CN108637842A - A kind of high magnetic conduction embryo surface treatment process - Google Patents

A kind of high magnetic conduction embryo surface treatment process Download PDF

Info

Publication number
CN108637842A
CN108637842A CN201810445272.0A CN201810445272A CN108637842A CN 108637842 A CN108637842 A CN 108637842A CN 201810445272 A CN201810445272 A CN 201810445272A CN 108637842 A CN108637842 A CN 108637842A
Authority
CN
China
Prior art keywords
embryo
component
magnetic
surface treatment
treatment process
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201810445272.0A
Other languages
Chinese (zh)
Other versions
CN108637842B (en
Inventor
俞文敏
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hangzhou Lin'an he paramagnetic flux Electronics Co.,Ltd.
Original Assignee
Ling'an Hun Shun Flux Electronics Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ling'an Hun Shun Flux Electronics Co Ltd filed Critical Ling'an Hun Shun Flux Electronics Co Ltd
Priority to CN201810445272.0A priority Critical patent/CN108637842B/en
Publication of CN108637842A publication Critical patent/CN108637842A/en
Application granted granted Critical
Publication of CN108637842B publication Critical patent/CN108637842B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a kind of high magnetic conduction embryo surface treatment process, including sequentially connected feed end, transportation section and processing sections, transportation section includes horizontal conveyor belt, overturns component and close up component, overturning component includes the screw thread guide post that at least twice make magnetic embryo from flip horizontal at vertical state, close up component include multiple tracks be connected to screw thread guide post sliding groove, be connected to the pushing meanss that the end of sliding groove is used to that polylith magnetic embryo to be made to be bonded to each other, and setting is gradually drawn close in the end of multi-trace smoothing slot.The present invention passes through above-mentioned setting, magnetic embryo is directly entered after machine-shaping on horizontal transport band, by can be adjusted the angle in time after overturning the effect of component, prepare for the working face polishing that is harmonious of next step, due to the adjustment also by closing up component, multi-disc magnetic embryo is enable mutually to draw close abutting, the forced area for increasing bottom is not easy to tilt in polishing, improves polishing quality, so that the working face fitting that is harmonious of magnetic embryo is tighter, and then improve the stable work in work of magnetic embryo.

Description

A kind of high magnetic conduction embryo surface treatment process
Technical field
The present invention relates to magnetic embryos to produce treatment technology, more particularly to a kind of high magnetic conduction embryo surface treatment process.
Background technology
The soft magnetism magnetic embryo of magnetic material is susceptible to not smooth enough the situation of working face that is harmonious in general processing, But whether the working face splicing that is harmonious of magnetic embryo is tightly directly related to the transmission stability of signal, results even in common electricity The phenomenon that inductance value of sensor fluctuates widely finally results in the entire lowering of overall performance.Especially high permeability iron Oxysome combines, and magnetic embryo is harmonious working face after being cast by dispensing, baking, by the influences such as temperature and time, inductance value fall It between reaching 20%-40%, frequently results in device and can not work normally in equipment complete machine, even failure is shut down sometimes, to production Bring harmful effect.
Therefore, the face surface processing that is harmonious of magnetic embryo is most important, in view of this, it is quite necessary to provide a kind of high lead Magnetic embryo surface treatment process promotes the signal transduction intensity of magnetic embryo junction to improve the flatness of the working face that is harmonious of magnetic embryo.
Invention content
The object of the present invention is to provide a kind of high magnetic conduction embryo surface treatment process, have the working face that is harmonious for improving magnetic embryo Flatness promotes the effect of the signal transduction intensity of magnetic embryo junction.
The present invention above-mentioned technical purpose technical scheme is that:A kind of high magnetic conduction embryo surface processing Technique, including sequentially connected feed end, transportation section and processing sections, transportation section include conveyer belt, overturn component and close up component, Overturning component includes the screw thread guide post that at least twice make magnetic embryo from flip horizontal at vertical state, and it includes multiple tracks and spiral shell to close up component The pushing meanss that the sliding groove of line guide post connection, the end for being connected to sliding groove are used to that polylith magnetic embryo to be made to be bonded to each other, and multiple tracks Setting is gradually drawn close in the end of sliding groove.
