CN108908807A - It is a kind of hot with mould method and mold production method - Google Patents

It is a kind of hot with mould method and mold production method Download PDF

Info

Publication number
CN108908807A
CN108908807A CN201811063843.0A CN201811063843A CN108908807A CN 108908807 A CN108908807 A CN 108908807A CN 201811063843 A CN201811063843 A CN 201811063843A CN 108908807 A CN108908807 A CN 108908807A
Authority
CN
China
Prior art keywords
mold
default
mold insert
injection mold
heat
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201811063843.0A
Other languages
Chinese (zh)
Inventor
王友金
陈武展
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Aux Air Conditioning Co Ltd
Original Assignee
Aux Air Conditioning Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Aux Air Conditioning Co Ltd filed Critical Aux Air Conditioning Co Ltd
Publication of CN108908807A publication Critical patent/CN108908807A/en
Pending legal-status Critical Current

Abstract

The present invention provides a kind of heat to match mould method and mold production method, is related to technical field of mold.The default mold insert in injection mold is heated to preset temperature first, then injection mold is molded, is then opened and measures the deflection after default mold insert thermal expansion, finally the gap between injection mold and default mold insert is modified according to deflection.Compared with prior art, since heat of the present invention uses the step of default mold insert in injection mold is heated to preset temperature with mould method, so the environment temperature of mold in process of production can be simulated, and it is carried out at such a temperature with mould, sealing effect is good, with the product non-trimming produced after mould and burr, presentation quality is high.

