CN109138354A - Inorganic grinding stone terrace - Google Patents

Inorganic grinding stone terrace Download PDF

Info

Publication number
CN109138354A
CN109138354A CN201810913595.8A CN201810913595A CN109138354A CN 109138354 A CN109138354 A CN 109138354A CN 201810913595 A CN201810913595 A CN 201810913595A CN 109138354 A CN109138354 A CN 109138354A
Authority
CN
China
Prior art keywords
grinding
parts
stone
setting
ground
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810913595.8A
Other languages
Chinese (zh)
Inventor
熊洪亮
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shenzhen Dingshun Xin Decoration Engineering Co Ltd Chongqing Branch
Original Assignee
Shenzhen Dingshun Xin Decoration Engineering Co Ltd Chongqing Branch
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shenzhen Dingshun Xin Decoration Engineering Co Ltd Chongqing Branch filed Critical Shenzhen Dingshun Xin Decoration Engineering Co Ltd Chongqing Branch
Priority to CN201810913595.8A priority Critical patent/CN109138354A/en
Publication of CN109138354A publication Critical patent/CN109138354A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of inorganic grinding stone terraces, are related to terrazzo field, mainly include quality proportioning: 5 parts of magnesia, 2 parts of magnesium chlorides, 50 parts of aggregates and 6 parts of water, to realize seamless surface, stain resistant, the function of maintenance easy to clean.

