CN108060597A - A kind of production method of the household paper pulp of environmental protection and energy saving - Google Patents

A kind of production method of the household paper pulp of environmental protection and energy saving Download PDF

Info

Publication number
CN108060597A
CN108060597A CN201711214659.7A CN201711214659A CN108060597A CN 108060597 A CN108060597 A CN 108060597A CN 201711214659 A CN201711214659 A CN 201711214659A CN 108060597 A CN108060597 A CN 108060597A
Authority
CN
China
Prior art keywords
slurry
boiling
chlorination
environmental protection
energy saving
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201711214659.7A
Other languages
Chinese (zh)
Inventor
许亦南
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI BILUN LIVING PAPER Co Ltd
Original Assignee
ANHUI BILUN LIVING PAPER Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI BILUN LIVING PAPER Co Ltd filed Critical ANHUI BILUN LIVING PAPER Co Ltd
Priority to CN201711214659.7A priority Critical patent/CN108060597A/en
Publication of CN108060597A publication Critical patent/CN108060597A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of production methods of the household paper pulp of environmental protection and energy saving, are related to paper for daily use technical field, comprise the following steps:(1)Stock;(2)Boiling;(3)Grinding;(4)Chlorination;(5)Vacuum impregnation is handled;(6)Acid treatment;After the present invention to slurry by carrying out boiling, bamboo fibre in slurry is in soft state, then defibrination is carried out, a certain amount of zinc flake is added in defibrination, defibrination efficiency can effectively be improved, the ash in bamboo fibre can significantly be reduced, pentose content, improve the purity of slurry, simultaneously, pass through the physical arrangement of zinc flake uniqueness, when carrying out defibrination in the slurry, can fully be contacted with each other friction with the bamboo fiber in slurry, during defibrination, bamboo fiber hardness and heavy wall can be effectively reduced, broken bamboo fiber tissue, discharge bamboo fiber cell content material, so as to effectively improve the quality of slurry, improve into the performance of paper.