Description

It is a kind of hot with mould method and mold production method
Technical field
The present invention relates to technical field of mold, in particular to a kind of heat matches mould method and mold production method.
Background technique
As people's living standard is continuously improved and industrial technology is constantly progressive, the application of plastic cement products is more and more wider It is general, and people are higher and higher to the exterior quality requirement of plastic cement products.However, the exterior quality of plastic cement products largely takes Certainly in the manufacture level of plastic mould.Matching mould mode at present is just to match mould after mold all assembles, this common with mould side Method has following drawback:1, mold insert has gap, and leakproofness missing leads to problems such as product have overlap, burr, affects plastic cement products Exterior quality;2, temperature changes in process of production for the dynamic model of mold and cover half, between causing the active and inactive mold of mold to occur Gap, four serious overlaps in turning of parting line and product;3, the appearance and quality of product are affected and product processing success rate is low, Increase manufacturing cost.
Summary of the invention
In view of this, the present invention is directed to propose a kind of heat can simulate the environment of mold in process of production with mould method Temperature, and carried out at such a temperature with mould, sealing effect is good, and with the product non-trimming produced after mould and burr, presentation quality is high.
In order to achieve the above objectives, the technical proposal of the invention is realized in this way:
It is a kind of hot with mould method, including:Default mold insert in injection mold is heated to preset temperature;To injection mold into Row molding;It is opened and measures the deflection after default mold insert thermal expansion;According to deflection between injection mold and default mold insert Gap be modified.
Further, presetting mold insert is mavable module core, fixed mold core or sliding block.
Further, the step of default mold insert in injection mold being heated to preset temperature include:By die heater and note Mould connection;The heating agent of circulation is passed through to injection mold.
Further, in the step of default mold insert in injection mold being heated to preset temperature, preset temperature is at 40 degree To in the range of 70 degree.
Further, preset temperature is 55 degree.
Further, the step of molding to injection mold include:The moving template of injection mold is fixedly installed in conjunction One end of mould machine;The solid plate of injection mold is fixedly installed in the other end of clapper die spotting press;To moving template and determined using clapper die spotting press Template is molded.
Further, it is opened and includes the step of measuring the deflection after default mold insert thermal expansion:It will be moved using clapper die spotting press Template translates die sinking to the side far from solid plate;Deflection after the thermal expansion of default mold insert is measured.
Further, in the step of being measured to the deflection after the thermal expansion of default mold insert, using feeler gauge to deflection It measures.
Further, in the step of being modified according to deflection to the gap between injection mold and default mold insert, benefit Polishing processing is carried out to default mold insert with sander, to compensate to gap.
Compared with the existing technology, heat of the present invention has the advantage that with mould method:
Heat of the present invention matches mould method, the default mold insert in injection mold is heated to preset temperature first, then Injection mold is molded, be then opened and measures the deflection after default mold insert thermal expansion, finally according to deflection to note Gap between mould and default mold insert is modified.Compared with prior art, since heat of the present invention matches mould method Using the step of default mold insert in injection mold is heated to preset temperature, so mold can be simulated in process of production Environment temperature, and carried out at such a temperature with mould, sealing effect is good, with the product non-trimming produced after mould and burr, outside Appearance quality is high.
Another object of the present invention is to propose a kind of mold production method, it includes heat can simulate mould with mould method The environment temperature of tool in process of production, and carried out at such a temperature with mould, sealing effect is good, with the product produced after mould without winged Side and burr, presentation quality is high, high yield rate, reduces manufacturing cost.
In order to achieve the above objectives, the technical proposal of the invention is realized in this way:
A kind of mold production method matches mould method including above-mentioned heat, which includes with mould method:It will be in injection mold Default mold insert is heated to preset temperature;Injection mold is molded;It is opened and measures the deflection after default mold insert thermal expansion; The gap between injection mold and default mold insert is modified according to deflection.
Compared with the existing technology, mold production method of the present invention has the advantage that:
Mold production method of the present invention, it includes heat can simulate mold in process of production with mould method Environment temperature, and carried out at such a temperature with mould, sealing effect is good, with the product non-trimming produced after mould and burr, appearance Quality is high, high yield rate, reduces manufacturing cost.
With mould method, possessed advantage is identical compared with the existing technology with above-mentioned heat for the mold production method, herein not It repeats again.
Detailed description of the invention
The attached drawing for constituting a part of the invention is used to provide further understanding of the present invention, schematic reality of the invention It applies example and its explanation is used to explain the present invention, do not constitute improper limitations of the present invention.In the accompanying drawings:
Fig. 1 is the step block diagram that heat described in first embodiment of the invention matches mould method;
Fig. 2 is the step block diagram of mold production method described in second embodiment of the invention.
Specific embodiment
It should be noted that in the absence of conflict, the feature in embodiment and embodiment in the present invention can phase Mutually combination.
The present invention will be described in detail below with reference to the accompanying drawings and embodiments.
First embodiment
Please refer to Fig. 1, the embodiment of the invention provides it is a kind of heat match mould method, for machine-shaping cover half part and Dynamic model part is cooperated for the first time, and corrects the gap between cover half part and dynamic model part.It can simulate mold and produce Environment temperature in the process, and carried out at such a temperature with mould, sealing effect is good, with the product non-trimming produced after mould and hair Thorn, presentation quality are high.
The heat includes the following steps with mould method:
Step S101:Default mold insert in injection mold is heated to preset temperature.
Specifically, preset temperature is the environment temperature of the injection mold in process of production.In the prior art, cover half portion Divide and dynamic model part is carried out at normal temperature with mould, cover half part and dynamic model part cooperation are close, are warming up to after the completion with mould default Temperature produce product, at this time since the mold insert in cover half part and dynamic model part is made of Steel material, thus cover half part and Dynamic model part can thermally expand at an elevated temperature, cause the cooperation between cover half part and dynamic model part no longer tight It is close, gap can be generated between mold and mold insert in it, molten plastic can be flowed out by the gap so that product generate overlap and Burr.And in the present embodiment, carried out under preset temperature with mould so that in process of production cover half part and dynamic model part it Between cooperation it is still close, the sealing effect between injection mold and default mold insert in it is good, product be not in overlap and The phenomenon that burr.
It it should be noted that default mold insert is mold insert corresponding with product appearance forming surface in injection mold, or is note In mould with molten plastic circulation it is poor, be not easy the corresponding mold insert in the position filled up, or be matching requirements in injection mold More accurate mold insert, such as mavable module core, fixed mold core and sliding block.Specifically, default mold insert can be mavable module core, or cover half Benevolence can also be sliding block;Default mold insert can be the combination of mavable module core and fixed mold core, be also possible to the group of mavable module core and sliding block It closes, can also be the combination of fixed mold core and sliding block;Default mold insert can also be the combination of mavable module core, fixed mold core and sliding block three.
It is worth noting that, preset temperature is in the range of 40 degree to 70 degree, to simulate the production temperature of injection mold.This In embodiment, preset temperature is 55 degree, it is not limited to this, preset temperature can be 40 degree, or 70 degree, to default The size of temperature is not especially limited.
Specifically, step S101 includes two steps, respectively:
Step S1011:Die heater is connected to injection mold.
It is worth noting that, being provided with runner in default mold insert, one end of runner is connected to the inlet of injection mold, separately One end is connected to the leakage fluid dram of injection mold.The liquid outlet of die heater and the inlet of injection mold connect, and die heater can lead to It crosses liquid outlet and inlet and is passed through heating agent into default mold insert.The liquid return hole of die heater and the leakage fluid dram of injection mold connect, heat Matchmaker can return in die heater simultaneously after flowing in default mold insert.
Step S1012:The heating agent of circulation is passed through to injection mold.
In the present embodiment, when needing to heat default mold insert, die heater is opened, die heater heats heating agent, heats Heating agent afterwards respectively enters injection mold, and flows in default mold insert, transfers heat in default mold insert, to default edge Part carries out heat temperature raising, and then the heating agent after heat loss is returned in die heater, and die heater heats heating agent again, Zhou Erfu Begin, default mold insert is heated to preset temperature.
Step S102:Injection mold is molded.
Specifically, step S102 includes three steps, respectively:
Step S1021:The moving template of injection mold is fixedly installed in one end of clapper die spotting press.
Step S1022:The solid plate of injection mold is fixedly installed in the other end of clapper die spotting press.
Step S1023:Moving template and solid plate are molded using clapper die spotting press.
It should be noted that clapper die spotting press is a kind of mold bedding-in detection device of profession, it is mainly used for the Mold Making later period Pressurization molding is carried out to upper and lower mould when bedding-in.In the present embodiment, moving template and solid plate are cooperated using clapper die spotting press, so that dynamic model The mode in mode and solid plate in plate is bonded to each other shape forming cavity.
Step S103:It is opened and measures the deflection after default mold insert thermal expansion.
Specifically, step S103 includes three steps, respectively:
Step S1031:Moving template is translated into die sinking to the side far from solid plate using clapper die spotting press.
Step S1032:Deflection after the thermal expansion of default mold insert is measured.
It is worth noting that, in the present embodiment, being measured using feeler gauge to deflection, and record, after being convenient for Phase processing amendment.
Step S104:The gap between injection mold and default mold insert is modified according to deflection.
It is worth noting that, pincers processing is carried out to default mold insert in step S104, to be compensated to gap, so that Efficient sealing is kept between injection mold and default mold insert in it under preset temperature, gap will not be generated, to prevent There is overlap and burr in product.In the present embodiment, polishing processing is carried out to default mold insert using sander, to improve default mold insert Machining accuracy, prevent from generating gap between injection mold and default mold insert in it.
Heat described in the embodiment of the present invention matches mould method, and the default mold insert in injection mold is heated to default temperature first Degree, then molds injection mold, is then opened and measures the deflection after default mold insert thermal expansion, finally according to deformation Amount is modified the gap between injection mold and default mold insert.Compared with prior art, since heat of the present invention is matched Mould method uses the step of default mold insert in injection mold is heated to preset temperature, is producing so mold can be simulated Environment temperature in the process, and carried out at such a temperature with mould, sealing effect is good, with the product non-trimming produced after mould and hair Thorn, presentation quality are high.
Second embodiment
Referring to figure 2., the embodiment of the invention provides a kind of mold production methods, are used for production mould.Mold production Match mould method comprising heat in method.Wherein, heat matches the step of mould method and principle and the technical effect and first embodiment of generation Identical, to briefly describe, the present embodiment part does not refer to place, can refer to corresponding contents in first embodiment.
The mold production method includes the following steps:
Step S201:Injection mould processing is formed.
Step S202:Default mold insert in injection mold is heated to preset temperature.
Step S203:Injection mold is molded.
Step S204:It is opened and measures the deflection after default mold insert thermal expansion.
Step S205:The gap between injection mold and default mold insert is modified according to deflection.
The beneficial effect of mold production method and the beneficial effect of first embodiment described in the embodiment of the present invention are identical, This is repeated no more.
The foregoing is merely illustrative of the preferred embodiments of the present invention, is not intended to limit the invention, all in essence of the invention Within mind and principle, any modification, equivalent replacement, improvement and so on be should all be included in the protection scope of the present invention.