By using above-mentioned technical proposal, magnetic embryo is directly entered after machine-shaping on conveyer belt, by overturning component It can adjust the angle, prepare for the working face polishing that is harmonious of next step, due to the tune also by closing up component in time after effect It is whole so that multi-disc magnetic embryo can mutually draw close abutting, increase the forced area of bottom, be not easy to tilt in polishing, improve polishing Quality so that the working face fitting that is harmonious of magnetic embryo is tighter, and then the stable work in work for improving magnetic embryo is connected with magnetic embryo The signal transduction intensity at place.
The further setting of the present invention is:The conveyer belt includes for the magnetic embryo of machine-shaping to be delivered to overturning component On conveyer belt and contraposition component for correcting magnetic embryo position on the conveyer belt.
By using above-mentioned technical proposal, magnetic embryo enters after machine-shaping on conveyer belt, and position at this time can not ensure It is corresponding respectively with the screw thread guide post on overturning component, therefore in order to which magnetic embryo can be smoothly entered in screw thread guide post, be provided with Contraposition component adjusts the position of magnetic embryo on the conveyor belt in time.
The further setting of the present invention is:The contraposition component includes the rotation for being symmetrically disposed on the conveyer belt both sides Disk, the rotating disc includes a rotation axis being vertically arranged and multiple pushing plates for being fixedly connected in the rotation axis, more A pushing plate is circumferentially uniformly distributed along the rotation axis, and between the bottom end of the pushing plate and the conveyer belt upper surface The thickness for being smaller than the magnetic embryo, being additionally provided between the pushing plate and the rotation axis makes pushing plate far from rotation axis And the telescopic component resetted.
By using above-mentioned technical proposal, it is equipped with rotating disc on the both sides of conveyer belt, the pushing plate on rotating disc is being stretched It can be moved back and forth under the action of contracting component, reach and the magnetic embryo on conveyer belt is pushed to specified position to centre position, be convenient for Magnetic embryo can smoothly enter into be overturn in screw thread guide post.
The further setting of the present invention is:Rotating drive part is connected in the rotation axis, described telescopic component one end is solid Surely it is connected in the pushing plate, the other end is fixedly connected on rotating disc, and the flexible stroke of multiple telescopic components is each It differs.
By using above-mentioned technical proposal, multiple circumferentially disposed pushing plates are set, and what is be arranged in each pushing plate stretches The formation of contracting component is different, therefore the telescopic component of suitable flexible stroke can be selected according to the quantity of magnetic embryo, reaches Magnetic embryo is pushed to the effect of suitable position.
The further setting of the present invention is:The screw thread guide post upper edge magnetic embryo direction of motion offers thread groove upwards, institute It is horizontally disposed to state thread groove and the one end open of conveying band connection, and the thread groove is with the one end open that component is connect is closed up It is vertically arranged.
By using above-mentioned technical proposal, thread groove is to open up upwards, when avoiding magnetic embryo and deflecting direction in thread groove The case where falling, and one end of thread groove is vertically arranged for the horizontal other end so that magnetic embryo can be from level after thread groove The state of placement is changed into vertical state, polishes convenient for the working face that is harmonious to magnetic embryo end of next step.
The further setting of the present invention is:The depth of the thread groove is more than or equal to the half of the core length, and institute The width for stating thread groove is less than or equal to twice of thickness of the magnetic core.
By using above-mentioned technical proposal, magnetic embryo is in thread groove since the abutting for subsequently entering the magnetic embryo in thread groove is made With the mobile status advanced, and above-mentioned setting can be kept to can guarantee that the abutting that can be received by follow-up magnetic embryo per a piece of magnetic embryo pushes away Action is used.
The further setting of the present invention is:The number of the sliding groove is equal to the number of the screw thread guide post, described to close up The width of sliding slot is more than the thickness of the magnetic embryo and less than twice of the magnetic flake thickness degree.
By using above-mentioned technical proposal, movement of the magnetic embryo in sliding groove is also the magnetic embryo by subsequently entering sliding groove Impetus, therefore above-mentioned setting can ensure that every a piece of magnetic embryo can be by subsequent impetus.
The further setting of the present invention is:The component that closes up further includes for connecting the sliding groove and the processing sections Connecting plate, the pushing meanss are set at least side of the connecting plate, and the stroke of the pushing meanss is adjustable sets It sets.
By using above-mentioned technical proposal, although the end of multi-trace smoothing slot is gradually mutually to draw close setting, magnetic embryo After being detached from sliding groove, between multi-disc magnetic embryo or there can be gap, it can not shape between multi-disc magnetic embryo in follow-up polished At the effective effect of supporting each other, therefore pushing meanss are arranged in at least side of connecting plate, can be effectively by multi-disc magnetic embryo It is pushed to mutually to draw close and be close to, and the stroke of pushing meanss is adjustable setting, to also can adapt to the magnetic embryo of different the piece numbers.