Description

A kind of production method of the household paper pulp of environmental protection and energy saving
Technical field
The invention belongs to paper for daily use technical fields, and in particular to a kind of producer of the household paper pulp of environmental protection and energy saving Method.
Background technology
With the development of China's paper for daily use industry, domestic enterprise mostly using Cotton Pulp as the raw materials for production of paper for daily use, But restricted by cultivated area and growth cycle, the raw material is increasingly short, has seriously affected China's paper for daily use industry Development.There is only a few enterprise to attempt the raw materials for production using bamboo pulp as paper for daily use therefore, and have been achieved with initial success, Such as Patent No. CN02112175.3, the patent of invention of entitled " bamboo pulp denatured productive technology " discloses a kind of bamboo pulp Production technology, but bamboo fibre average length is less than papermaking wood-fibred, and because its ash is more, pentose content is high, and bamboo fiber Matter is hard, heavy wall, lumen is narrow, fibr tissue is fine and close, there are cause production difficulty the problems such as air, it is necessary to raw material in cell It is more, it is of high cost, thus also fail to be widely applied.To reduce production cost, steady production operation, research and development meet paper for daily use life The dissolving pulp substitute products of production requirement have become a top priority.
The content of the invention
The purpose of the present invention is being directed to the problem of existing, a kind of producer of the household paper pulp of environmental protection and energy saving is provided Method.
The present invention is achieved by the following technical solutions:
A kind of production method of the household paper pulp of environmental protection and energy saving, comprises the following steps:
(1)Stock:Bamboo pulp is scattered through alkali spray and discongesting for blender, it is then re-fed into squeezer and carries out extrusion dehydration, Obtain slurry;
(2)Boiling:By step(1)Obtained slurry carries out boiling using kraft cooking technique;Wherein, amount of caustic soda accounts for absolutely The 10-12% of dry pulp, sulphidity 20%, bath raio 1:5, boiling temperature be 100 DEG C of early period, 110 DEG C of later stage, early period digestion time For 50-60min, later stage digestion time is 45-50min, and the Kappa number of slurry is 35-65 after boiling;
(3)Grinding:To step(2)The zinc flake of its quality 5-8% is added in slurry after middle boiling, then at 60-80 DEG C Be ground 3-5 it is small when;
(4)Chlorination:By step(3)Slurry after middle milled processed carries out chlorination, adds in hydrochloric acid, liquid chlorine, caustic soda, before ensureing chlorination Containing chloride for 12-18g/m containing alkali after 0.08-0.12g/L, chlorination after sour 0.04-0.06g/L, chlorination3
(5)Vacuum impregnation is handled:By chlorination, treated that slurry is added in vacuum reaction kettle carries out processing 15-20min;
(6)Acid treatment:Citric acid is added in vacuum impregnation treated slurry and carries out acid treatment 15-20min, through spray into drift Pond is 0.3g/L containing acid, manufactures paper with pulp through paper machine, is packaged as fixed weight 550g/m2Bamboo pulp.
Further, the step(1)The slurry concentration of middle slurry is 10%.
Further, the step(2)Mid-early stage boiling and later stage boiling intermediate period are 3-5min, boiling early period With being placed naturally in the later stage boiling midfeather time.
Further, the step(3)Middle zinc flake granularity is 800 mesh.
Further, the step(3)Middle zinc flake preparation method is:Its quality is added in 350 mesh spherical zinc powders The silica flour of 3.5% pentaerythrite and its quality 0.02%, uniformly after mixing, when progress ball milling 2 is small, ball material mass ratio is 100:1, Then sieved, obtain 800 mesh zinc flakes to get.
Further, the step(6)Acid treatment:Add in citric acid, citric acid drop rate be 0.35mL/min, acid at Manage time 18min.
The present invention has the following advantages compared with prior art:After the present invention to slurry by carrying out boiling, the bamboo in slurry Fiber is in soft state, then carries out defibrination, and a certain amount of zinc flake is added in defibrination, can effectively improve defibrination Efficiency can significantly reduce ash in bamboo fibre, pentose content, improve the purity of slurry, meanwhile, it is only by zinc flake Special physical arrangement, when carrying out defibrination in the slurry, can fully contact with each other friction with the bamboo fiber in slurry, in defibrination During, bamboo fiber hardness and heavy wall can be effectively reduced, crushes bamboo fiber tissue, release bamboo fiber is intracellular Tolerant matter so as to effectively improve the quality of slurry, improves into the performance of paper, and paper is tear-resistant after being especially formed into paper Performance is greatly enhanced, slurry primary quality measure produced by the present invention:Dynamic viscosity 10-14mpa.s;First kind fiber Element >=95%;Ash≤0.02%;Irony≤10ppm;Whiteness >=90%;Moisture≤10%;Reactivity worth≤200s;The degree of polymerization 400-600, slurry produced by the present invention meet the production requirement of paper for daily use.The production method of the present invention is simple for process, operation Convenient, the slurry of production meets the production requirement of paper for daily use, energy conservation and environmental protection, and the paper for daily use strength character of preparation is more preferable.
Specific embodiment
Embodiment 1
A kind of production method of the household paper pulp of environmental protection and energy saving, comprises the following steps:
(1)Stock:Bamboo pulp is scattered through alkali spray and discongesting for blender, it is then re-fed into squeezer and carries out extrusion dehydration, Obtain slurry;
(2)Boiling:By step(1)Obtained slurry carries out boiling using kraft cooking technique;Wherein, amount of caustic soda accounts for absolutely The 10% of dry pulp, sulphidity 20%, bath raio 1:5, boiling temperature is 100 DEG C of early period, and in 110 DEG C of later stage, early period, digestion time was 50min, later stage digestion time are 45min, and the Kappa number of slurry is 35 after boiling;
(3)Grinding:To step(2)The zinc flake of its quality 5% is added in slurry after middle boiling, is then carried out at 60 DEG C Grind 3 it is small when;