Claims (10)

1. a kind of heat matches mould method, which is characterized in that including:
Default mold insert in injection mold is heated to preset temperature;
The injection mold is molded;
It is opened and measures the deflection after the default mold insert thermal expansion;
The gap between the injection mold and the default mold insert is modified according to the deflection.
2. it is according to claim 1 heat match mould method, which is characterized in that the default mold insert be mavable module core, fixed mold core or Person's sliding block.
3. heat according to claim 1 matches mould method, which is characterized in that the default mold insert by injection mold heats Include to the step of preset temperature:
Die heater is connected to the injection mold;
The heating agent of circulation is passed through to the injection mold.
4. heat according to claim 1 matches mould method, which is characterized in that the default mold insert by injection mold heats In the step of to preset temperature, the preset temperature is in the range of 40 degree to 70 degree.
5. heat according to claim 4 matches mould method, which is characterized in that the preset temperature is 55 degree.
6. heat according to claim 1 matches mould method, which is characterized in that the step molded to the injection mold Suddenly include:
The moving template of the injection mold is fixedly installed in one end of clapper die spotting press;
The solid plate of the injection mold is fixedly installed in the other end of the clapper die spotting press;
The moving template and the solid plate are molded using the clapper die spotting press.
7. heat according to claim 6 matches mould method, which is characterized in that the die sinking and to measure the default mold insert heat swollen The step of deflection after swollen includes:
The moving template is translated into die sinking to the side far from the solid plate using the clapper die spotting press;
Deflection after the default mold insert thermal expansion is measured.
8. heat according to claim 7 matches mould method, which is characterized in that the change to after the default mold insert thermal expansion In the step of shape amount measures, the deflection is measured using feeler gauge.
9. it is according to claim 1 heat match mould method, which is characterized in that it is described according to the deflection to the injection mould In the step of gap between tool and the default mold insert is modified, polishing is carried out to the default mold insert using sander and is added Work, to be compensated to the gap.
10. a kind of mold production method, which is characterized in that match mould method including heat as described in any one of claim 1 to 9.
CN201811063843.0A 2018-08-22 2018-09-12 It is a kind of hot with mould method and mold production method Pending CN108908807A (en)