Description

Inorganic grinding stone terrace
Technical field
The present invention relates to a kind of inorganic grinding stone terraces, relate generally to terrazzo field.
Background technique
The stone materials such as artificial marble splice ground, and this floor material is easy to stockpile dirt there are gap, carry out pattern and set The difficulty of meter is big;And use the artificial marble plate of unsaturated polyester resin synthesis in the production process due to unsaturated polyester (UP) tree The big disadvantage of rouge cure shrinkage, so that prefabricated plate the shortcomings that there are poor flatness, while these material stiffness are too strong, Not impact resistance, epoxy grinding stone terrace not environmentally, are not prevented fires by epoxy resin, diluent, the synthesis of curing agent different materials.
Summary of the invention
For the above the deficiencies in the prior art, the present invention proposes a kind of inorganic grinding stone terrace, realizes seamless surface, resistance to be stained with Dirt, the technical effect of maintenance easy to clean.
In order to achieve the above objectives, the technical scheme is that its raw material includes following mass ratio: 5 parts of magnesia, 2 parts Magnesium chloride, 50 parts of aggregates and 6 parts of water.Wherein aggregate includes high-purity quartz stone particle, various colors glass particle and hard Ceramic particle.
Including basal plane processing, inorganic grinding stone base paint special, grid cloth laying, setting-out, it is laid with divider, stone, corase grinding, benefit Slurry, fine grinding, crystal face processing and waxing are mended in slurry, fine grinding.
The first step, basal plane processing: with airless shot machine handle ground, reach " precast concrete coat front surface it is clear Clean processing ASTM D4261-1983 " SP2 grades requirement, it is desirable that in bruting process guiding ruler measure, emphatically out-of-flatness place beat again It grinding, within 2 meters of guiding ruler 3mm of flatness requirement after polishing, expansion joint, subsiding crack, stress joint require perfusion India-rubber gum elastic processing, Preformed hole is covered by square round type to be retained, and corner is neat;
Inorganic grinding stone base paint special: second step carries out closing bottoming with osmosis type priming paint, and part carries out equating;
Third step, grid cloth are laid with, carry out ground laying with fiberglass gridding cloth, prevent grinding stone terrace from cracking.
4th step, setting-out: according to the shape of drawing, carrying out field lofting, and when setting-out pays attention to reference point, guarantees the standard of setting-out Really, while with coloured pencil setting-out lines are indicated, corrected repeatedly, it is ensured that keep the shape;
5th step is laid with divider: according to the route of setting-out, divider being fixed on the ground, is corrected repeatedly, guarantees divider Lower step construction can be carried out after acceptance(check) with the harmony of lines of setting-out;
6th step, stone: 5 parts of magnesia, 2 parts of magnesium chlorides, 50 parts of aggregates and 6 parts of water according to the proportion are stirred evenly with blender, It is laid with, then is smoothed out with trowelling machine, whether there is or not leakages to spread for re-inspection;
Corase grinding: 7th step after stone is completed 24 hours, carries out grinding process with the sander of the Buddha's warrior attendant bistrique of corase grinding, makes its bone Material exposes 70%, and edge is polished with manual angle grinder, while carrying out flatness control, guarantees within 2m guiding ruler 2mm;
8th step mends slurry: after corase grinding, arranging cleaning, carries out mending slurry processing, closed air bubbles hole and pore, reach plentiful It is smooth;
9th step, fine grinding: mending slurry after 24 hours, carries out fine grinding to the ground after mending slurry with fine grinding head sander, then confirm smooth Degree ensures within 3m guiding ruler 2mm while checking whether coating is uniform, after being chiseled out such as uneven place, stone again, and burnishing part Reason;
Tenth step mends slurry: after fine grinding, cleaning entire ground with floor-cleaning machine, after dry, mend slurry processing again, supply a gap;
Fine grinding: 11st step after 24 hours dry, then changed fine grinding bistrique and is refined, entire ground is made to reach unified standard Afterwards, this step is repeated twice carries out next step step again;
12nd step, crystal face processing: being processed by shot blasting after to be dried with fast polishing machine, need to use polishing machine when spraying buffing wax Cooperate white clean pad, reaches uniformly exhaustively effect;
13rd step, waxing: before formally coming into operation, cleaning ground with detergent, with the crystal face processor pair ground of 3M into Row waxing polishing, surface gloss ensure that sense organ is soft comfortable between 60-70, can come into operation after 24 hours.
It technical principle of the invention and has the beneficial effect that:
Bed course can pour rapidly with surface layer, pave, and can walk after 5 hours, can grind within 24 hours, polishing, nervous for the duration, The more building site of cross-operation, with being able to achieve wall integrated, integral seamless, arbitrary graphic pattern, moulding;Splendid incrustation effect Fruit, arbitrary hue leave to customize;It is waterproof, it does not absorb water, it is impermeable;Seamless surface, stain resistant, maintenance easy to clean;It does not crack, It is wear-resistant, not cracked, long service life;Possess the super ability of setting fire, grade of setting fire is up to A grades;Dry smooth surface With good non-skid property;Even if being also easy to repair and renovate after using many years;Soundproof effect is good, can reduce noise;Longevity Ordering period epoxy grinding stone is -40 years 20 years, and inorganic grinding stone can be with the building same service life.
Can sufficiently be withdrawn deposit architectural feature, the marble material characteristic having, and by the cast-in-place laying of large area, can be with Accomplish whole jointless construction, unavoidable splicing gap when marble being avoided to be laid with, no cutting, no splicing, globality is strong, The artistic floors that the surface layer of unique style is seamless.
Specific embodiment
Below in conjunction with embodiment, the technical solution in the present invention is clearly and completely described, it is clear that described Embodiment be only presently preferred embodiments of the present invention, instead of all the embodiments.Based on the embodiments of the present invention, originally Field those of ordinary skill every other embodiment obtained without making creative work, belongs to this hair The range of bright protection.
Embodiment
Its raw material includes following mass ratio: 5 parts of magnesia, 2 parts of magnesium chlorides, 50 parts of aggregates and 6 parts of water.Wherein aggregate includes There are high-purity quartz stone particle, various colors glass particle and hard ceramic particle.
