CN109076741A - 碱化土壤的改良方法 - Google Patents
碱化土壤的改良方法 Download PDFInfo
- Publication number
- CN109076741A CN109076741A CN201811197696.6A CN201811197696A CN109076741A CN 109076741 A CN109076741 A CN 109076741A CN 201811197696 A CN201811197696 A CN 201811197696A CN 109076741 A CN109076741 A CN 109076741A
- Authority
- CN
- China
- Prior art keywords
- soil
- thickness
- yellow mud
- desulfurized gypsum
- cotton stalk
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
本发明公开了碱化土壤的改良方法,包括以下步骤:(1)在土壤上挖出厚度为0.3m的深坑,并在坑中铺上厚度为0.1~0.2m的碳化棉杆,并将棉杆捣碎;(2)在碳化棉杆上铺上厚度为0.1m的黄泥,并在黄泥中浇水搅拌成流体,在流体的黄泥上均匀的撒上2cm的脱硫石膏;(3)在脱硫石膏上均匀的撒上复合肥,所述复合肥包括组分及重量比的碳铵5~7%、尿素2~4%、秸秆10~15%、磷肥1~2%、硫酸镁2~4%和黏土余量混合均匀后得到;(4)在土壤改良剂上铺设沙质土壤至与地面齐平。本发明能通过置换土壤中大量的钠离子,改善土壤化学组成,使得土壤形成团聚结构,增加土壤透水性、通气性,为作物生长创造良好的环境。
Description
技术领域
本发明涉及土壤改良领域,特别是涉及碱化土壤的改良方法。
背景技术
由于需要造林的区域大部分属于干旱风沙区,该区域的蒸发量高、土壤立地条件及结构较差、造林地土壤可溶性盐类较多并呈较高的碱性、渗透性和保水性差,该区域的土壤属于造林地盐碱化土壤,因此阻碍了造林苗木的正常生长。
根据调查,中国盐碱化土地已达23.3万平方公里,其中相当一部分分布在中国西北地区,如新疆、内蒙古、甘肃、青海、陕西等省或自治区。土壤盐碱化问题严重限制了当地的农业发展和生态防护林的建改,是西部生态环境建设中首先必需解决的问题之一。
发明内容
本发明的目的在于提供碱化土壤的改良方法。
本发明的目的是通过以下技术方案实现的:
碱化土壤的改良方法,包括以下步骤:
(1)在土壤上挖出厚度为0.3m的深坑,并在坑中铺上厚度为0.1~0.2m的碳化棉杆,并将棉杆捣碎;
(2)在碳化棉杆上铺上厚度为0.1m的黄泥,并在黄泥中浇水搅拌成流体,在流体的黄泥上均匀的撒上2cm的脱硫石膏;
(3)在脱硫石膏上均匀的撒上复合肥,所述复合肥包括组分及重量比的碳铵5~7%、尿素2~4%、秸秆10~15%、磷肥1~2%、硫酸镁2~4%和黏土余量混合均匀后得到;
(4)在土壤改良剂上铺设沙质土壤至与地面齐平。
所述脱硫石膏的水分为10~15%。
本发明能通过置换土壤中大量的钠离子,改善土壤化学组成,使得土壤形成团聚结构,增加土壤透水性、通气性,为作物生长创造良好的环境,同时,本发明制备的碱化土壤改良剂还含有促进植物生长的成分,能提高植物在碱化土壤中的生长活力;同时通过复合肥能够降低盐碱化土壤的pH值、土壤碱化度和土壤总盐量,并且降低了盐碱化土壤的改良成本,有效地提高了盐碱化土壤的改良效果,从而改善了土壤的质地和肥力。