The further setting of the present invention is:The processing sections include the grinding device for magnetic embryo end of polishing, institute It states and is also equipped with grinding aid device on grinding device, the grinding aid device is equipped with grinding aid part.
The further setting of the present invention is:It is 8 that the grinding aid part, which is by weight percent,:36:13:43 smart steel stone is ultra-fine Powder, resin-oatmeal, silicon carbide ultrafine powder, chromium oxide powder are uniformly mixed, and pour into mold and carry out baking 3-3.5h, keep baking temperature Degree is 80-125 DEG C, carries out after the completion cooling and finished product grinding aid part is fixedly connected on the grinding aid device.
On the one hand be conducive to being harmonious for magnetic embryo in polishing due to the presence of grinding aid part by using above-mentioned technical proposal Working face is polished into mirror status, is conducive to splice tight, the constituent of another aspect grinding aid part itself each other between magnetic embryo The working face that is harmonious that middle essence steel stone superfine powder, resin-oatmeal, silicon carbide ultrafine powder and chromium oxide powder not only facilitate magnetic embryo forms mirror Surface state, can also promote the intensity for the working face junction that is harmonious, at the same be also possible that two magnetic embryos be harmonious working face that This is more adapted to when abutting, connection it is more tight, reduce the air gap of junction, reduce the vacuum degree of junction, promoted The signal transduction strength and stability of junction.
In conclusion the invention has the advantages that:It is provided with continuous and cooperation conveyer belt, overturning component and conjunction Hold together component so that magnetic embryo also forms multi-disc combination shape arranged side by side while completing overturning, is conducive to when polishing in the later stage more Stablize, reduce the generation of tilt condition, is conducive to the more smooth of working face polishing that be harmonious;By the way that grinding aid part is arranged so that magnetic The working face that is harmonious of embryo can preferably form mirror status, be conducive to the more fitting spliced in connection and close, promotion The working performance and stability of component.
Description of the drawings
Fig. 1 is the overall structure diagram of embodiment 1;
Fig. 2 is the structural schematic diagram for aligning component;
Fig. 3 is the structural schematic diagram for overturning component and closing up component;
Fig. 4 is the structural schematic diagram of grinding device and grinding aid device.
In figure:1, horizontal conveyor belt;2, component is overturn;3, close up component;4, screw thread guide post;5, thread groove;6, sliding groove; 7, pushing meanss;8, conveyer belt;9, component is aligned;10, rotating disc;11, rotation axis;12, pushing plate;13, telescopic component;14、 Rotating drive part;15, connecting plate;16, feed end;17, transportation section;18, processing sections;19, grinding device;20, grinding aid device; 21, grinding aid part.
Specific implementation mode
Below in conjunction with attached drawing, invention is further described in detail.
Specific embodiment is only explanation of the invention, is not limitation of the present invention, those skilled in the art The modification that not creative contribution can be made to the present embodiment as needed after reading this specification, but as long as in this hair It is all protected by Patent Law in bright right.
Embodiment 1:A kind of high magnetic conduction embryo surface treatment process, as shown in Figure 1, including sequentially connected feed end 16, defeated Send section 17 and processing sections 18.The machine-shaping in feed end 16 of magnetic embryo enters processing sections using the conveying effect of transportation section 17 In 18, polish etc. further finishing, to which finished product discharges.
As shown in Figure 1, transportation section 17 includes horizontal conveyor belt 1, overturning component 2 and closes up component 3, horizontal conveyor belt 1 one End is directly connected to processing sections 18, and the other end is connected to overturning component 2, and horizontal transport section includes conveyer belt 8 and contraposition component 9。
As illustrated in fig. 1 and 2, contraposition component 9 is installed on the both sides of conveyer belt 8, and contraposition component 9 includes being symmetrically disposed on transmission Rotating disc 10 with both sides, rotating disc 10 include a rotation axis 11 being vertically arranged and are fixedly connected on more in rotation axis 11 A pushing plate 12, multiple pushing plates 12 are circumferential uniformly distributed along rotation axis 11, and the bottom end of pushing plate 12 and 8 upper surface of conveyer belt Between the thickness for being smaller than magnetic embryo, being additionally provided between pushing plate 12 and rotation axis 11 makes pushing plate 12 far from rotation axis 11 And the telescopic component 13 resetted.Rotating drive part 14 is connected in rotation axis 11,13 one end of telescopic component is fixedly connected on promotion On plate 12, the other end is fixedly connected on rotating disc 10, and the flexible stroke of multiple telescopic components 13 is different.According to reality Situation can select the cylinder of different trips as telescopic component 13.