Modulating process:
The first step, magnesium chloride weigh up 1 kilogram weight of magnesium chloride by weight;
Water dissolution is added in second step, magnesium chloride, and the dilution dissolution of 5 kg of water is added in 1 kilogram of magnesium chloride, and dissolved solubility is 30 Degree, (solubility of weather temperature difference magnesium chloride is different, and temperature is 20 degree in 25-35 degree, solubility proportion, temperature in 25-15 degree, Solubility proportion is 25 degree, and temperature is at 15 degree hereinafter, solubility proportion is 30 degree, as magnesium chloride solubility bottom curing time longer can be made Product to will appear hardness inadequate, play dirt, counter tide, solubility excessively high curing time will appear compared with the product to get outta there, crack, and become Color, hollowing fall off)
0.2 kilogram of toner is added in third step, color proportion, 1 kilogram of magnesia (the very few product made of toner will appear color difference);
4th step, aggregate proportion, aggregate different ratio varies in weight, and (5 kilograms of glass are added in 1 kilogram by taking bone glass sand as an example magnesia Glass sand aggregate, aggregate are that 2 kilograms of chicken girts are added in 1 kilogram of magnesia of chicken girt);
5th step, material mixture ratio construction, 1 kilogram of magnesia are added proportioned 0.5 kilogram of magnesium chloride, and 5 kilograms of glass sands stir Uniformly, mixing time 3 minutes, (magnesia can not stir evenly when magnesium chloride is less than ratio, solidification when ratio is higher than for construction laying Mgo surface afterwards can go out apparent magnesia and float powder, and aggregate will affect density and hardness less than Belgium, aggregate be higher than than It will affect adhesive force when example).
Including basal plane processing, inorganic grinding stone base paint special, grid cloth laying, setting-out, it is laid with divider, stone, corase grinding, benefit Slurry, fine grinding, crystal face processing and waxing are mended in slurry, fine grinding.
Working procedure: basal plane processing, setting-out, is laid with divider, stone, corase grinding, mends slurry, is thin inorganic grinding stone base paint special Mill mends slurry, fine grinding-crystal face processing-waxing.
1, basal plane is handled: being handled ground with the sharp Tyke 1-10DS airless shot machine in the U.S. one hundred, is reached " precast concrete painting Cover the cleaning treatment ASTM D4261-1983 of front surface " SP2 grades of requirements, large area Shot Blasting, detail sanding processing, enhancing The adhesive force on its ground, make ground without coarse granule, anhydrous clot, without dust, it is smooth.Standard: it is required that mattess is polished Uniformly, it cleans.Side measures the flatness of terrace, and side is polished emphatically.It is required that guiding ruler measures in bruting process, the ground of out-of-flatness emphatically Side polishes emphatically, the processing such as gap, crackle, preformed hole, corner within 2 meters of guiding ruler 3mm of flatness requirement after polishing.It is flexible Seam, subsiding crack, stress joint require perfusion India-rubber gum elastic processing, and preformed hole is covered by square round type to be retained, and corner is neat.
Stress joint, subsiding crack, expansion joint, Epo-Flex Terrazzo Membrane band flexible inorganic film Anti-crack layer.
2, inorganic grinding stone base paint special
Closing bottoming is carried out with osmosis type priming paint, and part carries out equating.
3, grid cloth is laid with
Terrace laying is carried out with fiberglass gridding cloth, prevents terrace from cracking.
4, setting-out
According to the shape of drawing, field lofting is carried out.Reference point is paid attention to when setting-out, guarantees the accurate of setting-out, while with coloured pencil mark Setting-out lines are shown, are corrected repeatedly, it is ensured that are kept the shape.
5, it is laid with divider
According to the route of setting-out, divider is fixed on the ground, is corrected repeatedly, guarantees the harmony of lines of divider and setting-out, After acceptance(check), lower step construction can be carried out.
6, stone
With 5 parts of magnesia according to the proportion, 2 parts of magnesium chlorides, 50 parts of aggregates and 6 parts of water, is stirred evenly, be laid with blender. It is smoothed out again with trowelling machine, whether there is or not leakages to spread for re-inspection.
7, it roughly grinds
After stone is completed 24 hours, grinding process is carried out with sander (the Buddha's warrior attendant bistrique of corase grinding), so that its aggregate is exposed 70%, side It is polished at angle with manual angle grinder, while carrying out flatness control, guaranteed within 2m guiding ruler 2mm.
8, slurry is mended
After corase grinding, cleaning (dust catcher) is arranged, carries out mending slurry processing, closed air bubbles hole and pore, reach plentiful smooth.
9, fine grinding
Slurry is mended after 24 hours, fine grinding is carried out to the ground after mending slurry with sander (fine grinding head), then confirm that flatness ensures that 3m is leaned on Within ruler 2mm, while checking whether coating is uniform, after being chiseled out such as uneven place, stone again, grinding process
10, slurry is mended
After fine grinding, entire ground is cleaned with floor-cleaning machine, after dry, slurry processing mended again, supplies a gap.
11, it refines
It after 24 hours dry, then change fine grinding bistrique and is refined, after so that entire ground is reached unified standard, this step repeats two It is secondary to carry out next step step again.
12, crystal face is handled
It is processed by shot blasting after to be dried with fast polishing machine, pays attention to that a people need to be sent specially to be processed by shot blasting corner.Sprinkling White clean pad need to be cooperated with polishing machine when buffing wax, reach uniformly exhaustively effect.
13, it waxes
Before formally coming into operation, ground is cleaned with detergent, carries out waxing polishing, surface with the crystal face processor pair ground of 3M Glossiness ensures that sense organ is soft comfortable between 60-70, can come into operation after 24 hours.
Suitable for the large public buildings such as domestic airport, hotel, star hotel, conference centre, exhibition center and advanced private The inorganic grinding stone terrace such as people's house plays the effect that can not be despised as emerging green material.
The foregoing is merely illustrative of the preferred embodiments of the present invention, is not intended to limit the invention, all in essence of the invention Within mind and principle, any modification, equivalent replacement, improvement and so on be should all be included in the protection scope of the present invention.