具体实施方式
实施例1
本实施例提供的碱化土壤的改良方法,包括以下步骤:
(1)在土壤上挖出厚度为0.3m的深坑,并在坑中铺上厚度为0.1~0.2m的碳化棉杆,并将棉杆捣碎;
(2)在碳化棉杆上铺上厚度为0.1m的黄泥,并在黄泥中浇水搅拌成流体,在流体的黄泥上均匀的撒上2cm的脱硫石膏,所述脱硫石膏的水分为13%;
(3)在脱硫石膏上均匀的撒上复合肥,所述复合肥包括组分及重量比的碳铵6%、尿素3%、秸秆14%、磷肥2%、硫酸镁3%和黏土余量混合均匀后得到;
(4)在土壤改良剂上铺设沙质土壤至与地面齐平。
实施例2
本实施例提供的碱化土壤的改良方法,包括以下步骤:
(1)在土壤上挖出厚度为0.3m的深坑,并在坑中铺上厚度为0.1~0.2m的碳化棉杆,并将棉杆捣碎;
(2)在碳化棉杆上铺上厚度为0.1m的黄泥,并在黄泥中浇水搅拌成流体,在流体的黄泥上均匀的撒上2cm的脱硫石膏,所述脱硫石膏的水分为10%;
(3)在脱硫石膏上均匀的撒上复合肥,所述复合肥包括组分及重量比的碳铵5%、尿素4%、秸秆10%、磷肥2%、硫酸镁2%和黏土余量混合均匀后得到;
(4)在土壤改良剂上铺设沙质土壤至与地面齐平。
实施例3
本实施例提供的碱化土壤的改良方法,包括以下步骤:
(1)在土壤上挖出厚度为0.3m的深坑,并在坑中铺上厚度为0.1~0.2m的碳化棉杆,并将棉杆捣碎;
(2)在碳化棉杆上铺上厚度为0.1m的黄泥,并在黄泥中浇水搅拌成流体,在流体的黄泥上均匀的撒上2cm的脱硫石膏,所述脱硫石膏的水分为15%;
(3)在脱硫石膏上均匀的撒上复合肥,所述复合肥包括组分及重量比的碳铵7%、尿素2%、秸秆15%、磷肥1%、硫酸镁4%和黏土余量混合均匀后得到;
(4)在土壤改良剂上铺设沙质土壤至与地面齐平。
实施例4
本实施例提供的碱化土壤的改良方法,包括以下步骤:
(1)在土壤上挖出厚度为0.3m的深坑,并在坑中铺上厚度为0.1~0.2m的碳化棉杆,并将棉杆捣碎;
(2)在碳化棉杆上铺上厚度为0.1m的黄泥,并在黄泥中浇水搅拌成流体,在流体的黄泥上均匀的撒上2cm的脱硫石膏,所述脱硫石膏的水分为12%;
(3)在脱硫石膏上均匀的撒上复合肥,所述复合肥包括组分及重量比的碳铵7%、尿素2%、秸秆12%、磷肥1%、硫酸镁4%和黏土余量混合均匀后得到;
(4)在土壤改良剂上铺设沙质土壤至与地面齐平。
以上所述仅是本发明优选的实施方式,但本发明的保护范围并不局限于此,任何基于本发明所提供的技术方案和发明构思进行的改造和替换都应涵盖在本发明的保护范围内。
Claims (2)
1.碱化土壤的改良方法,其特征在于包括以下步骤:
(1)在土壤上挖出厚度为0.3m的深坑,并在坑中铺上厚度为0.1~0.2m的碳化棉杆,并将棉杆捣碎;
(2)在碳化棉杆上铺上厚度为0.1m的黄泥,并在黄泥中浇水搅拌成流体,在流体的黄泥上均匀的撒上2cm的脱硫石膏;
(3)在脱硫石膏上均匀的撒上复合肥,所述复合肥包括组分及重量比的碳铵5~7%、尿素2~4%、秸秆10~15%、磷肥1~2%、硫酸镁2~4%和黏土余量混合均匀后得到;
(4)在土壤改良剂上铺设沙质土壤至与地面齐平。
2.根据权利要求1所述的碱化土壤的改良方法,其特征在于:所述脱硫石膏的水分为10~15%。