line 10 and high resiliency glue-line 8 are pressure gram Power glue, the thickness of the first glue-line 6, the second glue-line 10 and high resiliency glue-line 8 are 0.001~1mm, and the first glue-line 6 and high-elastic Property glue-line 8 viscosity be 10g~10000g, the viscosity of the second glue-line 10 is 0g~1000g, and release film 11 is silicon release film, It is with a thickness of 0.001~1mm.
Example IV:
Referring to Fig. 1, shielding lower identification of fingerprint tempered glass film layered structure, including AF layer 1, AG or AR layer 2, filling glue-line or benefit Glue-line 3, toughened glass layer 4, silk-screen layer 5, the first glue-line 6, first base material layer 7, high resiliency glue-line 8, the second substrate layer 9, second Glue-line 10, release film 11 and identification of fingerprint regional opening 12, AF layer 1 uses Vacuum Deposition, and AF layer 1 is AF anti-fingerprint ingot, thick Degree is 0.0001~1mm, and the bottom of AF layer 1 is connected with AG or AR layer 2, and AG or AR layer 2 can be cancelled, and forms whooe-rubber type or side glue Formula tempering film another kind structure, AG or AR layer 2 use Vacuum Deposition, and AG or AR layer 2 is AR(antireflection) resin, AG or AR layer 2 It is connected with toughened glass layer 4 with a thickness of the bottom of 0.0001~1mm, and AG or AR layer 2, toughened glass layer 4 is soda-lime glass, With a thickness of 0.001~1mm, the right end of 4 inner surface of toughened glass layer offers identification of fingerprint regional opening 12, identification of fingerprint region The shape of aperture 12 is polygon, and the inner surface of identification of fingerprint regional opening 12 is provided with filling glue-line or glue layer 3, is utilized The mode that high transparent resin or organosilicon are poured into, filled, supplementing, splicing is combined with identification of fingerprint regional opening 12, reaches opposite Smooth integrated tempered glass film, while photoresist type, ultrasonic type and acoustic wave type can be made smooth using filling glue-line or glue layer 3 By, across to reach identification of fingerprint effect, while meeting the protection glass of hand-set lid curved surface or plane, identification of fingerprint region Aperture 12 is circle, ellipse, triangle, square, quadrangle, polygon etc., utilizes single-layer or multi-layer coating structure group Tempered glass film surface is synthesized, to reach anti-fingerprint (AF) and anti-dazzle (AG) or antireflection (AR), fills glue-line or glue layer 3 For UV type high transparent resin, the bottom of toughened glass layer 4 is connected with silk-screen layer 5, silk-screen layer 5 can also as under first base material 7, Silk-screen layer 5 is offset printing, and with a thickness of 0.0001~1mm, and the bottom of silk-screen layer 5 is connected with first by the first glue-line 6 The bottom of substrate layer 7, first base material layer 7 is connected with the second substrate layer 9, first base material layer 7 and the second base by high resiliency glue-line 8 Material layer 9 is PP film, and the thickness of first base material layer 7 and the second substrate layer 9 is 0.001~1mm, and the second substrate layer 9 Bottom release film 11 is connected with by the second glue-line 10, the first glue-line 6, the second glue-line 10 and high resiliency glue-line 8 are pressure-sensitive Thermosol, the thickness of the first glue-line 6, the second glue-line 10 and high resiliency glue-line 8 are 0.001~1mm, and the first glue-line 6 and height The viscosity of elastic glue-line 8 is 10g~10000g, and the viscosity of the second glue-line 10 is 0g~1000g, and release film 11 is that non-silicon is release Film, with a thickness of 0.001~1mm.
In use, the right end in 4 inner surface of toughened glass layer offers identification of fingerprint regional opening 12, and in identification of fingerprint The inner surface of regional opening 12 is provided with filling glue-line or glue layer 3, is poured into, filled, mended using high transparent resin or organosilicon The mode fill, spliced is combined with identification of fingerprint regional opening 12, reaches opposed flattened integrated tempered glass film, while utilizing and filling out It fills glue-line or glue layer 3 can be such that photoresist type, ultrasonic type and acoustic wave type passes through, across to reach identification of fingerprint effect, together The protection glass of Shi Fuhe hand-set lid curved surface or plane, identification of fingerprint regional opening 12 are circle, ellipse, triangle, just Rectangular, quadrangle, polygon etc. are combined into tempered glass film surface using single-layer or multi-layer coating structure, to reach anti-finger Line (AF) and anti-dazzle (AG) or antireflection (AR).
