CN108411185A - oxidation-resistant alloy - Google Patents
oxidation-resistant alloy Download PDFInfo
- Publication number
- CN108411185A CN108411185A CN201810350832.4A CN201810350832A CN108411185A CN 108411185 A CN108411185 A CN 108411185A CN 201810350832 A CN201810350832 A CN 201810350832A CN 108411185 A CN108411185 A CN 108411185A
- Authority
- CN
- China
- Prior art keywords
- oxidation
- resistant alloy
- present
- cerium
- manganese
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
The present invention provides a kind of oxidation-resistant alloy, and ingredient is grouped as by the group of following weight percentage:Silicon 17~26%, iron 16~33%, copper 12~30%, titanium 10~22%, zinc 11 30%, chromium 11 18%, cerium 12~40%, manganese 14~36%.Surface cold shut of the present invention, crackle are reduced, and good percentage elongation improves elongation and impact flexibility.
Description
Technical field
The present invention relates to a kind of oxidation-resistant alloys.
Background technology
Oxidation-resistant alloy is most widely used one kind non-ferrous metal structural material in industry, Aeronautics and Astronautics, automobile,
It has been widely applied in machine-building, ship and chemical industry.Oxidation-resistant alloy density is low, but intensity is relatively high, near or above
High-quality steel, plasticity is good, can be processed into various proximate matters, has excellent electric conductivity, thermal conductivity and corrosion stability, industrially makes extensively
With usage amount is only second to steel.Some oxidation-resistant alloys may be used heat treatment and obtain good mechanical performance, physical property and anti-
Corrosive nature.Existing oxidation-resistant alloy crackle is more, and elongation percentage is poor.
Invention content
The problem to be solved in the present invention is to provide a kind of oxidation-resistant alloy, to overcome oxidation-resistant alloy crackle in the prior art
It is more, the defect of elongation percentage difference.
According to an aspect of the present invention, a kind of oxidation-resistant alloy is provided, which is characterized in that ingredient is by following weight percentage
The group of ratio is grouped as:Silicon 17~26%, iron 16~33%, copper 12~30%, titanium 10~22%, zinc 11-30%, chromium 11-18%,
Cerium 12~40%, manganese 14~36%.
The oxidation-resistant alloy of the present invention, surface cold shut, crackle are reduced, and good percentage elongation improves elongation and impact flexibility.
Specific implementation mode
Explanation is described in further detail to technical scheme of the present invention with reference to specific embodiment.
Embodiment 1:
The oxidation-resistant alloy of the offer of the present invention, which is characterized in that ingredient is grouped as by the group of following weight percentage:Silicon
17~26%, iron 16~33%, copper 12~30%, titanium 10~22%, zinc 11-30%, chromium 11-18%, cerium 12~40%, manganese 14
~36%.
Embodiment 2:
The oxidation-resistant alloy of the offer of the present invention, which is characterized in that ingredient is grouped as by the group of following weight percentage:Silicon
12%, iron 12%, copper 13%, titanium 24%, zinc 5%, chromium 4%, cerium 12%, manganese 5%.
Claims (2)
1. oxidation-resistant alloy, which is characterized in that ingredient is grouped as by the group of following weight percentage:Silicon 17~26%, iron 16~
33%, copper 12~30%, titanium 10~22%, zinc 11-30%, chromium 11-18%, cerium 12~40%, manganese 14~36%.
2. a kind of oxidation-resistant alloy according to claim 1, which is characterized in that ingredient by following weight percentage component
Composition:Silicon 3~7%, iron 4~8%, copper 5~17%, titanium 15~35%, zinc 20-30%, chromium 21-28%, cerium 22~30%, manganese
24~26%.