CN109358094A - 一种测量管道内壁涂层破损率的装置及方法 - Google Patents
一种测量管道内壁涂层破损率的装置及方法 Download PDFInfo
- Publication number
- CN109358094A CN109358094A CN201811318707.1A CN201811318707A CN109358094A CN 109358094 A CN109358094 A CN 109358094A CN 201811318707 A CN201811318707 A CN 201811318707A CN 109358094 A CN109358094 A CN 109358094A
- Authority
- CN
- China
- Prior art keywords
- electrode
- pipeline
- tubing
- protection system
- potentiostat
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (10)