In addition there are also other alternative structure schemes, such as silk-screen layer to be located under first base material layer for this technical solution, Form new structure.AG or AR layers of formation another structure can also be cancelled.It is all the frame mode of this patent protection.
It although an embodiment of the present invention has been shown and described, for the ordinary skill in the art, can be with A variety of variations, modification, replacement can be carried out to these embodiments without departing from the principles and spirit of the present invention by understanding And modification, the scope of the present invention is defined by the appended.

Claims (10)

1. identification of fingerprint tempered glass film layered structure under screen, including AF layers (1), AG or AR layers (2), filling glue-line or glue layer (3), toughened glass layer (4), silk-screen layer (5), the first glue-line (6), first base material layer (7), high resiliency glue-line (8), the second substrate Layer (9), the second glue-line (10), release film (11) and identification of fingerprint regional opening (12), it is characterised in that: AF layers described (1) Bottom is connected with AG or AR layers (2), and the bottom of AG or AR layers (2) is connected with toughened glass layer (4), the toughened glass layer (4) right end of inner surface offers identification of fingerprint regional opening (12), and the inner surface setting of identification of fingerprint regional opening (12) There are filling glue-line or glue layer (3), the bottom of the toughened glass layer (4) is connected with silk-screen layer (5), and the bottom of silk-screen layer (5) Portion is connected with first base material layer (7) by the first glue-line (6), and the bottom of the first base material layer (7) passes through high resiliency glue-line (8) It is connected with the second substrate layer (9), and the bottom of the second substrate layer (9) is connected with release film (11) by the second glue-line (10).
2. identification of fingerprint tempered glass film layered structure under screen according to claim 1, it is characterised in that: AF layers described (1) using hand apply, spraying, plating or Vacuum Deposition, and AF layer (1) be AF anti-fingerprint liquid or AF anti-fingerprint ingot, with a thickness of 0.0001~1mm.
3. identification of fingerprint tempered glass film layered structure under screen according to claim 1, it is characterised in that: the AG or AR Layer (2) applied using hand, spraying, plating or Vacuum Deposition, and AG or AR layer (2) is AG(anti-glare) organosilicon or resin or AR(resist Reflection) organosilicon or resin, AG or AR layers (2) are with a thickness of 0.0001~1mm.
4. identification of fingerprint tempered glass film layered structure under screen according to claim 1, it is characterised in that: the filling glue Layer or glue layer (3) are high transparent resin (heat curing type, vulcanization type, AB agent mixing type, UV type).
5. identification of fingerprint tempered glass film layered structure under screen according to claim 1, it is characterised in that: the tempering glass Glass layer (4) is sodium calcium, middle aluminium or high aluminosilicate glass, with a thickness of 0.001~1mm.
6. identification of fingerprint tempered glass film layered structure under screen according to claim 1, it is characterised in that: the silk-screen layer It (5) is silk-screen, bat printing, transfer, printing, spraying, UV development or offset printing, with a thickness of 0.0001~1mm.
7. identification of fingerprint tempered glass film layered structure under screen according to claim 1, it is characterised in that: first glue Layer (6), the second glue-line (10) and high resiliency glue-line (8) be silica gel, rubber, silicon rubber, PU glue, acryl glue, OCA, UV glue, Thermosol or pressure-sensitive thermosol, the thickness of the first glue-line (6), the second glue-line (10) and high resiliency glue-line (8) is 0.001~ 1mm, and the viscosity of the first glue-line (6) and high resiliency glue-line (8) is 10g~10000g, the viscosity of the second glue-line (10) is 0g ~1000g.
8. identification of fingerprint tempered glass film layered structure under screen according to claim 1, it is characterised in that: first base Material layer (7) and the second substrate layer (9) are transparent, optical grade, anti-blue light PET, Pi, PU, TPU, PE, PC, PMMA or PP film, And the thickness of first base material layer (7) and the second substrate layer (9) is 0.001~1mm.
9. identification of fingerprint tempered glass film layered structure under screen according to claim 1, it is characterised in that: the release film It (11) is fluorine element release film, non-silicon release film or silicon release film, with a thickness of 0.001~1mm.
10. identification of fingerprint tempered glass film layered structure under screen according to claim 1, it is characterised in that: the fingerprint The shape for recognizing regional opening (12) is circle, ellipse, triangle, square, quadrangle, polygon etc..
CN201910095294.3A 2019-01-31 2019-01-31 Shield lower identification of fingerprint tempered glass film layered structure Pending CN109722177A (en)