As shown in figs. 1 and 3, overturning component 2 includes two screw thread guide posts 4, the movement side of 4 upper edge conveyer belt 8 of screw thread guide post To offering thread groove 5 upwards, the one end open that thread groove 5 is connect with conveyer belt 8 be it is horizontally disposed, thread groove 5 with close up group The one end open that part 3 connects is vertically arranged, and the opening that twice thread groove 5 is connected to conveyer belt 8 is setting close to each other, together When twice thread groove 5 with the opening that component 3 is connected to is closed up be to be located remotely from each other, therefore just need to close up component 3 by two pieces of magnetic embryo phases Mutually draw close.Meanwhile in order to avoid magnetic embryo falls thread groove 5, the depth of thread groove 5 is more than the half of core length, and thread groove 5 Width be less than twice of thickness of magnetic core.
As shown in figs. 1 and 3, close up the sliding groove 6 that component 3 is correspondingly arranged with twice thread groove 5 respectively including twice, and two The end of road sliding groove 6 is gradually mutually to draw close setting so that sliding groove 6 is oblique.After two pieces of magnetic embryos are by thread groove 5 It is transformed into vertical shape from horizontal, passes through sliding groove 6 again at this time so that two pieces of magnetic embryos moves closer to.Meanwhile in order to enable sliding The motive force that magnetic embryo in slot 6 can be acted on subsequently, the number of sliding groove 6 are equal to the number of screw thread guide post 4, close up cunning The width of slot is more than the thickness of magnetic embryo and less than twice of magnetic flake thickness degree.
As shown in figs. 1 and 3, close up the connecting plate that component 3 further includes one end connection 6 other end of sliding groove connection processing sections 18 15, the side of connecting plate 15 is equipped with pushing meanss 7, and pushing meanss 7 are the adjustable cylinder of stroke, when twice sliding groove 6 After interior magnetic embryo passes through sliding groove 6, due to still can not also can be completely bonded, therefore at this time there are gap between two pieces of magnetic embryos Need pushing meanss 7 that two pieces of magnetic embryos are pushed to the state being bonded each other, be conducive to post-production polishing when magnetic embryo can be each other The contact area for increasing stress is abutted, inclined possibility is reduced.
The magnetic embryo of two pieces of colleagues is now arranged in the working face that mutually relies on and be harmonious after transport, overturning and pushing State upward entered processing sections 18 after sliding connecting plate 15 at this time, and carried out the finishing such as polish.
As shown in figs. 1 and 4, processing sections 18 include grinding device 19, and grinding device 19 uses common grinding wheel.Polishing It is also equipped with grinding aid device 20 on device 19, grinding aid part 21 is installed in grinding aid device 20.
After magnetic embryo machine-shaping, being transported on conveyer belt 8 in pairs, by aligning component 9 by the position of magnetic embryo The opening corresponding position being readjusted to thread groove 5 is set, vertical shape is changed into from horizontality by magnetic embryo after overturning component 2 State, and the work of the two pieces of magnetic embryos face that is harmonious is state upward.Abutting due to subsequently entering the magnetic embryo in thread groove 5 is made With promotion magnetic embryo moves forward until processing sections 18, make the work phase of upper end end under the action of grinding device 19 Conjunction face tends to mirror effect.And due to being additionally provided with the reason of grinding aid part 21, polishing it is finer and smoother, surface being capable of duration Also further extend.
Embodiment 2:A kind of grinding aid part, constituent, which is weight percentage, is followed successively by 8:36:13:43 smart steel stone is ultra-fine Powder, resin-oatmeal, silicon carbide ultrafine powder, chromium oxide powder.
When manufacturing grinding aid part 21, said components are uniformly mixed according to weight ratio, pours into mold and carries out baking 3- 3.5h, it is 80-125 DEG C to keep baking temperature, carries out after the completion cooling and finished product grinding aid part 21 is fixedly connected on grinding aid device On 20, the setting of grinding aid part 21, the work for being conducive to magnetic embryo is harmonious on face and forms mirror effect, mutual convenient for promoting magnetic embryo The laminating degree of junction and the conductive strength of electric signal.