Claims (4)

1. inorganic grinding stone terrace, which is characterized in that its raw material includes following mass ratio: 5 parts of magnesia, 2 parts of magnesium chlorides, 50 parts of bones Material and 6 parts of water.
2. inorganic grinding stone terrace according to claim 1, it is characterised in that: the aggregate includes high-purity quartz stone Grain, various colors glass particle and hard ceramic particle.
3. the construction technology of inorganic grinding stone terrace according to claim 1, it is characterised in that: handled including basal plane, is inorganic Grinding stone base paint special, setting-out, is laid with divider, stone, corase grinding, mends slurry, fine grinding, mend slurry, refine, at crystal face grid cloth laying Reason and waxing.
4. the construction technology of inorganic grinding stone terrace according to claim 2, it is characterised in that:
The first step, basal plane processing: handling ground with airless shot machine, reaches " at the cleaning of precast concrete coating front surface Manage ASTM D4261-1983 " SP2 grades of requirements, it is desirable that guiding ruler measures in bruting process, and the place of out-of-flatness is polished emphatically emphatically, Within 2 meters of guiding ruler 3mm of flatness requirement after polishing, expansion joint, subsiding crack, stress joint require perfusion India-rubber gum elastic processing, in advance It boxes out to cover by square round type and retain, corner is neat;
Inorganic grinding stone base paint special: second step carries out closing bottoming with osmosis type priming paint, and part carries out equating;
Third step, grid cloth are laid with, carry out terrace laying with fiberglass gridding cloth, prevent grinding stone terrace from cracking '
4th step, setting-out: according to the shape of drawing, carrying out field lofting, and when setting-out pays attention to reference point, guarantees the accurate of setting-out, Setting-out lines are indicated with coloured pencil simultaneously, are corrected repeatedly, it is ensured that keep the shape;
5th step is laid with divider: according to the route of setting-out, divider being fixed on the ground, is corrected repeatedly, guarantees divider Lower step construction can be carried out after acceptance(check) with the harmony of lines of setting-out;
6th step, stone: 5 parts of magnesia, 2 parts of magnesium chlorides, 50 parts of aggregates and 6 parts of water according to the proportion are stirred evenly with blender, It is laid with, then is smoothed out with trowelling machine, whether there is or not leakages to spread for re-inspection;
Corase grinding: 7th step after stone is completed 24 hours, carries out grinding process with the sander of the Buddha's warrior attendant bistrique of corase grinding, makes its bone Material exposes 70%, and edge is polished with manual angle grinder, while carrying out flatness control, guarantees within 2m guiding ruler 2mm;
8th step mends slurry: after corase grinding, arranging cleaning, carries out mending slurry processing, closed air bubbles hole and pore, reach plentiful It is smooth;
9th step, fine grinding: mending slurry after 24 hours, carries out fine grinding to the ground after mending slurry with fine grinding head sander, then confirm smooth Degree ensures within 3m guiding ruler 2mm while checking whether coating is uniform, after being chiseled out such as uneven place, stone again, and burnishing part Reason;
Tenth step mends slurry: after fine grinding, cleaning entire ground with floor-cleaning machine, after dry, mend slurry processing again, supply a gap;
Fine grinding: 11st step after 24 hours dry, then changed fine grinding bistrique and is refined, entire ground is made to reach unified standard Afterwards, this step is repeated twice carries out next step step again;
12nd step, crystal face processing: being processed by shot blasting after to be dried with fast polishing machine, need to use polishing machine when spraying buffing wax Cooperate white clean pad, reaches uniformly exhaustively effect;
13rd step, waxing: before formally coming into operation, cleaning ground with detergent, with the crystal face processor pair ground of 3M into Row waxing polishing, surface gloss ensure that sense organ is soft comfortable between 60-70, can come into operation after 24 hours.
CN201810913595.8A 2018-08-13 2018-08-13 Inorganic grinding stone terrace Pending CN109138354A (en)