(4)Chlorination:By step(3)Slurry after middle milled processed carries out chlorination, adds in hydrochloric acid, liquid chlorine, caustic soda, before ensureing chlorination Containing chloride for 12g/m containing alkali after 0.08g/L, chlorination after sour 0.04g/L, chlorination3
(5)Vacuum impregnation is handled:By chlorination, treated that slurry is added in vacuum reaction kettle carries out processing 15min;
(6)Acid treatment:Citric acid, which is added in, to vacuum impregnation treated slurry carries out acid treatment 15min, through spray into drift pond, It is 0.3g/L containing acid, manufactures paper with pulp through paper machine, is packaged as fixed weight 550g/m2Bamboo pulp.
Further, the step(1)The slurry concentration of middle slurry is 10%.
Further, the step(2)Mid-early stage boiling and later stage boiling intermediate period are 3min, boiling early period with Later stage boiling is placed naturally in the midfeather time.
Further, the step(3)Middle zinc flake granularity is 800 mesh.
Further, the step(3)Middle zinc flake preparation method is:Its quality is added in 350 mesh spherical zinc powders The silica flour of 3.5% pentaerythrite and its quality 0.02%, uniformly after mixing, when progress ball milling 2 is small, ball material mass ratio is 100:1, Then sieved, obtain 800 mesh zinc flakes to get.
Further, the step(6)Acid treatment:Add in citric acid, citric acid drop rate be 0.35mL/min, acid at Manage time 18min.
Embodiment 2
A kind of production method of the household paper pulp of environmental protection and energy saving, comprises the following steps:
(1)Stock:Bamboo pulp is scattered through alkali spray and discongesting for blender, it is then re-fed into squeezer and carries out extrusion dehydration, Obtain slurry;
(2)Boiling:By step(1)Obtained slurry carries out boiling using kraft cooking technique;Wherein, amount of caustic soda accounts for absolutely The 12% of dry pulp, sulphidity 20%, bath raio 1:5, boiling temperature is 100 DEG C of early period, and in 110 DEG C of later stage, early period, digestion time was 60min, later stage digestion time are 50min, and the Kappa number of slurry is 65 after boiling;
(3)Grinding:To step(2)The zinc flake of its quality 8% is added in slurry after middle boiling, is then carried out at 80 DEG C Grind 5 it is small when;
(4)Chlorination:By step(3)Slurry after middle milled processed carries out chlorination, adds in hydrochloric acid, liquid chlorine, caustic soda, before ensureing chlorination Containing chloride for 18g/m containing alkali after 0.12g/L, chlorination after sour 0.06g/L, chlorination3
(5)Vacuum impregnation is handled:By chlorination, treated that slurry is added in vacuum reaction kettle carries out processing 20min;
(6)Acid treatment:Citric acid, which is added in, to vacuum impregnation treated slurry carries out acid treatment 20min, through spray into drift pond, It is 0.3g/L containing acid, manufactures paper with pulp through paper machine, is packaged as fixed weight 550g/m2Bamboo pulp.
Further, the step(1)The slurry concentration of middle slurry is 10%.
Further, the step(2)Mid-early stage boiling and later stage boiling intermediate period are 5min, boiling early period with Later stage boiling is placed naturally in the midfeather time.
Further, the step(3)Middle zinc flake granularity is 800 mesh.
Further, the step(3)Middle zinc flake preparation method is:Its quality is added in 350 mesh spherical zinc powders The silica flour of 3.5% pentaerythrite and its quality 0.02%, uniformly after mixing, when progress ball milling 2 is small, ball material mass ratio is 100:1, Then sieved, obtain 800 mesh zinc flakes to get.
Further, the step(6)Acid treatment:Add in citric acid, citric acid drop rate be 0.35mL/min, acid at Manage time 18min.
Embodiment 3
A kind of production method of the household paper pulp of environmental protection and energy saving, comprises the following steps:
(1)Stock:Bamboo pulp is scattered through alkali spray and discongesting for blender, it is then re-fed into squeezer and carries out extrusion dehydration, Obtain slurry;
(2)Boiling:By step(1)Obtained slurry carries out boiling using kraft cooking technique;Wherein, amount of caustic soda accounts for absolutely The 11% of dry pulp, sulphidity 20%, bath raio 1:5, boiling temperature is 100 DEG C of early period, and in 110 DEG C of later stage, early period, digestion time was 55min, later stage digestion time are 46min, and the Kappa number of slurry is 50 after boiling;
(3)Grinding:To step(2)The zinc flake of its quality 6% is added in slurry after middle boiling, is then carried out at 70 DEG C Grind 4 it is small when;
(4)Chlorination:By step(3)Slurry after middle milled processed carries out chlorination, adds in hydrochloric acid, liquid chlorine, caustic soda, before ensureing chlorination Containing chloride for 15g/m containing alkali after 0.10g/L, chlorination after sour 0.05g/L, chlorination3
(5)Vacuum impregnation is handled:By chlorination, treated that slurry is added in vacuum reaction kettle carries out processing 18min;
(6)Acid treatment:Citric acid, which is added in, to vacuum impregnation treated slurry carries out acid treatment 18min, through spray into drift pond, It is 0.3g/L containing acid, manufactures paper with pulp through paper machine, is packaged as fixed weight 550g/m2Bamboo pulp.
Further, the step(1)The slurry concentration of middle slurry is 10%.
Further, the step(2)Mid-early stage boiling and later stage boiling intermediate period are 3-5min, boiling early period With being placed naturally in the later stage boiling midfeather time.
Further, the step(3)Middle zinc flake granularity is 800 mesh.
Further, the step(3)Middle zinc flake preparation method is:Its quality is added in 350 mesh spherical zinc powders The silica flour of 3.5% pentaerythrite and its quality 0.02%, uniformly after mixing, when progress ball milling 2 is small, ball material mass ratio is 100:1, Then sieved, obtain 800 mesh zinc flakes to get.
Further, the step(6)Acid treatment:Add in citric acid, citric acid drop rate be 0.35mL/min, acid at Manage time 18min.
Comparative example 1:It is differed only in embodiment 1 without step(3)Processing.
Comparative example 2:It is differed only in embodiment 1 without step(5)Processing.
Experiment:
Slurry primary quality measure produced by the present invention:Dynamic viscosity 10-14mpa.s;Alpha cellulose >=95%;Ash≤ 0.02%;Irony≤10ppm;Whiteness >=90%;Moisture≤10%;Reactivity worth≤200s;Degree of polymerization 400-600.
Slurry is obtained by embodiment and comparative example method, by quantitative 60g/m2 handsheets, every group is manufactured paper with pulp 5;It is dry, equilibrium water Point, survey physical property(Tear index):
Table 1
As can be seen from Table 1, paper made of the slurry that prepared by the present invention has good tear-resistant index.