Claims (10)

1. a kind of high magnetic conduction embryo surface treatment process, including sequentially connected feed end (16), transportation section (17) and processing sections (18), it is characterised in that:The transportation section (17) includes horizontal conveyor belt (1), overturning component (2) and closes up component (3), described Overturning component (2) includes the screw thread guide post (4) that at least twice make magnetic embryo from flip horizontal at vertical state, described to close up component (3) include multiple tracks be connected to the screw thread guide post (4) sliding groove (6), to be connected to the end of the sliding groove (6) more for making The pushing meanss (7) that block magnetic embryo is bonded to each other, and setting is gradually drawn close in the end of sliding groove described in multiple tracks (6).
2. a kind of high magnetic conduction embryo surface treatment process according to claim 1, it is characterised in that:Conveyer belt (8) packet Include conveyer belt (8) for being delivered to the magnetic embryo of machine-shaping in overturning component (2) and for correcting magnetic embryo in the conveying The contraposition component (9) of position on band (8).
3. a kind of high magnetic conduction embryo surface treatment process according to claim 2, it is characterised in that:The contraposition component (9) Rotating disc (10) including being symmetrically disposed on the conveyer belt (8) both sides, the rotating disc (10) include one and are vertically arranged Rotation axis (11) and the multiple pushing plates (12) being fixedly connected in the rotation axis (11), multiple pushing plates (12) are along institute It is circumferential uniformly distributed to state rotation axis (11), and between the bottom end of the pushing plate (12) and the conveyer belt (8) upper surface between Away from the thickness less than the magnetic embryo, being additionally provided between the pushing plate (12) and the rotation axis (11) keeps pushing plate (12) remote From rotation axis (11) and the telescopic component (13) of reset.
4. a kind of high magnetic conduction embryo surface treatment process according to claim 3, it is characterised in that:On the rotation axis (11) It is connected with rotating drive part (14), described telescopic component (13) one end is fixedly connected in the pushing plate (12), and the other end is solid Surely it is connected on rotating disc (10), and the flexible stroke of multiple telescopic components (13) is different.
5. a kind of high magnetic conduction embryo surface treatment process according to claim 1, it is characterised in that:The screw thread guide post (4) The upper edge magnetic embryo direction of motion offers thread groove (5) upwards, and the one end open that the thread groove (5) connect with conveyer belt (8) is Horizontally disposed, the thread groove (5) is vertically arranged with the one end open that component (3) is connect is closed up.
6. a kind of high magnetic conduction embryo surface treatment process according to claim 5, it is characterised in that:The thread groove (5) Depth is more than or equal to the half of the core length, and the width of the thread groove (5) is less than or equal to the thickness of the magnetic core Twice.
7. a kind of high magnetic conduction embryo surface treatment process according to claim 1, it is characterised in that:The sliding groove (6) Number is equal to the number of the screw thread guide post (4), and the width of the sliding groove (6) is more than the thickness of the magnetic embryo and less than described Twice of magnetic flake thickness degree.
8. a kind of high magnetic conduction embryo surface treatment process according to claim 7, it is characterised in that:It is described to close up component (3) Further include the connecting plate (15) for connecting the sliding groove (6) and the processing sections (18), the pushing meanss (7) are set to At least side of the connecting plate (15), and the stroke of the pushing meanss (7) is adjustable setting.
9. a kind of high magnetic conduction embryo surface treatment process according to claim 1, it is characterised in that:Processing sections (18) packet Include the grinding device for magnetic embryo end of polishing(19), the grinding device(19)On be also equipped with grinding aid device(20), The grinding aid device(20)It is equipped with grinding aid part(21).
10. a kind of high magnetic conduction embryo surface treatment process according to claim 9, it is characterised in that:The grinding aid part(21) To be 8 by weight percent:36:13:43 smart steel stone superfine powder, resin-oatmeal, silicon carbide ultrafine powder, chromium oxide powder mixing are equal It is even, baking 3-3.5h is poured into mold and carries out, it is 80-125 DEG C to keep baking temperature, carries out after the completion cooling and helps finished product Grind part(21)It is fixedly connected on the grinding aid device(19)On.
CN201810445272.0A 2018-05-10 2018-05-10 A kind of high magnetic conduction embryo surface treatment process Active CN108637842B (en)