Claims (6)

1. a kind of production method of the household paper pulp of environmental protection and energy saving, which is characterized in that comprise the following steps:
(1)Stock:Bamboo pulp is scattered through alkali spray and discongesting for blender, it is then re-fed into squeezer and carries out extrusion dehydration, Obtain slurry;
(2)Boiling:By step(1)Obtained slurry carries out boiling using kraft cooking technique;Wherein, amount of caustic soda accounts for absolutely The 10-12% of dry pulp, sulphidity 20%, bath raio 1:5, boiling temperature be 100 DEG C of early period, 110 DEG C of later stage, early period digestion time For 50-60min, later stage digestion time is 45-50min, and the Kappa number of slurry is 35-65 after boiling;
(3)Grinding:To step(2)The zinc flake of its quality 5-8% is added in slurry after middle boiling, then at 60-80 DEG C Be ground 3-5 it is small when;
(4)Chlorination:By step(3)Slurry after middle milled processed carries out chlorination, adds in hydrochloric acid, liquid chlorine, caustic soda, before ensureing chlorination Containing chloride for 12-18g/m containing alkali after 0.08-0.12g/L, chlorination after sour 0.04-0.06g/L, chlorination3
(5)Vacuum impregnation is handled:By chlorination, treated that slurry is added in vacuum reaction kettle carries out processing 15-20min;
(6)Acid treatment:Citric acid is added in vacuum impregnation treated slurry and carries out acid treatment 15-20min, through spray into drift Pond is 0.3g/L containing acid, manufactures paper with pulp through paper machine, is packaged as fixed weight 550g/m2Bamboo pulp.
2. the production method of the household paper pulp of a kind of environmental protection and energy saving according to claim 1, which is characterized in that described Step(1)The slurry concentration of middle slurry is 10%.
3. the production method of the household paper pulp of a kind of environmental protection and energy saving according to claim 1, which is characterized in that described Step(2)Mid-early stage boiling is 3-5min with later stage boiling intermediate period, when boiling early period is with later stage boiling midfeather It is interior to place naturally.
4. the production method of the household paper pulp of a kind of environmental protection and energy saving according to claim 1, which is characterized in that described Step(3)Middle zinc flake granularity is 800 mesh.
5. the production method of the household paper pulp of a kind of environmental protection and energy saving according to claim 1, which is characterized in that described Step(3)Middle zinc flake preparation method is:The pentaerythrite and its quality of its quality 3.5% are added in 350 mesh spherical zinc powders 0.02% silica flour, uniformly after mixing, when progress ball milling 2 is small, ball material mass ratio is 100:1, it is then sieved, obtains 800 mesh Zinc flake to get.
6. the production method of the household paper pulp of a kind of environmental protection and energy saving according to claim 1, which is characterized in that described Step(6)Acid treatment:Citric acid is added in, citric acid drop rate is 0.35mL/min, acid treatment time 18min.
CN201711214659.7A 2017-11-28 2017-11-28 A kind of production method of the household paper pulp of environmental protection and energy saving Pending CN108060597A (en)